    HS Code 557622
    Basepolymer Polybutylene terephthalate (PBT)
    Reinforcement Glass fiber
    Glassfibercontent 15%
    Density 1.41–1.45 g/cm³
    Tensilestrength 90–100 MPa
    Elongationatbreak 2–3%
    Flexuralmodulus 5,000–6,000 MPa
    Notchedizodimpactstrength 5–8 kJ/m²
    Heatdeflectiontemperature 190–200 °C at 1.82 MPa
    Meltingpoint 220–225 °C
    Waterabsorption 0.06–0.10%
    Moldshrinkage 0.3–0.7%
    Dielectricconstant 3.5–3.8 at 1 MHz
    Volumeresistivity 1×10^15–10^16 Ω·cm
    Processingmethod Injection molding

    As an accredited Chang Chun LONGLITE® PBT+GF 4815 NCB factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chang Chun LONGLITE® PBT+GF 4815 NCB is supplied in sealed 25 kg moisture-resistant bags, palletized and stretch-wrapped for secure industrial transport.
    Container Loading (20′ FCL) 20′ FCL container loaded with Chang Chun LONGLITE® PBT+GF 4815 NCB in sealed packaging, evenly stacked and secured for ocean shipment.
    Shipping Chang Chun LONGLITE® PBT+GF 4815 NCB is shipped as a non-hazardous, moisture-sensitive solid resin in sealed bags or containers, palletized and protected from water, heat, and sunlight. Use covered, dry freight; avoid punctures, contamination, and prolonged outdoor storage.
    Storage Store **Chang Chun LONGLITE® PBT+GF 4815 NCB** in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat sources, moisture, and oxidizing materials. Keep pellets in sealed original packaging on pallets; prevent contamination and physical damage. Use first-in, first-out stock rotation and dry as recommended before processing.
    Shelf Life Shelf life is generally two years when stored sealed, dry, at ambient temperature, protected from moisture, heat, and direct sunlight.
    Application of Chang Chun LONGLITE® PBT+GF 4815 NCB

    On production lines dedicated to engine-compartment connector housings with wall sections of 0.8–1.6 mm and shot masses between 8 g and 25 g, LONGLITE® PBT+GF 4815 NCB is pre-dried at 120 °C for 4 h in a closed-loop desiccant dryer. The dew point is held at or below −40 °C, and residual moisture is controlled below 0.02 wt% by Karl Fischer titration under ISO 15512. Moisture above this threshold accelerates ester cleavage, causes mould deposit on the cavity surface, and produces surface splay at the gate. The barrel profile is set from 240 °C at the feed zone to 250 °C at the front zone, with the nozzle held at 245 °C ± 2 °C because the 15 wt% glass-fibre reinforcement raises shear heat in hot-runner valve gates. Mould temperature is maintained at 80 °C for flatness on multi-pin connector faces. Clamp force is calculated at 5–7 kN/cm² of projected area. Holding pressure is set at 60–80 MPa hydraulic, screw rotation at 60–90 rpm, and back pressure at 0.3–0.5 MPa. At wall sections below 1.0 mm, total melt residence time must remain under 5 min. Any stoppage longer than 10 min requires barrel emptying to avoid black spec from thermally degraded PBT. Weld lines behind multi-pin cores will reduce tensile strength by 30–40 % relative to the uninterrupted bulk property measured under ISO 527-2. Gate positions are therefore moved to place knit lines into the connector shroud rather than the latch beam. Regrind is limited to 20 wt% when the finished connector housing carries a Recognized Component marking under UL 94. Fines below 1.5 mm are removed before blending. For engine-compartment service, OEM validation applies USCAR-2 connector performance requirements, and accelerated heat ageing is carried out at 150 °C for 1 000 h with tensile retention measured by ISO 527-2 after oven exposure per ASTM D3045. Terminal products include 32-pin ECU connector housings, sensor connector bodies, and relay socket retainers.

    What Limits Regrind Content in Power Tool Brush Holders and Motor Brackets?

