| HS Code | 798098 |
| Polymer Type | Polybutylene terephthalate (PBT) |
| Reinforcement | Glass fiber |
| Glass Fiber Content | 30% |
| Color | Black |
| Density | 1.53 g/cm³ |
| Mold Shrinkage | 0.2–0.5% |
| Tensile Strength | 130 MPa |
| Elongation At Break | 2.5% |
| Flexural Modulus | 8500 MPa |
| Notched Izod Impact Strength | 8 kJ/m² |
| Heat Deflection Temperature At 1 82 Mpa | 205 °C |
| Melting Point | 225 °C |
| Water Absorption | 0.07% |
| Flammability Rating | UL94 HB |
As an accredited Chang Chun LONGLITE® PBT+GF 4830 BK factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg moisture-barrier paper sacks, palletized at 1,000 kg per pallet; store sealed and dry. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Chang Chun LONGLITE® PBT+GF 4830 BK, packed in 25 kg bags, palletized, and securely stowed for ocean freight. |
| Shipping | Chang Chun LONGLITE® PBT+GF 4830 BK is a non-hazardous, glass-fiber-reinforced PBT compound supplied as pellets. It is not regulated for transport under DOT, IATA, IMDG, or ADR. Ship in original sealed moisture-barrier bags/containers, protected from heat, sunlight, and moisture; avoid packaging damage. |
| Storage | Store Chang Chun LONGLITE® PBT+GF 4830 BK in a cool, dry, well-ventilated area, protected from direct sunlight, heat, moisture, and ignition sources. Keep material in original, closed packaging on pallets; avoid dust generation, static buildup, and package damage. Segregate from incompatible chemicals, use first-in/first-out rotation, and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is approximately 24 months when stored unopened in a dry, cool, well-ventilated area, away from sunlight and moisture. |
Underhood electrical connector developments for 12 V and 48 V architectures have moved from polyamide 66 to 30% glass-filled PBT where resistance to hot transmission oil and glycol-water coolant is required at continuous soak temperatures of 120°C to 130°C. In this application, LONGLITE PBT+GF 4830 BK is processed in its supplied black color, with no external color masterbatch. The compliant formulation for series production is 100 wt% virgin compound or a closed-loop regrind blend limited to 15 wt% of dried sprue and runner regrind from the same grade; adding more than 15 wt% regrind can reduce tensile elongation at break and shorten bolt-hole stress relaxation life because the fiber length distribution shifts downward. Pre-drying is conducted in a desiccant wheel dryer at 120°C for 4 h to a dew point below -30°C, resulting in residual moisture below 0.04 wt% before material enters the injection unit. Industry compliance for underhood connectors includes SAE/USCAR-2 Revision 6 for terminal retention force and connector durability, ISO 16750-4 for temperature and humidity cycling, and UL 94 V-0 at 0.8 mm for flame retardance in engine compartment locations. The downstream production line uses all-electric injection molding machines with screw L/D between 20:1 and 24:1, barrel temperatures from 240°C to 265°C, mold temperature from 60°C to 90°C, and valve-gated hot runners on multi-cavity tools to reduce freeze-off at the gate. Critical process control centers on weld-line positioning; because the 30 wt% short glass fibers orient parallel to flow and remain transverse at weld lines, tensile strength at a weld line may fall to 45% to 60% of the unwelded value. Gate placement is therefore adjusted so that weld lines do not pass through terminal retention features or threaded inserts. Terminal products include engine harness connectors, cam position sensor enclosures, ABS sensor bodies, and throttle position sensor housings.
