| HS Code | 395460 |
| Base Polymer | PBT |
| Reinforcement | 30% glass fiber |
| Density | 1.53 g/cm³ |
| Tensile Strength | 120 MPa |
| Flexural Strength | 180 MPa |
| Flexural Modulus | 8000 MPa |
| Elongation At Break | 2.5% |
| Notched Izod Impact Strength | 9 kJ/m² |
| Heat Deflection Temperature At 1 82 Mpa | 200 °C |
| Ul 94 Flame Rating | V-0 |
| Water Absorption 24 H | 0.05% |
| Volume Resistivity | 1×10^16 Ω·cm |
| Dielectric Strength | 20 kV/mm |
| Mold Shrinkage | 0.2–0.5% |
As an accredited Chang Chun LONGLITE® PBT+GF 4130-104F factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chang Chun LONGLITE® PBT+GF 4130-104F is supplied in 25 kg moisture-proof paper bags, palletized for industrial handling. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Chang Chun LONGLITE® PBT+GF 4130-104F packed in palletized bags, loaded and secured in a 20-foot full container. |
| Shipping | Chang Chun LONGLITE® PBT+GF 4130-104F is shipped as non-hazardous, glass-fiber reinforced PBT compound pellets in sealed moisture-barrier bags or octabins. It is not classified as dangerous goods for transport. Keep dry, sheltered, and away from direct sunlight; avoid moisture uptake and package damage during handling. |
| Storage | Store Chang Chun LONGLITE® PBT+GF 4130-104F in a cool, dry, well-ventilated area, away from direct sunlight, heat, moisture, and ignition sources. Keep original packaging sealed and palletized off the floor; prevent dust, contamination, and static buildup. Maintain stable temperature and humidity, inspect containers regularly, and follow the SDS and local regulations. |
| Shelf Life | Shelf life: typically 24 months from date of manufacture when stored unopened in a cool, dry place in original packaging. |
Chang Chun LONGLITE® PBT+GF 4130-104F is typically evaluated for underhood connector shells and harness clips where dimensional stability and terminal retention after repeated temperature excursions are more decisive than tensile strength alone. In production injection moulding on 24- or 32-cavity hot-runner tools with clamp force from 1,000 kN to 1,800 kN, the material is dried at 120 °C for 4 h to a residual moisture below 0.02 % by ISO 15512 Method A, and melt temperature is maintained between 250 °C and 270 °C; mould surface temperature is held at 80 °C to 100 °C to limit differential shrinkage in the gate area. Terminal retention pins with 0.64 mm and 1.20 mm wide blade contacts are insert-moulded or heat-staked into the PBT housing; the 30 wt% short-glass reinforcement raises tensile modulus measured per ISO 527-2 into the 8,500 MPa to 9,500 MPa range, so the crimp wings resist pull-out after the housing reaches 120 °C under load. Underhood validation typically follows USCAR-2 Class 3 or OEM-specific thermal-cycling profiles from −40 °C to 120 °C, with retention force measured on a calibrated tensile tester after 1,000 cycles; the acceptance gate is a loss no greater than 15 % from initial value. In connectors with thick latch bosses above 3.0 mm, pack-and-hold pressure from 60 MPa to 90 MPa and hold time of 6 s to 10 s are used to prevent sink marks, but over-packing near the gate creates hoop stress that reduces retention after thermal aging. Nucleation of the PBT phase and the glass-fibre orientation distribution induce anisotropic mould shrinkage, typically 0.2 % to 0.5 % in the flow direction and 0.5 % to 0.8 % transverse when measured after 48 h at 23 °C and 50 % RH per ISO 291 and ISO 294-4. Pin spacing above 20 mm requires gate placement at the pin-field centre rather than at a side edge to keep terminal alignment within ±0.05 mm after shrinkage. The flame-retardant PBT matrix tolerates intermittent diesel engine compartment fluid splash, but continuous exposure to strong alkaline media at above 80 °C should be avoided because PBT hydrolyzes at surface ester groups. On hot-runner tools, melt residence time must remain below 6 min at 270 °C; longer residence time decomposes the flame-retardant package and creates black specks and lowered terminal retention. Underhood connectors moulded from this grade are found in engine control unit connectors, camshaft sensor connectors, and transmission solenoid connectors where dimensional stability through thermal shock is a release criterion. Tooling with flash gaps above 0.02 mm benefits from viscosity-controlled lot acceptance because glass-fibre length distribution shifts injection pressure requirements batch-to-batch by 5 % to 10 % at the transfer point, as recorded on an in-mould pressure transducer.
