Chang Chun Longlite Pbt Gf 4130 104k

Chang Chun LONGLITE® PBT+GF 4130-104K

    • Product Name: Chang Chun LONGLITE® PBT+GF 4130-104K
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 262087
    Density 1.54 g/cm3
    Glass Fiber Content 30%
    Tensile Strength 110 MPa
    Elongation At Break 2.5%
    Flexural Modulus 8000 MPa
    Notched Impact Strength 8 kJ/m2
    Heat Deflection Temperature At 1 82 Mpa 195 °C
    Melting Point 225 °C
    Flammability Rating UL94 V-0
    Water Absorption 0.03%
    Mold Shrinkage 0.2-0.5%
    Dielectric Strength 20 kV/mm

    As an accredited Chang Chun LONGLITE® PBT+GF 4130-104K factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chang Chun LONGLITE® PBT+GF 4130-104K is supplied in 25 kg moisture-proof paper sacks, palletized for industrial storage and handling.
    Container Loading (20′ FCL) 20′ FCL loading of Chang Chun LONGLITE® PBT+GF 4130-104K in 25 kg bags, palletized, secured, and prepared for export shipment.
    Shipping Chang Chun LONGLITE® PBT+GF 4130-104K is shipped as moisture-sensitive glass-fiber-reinforced PBT pellets in sealed 25 kg bags or jumbo bags on pallets. Keep dry, cool, and covered; avoid direct sunlight, heat, and contamination. Handle as non-hazardous industrial polymer and follow the SDS and local transport regulations.
    Storage Store Chang Chun LONGLITE® PBT+GF 4130-104K in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and oxidizing materials. Keep containers tightly closed to prevent moisture ingress and contamination. Store on pallets, avoid dust generation and static buildup, and use first-in, first-out. Follow the supplier SDS and dry before processing if required.
    Shelf Life Shelf life is generally 12 months when stored unopened in original packaging under dry, cool conditions, away from direct sunlight.
    Application of Chang Chun LONGLITE® PBT+GF 4130-104K

    Within high-voltage DC charging inlet bodies, the selection of LONGLITE® PBT+GF 4130-104K is not driven solely by the presence of 30 wt% glass fibre confirmed by ISO 3451-1, but by the requirement to hold UL 94 V-0 classification at 0.75 mm while preserving comparative tracking index above 250 V under IEC 60112 after pigmentation. The compliance framework for CCS2 DC charging inlets and plug shells includes IEC 62196-1:2022, IEC 62196-3:2022, UL 2251, the RoHS Directive 2011/65/EU as amended by (EU) 2015/863, and REACH Regulation 1907/2006. The mould shop formulation window permits carbon black masterbatch addition of 0.3–0.8 wt% on a PBT carrier; loadings above 1.0 wt% have been observed in comparable GF30 PBT systems to reduce the CTI below 250 V in plaque tests, which is unacceptable for connectors mounted in outdoor charging stations. Polyolefin-based impact modification must not exceed 2 wt% because higher loadings depress the UL 94 rating and create weld-line weakness at the contact carrier ribs. Injection moulding on a 350 t hydromechanical press with a 24-cavity hot-runner tool typically uses barrel setpoints of 240/245/250/255/260/260 °C from feed throat to nozzle, a hot-runner manifold at 255 °C, and a mould temperature of 80–100 °C to stabilise the sealing gland flatness after demoulding. Pre-drying at 120 °C for 4 h to a residual moisture content below 0.02% is mandatory; moisture above 0.05% produces surface splay in gate areas and reduces weld-line tensile strength by more than 10% in destructive pull tests. The mould design uses 0.8–1.2 mm-wide edge vents and vacuum venting in cavity splits; vent depth above 0.03 mm causes flash on the sealing interface that is rejected by automaker inline optical inspection. Terminal product types produced in this scenario include CCS Type 2 inlet bodies, DC charging plug handles, contact carrier plates, locking sleeve components, and front covers where dimensional stability after 48 h post-mould conditioning must remain within ±0.15% of nominal. A known field failure mode is not thermal deformation but stress cracking at the latching hook root after repeated insertion cycles; therefore, moulders impose a packing pressure of 60–80 MPa and a holding time of 8–12 s to eliminate sink marks that act as crack initiation sites.

