Chang Chun Longlite Pbt Gf 4830bkk

Chang Chun LONGLITE® PBT+GF 4830BKK

    • Product Name: Chang Chun LONGLITE® PBT+GF 4830BKK
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 891974
    Density 1.53 g/cm³
    Glass Fiber Content 30%
    Molding Shrinkage 0.2-0.8%
    Water Absorption 0.03%
    Tensile Strength 120 MPa
    Elongation At Break 2.0%
    Flexural Modulus 8000 MPa
    Notched Izod Impact Strength 8 kJ/m²
    Heat Deflection Temperature 200 °C at 1.82 MPa
    Melting Point 225 °C
    Flammability Rating HB
    Dielectric Strength 20 kV/mm

    As an accredited Chang Chun LONGLITE® PBT+GF 4830BKK factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg net moisture-resistant bags, palletized for safe handling and storage of Chang Chun LONGLITE® PBT+GF 4830BKK.
    Container Loading (20′ FCL) 20′ FCL dry container: 25 kg bags, palletized, approximately 18–20 metric tons net; secure load and observe carrier weight limits.
    Shipping Chang Chun LONGLITE® PBT+GF 4830BKK is shipped as black glass-fiber-reinforced PBT pellets in moisture-barrier 25 kg bags or jumbo bags on pallets. It is not regulated as dangerous goods for road, sea, or air transport. Store dry; avoid moisture, sunlight, and contamination; handle with standard industrial precautions.
    Storage Store Chang Chun LONGLITE® PBT+GF 4830BKK in a cool, dry, well-ventilated warehouse away from direct sunlight, heat sources, and moisture. Keep in original sealed packaging on pallets, protected from physical damage and contamination. Maintain stable ambient temperature and low humidity; use first-in, first-out rotation. Avoid open flames and incompatible chemicals. Inspect containers before use. Store only in designated chemical storage areas.
    Shelf Life Typically 24 months when stored dry, cool, and sealed in original packaging; keep away from moisture and sunlight.
    Application of Chang Chun LONGLITE® PBT+GF 4830BKK

    Chang Chun LONGLITE® PBT+GF 4830BKK is specified in automotive connector housings, terminal retainers, and engine-compartment sensor bodies where the 30 wt% short-glass reinforcement increases tensile modulus and reduces creep relative to unfilled PBT. The material is processed on hydraulic or servo-electric injection molding machines with clamp forces from 800 kN to 1,200 kN. Screw designs with an L/D ratio of 20:1 to 22:1 and a compression ratio near 2.5:1 are typical; a high-compression screw or an excessively short feed section can break fibers and lower notched impact energy. Drying is not a pre-treatment option but a production control: a desiccant dryer at 120 °C for 4 h is used to reach a residual moisture content below 0.02 wt%, and a dewpoint of -30 °C or lower is maintained at the hopper inlet. Melt volume-flow rate checked by ISO 1133-1 at 250 °C and 2.16 kg is typically within 10–20 cm³/10 min; lot-to-lot drift above ±15% from the reference value changes filling pressure in thin connector walls. If the material is not dried, the melt layer at the gate can exceed 270 °C, and microscopic voids around fibers become visible as silver streaks on dark surfaces. Barrel zone settings are normally set from 240 °C in the rear zone to 270 °C at the nozzle, with actual melt temperature checked by needle pyrometer and held between 250 °C and 265 °C. The mold cavity surface temperature is controlled between 60 °C and 90 °C; this range is selected because surface temperature controls the crystallinity gradient through the wall, and deviations larger than 5 °C across the cavity cause visible gloss variation and non-uniform shrinkage. Connector housings made from this grade are assessed by IEC 60512-15-1 for terminal insertion force and by USCAR-2 for multiple insertion cycles. Weld-line regions that form downstream of core pins and terminal separators require attention because short-glass orientation in the weld plane limits molecular entanglement and causes a measurable drop in tensile strength. The bulk flow-direction tensile strength of a 30 wt% short-glass PBT is commonly in the range 110–130 MPa when tested by ISO 527-2, but weld-line specimens can fall to 60–70 MPa depending on melt temperature and packing pressure. A higher melt temperature of 265 °C and a hold pressure of 60–80 MPa hydraulic-specific cavity pressure improve knit-line strength; however, the same high melt temperature shortens the safe residence time to 5 min at a shot cushion of 3–5 mm. If the cushion is smaller than 2 mm, shot-to-shot melt-temperature variation becomes visible as varying terminal retention force.