When a 30% glass-filled polybutylene terephthalate compound is used for battery management system carrier plates and high-voltage interlock connectors, the controlling variable shifts from mechanical strength to surface-tracking resistance and ionic contamination. For this application, the formulation should remain 100 wt% virgin LONGLITE PBT+GF 4830 BK when the part contains stamped busbars or nickel-coated copper inserts; if regrind is permitted on non-live, low-voltage clip features, the addition ratio is capped at 10 wt% of same-grade dried regrind, and the regrind must be screened to remove particles below 0.5 mm because fines increase moisture absorption and degrade creepage-current resistance. The relevant compliance environment is shaped by IEC 60664-1:2020, which determines creepage and clearance distances for pollution degree 3 in sealed battery compartments, and by IEC 60695-2-11:2014, which specifies glow-wire testing at 850°C for unattended equipment; the compound must also maintain UL 94 V-0 at 0.8 mm. Processing in this segment is complicated by the flat, thin-wall geometry of the carrier plate: manufacturers use injection-compression molding with a compression stroke of 0.3 mm to 0.8 mm after filling, an all-electric clamp force calculated from a cavity melt pressure range of 60 MPa to 90 MPa, and sequential valve-gate opening to shift weld lines toward low-stress central ribs. Barrel residence time is held below 5 min at melt temperatures not exceeding 260°C to limit thermal degradation; mold temperature is maintained at 80°C to 100°C to raise crystallinity and reduce post-molding shrinkage along the busbar retention slots. Terminal product types include 800 V BMS carrier plates, interlock slider housings, and high-voltage connector shells used in passenger electric vehicle battery packs.
Relay base molding in industrial control panels exposes the polymer to continuous coil-spring pressure, occasional arc leakage from contact gaps, and decades of thermal aging under load. For this application, the formulation uses LONGLITE PBT+GF 4830 BK as the sole resin component with 0 wt% external impact modifier, because an impact modifier reduces comparative tracking index and increases smoke density during glow-wire exposure. If thermally stable black concentrate is not required, addition of color masterbatch is omitted; if regrind is used from cold-runner systems, it is limited to 20 wt% and blended with virgin material for no more than 3 heat histories. The governing standards include IEC 61984:2008 for connectors and interconnection components, IEC 60695-2-11:2014 for glow-wire flammability at 850°C, and IEC 60068-2-30 for damp heat cyclic testing to validate terminal retention after moisture exposure. The production process is insert molding of brass or silver-plated contact blades; the mold is heated to 70°C to 90°C to minimize post-molding shrinkage around the inserts, and pack/hold pressure is maintained at 40 MPa to 60 MPa for 4 s to 8 s depending on gate freeze time. Because the compound contains 30 wt% short glass fiber, tool wear at the gate land is observed after 300,000 to 500,000 cycles on hardened H13 tooling without surface nitriding; gates with a diameter below 1.0 mm cause excessive fiber breakage and should be avoided. Terminal product types include DIN rail-mount relay sockets, contactor coil housings, and industrial terminal block bases.
For production planning, the following matrix aligns three of the above application segments with the governing compliance method, allowable regrind addition, and the drying boundary that must be met before melt plastication. The matrix is not exhaustive; additional end-product standards apply at the finished-device level.
| Application segment | Primary compliance method | Maximum regrind addition | Pre-molding drying boundary | Terminal product type |
|---|---|---|---|---|
| Automotive underhood connectors | SAE/USCAR-2 Revision 6; ISO 16750-4; UL 94 V-0 at 0.8 mm | 15 wt% same-grade dried regrind | 120°C for 4 h; dew point below -30°C; moisture below 0.04 wt% | Engine harness connectors, sensor enclosures |
| EV BMS carriers and high-voltage connectors | IEC 60664-1:2020; IEC 60695-2-11:2014 at 850°C; UL 94 V-0 at 0.8 mm | 10 wt% on non-live features; 0 wt% in busbar contact areas | 130°C for 3 h to 4 h; dew point below -40°C; moisture below 0.02 wt% | 800 V BMS carrier plates, interlock housings |
| Industrial relay bases and contactors | IEC 61984:2008; IEC 60695-2-11:2014 at 850°C; IEC 60068-2-30 | 20 wt% cold-runner regrind; max 3 heat histories; 0 wt% impact modifier | 120°C for 4 h; extend to 6 h when RH exceeds 60%; moisture below 0.03 wt% | Relay sockets, contactor coil housings, terminal block bases |
Brushless motor end caps injection-molded from 30% glass-filled PBT must withstand repeated hot/cold transitions when a cordless drill moves from a winter service van to a high-load cutting operation. Here LONGLITE PBT+GF 4830 BK is used at 100 wt% virgin material for the first shot, with regrind from sprue and runner limited to 10 wt% because higher regrind levels produce a measurable shift in flow length-to-wall thickness ratio and can cause core-pin deflection in thin rib sections. The application is assessed under IEC 62841-1 for motor-operated hand-held tools, with supplemental compliance to UL 94 V-0 at 0.8 mm and the notched Izod impact test according to ISO 180 to confirm low-temperature ductility at -30°C. Molding operations employ a two-plate cold-runner tool with gate diameters between 1.0 mm and 1.5 mm, a melt temperature of 250°C to 265°C, and a mold temperature of 80°C; core-pin cooling is provided by high-conductivity copper-beryllium inserts. Dimensional checks after ejection are performed after 24 h post-crystallization conditioning at 23°C and 50% RH, with maximum total shrinkage controlled to 0.3% to 0.5%. Terminal products include brushless drill motor end caps, angle grinder motor brackets, and battery pack receptacle housings.