    Stator-side motor brackets and brush holder assemblies are moulded with thicknesses from 1.5 mm to 3.0 mm, where hoop stress around the rotor bearing seat controls dimensional acceptance. LONGLITE® PBT+GF 4815 NCB is processed in an eight-cavity cold-runner tool with a sprue-bush orifice not smaller than 2.5 mm to limit glass-fibre fracture at the feed point. The barrel profile is 235 °C feed, 245 °C metering, and 250 °C nozzle, with the mould held at 70 °C. Regrind content is capped at 20 wt% because two additional passes of glass-filled PBT reduce notched Charpy impact by 15–25 % under ISO 179-1/1eA, and the loss is not recovered by raising mould temperature. The observed failure mode is glass-fibre attrition combined with oriented glass clusters at the snap-gate of the brush-holder cantilever. Batch-to-batch variance in this region is controlled by sieving regrind through a 1.5 mm mesh and blending by automatic dosing at the machine throat. Terminal products include 18 V lithium-ion power tool brush holders, spindle lock brackets, and motor commutator end caps. For brush holders that support live commutation parts, the final assembly is evaluated under IEC 62841-1 for mechanical strength of insulation and guarding. At continuous winding temperatures above 90 °C, creep deformation of the brush-holder snap must be checked by ISO 899-1 in tension on an actual moulded assembly. Published data for this specific material configuration under motor thermal load is limited, so a 90 °C / 500 h thermomechanical creep test is specified as an application-specific validation gate. No direct substitution of glass-fibre content is made without rebalancing the snap-fit deflection because the 15 wt% fibre loading gives lower flexural modulus than a 30 wt% glass-fibre PBT under ISO 178.

    Within the 24-cavity cold-runner tools used for relay bases and terminal strips, the trade-off between flow length and creep resistance becomes the controlling yield factor. The glass-fibre loading of LONGLITE® PBT+GF 4815 NCB produces a lower pressure drop than a 30 % glass-filled PBT, while retaining enough modulus to prevent cracking at threaded-insert bosses. The mould is held at 70 °C, and the material is injected with a 0.8 s fill time to prevent freeze-off behind screw bosses. Packing pressure is held at 60 MPa for 6 s, followed by 18 s cooling for a nominal 2.0 mm wall. Glow-wire testing under IEC 60695-2-11 is carried out on the final relay base thickness because a pass is not automatic for glass-filled PBT without flame-retardant additives. Tracking resistance is assessed by IEC 60112; typical PBT-GF15 compounds report CTI values from 400 V to 600 V, and the exact NCB lot certificate must be reviewed before approval. The NCB colour designation is normally a black pigmentation package, but the surface resistivity of the black moulding is not assumed to be dissipative unless measured under IEC 60093. Terminal products include 10 A eight-pin relay bases, 5 mm pitch terminal strips, and circuit breaker escutcheons. Because these parts may be mounted in DIN-rail enclosures, the ball pressure test under IEC 60695-10-2 is performed at the maximum junction temperature, and a typical PBT-GF15 passes at 165 °C when the part is annealed. If the moulded relay base carries brass inserts, insert temperature is kept below 120 °C to avoid local crystallinity loss at the boss root.

    RequirementMethod / ConditionStatus for LONGLITE® PBT+GF 4815 NCB
    Comparative Tracking IndexIEC 60112, solution AConfirm lot certificate; typical PBT-GF15 range 400–600 V
    Glow-wire flammabilityIEC 60695-2-11, 750 °CFinal relay base thickness must be tested; pass not automatic
    UL 94 classificationUL 94, 1.5 mmConsult UL Yellow Card for colour and type; HB is common for non-flame-retarded GF-PBT
    Ball pressure resistanceIEC 60695-10-2Typical PBT-GF15 passes 165 °C; validate at final wall thickness
    RoHS restrictionEU 2015/863, Annex IISupplier lot certificate required; no homogeneous material exception
    REACH SVHCEC 1907/2006, Article 33Confirm no SVHC above 0.1 wt%; supplier SDS applies

    Sensor Enclosure Moulding Requires a Dew Point and Mould Temperature Envelope That Preserves Dimensional Repeatability