    What Limits Minimum Wall Thickness in Relay Bases and Sensor Bodies?

    Relay bases and sensor bodies molded from this grade are constrained less by bulk thermal performance than by the effective flow-length-to-wall-thickness ratio and the gate geometry. The practical lower wall thickness is between 0.8 mm and 1.2 mm; below 0.8 mm, the short glass fibers orient strongly in the flow direction, and the frozen-layer fraction increases to a level where holding pressure cannot transmit across the cavity. The result is not simply sink, but an increase in post-mold warpage after 48 h of ambient storage because the cross-flow shrinkage remains higher than the flow-direction shrinkage. In relay base tools with 8–24 cavities, the runner system is often a heated sprue bushing feeding a cold runner; a subgate diameter below 0.8 mm can generate shear heating that locally exceeds 280 °C and causes yellowing or black specks. Replacing the subgate with a tab or edge gate of 1.0–1.5 mm thickness reduces gate-zone degradation but complicates automatic degating. The production solution on a high-cavitation line is a valve-gated hot runner with sequential opening set by cavity pressure sensors, not by timers. This technique is used because the material solidifies quickly once the melt falls below 220 °C; sequential opening maintains the melt front above the freeze point without requiring barrel temperatures above 270 °C.

    Dimensional checks on relay bases are referenced to ISO 294-4 for shrinkage and ISO 291 for conditioning at 23 °C and 50% relative humidity. When the product drawing requires a pitch dimension between terminal pins to remain within ±0.15 mm, the cavity insert must be cut using an anisotropic shrinkage allowance, not a uniform scale factor. Flow-direction allowance may be set to 0.4%, while cross-flow allowance may be 1.0%; moldmakers who use a single isotropic 0.6% number typically report that the connector does not fit the mating iron-core assembly at the end of the production run. The solution is not material change but shrink compensation combined with a post-molding cooling fixture that restrains the part for 60 s after ejection. In engine-bay sensor bodies, the same distortion control is required because the sealing face must remain flat within 0.1 mm over a 70 mm length; cavity pressure transfer into the thin wall is maintained by holding pressure of 60–80 MPa for 3–5 s.

    Comparative flow-direction and cross-flow values for 30 wt% short-glass PBT after conditioning per ISO 291
    Measured parameterTest standardFlow directionTransverse direction
    Mold shrinkageISO 294-40.2–0.5%0.8–1.2%
    Tensile strength at breakISO 527-2110–130 MPa70–90 MPa
    Tensile modulusISO 527-29–10.5 GPa6.5–8 GPa
    Notched Charpy impactISO 179-1/1eA8–10 kJ/m²6–8 kJ/m²

    In multi-cavity terminal block tools with 16–32 cavities, thermal demand concentrates at the hot runner manifold, and nozzle temperature balance must be held within ±2 °C to prevent cavity-to-cavity fill variation. The screw recovery stroke is set to leave a cushion between 3 mm and 5 mm at the end of hold; smaller cushions are associated with short shots at the last cavities in the stack mold, while larger cushions increase residence time and create black speck formation in the melt. The black pigmentation of grade 4830BKK reduces the visual impact of minor surface defects, but it also masks thermal-degradation speckling until the carbonized particles are large enough to change electrical surface resistivity. A clean screw pull is specified at the beginning of each shift because material left in the barrel during a 30-min production stop can adhere to the screw root. The subsequent restart with fresh material that contains internal moisture produces steam eruption at the gate that cannot be removed by increasing mold temperature alone. Terminal blocks made from this grade are evaluated for tracking resistance by IEC 60112 and for glow-wire ignitability by IEC 60695-2-11 where the final assembly requires a 650 °C glow-wire pass. The black glass-filled PBT body must maintain creep resistance at terminal screw torques from 0.4 N·m to 0.8 N·m depending on terminal size; creep modulus measured after 1,000 h at 80 °C by ISO 899-2 shows a larger reduction in the cross-flow direction than in the flow direction. Because the material is not inherently flame-retardant, end users specify it for terminal blocks where UL 94 HB is acceptable; if the assembly requires UL 94 V-0, the project must use a flame-retarded PBT formulation or select a different polymer family.