Coil formers for solenoid and pump-motor applications are wound with enameled copper wire at tensions that create long-term hoop stress on the bobbin flange. LONGLITE PBT+GF 4830 BK is used as a 100 wt% virgin compound when the coil former will be subjected to winding tensions above 0.6 N; regrind is not recommended for thin-wall flanges below 0.8 mm because fiber-length degradation from recompounding reduces hoop-stress retention. The relevant compliance path is the UL 1446 insulation system recognition, where the PBT bobbin is evaluated as a component within a specific enameled wire and varnish system, together with IEC 60335-1:2020 Clause 30.2 for glow-wire flammability in motor-operated appliances if the coil former is not enclosed by metal. Molding requires a mold temperature of 80°C to 100°C and a hold-pressure profile that compensates for anisotropic shrinkage around the central steel core; because the glass fibers orient circumferentially around the core, the radial shrinkage can differ from axial shrinkage by 0.1 to 0.3 percentage points, producing taper in the flange gap. Injection gates are positioned at the sprue side opposite the flange to avoid weld lines on the winding surface. Terminal product types include solenoid valve bobbins, relay coil formers, and stator bobbins for small pump motors.
Photovoltaic junction box molding for 1,000 V DC and 1,500 V DC rooftop systems subjects the insulation material to damp heat, partial discharge, and surface carbonization from electrical tracking. In this segment, LONGLITE PBT+GF 4830 BK is specified as a 100 wt% virgin compound because outdoor aging amplifies the negative effect of even low levels of regrind on comparative tracking index and color fade uniformity; no external flame-retardant masterbatch or glass fiber is added at the molding shop. Compliance rests on IEC 62790:2020 for junction boxes, IEC 60664-1:2020 for creepage under pollution degree 3, and UL 94 V-0 at 0.8 mm for the enclosure body; glow-wire testing under IEC 60695-2-11:2014 at 850°C is applied when the box is mounted on a building surface. The production process is a high-injection-speed fill at 250°C to 265°C melt temperature into a mold held at 100°C to 110°C to maximize crystallinity and reduce post-molding thermal shrinkage after roof exposure. To prevent voiding around copper diode leads, injection speed is profiled so that melt flow fills the lead-frame cavities before the flow front cools below the glass-transition temperature; mold inserts are nitrided to resist erosion by 30 wt% glass fiber in the gate area. Published data for this specific configuration is limited for UV stabilization beyond the black pigment package; projects requiring direct sunlight exposure beyond 5 years should verify long-term surface erosion testing according to ISO 4892-2. Terminal product types include photovoltaic junction box bodies, diode module holders, and DC disconnect switch insulators.
Competitive Chang Chun LONGLITE® PBT+GF 4830 BK prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chang Chun LONGLITE® PBT+GF 4830 BK is a black-pigmented polybutylene terephthalate injection-moulding compound reinforced with 30 wt% short glass fibre. The grade is supplied in pellet form by Chang Chun Plastics Co., Ltd. under the LONGLITE® engineering polyester series. The suffix BK designates black colour; it does not, by itself, identify a flame-retardant system or a UV-stabilised formulation. The compound is intended for precision electrical connectors, relay bases, sensor housings, fuse covers and under-hood automotive housings in which high stiffness, dimensional stability and electrical insulation are required. Typical mechanical data are generated on ISO 527-2 1A specimens conditioned for 88 h at 23°C and 50% relative humidity, unless another conditioning protocol is cited in the producer’s current datasheet. This material is not recommended for continuous hot-water immersion above 80°C unless hydrolysis-resistant performance is validated for the specific part geometry and service fluid.