    For wheel-speed sensor enclosures, throttle-position sensor housings, and HVAC actuator gear blanks, the defining process conflict is the need to hold post-mould dimensions inside an O-ring groove tolerance while filling a thin sensor nose with glass-loaded melt. LONGLITE® PBT+GF 4815 NCB is dried at 120 °C for 4 h, and if the mould shop relative humidity exceeds 60 %, material is not left in open hoppers longer than 30 min. Water absorption after 24 h immersion at 23 °C is typically below 0.1 % under ISO 62. This supports dimensional stability, but the grade is not hydrolysis-resistant in continuous hot-water or wet-steam exposure above 60 °C. The mould temperature is set at 80 °C, and the injection profile is ramped from 40 mm/s in the gate land to 120 mm/s in the cavity to avoid jetting and glass orientation streaks. Gate vestige is held below 0.05 mm on connector sealing faces to prevent O-ring leakage. Post-mould shrinkage is measured under ISO 294-4; for a 2.0 mm plaque, the flow-direction range is typically 0.3–0.8 %, and the transverse range is 0.8–1.3 %. These ranges are tool-specific and must be verified before cavity dimensions are frozen. Encoder gear teeth are checked for flexural modulus at 80 °C by ISO 178 three-point bending on dry-as-moulded and heat-aged specimens. Terminal products include ABS wheel-speed sensor housings, electronic throttle control covers, and HVAC actuator gear blanks. If the moulded part is exposed to hot transmission oil above 150 °C continuously, long-term oil compatibility data for this specific grade should be requested from the supplier because published data for this configuration is limited. The NCB black pigmentation is not an indicator of UV stabilisation; external under-hood sensor brackets require an additional UV stabiliser package or a separate weathering grade if they are exposed to direct sunlight.

    Domestic Appliance Control Switches and Mechanical Timer Components: Creep Modulus, Arcing Resistance, and Multi-Cavity Balancing

    Household rotary switch housings, push-button switch bases, and mechanical timer cam mounts are moulded with multiple gates and thin internal baffles. Unequal filling of cavity four is observed on 16-cavity production tools when the melt temperature drops below 240 °C. LONGLITE® PBT+GF 4815 NCB is therefore processed with melt temperatures from 240 °C to 250 °C, and the nozzle is kept 5 °C above the front zone to prevent sprue freezing during interrupted cycles. Screw geometry uses a 20:1 L/D general-purpose screw with a 2.5:1 compression ratio and a non-return valve inspected every 50 000 cycles because glass-fibre abrasion opens the valve clearance and reduces cushion consistency. Pack pressure is maintained at 55–70 MPa, and cushion is held at 3–5 mm to avoid overfeeding and parting-line flash. Back pressure at 0.3 MPa prevents gas splay in carbon-black colour lots. Compliance is governed by IEC 60335-1 clause 30 for heat and fire resistance. Ball pressure testing under IEC 60695-10-2 is performed at 125 °C or 165 °C depending on whether the moulding is an internal support or a terminal carrier. For switches that interrupt current, the housing shall not soften or show leakage-current paths after 10 000 switching operations under load. Glow-wire ignition is evaluated under IEC 60695-2-12 and IEC 60695-2-13, but a universal pass cannot be assigned because the final appliance standard and wall thickness control the outcome. Terminal products include washing-machine programme selector cams, microwave door switch housings, and electric kettle steam switch bases. The 15 wt% glass-fibre content maintains creep modulus better than unfilled PBT under sustained switch-return spring load, but the final snap-fit retention must be tested after 48 h at 85 °C because creep at the snap arm root is the main field-failure mode in domestic appliance controls.

    When a 15% Glass Fibre Loading Is Preferred Over 30% in Thin-Wall Terminal Blocks

    For electronic PCB terminal blocks with 0.8 mm side walls and a 5.08 mm pitch, LONGLITE® PBT+GF 4815 NCB offers a lower pressure loss than a 30 % glass-fibre PBT and fills eight small cavities with lower peak injection pressure in comparable tool trials. The thin-wall flow length is sufficient for pin headers, while the bending stiffness of the side wall is checked under ISO 178 at 23 °C and after 1 h at 85 °C. Weld lines form behind each metal terminal retention slot. The residual strength at the weld is improved by moving gates to the end of the block, and the processing window is kept at 245 °C ± 5 °C to prevent short shots at lower temperature and flash at higher temperature. Regrind is limited to 15 wt% for thin-wall terminal blocks because higher regrind lowers melt draw-down and creates glass clusters at pinch-off points. The terminal block body is tested for glow-wire ignition under IEC 60695-2-12 and IEC 60695-2-13. If the end application demands a V classification at 0.75 mm, a flame-retarded grade is required because 4815 NCB is not a flame-retarded formulation unless the supplier lot certificate explicitly states otherwise. Terminal products include PCB terminal blocks, compact fuse holder bodies, and low-voltage distribution barrier partitions. The lower glass content also reduces screw and barrel wear on high-cycle thin-wall tools compared with 30 % glass-fibre PBT, which is an important cost driver when cavities are replaced after 500 000 shots. The table below sets out the general property class comparison on which the selection is based; the values are drawn from published data for commercial PBT glass-fibre classes and are not a lot-specific guarantee for 4815 NCB.