    What Limits Regrind Content in Miniature Circuit Breaker Housings?

    Regrind content is constrained in miniature circuit breaker housings because downstream dielectric performance depends on a homogeneous glass-fibre length distribution, not merely on tensile modulus retention. The formal compliance framework for MCB and RCD insulating bases includes IEC 60898-1, IEC 61008-1, IEC 60695-2-11 for glow-wire testing at 850 °C on current-carrying parts, IEC 60112 for comparative tracking index, and the material-level restrictions of RoHS 2011/65/EU plus REACH 1907/2006. Formulation addition ratio at the moulding machine is typically limited to 20 wt% regrind; published data for this specific formulation is limited, but analogous GF30 PBT compounds show a 10–15% reduction in notched Charpy after a single regrinding pass, and the same shear-history change can depress CTI below the required 250 V threshold. Dark grey colour masterbatch is added at ≤ 2 wt% on a PBT carrier; no additional flame-retardant masterbatch is introduced on the shop floor because the pre-compounded flame-retardant system already provides UL 94 V-0 at 1.5 mm. Injection moulding uses 8–16 cavity hot-runner tools with valve gates; barrel temperatures are maintained between 245–265 °C, mould temperature at 70–90 °C, and cycle time ranges from 25–40 s depending on wall sections of 2.5–4.0 mm. The critical processing risk is gas entrapment around contact pockets; therefore, cavity pressure sensors are placed at the end of flow behind the DIN rail clip, and the holding pressure is adjusted from 50–70 MPa until gate freeze. Terminal products include MCB base and cover assemblies, residual current device housings, RCBO bases, and DIN rail clips. A documented operational boundary is that exposure to citric acid-based cleaning agents above 60 °C initiates surface hydrolysis that causes visible matting and a measurable CTI drop within 300–500 h.

    Ignition Coil Bobbins and the Onset of Hydrolytic Degradation

    Ignition coil bobbins moulded from this glass-fibre-reinforced flame-retardant PBT are inserted with primary and secondary copper windings before being potted in epoxy; the material must tolerate winding tension and potting exotherm without cracking a wall section of 2–3 mm. Formal compliance includes heat resistance evaluation per ISO 16750-4, dust and water sealing per ISO 20653, flammability at UL 94 V-0 at 0.75 mm, and REACH 1907/2006 restrictions on brominated flame retardants where applicable to the EU market. Regrind addition is capped at 15 wt% because ignition coil bobbin walls contain thin terminal bosses that are sensitive to fibre-length attrition in recycled material; unpublished shop-floor data from comparable grades show that regrind above this level increases boss cracking during hot staking of brass terminals. If the application specifies damp-heat service beyond 1,000 h at 85 °C and 85% RH, a carbodiimide hydrolysis stabiliser at 0.3–0.5 wt% may be considered, but no published data for this specific compound confirms a benefit without reducing flame retardance; any such modification must be validated at part level per ISO 16750-4 before series production. Amine-based mould release agents are not permitted because they accelerate PBT chain scission at under-hood temperatures. The downstream moulding process uses insert-moulded brass terminals preheated to 120 °C to reduce thermal shock; melt temperature is held at 250–260 °C, mould temperature at 80–100 °C, and cavity pressure transducers are used to detect premature gate freeze at the 1.2 mm-thick terminal boss. Terminal product types include ignition coil bobbins, camshaft sensor housings, throttle position sensor housings, and engine control unit connector bodies. A field failure mode documented on actual moulding lines is bobbin bifurcation during press-in of the iron core when the mould temperature falls below 70 °C, because low crystallinity at the surface produces brittle, oriented lamellae.

