Chang Chun Longlite Pbt Gf 4830 Ncf

Chang Chun LONGLITE® PBT+GF 4830 NCF

    • Product Name: Chang Chun LONGLITE® PBT+GF 4830 NCF
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 423282
    Polymer Base Polybutylene terephthalate (PBT)
    Glass Fiber Content 30%
    Flame Retardant Yes
    Density 1.53 g/cm³
    Tensile Strength 110 MPa
    Elongation At Break 2.0%
    Flexural Modulus 8000 MPa
    Notched Izod Impact Strength 7 kJ/m²
    Heat Deflection Temperature At 1 82 Mpa 200 °C
    Ul 94 Rating V-0 at 0.8 mm
    Dielectric Strength 20 kV/mm
    Volume Resistivity 1E15 Ω·cm
    Molding Shrinkage 0.2-0.5%
    Water Absorption 0.03%

    As an accredited Chang Chun LONGLITE® PBT+GF 4830 NCF factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chang Chun LONGLITE® PBT+GF 4830 NCF is supplied in 25 kg net moisture-barrier paper bags, palletized for industrial handling.
    Container Loading (20′ FCL) 20′ FCL container loads Chang Chun LONGLITE® PBT+GF 4830 NCF in 25 kg bags on pallets, shrink-wrapped and strapped securely.
    Shipping Chang Chun LONGLITE® PBT+GF 4830 NCF is supplied as non-hazardous glass-fiber-reinforced PBT pellets in sealed moisture-barrier bags or drums on pallets. Ship in cool, dry, ventilated conditions, avoiding moisture, heat, and UV. No special transport classification; follow standard industrial handling and hygiene. Protect packaging from damage and keep containers closed until use.
    Storage Store Chang Chun LONGLITE® PBT+GF 4830 NCF in a cool, dry, well-ventilated area away from direct sunlight, heat sources, flames, and oxidizing materials. Keep original containers tightly closed to prevent moisture pickup and contamination. Avoid dust generation and electrostatic buildup. Maintain good housekeeping; do not store near food or beverages. Follow local regulations and the SDS.
    Shelf Life Shelf life is typically two years when stored dry, cool, and sealed in original packaging, protected from moisture, heat, and sunlight.
    Application of Chang Chun LONGLITE® PBT+GF 4830 NCF

    Chang Chun LONGLITE® PBT+GF 4830 NCF is processed into connector bodies and terminal carriers where the design requires a non-chlorinated flame-retardant package, a UL 94 V-0 rating at 0.8 mm wall thickness, and sufficient glass reinforcement to keep contact pitch stable after moulding. Pin headers and wire-to-board housings with nominal wall sections from 0.8 mm to 1.2 mm are dried to a residual moisture content below 0.02% using desiccant drying at 120°C for 4 h, with the dew point of the drying air held below −30°C. Melt temperature is set between 250°C and 270°C; the maximum melt temperature should not exceed 275°C because the flame-retardant system begins to degrade above this threshold, producing surface deposits on the cavity and reducing afterglow consistency in UL 94 vertical burning tests. Mould surface temperature is maintained at 80–100°C to ensure sufficient crystallinity and dimensional stability; lower mould temperatures increase the frozen-layer fraction and produce higher residual stress, which appears as bow along the longest dimension after unconstrained cooling. Gate placement is selected to push the weld line away from pin retention features because glass fibres at the weld line align perpendicular to the flow front and reduce local tensile strength to approximately 50–70% of the un-welded value when measured on ISO 527-2:2012 type 1A tensile specimens with a deliberate weld line. In multi-cavity hot runner tools, the hot runner manifold is held at 260–280°C, and the total residence time is kept below 6 min to avoid degradation of the non-chlorinated additive package. Production-scale experience with clamp capacities from 120 tons to 250 tons shows that the most reliable pin retention and flatness are achieved when cavity pressure at transfer from velocity to pressure control is not forced above 45 MPa. Dimensional control is checked by ISO 294-4:2018 shrinkage specimens; the difference between flow-direction and transverse shrinkage is typically reported as an anisotropic range from 0.2% to 0.5% that must be compensated by tooling allowances. Compliance with IEC 60695-2-11 glow-wire testing at 750°C is required for unattended appliance terminals; the material must not ignite or must self-extinguish within 2 s after glow-wire removal. For tracking resistance, IEC 60112:2020 Method A is used to determine the comparative tracking index; the resulting PLC category is then applied to derive creepage distances under IEC 60664-1:2020 pollution degree 2. End products include appliance terminal blocks, elevator control connectors, power tool switch housings, and sensor connectors.