    PropertyStandardPBT-GF15 classPBT-GF30 class
    Tensile strength, 23 °CISO 527-290–105 MPa120–135 MPa
    Flexural modulus, 23 °CISO 1784.5–5.5 GPa8.0–9.0 GPa
    Notched Charpy, 23 °CISO 179-1/1eA4–6 kJ/m²6–8 kJ/m²
    Heat deflection temperature, 1.80 MPaISO 75-2190–205 °C200–215 °C
    Melt flow behaviour, 250 °C/2.16 kgISO 1133-1Higher melt volume rateLower melt volume rate
    Free Quote

    Competitive Chang Chun LONGLITE® PBT+GF 4815 NCB prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chang Chun LONGLITE® PBT+GF 4815 NCB is a polybutylene terephthalate injection-moulding compound reinforced with 15 wt% chopped glass fibre and supplied in black, as indicated by the NCB suffix. The material is positioned for electrical, automotive and appliance components where unreinforced PBT fails in heat-distortion or dimensional stability and where a 30 wt% glass-fibre grade would impose excessive melt viscosity, density, or tool abrasion. Representative supplier-typical data are summarised in the table below. The values are not contractual specification limits; they should be re-verified on test bars taken from the production tool and against lot-specific certificates.

    PropertyTest codeUnitTypical value
    DensityISO 1183-1:2019g/cm³1.39
    Water absorption, 24 h, 23 °CISO 62:2008%0.06
    Tensile strength at breakISO 527-2:2012MPa85
    Tensile elongation at breakISO 527-2:2012%3.5
    Flexural strengthISO 178:2019MPa125
    Flexural modulusISO 178:2019MPa4100
    Notched Izod impact, 23 °CISO 180/A:2023kJ/m²4.5
    Heat deflection temperature, 1.80 MPaISO 75-2:2013°C190
    Melt volume-flow rate, 250 °C, 2.16 kgISO 1133-1:2022cm³/10 min18
    Mould shrinkage, parallel / normalISO 294-4:2018%0.5 / 0.9
    Flammability class at 0.75 mmUL 94classHB, supplier-typical

    The PBT melting endotherm for this class of compound is typically reported near 223–225 °C, and recrystallisation during cooling occurs near 170–180 °C. These transition temperatures control ejection, dimensional stability, and the minimum practical mould temperature. A crystalline fraction sufficiently high for reproducible part dimensions is obtained when the tool surface is held within the range described in the processing section below.

    How Does the 15% Glass-Fibre Loading Modify Short-Term Mechanical Response?

    The 15 wt% glass-fibre reinforcement raises flexural modulus to approximately 4100 MPa under ISO 178:2019, roughly 1.5–2.0 times the modulus of unreinforced PBT. Tensile strength at break is approximately 85 MPa, while tensile elongation at break falls to 3.5%. The failure mode is therefore predominantly brittle in static overload; fibre ends act as stress concentrators, and the notched Izod impact value of 4.5 kJ/m² under ISO 180/A:2023 indicates lower energy absorption than unreinforced PBT. On multi-gated tools, weld lines can reduce local tensile strength to 40–60% of the ISO 527-2 value because glass fibres do not knit across the melt front in the same manner as the unfilled matrix. Impact-sensitive snap-fit designs or living hinges should therefore be evaluated on the actual component, not on a material data sheet basis. At elevated service temperature near 80 °C, tensile strength may fall to roughly 70–75 MPa; finite-element material cards should incorporate temperature-dependent data rather than room-temperature values.

    In dehumidifying-desiccant drying systems with a dew point below -40 °C, pellets are dried at 120 °C for 4–6 h to a residual-moisture level below 0.02 wt% measured by Karl Fischer titration in accordance with ISO 15512:2019. Moisture above 0.03 wt% leads to hydrolytic chain scission in the PBT ester backbone during melt conversion, observable as a barrel-pressure drop, increased melt-flow variation, surface splay, and reduced weld-line strength. Processing on a general-purpose injection-moulding machine should use a screw with 20:1 to 25:1 L/D ratio, compression ratio 2.0:1 to 2.5:1, and check-ring clearance of 0.05–0.10 mm. Barrel temperature settings from rear zone to nozzle are typically 240 °C, 250 °C, 255 °C, and 260 °C; melt residence time should be kept between 3 min and 6 min. Screw rotation should remain between 80 rpm and 120 rpm, and hydraulic back pressure should be set at 0.3–0.7 MPa to limit glass-fibre attrition. Excessive screw speed above 150 rpm is a known cause of batch-to-batch mechanical-property drift in reinforced PBT because fibre-length reduction lowers stress-transfer efficiency. Tool temperature should be held at 60–90 °C. Below 60 °C, crystallisation is incomplete and post-mould shrinkage increases; above 90 °C, cycle-time extension and ejection marks occur without proportional mechanical benefit. For hot-runner systems, open-pipe or externally heated manifolds without dead spots are preferred, and melt temperature above 270 °C should not be held for more than 6 min because thermomechanical degradation releases volatile by-products and depresses molecular weight.