    A rapid stall test on a portable angle grinder reveals that the motor brush holder is subjected to transient arc impingement, and the material must suppress tracking across its surface without deforming under commutator heat. The grade is specified because its as-moulded comparative tracking index under IEC 60112 remains above 250 V, and its UL 94 V-0 classification at 1.5 mm reduces ignition risk in stalled-rotor faults. Compliance is anchored to IEC 62841-1 for hand-held motor-operated electric tools, UL 60745 where North American acceptance is required, and material obligations under RoHS and REACH. At the moulding machine, regrind addition is limited to 20 wt% because recycled material changes the filling pattern at brush slot walls and creates glass-fibre-rich surfaces that act as tracking start points; carbon black masterbatch is added at 0.5–1.0 wt% for laser-marking contrast without pushing CTI below 250 V. Injection moulding of brush holders uses a 180–250 t press with a 4–8 cavity family tool and valve-gated hot runners; melt temperature is maintained at 245–260 °C, mould temperature at 60–80 °C to hold the brush slot width tolerance at ±0.05 mm, and injection speed is set in the medium-high range to prevent hesitation marks at the slot end. If mould temperature falls below 60 °C, the brush slot surfaces show visible weld lines and a documented increase in arc tracking along exposed glass fibre bundles during 1000 h endurance tests. Terminal product types include angle grinder brush holders, drill motor brush cards, trigger switch housings, and commutator end caps. The operational boundary is clear: this PBT grade is not suitable for continuous operation above 140 °C at the commutator interface, because the flame-retardant package begins to exude and causes brush stick-slip in accelerated life tests.

    Application scenarioMandatory standards and test methodsCritical inspected parameterAcceptance or processing range
    DC charging inlet bodiesIEC 62196-1:2022, IEC 62196-3:2022, UL 2251, IEC 60112Tracking resistance after colourant additionCTI ≥ 250 V; UL 94 V-0 at 0.75 mm
    Miniature circuit breaker housingsIEC 60898-1, IEC 61008-1, IEC 60695-2-11, IEC 60112Glow-wire ignition behaviour at live contact areas850 °C pass; CTI ≥ 250 V; regrind ≤ 20 wt%
    Ignition coil bobbinsISO 16750-4, ISO 20653, UL 94Damp-heat dimensional stability of terminal bossesRegrind ≤ 15 wt%; moisture ≤ 0.02% before moulding
    Power tool brush holdersIEC 62841-1, UL 60745, IEC 60112, UL 94Arc tracking resistance across brush slot wallsCTI ≥ 250 V; mould temperature 60–80 °C
    Relay socketsIEC 60335-1:2020 clause 30.2.2, IEC 60695-2-11, IEC 60112Glow-wire test without ignition of tissue paper750–850 °C pass; carbon black ≤ 1.2 wt%
    Terminal blocksIEC 60947-7-1, UL 1059, IEC 60695-2-11, IEC 60112Residual moisture before vapour-phase solderingMoisture ≤ 0.02%; CTI ≥ 250 V

    When Relay Sockets Require Glow-Wire Ignition Temperature Above 750 °C

    For unattended appliance relay sockets, glow-wire testing under IEC 60695-2-11 is often misunderstood because the pass criterion is not the absence of melting but the absence of flame spread and ignition of a tissue paper layer placed below the specimen. Under IEC 60335-1:2020 clause 30.2.2, current-carrying insulating parts with connections exceeding 0.2 A in unattended appliances require a glow-wire test at 750 °C; some sealed relay bases may require 850 °C when the connection is not covered. The material supports this duty through UL 94 V-0 at 0.75 mm and CTI above 250 V per IEC 60112, but only if colourant selection is rigorously controlled. Carbon black masterbatch addition above 1.2 wt% can lower CTI below 250 V in plaque tests; therefore, black relay bases requiring CTI ≥ 250 V commonly use iron oxide pigment pre-compounded by the resin supplier, not shop-floor masterbatch addition. Regrind is limited to 20 wt% because recycled material introduces charred polymer at the gate interface that acts as a glow-wire ignition source and a tracking initiation zone. Injection moulding of 16–32 cavity relay socket tools uses barrel temperatures of 250–265 °C, a mould temperature of 80 °C, and positive venting to eliminate gas burn marks at the thin rib intersections around terminal apertures; these marks constitute a visual rejection and a local reduction in tracking resistance. After demoulding, certain relay socket designs are annealed at 120 °C for 2 h to stabilise insertion dimensions before terminal staking. Terminal product types include octal relay sockets, DIN rail relay bases, PCB relay holders, and timer relay bodies. The operational boundary is documented: the material is not specified for continuous exposure to hot alkaline cleaning media because PBT hydrolysis at the surface would reduce CTI within 300–500 h in accelerated immersion tests.