    When an Automotive Fuse Box Must Meet Multi-Point Thermal Ageing Without Losing Snap-Fit Reaction Force

    In under-hood relay modules and fuse boxes, the material is selected for a UL 94 V-0 rating at 0.8 mm and the ability to survive continuous ambient temperatures near 105°C after high-load operation. Housings and internal partitions are moulded with nominal wall thickness from 1.2 mm to 2.5 mm to maintain snap-fit engagement force without excessive filling pressure. Injection moulding is typically performed on 250-ton clamp machines using a reciprocating screw with an L/D ratio of 40:1; this screw geometry distributes the glass fibre without excessive shear heating. Shot-to-shot variation in flame-retardant package distribution is observed when screw recovery time exceeds 10 s or when the cushion is held below 3 mm; the resulting streaks and afterglow inconsistency can be detected in UL 94 vertical burning tests. Injection speed is set to fill the cavity in 1.5–2.5 s; speeds above 300 mm/s at the flow front generate frictional heat that causes silver streaks around fuse blade slots and rapid thermal decomposition of the non-chlorinated additive. The material is dried to a residual moisture content below 0.02% because hydrolysis during plastication reduces molecular weight and lowers tensile strength at break measured in accordance with ISO 527-2:2012. Long-term heat ageing is screened using ISO 188:2019 at 150°C for 1,000 h; retained tensile impact strength should be at least 60% of the as-moulded value, although published data for this specific grade configuration is limited and must be confirmed against the supplier lot datasheet. The end products are engine-compartment fuse boxes, relay carriers, and power distribution units for 12 V and 24 V vehicle electrical systems.

    Compliance verification matrix for Chang Chun LONGLITE® PBT+GF 4830 NCF in electrical insulation applications
    Test / propertyStandard designationConditionAcceptance criterion
    Vertical burningUL 94specimen thickness 0.8 mmV-0
    Glow-wire end-product testIEC 60695-2-11750°C or 850°C depending on current carriedno ignition or self-extinguish within 2 s
    Comparative tracking indexIEC 60112:2020Method A, solution A, 4.0 mm electrode spacingPLC category reported to designer
    Tensile strength at breakISO 527-2:2012type 1A specimen, 5 mm/minsupplier datasheet value required
    Moulding shrinkageISO 294-4:201860 mm × 60 mm × 2.0 mm plaquereport flow/transverse difference
    Water absorptionISO 62:2008immersion at 23°C in deionised waterreport % mass gain

    AC wallbox charging controllers and charging connector latch bodies use the 4830 NCF grade where the terminal carrier must satisfy IEC 60695-2-11 at 850°C and maintain isolation between pilot, neutral, and phase conductors under condensation cycling. Unlike PA66, polybutylene terephthalate reinforced with 30 wt% glass fibre shows lower moisture absorption and less post-mould dimensional change in humid conditions; water absorption is evaluated under ISO 62:2008 at 23°C in deionised water. Field returns of charging inlets indicate that tracking failures initiate where condensed water combines with copper alloy wear particles at the base of inserted pins, so the comparative tracking index is determined by IEC 60112:2020 Method A with solution A and an electrode spacing of 4.0 mm. The resulting performance level category is applied to creepage distances in accordance with IEC 60664-1:2020; the design engineer selects the distance from the standard insulation coordination tables after the rated impulse voltage and pollution degree are set for the charging circuit. The moulded part is produced in multi-cavity hot runner tooling with manifold temperature held at 270–280°C and total residence time below 6 min; longer residence degrades the non-chlorinated additive package and produces acidic by-products that haze the tool surface and interfere with laser-marking contrast on the charging connector latch. Shrinkage is anisotropic after ISO 294-4:2018 plaque testing; the transverse-flow value commonly exceeds the flow-direction value by 0.2% to 0.4%, and unbalanced cooling across a 150 mm long wallbox terminal board produces warpage above 0.5 mm if the cooling circuit is not divided into separate temperature-controlled zones. End products include AC charging cable plugs, wallbox terminal boards, and charging connector latch bodies.