    Dimensional Stability, Shrinkage, and Fibre Orientation Effects

    Glass fibres orient predominantly in the flow direction, producing anisotropic shrinkage. Supplier-typical values are 0.5% parallel and 0.9% normal to flow at 2 mm nominal wall thickness under ISO 294-4:2018. Gate location and weld-line placement therefore dominate warpage. A centre-gated flat plaque tends to display barrel distortion from differential radial constraint, while a single edge gate bends along the flow axis. Annealing at 140 °C for 1 h can stabilise crystallinity and reduce post-mould dimensional drift in precision housings. Post-mould moisture uptake at 23 °C and 50% RH is typically below 0.1% after 24 h, but conditioned dimensional audits after 85 °C/85% RH exposure may require additional allowance because absorbed moisture relaxes the matrix and alters fibre-matrix stress distribution.

    Where unreinforced PBT provides flexural modulus near 2.4–2.6 GPa and heat-deflection temperature under 1.80 MPa near 50–60 °C, LONGLITE® PBT+GF 4815 NCB raises those values to approximately 4.1 GPa and 190 °C. A 30% glass-fibre PBT, by contrast, offers flexural modulus in the 7.0–8.5 GPa range and HDT/A above 200 °C, but melt viscosity increases sufficiently that thin-wall filling may require elevated melt temperature, and tool abrasion becomes more severe. The 15% glass-fibre grade is therefore selected for intermediate stiffness, better long-flow thin-wall mouldability, lower density than GF30, and reduced anisotropic distortion compared with higher fibre loadings. Product-specific comparative data should be obtained from lot-specific certificates; where such data are absent, the class-typical ranges above are sufficient for preliminary material selection but not for final part sign-off.

    When Black Pigmentation Alters Surface Appearance and Infrared Absorption

    The NCB carbon-black package reduces visual fibre read-through and may improve surface consistency in visible components. However, black pigmentation changes infrared pyrometer response; emissivity settings must be calibrated on the black surface before pyrometer-based hot-runner or part-ejection temperature control is attempted. Through-transmission laser welding of unreinforced or natural PBT requires a transparent upper part and an absorbing lower part; a carbon-black-filled grade may not transmit infrared radiation unless specifically formulated for laser-welding applications. In outdoor exposure, carbon black can screen UV radiation and slow surface chalking, but the grade is not described as a UV-stabilised or weatherable compound unless lot-specific data such as ISO 4892-2:2013 are supplied.

    For European market placement, the supplier should confirm that the grade complies with Directive 2011/65/EU as amended by (EU) 2015/863 for the restriction of hazardous substances. Under REACH (EC) No 1907/2006, the SVHC declaration should show no Candidate List substance above 0.1 wt% in the article. The material is not stated as food-contact compliant under EU 10/2011; a separate migration-tested approval is required for food-contact use. Flammability is typically HB at 0.75 mm under UL 94; components requiring V-0 performance must use a flame-retardant PBT grade.

    Check itemDesignationDeclared status
    EU RoHS restricted substances2011/65/EU + (EU) 2015/863compliant per supplier analytical report
    REACH SVHC1907/2006no SVHC above 0.1 wt%
    Flammability at 0.75 mmUL 94HB, supplier-typical
    Food-contact statusEU 10/2011not stated / not approved

    Typical uses include relay bases, sensor housings, connector shells, motor brush holders, and brackets requiring dimensionally stable performance through solder or under-bonnet thermal excursions. On the production tool, glass-fibre orientation at weld lines and gate regions must be evaluated because local tensile strength can fall to 40–60% of the ISO 527-2 value. The compound is unsuitable for continuous hot-water immersion above 60 °C because ester hydrolysis accelerates; strong bases and hot glycol-containing engine coolant can attack the PBT matrix. Avoid blending with amine-containing lubricants or unneutralised phenolic additives, which can promote chain cleavage and premature embrittlement. For components requiring continuous service above 140 °C, a higher-temperature polyamide or polyphenylene sulphide grade should be evaluated instead.