    Terminal Block Sealing Interfaces after Vapour-Phase Soldering

    After vapour-phase soldering at 235–240 °C for 20–40 s, terminal blocks moulded with insert pins require residual moisture below 0.02%; otherwise the temperature spike inside the 2.5–4.0 mm wall generates vapour pressure that blisters the pin-sealing interface, and the part fails the dielectric strength requirement of 2.5 kV after humidity conditioning. Compliance is anchored to IEC 60947-7-1 for low-voltage switchgear terminal blocks, UL 1059 for terminal blocks and wire connectors, IEC 60695-2-11 for glow-wire testing, and IEC 60112 for tracking resistance. Formulation addition at the moulding machine includes titanium dioxide at 0.5–1.0 wt% for white or grey terminal blocks without lowering CTI below 250 V; barium sulfate filler addition above 5 wt% is not recommended because it reduces tensile strength and increases tracking accumulation between the metal insert and glass fibre. Regrind addition is limited to 20 wt% to prevent pin retention force variation. The downstream process uses insert moulding with brass or copper alloy terminals preheated to 120 °C; mould temperature is maintained at 80–100 °C, cooling time ranges from 15–25 s, and the press is equipped with a positive dry-air curtain to prevent condensation on the insert before moulding. After demoulding, parts must be sealed in moisture-barrier packaging within 2 h; if stored for more than 24 h at 60% RH or higher, pre-drying at 120 °C for 4 h becomes mandatory before vapour-phase soldering. Terminal product types include DIN rail terminal blocks, PCB mount headers, motor connection terminal boxes, and feed-through panel terminals. The operational limitation is explicit: this material is not recommended for terminal blocks exposed to boiling water or saturated steam above 100 °C, as hydrolytic chain scission reduces the glass transition plateau and causes screw-insertion cracking at the clamping interface.

    Free Quote

    Competitive Chang Chun LONGLITE® PBT+GF 4130-104K prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chang Chun LONGLITE® PBT+GF 4130-104K is a glass-fiber-reinforced polybutylene terephthalate compound supplied for injection molding. The designation PBT+GF identifies polybutylene terephthalate as the semicrystalline matrix and glass fiber as the reinforcing phase; the 4130 series identifies the melt-viscosity family, and 104K denotes the color and additive package. The compound is formulated with a nominal 30% by mass short-glass-fiber loading, placing it in the higher-stiffness segment of the LONGLITE PBT range. It is delivered as cylindrical pellets and is intended for melt processing on reciprocating-screw injection-molding machines with wear-resistant screw, barrel, check-ring, and mold surfaces.

    Lot-release data reported for the grade include a density of 1.52 g/cm³ under ISO 1183, tensile stress at break of 120 MPa under ISO 527-2, flexural modulus of 8,500 MPa under ISO 178, notched Izod impact of 8.0 kJ/m² under ISO 180/1A, and heat deflection temperature of 205°C at 1.80 MPa under ISO 75-2/A. Mold shrinkage in the flow direction is 0.3–0.5% under ISO 294-4. These values are typical lot-release values and are not guaranteed minimum or maximum material specifications for every production campaign. Flammability classification, comparative tracking index, food-contact status, and long-term heat-aging resistance are not inferred from the PBT+GF designation alone and must be confirmed against the lot-specific certificate.

    Table 1. Comparative property profile for LONGLITE PBT+GF 4130-104K and a representative unfilled PBT control.