    What Happens to Coil Bobbin Wall Flatness When Glass Fibres Orient Circumferentially in a 0.8 mm Wall Section?

    For small shaded-pole motor bobbins and solenoid valve coil formers, flange parallelism is critical because enameled copper winding tension above 1.5 N can deflect a thin wall and cause wire crossover that becomes a turn-to-turn insulation failure. In an edge-gated bobbin, glass fibres align predominantly along the flow path, producing anisotropic shrinkage that tilts the flanges; a core gate from the centre pin produces a more radial orientation and less flange distortion. For this grade, a melt temperature of 255°C and a mould temperature of 90°C are common starting points, with packing pressure held between 60 MPa and 80 MPa for 4–6 s to control sink around terminal pins. Inserted terminal pins are retained by local bosses; pull-out force is tested at 100 mm/min crosshead speed on a universal testing machine using a fixture that grips the pin shaft perpendicular to the boss face. The glass-reinforced material is stiff but notch-sensitive; a root radius below 0.3 mm at the pin boss causes local cracking during pin insertion because the local stress exceeds the impact tolerance of the flame-retardant PBT matrix. Moulded bobbins are not used alone as primary insulation unless the assembly is evaluated as part of an insulation system under UL 1446; the grade can be included in a recognised insulation system with specific varnish and magnet wire combinations. The terminal products are shaded-pole motor bobbins, compressor relay coil formers, and solenoid valve bobbins.

    HVAC and appliance stand-offs, thermostat covers, and flame-retardant enclosures specify the 4830 NCF grade where UL 94 V-0 at 0.8 mm is the minimum requirement and the continuous operating temperature does not exceed 120°C; the material must not be exposed to hot water above 80°C for extended periods because the PBT backbone undergoes hydrolytic chain scission, and in condensing boiler controls the housing is therefore positioned outside the direct flue gas condensate drip path.

    Arc Chamber and Switching Component Requirements in Miniature Circuit Breakers

    In miniature circuit breaker outer shells, toggle actuators, and terminal covers made from the 4830 NCF grade, the material is evaluated for its ability to contain low-energy arc events without forming a conductive carbon track. The non-chlorinated flame-retardant package is screened by IEC 60695-2-13:2021 glow-wire ignition temperature and IEC 60695-2-12:2021 glow-wire flammability index, in addition to the standard UL 94 vertical burn at 0.8 mm. The glass fibre reinforcement raises the flexural modulus and reduces the probability that an arc event will mechanically eject a terminal cage, but fibre-rich regions at the surface retain carbonised particles after exposure; the designer therefore applies minimum creepage distances from IEC 60664-1:2020 and avoids locating vent slots directly above contact pivot points. Moulded MCB covers are produced with a melt temperature of 260°C and a mould temperature of 100°C; the tooling is designed with sequential valve gates to prevent weld lines at the latch hook. Because the actuator experiences repeated snap engagement, internal qualification often includes thermal cycling per IEC 60068-2-14 and mechanical shock per IEC 60068-2-27, but no single ISO standard for injection-moulded MCB actuator fatigue exists; the acceptance limit is defined by the electrical equipment manufacturer. The material is not a substitute for arc-quenching ceramics or metal arc splitter plates; its function is limited to structural insulation and mechanical support in the switching chamber. End products are miniature circuit breaker housings, residual current device bases, and toggle levers.