    Verification matrix for connector, relay, and terminal block applications
    RequirementStandard / methodTypical acceptance criterion
    Heat deflection temperatureISO 75-2 at 1.8 MPaReported value only; grade-specific datasheet required
    Flammability classUL 94HB unless FR package specified
    Relative temperature index electricalUL 746BVerify against UL yellow card
    Terminal insertion forceUSCAR-2 or IEC 60512-15-1No crack or deformation after full terminal cycle
    Tracking resistanceIEC 60112CTI value from datasheet
    Restriction of hazardous substancesEU RoHS 2011/65/EU + (EU) 2015/863Supplier compliance certificate

    Cooling Fan Blade Imbalance Is Controlled by Gate Placement, Not Only Balance Testing

    Gate placement at the fan hub is the primary process control for radial fiber orientation, because the fan blade is a rotating component in which mass distribution and stiffness anisotropy create imbalance and aerodynamic flutter. A single center sprue gate creates radial flow from hub to blade tip, aligning fibers radially along each blade; this orientation is desirable for flexural strength along the blade length but produces high hoop-direction shrinkage in the hub ring. The resulting hub ovality can exceed 0.2 mm on a 140 mm outer-diameter fan, producing an imbalance that static balancing after assembly cannot fully correct if the material is not uniformly crystallized. The mold temperature control for fan tools is therefore zoned: hub cavity inserts are run at 90 °C to maximize crystallinity, while blade tip regions are run at 70 °C to reduce distortion. The temperature difference across the cavity is managed by independent water circuits, and the circuit delta is maintained below 5 °C to avoid differential shrinkage that appears as a visible knit line at the blade root. Fan blade fatigue testing is carried out under speed cycling from idle to 3,500 rpm at 85 °C; the PPAP submission includes a natural-frequency measurement because a glass-reinforced PBT fan that is too stiff at the trailing edge can excite resonance at the motor's slot-pass frequency. Specific grade data for blade resonance is usually developed from molded parts, not from raw material data, and published data for this exact grade in fan geometries is limited. The density of the material, measured by ISO 1183-1, is close to 1.53 g/cm³; this value is used for blade mass calculations. Flexural modulus from ISO 178 is typically above 8,000 MPa at 23 °C. The primary limitation for fan blades is fatigue strength at the root, where the material's surface morphology after long-term thermal aging can develop small cracks near the gate. These cracks are not spontaneous material failure but result from fiber-rich weld lines generated by the fixed core pins that form the hub bore.

    When Cold-Cranking Strength Governs Motor End Caps and Ignition Coil Brackets

    Low-temperature motor end cap performance is evaluated on parts conditioned for 4 h at -30 °C before a falling-dart impact test in accordance with ISO 6603-2. The glass transition temperature of the PBT matrix is near 45–60 °C by ISO 11357-2; this means the failure mode at low temperature is brittle crack propagation along the fiber-matrix interface. This behaviour is not a defect of the grade but a characteristic of short-glass reinforcement. To reduce sudden fracture at cold start, motor end cap designs avoid sharp inside corners below 0.5 mm radius; a minimum radius of 0.8 mm is specified in the PBT part drawing. Insert-molded brass threads and steel bushings introduce a thermal expansion mismatch: the linear coefficient of thermal expansion measured by ISO 11359-2 in the flow direction is generally lower than 4×10⁻⁵ K⁻¹, but the cross-flow value can exceed 8×10⁻⁵ K⁻¹. When the brass insert is placed in a cross-flow region, hoop stress after molding can cause microcracks that open during thermal cycling from -40 °C to 120 °C. The countermeasure is to orient the gate so that the flow front surrounds the insert uniformly and to maintain a melt temperature near 260 °C, because too low a melt temperature increases residual orientation and free volume near the metal surface. Ignition coil brackets made from 30 wt% glass-filled PBT are selected when the bracket must retain a coil on the engine head at continuous temperatures near 125 °C. At 120 °C, flexural modulus in 30 wt% short-glass PBT systems typically falls to 50–60% of the 23 °C value, so the bracket's short-term stiffness is adequate but creep under bolt torque must be checked. Clamp force relaxation after 1,000 h at 120 °C is higher for PBT than for polyphenylene sulfide when evaluated by torque-tension audit on a rigid test fixture. A steel compression limiter is recommended when the bolt clamp load exceeds 2,000 N; without the limiter, the material under the bolt head can deform and cause torque loss during thermal cycling. Published creep data for this exact formulation is limited, and qualification trials should include joint relaxation measured according to an OEM-specific procedure.