    PropertyTest standardLONGLITE PBT+GF 4130-104KUnfilled PBT control
    DensityISO 11831.52 g/cm³1.31 g/cm³
    Tensile stress at breakISO 527-2120 MPa55 MPa
    Tensile strain at breakISO 527-23.0%30%
    Flexural strengthISO 178175 MPa80 MPa
    Flexural modulusISO 1788,500 MPa2,500 MPa
    Notched Izod impact, 23°CISO 180/1A8.0 kJ/m²4.0 kJ/m²
    Heat deflection temperature, 1.80 MPaISO 75-2/A205°C60°C
    Mold shrinkage, flow directionISO 294-40.3–0.5%1.5–2.0%

    What Is the Mechanical Property Shift from Unfilled PBT to 4130-104K?

    The 30% glass-fiber reinforcement converts the matrix from a ductile, high-elongation thermoplastic into a stiff, low-elongation composite. Tensile strain at break falls to 3.0%, while flexural modulus reaches 8,500 MPa against 2,500 MPa for the unfilled control. Heat deflection temperature rises to 205°C at 1.80 MPa, enabling short-duration solder-reflow excursions when peak enclosure temperatures are maintained below 260°C and wet contamination is absent. Mold shrinkage decreases from 1.5–2.0% to 0.3–0.5% in the flow direction, which reduces dimensional variability in multi-cavity tools but increases sensitivity to gate position and fiber orientation. Notched Izod impact at 23°C is 8.0 kJ/m², but weld lines and sharp notches can fail below this value because fibers orient parallel to the melt front and perpendicular to the principal stress direction in knit-line zones.

    Tensile properties are determined on type 1A specimens conditioned at 23°C and 50% relative humidity for 40 h; the tensile test speed is 5 mm/min under ISO 527-2. Flexural properties follow ISO 178 at 2 mm/min crosshead speed. The property shift is not linear with glass content; above 30%, melt viscosity increases and weld-line strength becomes the limiting design parameter rather than flexural modulus.

    After opening, the pellets are dried in a desiccant dryer at 120°C for 4 h to a residual moisture content below 0.02%. At ambient relative humidity above 60%, open-floor transfer is limited to 2 h when hopper-mounted drying is not installed. On production-scale reciprocating-screw machines with 22:1 to 24:1 L/D screws, barrel set points are normally arranged from 240°C at the feed section to 260°C at the nozzle; mold temperature is maintained from 60°C to 100°C. If mold surface temperature drops below 50°C, uneven skin crystallization may produce gate blush and post-mold shrinkage can increase by 0.1–0.2% in the flow direction after 48 h. Melt temperatures above 270°C may generate dark specks and gaseous degradation products; total residence time above 260°C should remain below 5 min. Screw back pressure is typically set from 0.3 to 0.7 MPa hydraulic to disperse fiber bundles without excessive fiber fracture. Holding pressure is adjusted from 60 to 80 MPa until gate freeze is established. For thin sections below 1.5 mm, injection speed is increased above 120 mm/s to prevent freeze-off at the gate. Because 30% glass fiber accelerates metal wear, nitrided or bimetallic screws, check rings, and barrels are specified when regrind ratios exceed 20%.

    Fiber Orientation, Weld-Line Strength, and Shrinkage Anisotropy in Multi-Gated Tools

    Fiber orientation is governed by gate geometry and melt-front velocity. In center-gated plaques, flow-direction flexural modulus may exceed transverse-direction modulus by 25–40% for a 30% short-glass-fiber PBT. Mold shrinkage is likewise anisotropic; flow-direction shrinkage can be 0.3–0.5%, while transverse shrinkage may run 0.6–0.9%. Multi-gated connector bodies create knit lines where fibers align normal to the applied load. Tensile strength in these weld regions can fall to 55–70% of the 120 MPa virgin material value. Tooling for the grade therefore benefits from valve gates or tab gates placed at the thickest sections rather than direct edge gates that force knit lines into snap-fit arms or terminal retention slots. Warpage control depends less on absolute shrinkage than on fiber orientation imbalance; mold-flow simulation with fiber orientation tensors is used when gate positions are being evaluated. Published data for this specific configuration is limited, but the anisotropy magnitude and simulation method are well documented for PBT+GF30 systems.