    Free Quote

    Competitive Chang Chun LONGLITE® PBT+GF 4830 NCF prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chang Chun LONGLITE® PBT+GF 4830 NCF is a 30 wt% short-glass-fibre-reinforced polybutylene terephthalate compound formulated with a non-chlorine flame-retardant package. The NCF suffix is a manufacturer designation indicating non-chlorine flame-retardant chemistry; it is not equivalent to a total halogen-free declaration unless separately certified. The grade is supplied in pellet form for injection moulding of electrical insulating parts, connectors, relay carriers, and structural housings. Representative values from published datasheets are compiled in Table 1; these are typical values and are not specification limits.

    Table 1. Representative property envelope for Chang Chun LONGLITE® PBT+GF 4830 NCF
    PropertyTest standardUnitTypical value
    Glass fibre contentISO 3451-1wt%30
    DensityISO 1183-1g/cm³1.58
    Tensile strengthISO 527-2MPa120
    Tensile elongation at breakISO 527-2%2.5
    Flexural strengthISO 178MPa185
    Flexural modulusISO 178MPa9 600
    Notched Charpy impact, +23 °CISO 179-1/1eAkJ/m²7.0
    Melt volume-flow rate, 250 °C/2.16 kgISO 1133-1cm³/10 min14
    Heat deflection temperature, 1.80 MPaISO 75-2/A°C203
    UL 94 flame rating at 0.8 mmUL 94classV-0
    Water absorption, 24 hISO 62%0.06

    Mechanical anisotropy is expected from the 30 wt% glass content. The flexural modulus near 9 600 MPa indicates load-bearing capacity, while the 2.5 % tensile elongation indicates limited ductility. Snap-fit designs requiring tensile strain above 2 % should be analysed for local strain concentration using finite-element methods rather than uniform elongation assumptions.

    When Non-Chlorine Ignition Resistance Is Required in 30% Glass-Filled PBT

    Where moulded parts must satisfy a 0.8 mm UL 94 V-0 classification in a glass-reinforced PBT matrix, the NCF formulation provides controlled combustion response without chlorine-bearing flame-retardant additives. In forced combustion testing under UL 94, the grade is reported to meet V-0 at 0.8 mm; for thickness below 0.8 mm, published data for this specific configuration is limited, and lot-specific testing is recommended. The non-chlorine package reduces hydrogen chloride generation during thermal decomposition, which is relevant in enclosed electrical cabinets where corrosive acid gas attack on relay contacts and printed-circuit-board pads must be controlled. The reduction in chloride species does not automatically eliminate brominated synergists; a total halogen-free specification should be verified against IEC 61249-2-21 or comparable customer requirements.

    In dehumidified hopper drying, pellets are held at 120 °C for 4 h to a residual moisture content below 0.02 %. Drying equipment should deliver a dew point of -30 °C or lower. At production sites where ambient relative humidity exceeds 60 %, drying should be verified by moisture analysis rather than fixed time alone. Residual moisture above 0.02 % at melt temperature can hydrolyse PBT; field evidence on production-scale injection moulding lines shows silver streaking at the gate and reduced notched Charpy impact before tensile strength falls below specification. The material should be processed in a reciprocating screw injection moulding machine. A screw L/D of 18:1 to 22:1 with a compression ratio of 2:1 to 3:1 is suitable; high-shear dispersion is unnecessary because the glass fibre is pre-compounded. Back pressure above 0.7 MPa is not recommended because fibre-length attrition lowers Charpy impact. Barrel profiles from rear to nozzle are typically maintained between 240 °C and 260 °C, with mould temperature between 80 °C and 100 °C. Residence time above 10 min at melt temperature over 260 °C should be avoided to limit ester hydrolysis.

    For short-glass-fibre PBT with filler content at 30 wt%, the melt volume-flow rate is listed under ISO 1133-1 at 250 °C/2.16 kg as approximately 14 cm³/10 min. This moderate flow permits filling of thin-wall sections down to 0.4 mm in tools with adequate venting, although flame classification below 0.8 mm must be revalidated. The presence of 30 wt% fibre raises melt viscosity relative to unfilled PBT and produces shear-thinning behaviour; mould-filling simulations should use Cross-WLF or Bird-Carreau parameters fitted to capillary rheometry data at shear rates of 100, 1 000, and 10 000 s⁻¹. Gate land width should be at least 60 % of wall thickness in thin sections to prevent jetting; submarine and tunnel gates should be positioned to orient glass fibres parallel to the main tensile load in snap-fit geometries. Published pressure-volume-temperature data for this specific formulation is limited; users performing in-mould shrinkage prediction should request two-domain Tait coefficients from the supplier.