    Hydrolysis Resistance Boundaries in Pump and Water-Meter Components

    The hydrolysis boundary for this grade is set not by the glass reinforcement but by the ester linkage in the PBT chain. In cold-water meter chambers and pump end covers operating below 40 °C, dimensional stability and low water absorption make the grade suitable. Water absorption by ISO 62 at 23 °C for 24 h is commonly below 0.1%, and the mechanical property loss is small. At elevated water or water-glycol temperatures, hydrolysis accelerates; service above 70 °C in 50% ethylene glycol is not recommended without extensive testing because tensile strength retention can fall below 50% after 1,000 h. The failure mode is surface whitening and a drop in burst pressure at the pump cover seal. If the application requires a coolant-contact pump housing at 95 °C, a hydrolysis-resistant PBT with a chain extender package or a polyphenylene-based material should be evaluated instead. Published data for this specific grade under long-term glycol exposure is limited, and the processor must not rely on short-term tensile values for service predictions. Water-meter components benefit from the low creep of the glass-filled grade under constant water pressure; but the material choice must consider the chemical quality of the water supply. Free chlorine at concentrations above 1 ppm can oxidize the PBT surface after several years, causing gloss loss and pitting; a chlorine-resistant polypropylene or polyphenylene sulfide may be required in drinking-water systems with aggressive disinfection residuals.

    Free Quote

    Competitive Chang Chun LONGLITE® PBT+GF 4830BKK prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chang Chun LONGLITE® PBT+GF 4830BKK is a black, 30 wt% short-glass-fibre-reinforced polybutylene terephthalate injection-moulding compound carrying a flame-retardant additive package. The product designation places it in the glass-fibre-reinforced flame-retardant PBT family, distinct from unfilled PBT grades, from non-flame-retardant PBT+GF30 grades, and from flame-retardant PBT grades without fibre reinforcement. The nominal 30 wt% fibre fraction reduces mould shrinkage, raises tensile modulus, and increases heat deflection temperature relative to unfilled PBT; the black package is intended for components where dimensional reproducibility and mechanical strength are more important than colour flexibility. Because the compound is a heterogeneous melt, properties are anisotropic: glass-fibre orientation in the frozen skin layer differs from the core, and this through-thickness variation controls part flatness, weld-line strength, and post-mould dimensional stability more than any single data-sheet value.

    The material is normally processed on reciprocating-screw injection-moulding machines with closed-loop screw-speed and transfer-pressure control. Published data for this specific configuration is limited; however, industrial datasheets for the surrounding 30 wt% glass-fibre flame-retardant PBT class can be used only as a screening basis. The grade-specific technical datasheet and UL Yellow Card remain the controlling references for all design calculations and tooling decisions.

    What Boundaries Emerge When 30 wt% Glass Fibre and Flame Retardant Are Combined in PBT?

    In a 30 wt% glass-fibre PBT matrix, the reinforcing phase reduces ultimate tensile elongation because the fibre ends act as stress concentrators at the interface. The flame-retardant solid phase further embrittles the matrix, particularly at high injection speeds where shear heating lowers melt viscosity and may orient the flame-retardant phase into plate-like domains. This combination narrows the ductile-to-brittle transition in impact loading and means that the Charpy notched impact value cannot be optimized by fibre concentration alone. Under ISO 527-2, the broader class of 30 wt% glass-fibre flame-retardant PBT compounds typically reports tensile strengths from 110 to 135 MPa; flexural moduli under ISO 178 from 8 500 to 10 500 MPa; notched Charpy impact values under ISO 179-1/1eA from 6 to 10 kJ/m²; and heat deflection temperatures under ISO 75-2/A at 1.8 MPa from 195 to 210 °C. The same class can show density from 1.60 to 1.70 g/cm³ under ISO 1183-1. These ranges cannot be transferred directly to LONGLITE® PBT+GF 4830BKK, but they identify the mechanical envelope in which a 30 wt% glass-fibre flame-retardant PBT is expected to operate.