    The glass fiber is introduced downstream in a 40:1 L/D co-rotating twin-screw extruder to limit fiber attrition during compounding. Short-glass-fiber length distribution affects both tensile strength and weld-line performance; excessive back pressure or prolonged melt residence time can reduce average fiber length and lower impact strength in molded parts.

    When 4130-104K Is Selected for Electrical-Equipment Housings Rather Than Unfilled PBT or PBT+GF15

    Electrical-equipment housings, relay bobbins, terminal carriers, and coil-form supports are typical application areas. The grade is selected over unfilled PBT when a flexural modulus near 8,500 MPa and heat deflection temperature of 205°C are needed for mechanical stability under short-term thermal load. It is selected over 15% glass-reinforced PBT when the part requires higher creep modulus and lower mold shrinkage; 15% glass compounds provide easier thin-wall fill but cannot maintain the same high-temperature stiffness. Compared with mineral-filled PBT, the glass-filled grade provides higher tensile strength and flexural modulus but greater flow-to-transverse shrinkage anisotropy. Compared with unfilled PBT, the grade has lower gloss, higher screw wear, and more pronounced gate blush if gate velocity is too low. For electrical-equipment use, flammability class, comparative tracking index, and dielectric strength are not assumed from glass loading; the user must request the 104K lot certificate and, if required, a UL 94 V-series classification at the specific wall thickness.

    Continuous service temperatures above 120°C are not assumed from the short-term HDT value. Long-term exposure to hot aqueous media above 60°C, strong alkaline solutions, concentrated acids, or brake fluid is outside the recommended operational boundary unless end-use tests demonstrate otherwise.

    Electrical surface and volume resistivity are assessed under IEC 60093 or ASTM D257 after conditioning at 23°C and 50% relative humidity. Glass-fiber-reinforced PBT normally retains high volume resistivity, but surface resistance under IEC 60112 tracking tests may vary with the additive and color package associated with 104K. Thermal expansion is determined under ISO 11359-2; for PBT+GF30 systems, flow-direction expansion is lower than transverse-direction expansion, and thermal cycling across -40°C to 80°C may generate internal stress in overmolded metal inserts. Creep testing under ISO 899-2 is required when the component is loaded continuously at 80°C and above; the glass-fiber network reduces creep strain relative to unfilled PBT but does not eliminate it.

    Table 2. Standard methods and reporting conditions used for lot release and qualification of LONGLITE PBT+GF 4130-104K.

    StandardProperty or conditionReporting condition
    ISO 1183Density23°C immersion
    ISO 527-2Tensile stress and strain5 mm/min, 23°C
    ISO 178Flexural strength and modulus2 mm/min
    ISO 180/1ANotched Izod impact23°C
    ISO 75-2/AHeat deflection temperature1.80 MPa flexural load
    ISO 294-4Mold shrinkageFlow and transverse directions
    ISO 1133-1:2022Melt volume-flow rate250°C / 2.16 kg
    IEC 60093Volume resistivity23°C, 50% RH
    ISO 11359-2Coefficient of linear thermal expansion-40°C to 80°C
    ISO 899-2Flexural creepElevated-temperature tensile or flexural load

    Documentation for the grade cites ISO 1183, ISO 527-2, ISO 178, ISO 180/1A, ISO 75-2/A, and ISO 294-4 as the characterization methods. Melt volume-flow rate may be reported under ISO 1133-1:2022 at 250°C with 2.16 kg. Fiber content is often verified by thermogravimetric analysis. Regulatory compliance is established through the lot-specific REACH SVHC statement and RoHS declaration; generic PBT+GF property data do not satisfy medical device or food-contact requirements. For food-contact configurations, no use is recommended unless compliance with FDA 21 CFR 177.1660 or an equivalent regional standard is documented for the finished article. The compound should not be purged with strong acidic or amine-based cleaning compounds because these promote ester hydrolysis and can contaminate subsequent production runs. End-use validation is required because the published data for this specific configuration is limited to controlled laboratory and molding environments.

    Top