    What Separates the NCF Chemistry from Chlorinated Flame-Retardant 30% GF PBT in Humid Electrical Enclosures?

    The principal departure appears in wet-contact electrical behaviour rather than in bulk mechanical strength. Standard chlorinated flame-retardant PBT compounds may release ionic chloride species under humid bias and partial discharge, accelerating dendritic growth on phosphor bronze, brass, or silver-plated contacts. The NCF package reduces the available chloride pool; comparative corrosion testing of contact materials is still required because ester hydrolysis products from PBT itself can generate weak organic acids at high humidity. Comparative tracking index under IEC 60112 for this specific formulation is not always published; designs requiring CTI above 600 V should request lot-specific data because tracking performance depends on glass-fibre sizing, flame-retardant synergist, and surface contamination. In terms of mechanical properties, NCF and conventional chlorinated 30% glass-filled PBT are broadly similar; differences in tensile strength and flexural modulus are often smaller than lot-to-lot variation. The selection driver is therefore lower corrosive potential in confined electrical environments, not a step change in stiffness or strength.

    Table 2. Regulatory and safety assessment framework
    Standard or directiveAssessment areaRelevant designation
    UL 94Flammability class, 0.8 mmV-0
    IEC 60112Comparative tracking indexrequest lot-specific data
    RoHS 2011/65/EU as amendedRestricted substancesmanufacturer conformity declaration
    REACH SVHC candidate listSubstances of very high concernmanufacturer lot declaration
    IEC 61249-2-21Halogen-free component limitsonly if separately certified

    Under sustained 85 °C/85 % RH ageing, connector housings moulded from the NCF grade are assessed for dimensional growth, contact retention force, and insulation resistance. Typical applications include automotive relay carriers, sensor connectors, terminal blocks, PLC terminal sockets, and motor end caps. The 30 wt% glass content provides a tensile modulus of approximately 9 600 MPa and an HDT of approximately 203 °C at 1.80 MPa, enabling compatibility with infrared reflow soldering and wave soldering profiles with peak temperatures up to 230 °C for short exposure; exposure above 260 °C can cause surface blistering in unreinforced sections. Chemical compatibility must be checked with alkaline cooling water, cutting fluids, and ester-based hydraulic oils; PBT is not recommended for continuous contact with strong alkaline solutions above 40 °C. Amine-based additives or colorants at levels above minor pigment loadings should be avoided because aminolysis can reduce melt viscosity and hydrolytic stability. If the component is located near copper conductors, the lower chloride contribution of NCF is beneficial for reducing galvanic corrosion under condensation conditions.

    Moulding Shrinkage, Fibre Orientation, and Dimensional Control in Automotive Connector Housings

    Post-mould shrinkage in this 30% glass-filled PBT is anisotropic. Flow-direction shrinkage is lower because glass fibres constrain matrix contraction; transverse shrinkage is higher, often producing differences of 0.2 % to 0.4 % between orthogonal axes in edge-gated rectangular coupons. Tool compensation for shrinkage in the flow direction typically begins at 0.2 % to 0.3 %, while transverse compensation may require 0.5 % to 0.6 %, depending on gate type, hold pressure, and wall thickness. Warpage in thin-wall connector bodies arises when differential fibre orientation freezes during filling; sequential valve-gate timing and mould temperature uniformity below ±5 °C across the cavity are used to control flatness. After ejection, moisture conditioning at 23 °C for 24 h yields water absorption around 0.06 %, and equilibrium dimensional growth in 50 % RH is generally below 0.2 % for 3 mm sections. Published data for this specific configuration under 85 °C/85 % RH for 1 000 h is limited; end-use validation should therefore include post-ageing contact force, push-back force, and dielectric withstand testing according to the relevant component specification.

    Top