    Table 1. Comparative property envelope for 30 wt% GF flame-retardant PBT compound class
    PropertyTest standardTypical rangeProcessing or design consequence
    DensityISO 1183-11.60–1.70 g/cm³Higher part weight than unfilled PBT; affects shot weight and cycle energy.
    Tensile strengthISO 527-2110–135 MPaControls load-bearing wall sections under short-term tensile stress.
    Flexural modulusISO 1788 500–10 500 MPaGoverns part stiffness and snap-fit clamp force.
    Notched Charpy impactISO 179-1/1eA6–10 kJ/m²Reflects brittle failure tendency in notched sections.
    Heat deflection temperatureISO 75-2/A, 1.8 MPa195–210 °CUseful for short-term heat resistance, not fatigue or creep life.
    UL 94 flammabilityUL 94V-0 at listed minimum thicknessYellow Card minimum thickness controls recognition.

    Pre-drying of LONGLITE® PBT+GF 4830BKK is not optional after exposure to ambient air. Desiccant-air drying at 120 °C for 4–6 h to residual moisture below 0.02 wt% prevents hydrolytic chain scission at melt temperature. The hopper dryer must deliver air at a dew point of -30 °C or lower; at relative humidity above 60%, open containers should not remain on the machine hopper for more than 30 min without supplemental dry-air sweep. Drying beyond 8 h at 120 °C may cause oxidative yellowing in black PBT even though the dark colour masks the early colour shift; the impact property loss is not masked.

    Barrel temperature profiles for screw diameters from 35 to 60 mm typically start at 240 °C in the feed zone, progress to 255–265 °C in the compression zone, and settle at 260–270 °C at the nozzle. The melt-temperature ceiling is 280 °C; above this, flame-retardant decomposition can generate acidic by-products that corrode tool surfaces and reduce the effective molecular weight. Moulders should record melt residence time in the barrel and hot runner as a process parameter. For hot-runner systems with heated manifolds above 270 °C, total residence time for this compound class should be verified on the actual tool because local overheating at the gate tip can occur even when the main melt temperature reads 265 °C.

    Screw geometry should use an L/D ratio between 18:1 and 22:1 and a compression ratio of 2.0:1–2.5:1 to homogenize fibre and flame-retardant dispersion without excessive glass breakage. On production lines with worn non-return rings, shot-weight variation can exceed 0.5% in multi-cavity tools and create cavity-to-cavity packing differences that alter fibre orientation and part mass; replacement of the screw tip and ring is required when cushion position is unstable beyond 3 mm. Back pressure of 0.3–0.7 MPa improves colour and glass dispersion but excessive back pressure accelerates fibre breakage and increases melt temperature.

    Mould temperature should be maintained from 60 to 100 °C. At 60 °C, the surface freezes rapidly and can produce a resin-rich skin with lower crystallinity and higher gloss; at 90–100 °C, crystallinity rises and post-mould shrinkage is more stable, but cooling time must be extended. Hold pressure is typically set between 50 and 80 MPa hydraulic, with hold-time determined by gate freeze-off as monitored by part-weight stabilisation. Injection speed should be moderate to high to fill thin sections before the melt front solidifies, but excessive speed generates shear heating that can locally exceed 270 °C and produce splay or surface streaks.

    The PBT matrix has a melting temperature near 223–230 °C as measured by ISO 11357-3; this places the typical melt-processing window between 240 and 270 °C. Recrystallisation behaviour depends on mould temperature: at 60 °C mould temperature, the surface layer may remain less crystalline, while at 90–100 °C the slower cooling produces more complete crystallinity and a smaller secondary shrinkage after moulding. Secondary shrinkage can continue for 24–48 h after demoulding; post-mould dimensional inspection should therefore be delayed until parts reach a constant mass at room temperature under 50 ± 5% relative humidity, unless the part is annealed. Published data for this specific configuration is limited; tool dimensions should use the manufacturer’s mould-shrinkage recommendations, not generic PBT+GF30 class values.

    Moulded Part Design Variables for Thin-Wall Connector Housing Applications

    For thin-wall connector housings and relay sockets, weld-line strength is the dominant structural limitation. With 30 wt% glass reinforcement, the tensile strength at a weld line can be 40%–60% lower than the strength perpendicular to flow because fibres align parallel to the meeting front rather than bridging it. Tools should use a single gate or sequential valve-gate sequencing to move weld lines into low-stress zones. If multiple edge gates cannot be avoided, a short shot study should be run on the production tool to locate the weld line before terminal-insertion testing per customer specifications. Wall thickness transitions should be radiused at not less than 0.5 mm; sharp internal corners reduce local fibre packing and initiate cracks during press-fit or snap-fit assembly.