The representative property set that follows is transcribed from published product information for the 30 wt% glass-fibre-reinforced black grade. These values are typical injection-moulded values, not specification limits. Where a producer datasheet is updated, the latest revision governs. Flammability classification must be verified on the final part thickness because UL 94 performance depends on wall section, colour, and moulding conditions.
| Property | Test method | Typical value | Unit |
|---|---|---|---|
| Specific gravity | ISO 1183-1:2019 | 1.53 | g/cm³ |
| Water absorption, 24 h at 23°C | ISO 62:2008 | 0.06 | % |
| Tensile stress at break | ISO 527-1:2019 | 130 | MPa |
| Tensile strain at break | ISO 527-1:2019 | 2.5 | % |
| Flexural strength | ISO 178:2019 | 200 | MPa |
| Flexural modulus | ISO 178:2019 | 9000 | MPa |
| Notched Izod impact strength at 23°C | ISO 180/A:2019 | 9.0 | kJ/m² |
| Notched Izod impact strength at -30°C | ISO 180/A:2019 | 7.0 | kJ/m² |
| Heat deflection temperature, 1.8 MPa | ISO 75-2/A:2013 | 205 | °C |
| Melting point | ISO 11357-1:2016 | 225 | °C |
| Volume resistivity | IEC 62631-3-1:2016 | 10^15 | Ω·cm |
| Surface resistivity | IEC 62631-3-2:2016 | 10^14 | Ω |
| Dielectric strength | IEC 60243-1:2013 | 22 | kV/mm |
| Comparative tracking index | IEC 60112:2020 | 250 | V |
| Flammability at 1.6 mm | UL 94 | HB | class |
| Mould shrinkage, flow direction | ISO 294-4:2018 | 0.3–0.6 | % |
| Mould shrinkage, transverse direction | ISO 294-4:2018 | 0.6–1.0 | % |
The principal processing constraint is hydrolytic degradation of the PBT ester backbone. The compound must be dried before moulding to a residual moisture content below 0.02 wt%. A closed-loop dehumidifying hopper dryer operated at 120°C for 4–6 h is the standard preparation method; if the dryer dew point rises above -30°C or ambient relative humidity exceeds 60%, drying time should be extended to 6–8 h. Material dried beyond 8 h at 120°C may begin oxidative degradation and surface powdering. Hopper airflow should not exceed the dryer manufacturer’s recommended velocity because high airflow can separate glass fibres from pellets and create feed-throat blockages.
On production-scale reciprocating-screw injection machines, barrel zones are normally set from 250°C at the rear to 270°C at the front, with nozzle temperature held between 260°C and 270°C. Melt temperatures above 280°C should be avoided because ester pyrolysis and oxidation can generate volatile degradation products, causing surface splay and loss of notched impact strength. A maximum barrel residence time of 5 min at temperatures above 270°C is a practical boundary; longer residence in hot-runner drops or during shutdown periods produces black specks and weld-line embrittlement. Screw speed and back pressure should be limited to 50–80 rpm and 2–4 MPa on a 40 mm general-purpose screw. Higher back pressure increases shear heating, shortens the safe processing window and accelerates glass-fibre attrition.
Mould temperature should be controlled between 60°C and 100°C. At mould temperatures below 60°C, the skin layer freezes too rapidly to develop full crystallinity, reducing heat deflection temperature and increasing post-moulding shrinkage. At mould temperatures above 100°C, cycle time increases and ejection may be impaired. For thin-wall connector bodies, a mould temperature of 80°C with coolant supply at 70°C and return below 78°C is common. In multi-cavity tools, a cavity-to-cavity fill-time imbalance above 5% produces measurable differences in glass orientation and warpage. Hot-runner systems should be configured with polished channels, no dead spaces, and valve gates where possible; thermal gates in long hot-runner drops can retain degraded material and release it intermittently into the melt stream.
In 48-pole automotive connector housings and under-hood relay bases, the 205°C heat deflection temperature at 1.8 MPa permits short-term exposure to lead-free soldering and engine peak soak conditions, while the 9.0 kJ/m² notched Izod resistance at 23°C provides assembly impact tolerance. Annealing for 2 h at 120°C is often applied to relieve moulded-in stress before thermal cycling from -40°C to 150°C. Unannealed parts with asymmetric glass orientation may crack at weld lines during the first 100 cycles. Published cycle-count data for this specific product configuration is limited; end-user validation on the actual part geometry and cycle profile is required.