    Rib height and thickness must follow sink-mark control rules: rib thickness at the base should not exceed 60% of the adjoining wall. In black glass-fibre PBT, sink marks are visually less obvious than in natural or light-coloured grades, but they remain critical in precision connectors because the local depression changes contact position by 0.05–0.15 mm depending on rib geometry and cooling layout. A freeze-off study on the tool can identify whether the gate or the rib root is the controlling cooling path; if the gate remains open after rib root freeze, cavity pressure is applied to a solidified rib base and does not reduce sink. Published data for this specific configuration is limited to mould-flow iterations on actual tooling; therefore short-shot and pressure-drop studies are mandatory before serial production.

    For insulating components exposed to condensation or direct current, the comparative tracking index must be read from the grade-specific IEC 60112 report rather than assumed from fibre content. Glass fibre generally lowers the CTI of PBT from values above 400 V for unfilled grades to the 200–300 V band in filled grades; a flame-retardant phase can shift the tracking resistance further depending on whether the package is char-forming or releases conductive decomposition products. Insulation coordination distances in connector bodies should be designed per IEC 60664-1 using the measured CTI group and pollution degree, not the nominal unfilled PBT value.

    Compared with a non-flame-retardant 30 wt% glass-fibre PBT, the 4830BKK grade restricts the melt-temperature ceiling and can reduce notched impact because of the flame-retardant solid phase; however, it permits the same component housing to be used in proximity to ignition sources without secondary shielding. Compared with a 15 wt% or 20 wt% glass-fibre PBT, this grade gives higher flexural modulus and better dimensional stability at elevated temperature under ISO 75-2/A but increases anisotropic shrinkage in the flow direction and can raise warpage in flat, thin-wall parts if the gate is not centrally located. Compared with an unfilled flame-retardant PBT, the 30 wt% glass fibre raises heat deflection temperature and reduces mould shrinkage, but the glass phase lowers comparative tracking index under IEC 60112 and can produce surface roughness in textured cavities.

    When Hot-Runner Residence Time Exceeds the Stabiliser’s Thermal Budget

    If total melt residence time in an insulated hot-runner system exceeds the heat-stabiliser budget at 270 °C, the material may show progressive yellowing, a reduction in melt viscosity, and a decrease in mechanical strength that is not detected by visual inspection alone. For black grades, surface silver streaking from volatile decomposition products can precede the viscosity drop; process engineers should monitor melt-pressure stability at the injection nozzle and compare shot weight against the initial validated value. On systems with manifold temperatures above 270 °C, the use of externally heated nozzles with smaller gate volumes is preferred over long internally heated probe tips because the gate wall can overheat the boundary layer even when the melt stream reads lower.

    The compound should not be combined with certain high-alkalinity processing aids because the polyester matrix undergoes chain scission in the presence of alkaline contaminants under melt conditions. Re-grind from moulded parts should be limited to 20 wt% in UL-recognised components unless the moulder holds a specific UL re-recognition file; a higher regrind fraction can shift the UL 94 classification and mechanical properties because glass fibre length degrades during reprocessing and flame-retardant concentration may be non-uniform across the regrind stream.

    The suffix BKK in LONGLITE® PBT+GF 4830BKK indicates the black colour package; the numeric stem identifies the 30 wt% glass-fibre flame-retardant PBT family. The designation should not be interpreted as a substitute for the UL Recognized Component Yellow Card, which specifies the minimum thickness at which the V-0 rating is recognised. In electrical and electronic applications, if the Yellow Card lists a minimum thickness of 0.8 mm, moulded wall sections below that thickness are not automatically covered unless the component is submitted for additional testing. Similarly, the product is not approved for food contact or potable water applications unless the supplier provides a specific conformity statement; generic PBT datasheets do not confer FDA 21 CFR or EU 10/2011 compliance.

    Table 2. Documentation and compliance checklist
    ClassReference or test methodRequired verification
    Restriction of hazardous substancesRoHS Directive 2011/65/EU Annex II, Delegated Directive (EU) 2015/863Supplier declaration per lot or production campaign
    SVHC communicationREACH Regulation (EC) No 1907/2006, Article 33Current Candidate List check for articles supplied
    Flammability classificationUL 94UL Yellow Card minimum thickness and colour designation
    Comparative tracking indexIEC 60112Measured on moulded plaques, not machined specimens
    Material identification markingISO 11469, ISO 1043-1Part marking for recycling and traceability
    Top