The selection logic for replacing an unfilled PBT or a modified PPO in a rigid housing is driven by the mechanical and thermal differences below. Values are representative and should be compared using the same specimen thickness, conditioning protocol and mould temperature.
| Attribute | Unfilled PBT | PBT+GF 4830 BK | Test method |
|---|---|---|---|
| Specific gravity | 1.31 | 1.53 | ISO 1183-1:2019 |
| Tensile stress at break | 55 | 130 | ISO 527-1:2019 |
| Tensile strain at break | 50 | 2.5 | ISO 527-1:2019 |
| Flexural modulus | 2.6 | 9.0 | ISO 178:2019 |
| Heat deflection temperature, 1.8 MPa | 60 | 205 | ISO 75-2/A:2013 |
| Notched Izod impact strength at 23°C | 4.0 | 9.0 | ISO 180/A:2019 |
| Mould shrinkage, flow direction | 1.5–2.2 | 0.3–0.6 | ISO 294-4:2018 |
| Water absorption, 24 h at 23°C | 0.08 | 0.06 | ISO 62:2008 |
The major benefit is thermal and dimensional. Heat deflection temperature at 1.8 MPa increases from approximately 60°C to 205°C, which permits replacement in soldering fixtures and under-hood brackets where unfilled PBT distorts. The trade-off is strain: unfilled PBT yields above 50% at break, while the glass-reinforced grade breaks at approximately 2.5%. Snap-fit designs transferred without modification may fail in brittle mode; the notch radius, undercut depth and gate location must be altered. Compared with a modified PPO equivalent, the PBT compound has better resistance to unleaded fuel, motor oil and alkaline cleaner contact at room temperature, but modified PPO may retain tensile properties more consistently in saturated humidity and at sub-zero impact conditions.
Compared with a glass-fibre-reinforced polyamide PA66 grade, the LONGLITE® product shows lower moisture absorption and better dimensional stability across humidity changes. Typical PA66 moisture absorption is 1.0–1.5% after 24 h water immersion by ISO 62:2008, whereas the PBT grade absorbs 0.06%. However, the PBT matrix has a lower continuous service temperature than heat-stabilised PA66 and should not be specified for sustained exposure above 140°C. A PET/PBT blend may provide a different surface finish and lower warpage in some flat parts, but it is often more sensitive to mould temperature; the PBT+GF 4830 BK grade can be processed at the lower end of the 60–100°C mould-temperature range.
End-use restrictions are primarily thermal, hydrolytic and chemical. The unmodified PBT matrix is not recommended for continuous immersion in water or aqueous coolant above 80°C; ester hydrolysis rates accelerate with temperature and pH extremes. In insert moulding or metal overmoulding, steel inserts preheated to 100–130°C reduce differential shrinkage, but the component should not be exposed to steam sterilisation above 121°C without a hydrolysis-resistance study. Strong acids and strong bases degrade the polyester backbone, and primary amines are particularly aggressive because they promote aminolysis. The compound should not be melt-blended with amine-functional masterbatch additives or with polyamide contamination above 0.5 wt%; incompatible polymers in recycled material may delaminate at the glass interface and reduce mechanical integrity.
Regrind use should be limited to a maximum of 20 wt% of the shot weight and must be dried with virgin material. Sifting and dust removal from regrind are required because glass-fibre fines and powder alter melt-flow balance and lower weld-line strength. Post-consumer recyclate is not covered by the producer’s datasheet and should not be introduced without migration testing and contamination analysis. Regulatory documentation supplied with the grade typically references RoHS Directive 2011/65/EU and REACH Regulation (EC) No 1907/2006. The black pigmentation system is carbon black or a carbon-black-containing masterbatch; it does not by itself confer outdoor weathering resistance. If the part is specified for exterior use, a UV-stabilised black grade or an additional weathering test according to ISO 4892-2:2013 is required.
For electrical safety, the producer datasheet reports a comparative tracking index of 250 V. This value may be insufficient for creepage-critical high-voltage parts above 250 V without additional creepage distance or a higher-CTI flame-retardant grade. Final part UL 94 classification depends on thickness, colour, gate position and moulding conditions, and must be validated on production tools at the minimum wall section when flammability is part of the end-product approval. The grade is not intended for direct food-contact applications unless specific regulatory clearance is confirmed in writing for the final article.