Inside angle-grinder gear housings and cordless drill motor end bells, the shift from unreinforced polyamide to a 30 wt% glass-fibre PBT is driven by lower moisture-induced dimensional change rather than by absolute stiffness alone. Moulding trials on 8-cavity cold-runner tools with sprue diameters from 4.0 mm to 5.5 mm show that a melt temperature of 255 °C and a screw back pressure of 0.3 MPa to 0.5 MPa keep the glass fibre distribution uniform without excessive fibre breakage in the plastication zone. End-bell bearing seats are machined after moulding when runout below 0.03 mm is required on a dial indicator, so the PBT grade must generate sufficient rigidity and a stable post-mould shrinkage plateau; parts are typically measured after 48 h conditioning at 23 °C and 50 % RH because PBT moisture uptake is below 0.1 % per ISO 62 and dimensions stabilize more rapidly than in PA6 or PA66. The moulding window narrows when internal threads are formed by screw insertion rather than machined: cold inserts cause microcracking at the glass-fibre ends if the insert temperature is below 80 °C, while heated inserts above 120 °C can re-melt the surrounding matrix and reduce thread pull-out strength by more than 20 % when tested on a universal tensile tester. Gear-housing walls from 2.5 mm to 3.5 mm are filled at injection velocities of 80 mm/s to 120 mm/s; below 60 mm/s, the glass-rich core freezes before full packing and creates sink opposite boss features, while above 150 mm/s, jetting at the gate produces surface glass streaks that lower fatigue resistance under vibration testing per IEC 60068-2-6. The terminal article in this category is a brushless drill motor end bell that retains a riveted bearing seat after a 1.0 m drop onto concrete at −20 °C; the glass-filled PBT passes this test when moulded-in residual stress remains below 20 MPa as measured by photoelastic stress analysis or toluene craze testing. Chemical resistance to cutting oils and lithium grease is relevant for angle-grinder gear compartments, where continuous oil contact at 60 °C does not soften the PBT matrix, but aggressive esters in some synthetic gear oils can reduce tensile strength after 1,000 h immersion by 5 % to 10 % when retested per ISO 527-2.
Washing-machine side brackets and lid-hinge bodies moulded from 30 wt% glass-fibre PBT must survive repeated alkaline detergent spills, high-humidity wash-chamber air, and occasional impact at 5 °C. The material is not intended for continuous immersion in hot water above 60 °C, so it is restricted to external structural components that see only splash and condensate. In an 8-point hinge boss with a 2.5 mm wall section, filling occurs at 245 °C melt and 70 °C mould; packing pressure of 55 MPa is held for 5 s until the gate freezes, producing post-mould warp below 0.4 mm over a 200 mm span. Dimensional stability after wash cycles is assessed under IEC 60335-1 clause 29 creep and clearance requirements, but published data for this specific bracket configuration is limited; most specifications rely on mould shrinkage verified by coordinate measuring machine after 24 h. The specified glass content reduces thermal expansion to 25 × 10⁻⁶ K⁻¹ to 30 × 10⁻⁶ K⁻¹ when tested per ISO 11359-2, lowering the gap variance between the hinge pin and housing from 0.10 mm to 0.04 mm compared with unfilled PBT. Hinge-boss screw-boss cracking at low temperature is controlled by avoiding sharp internal corners below 0.5 mm radius and by setting the tool temperature to at least 70 °C, which improves surface crystallinity and impact strength at 5 °C in ISO 179-1/1eA notched Charpy testing. Detergent contact at pH 9 to 10 and 40 °C does not cause visible surface degradation after 500 wipe cycles, but hypochlorite-based sanitisers at above 5 % active chlorine produce surface microcracking and should be avoided. The flame-retardant package does not interfere with mouldability at these wall thicknesses, but screw recovery time becomes the production bottleneck when shot size exceeds 70 % of barrel capacity on a 500 kN machine. These brackets are shallow-zone applications for processing science: the material requires standard drying and injection techniques, and release criteria are dominated by geometry-specific impact and detergent testing rather than by rheological limits.
Terminal-block and relay-base mouldings for industrial control panels use the 30 wt% glass-fibre PBT when dimensional accuracy of terminal apertures must remain stable after thermal aging at 105 °C for 1,000 h in an air-circulating oven per IEC 60216-1. The material is processed on multi-cavity hot-runner moulds with individually heated nozzles at 260 °C, and the mould temperature is kept at 90 °C to minimize post-crystallization drift after assembly. Comparative tracking index and arc resistance are evaluated under IEC 60112 and IEC 61621 respectively; the flame-retardant PBT grade is appropriate for insulation parts operating below 600 V in pollution degree 2 service if creepage and clearance distances follow IEC 60664-1. Screw-terminal torque retention in a 12-position rail-mounted terminal block depends on boss insert depth; moulded-in brass inserts with knurl depth 0.3 mm retain torque above 0.6 N·m after 500 insertion cycles when the boss outer diameter is at least 2.0 mm larger than the insert diameter, measured with a calibrated torque screwdriver. In contrast, self-tapping screws into pure PBT bosses show lower thread pull-out after 85 °C/85 % RH aging for 500 h, so metal inserts are specified for terminal blocks requiring repeated field wiring. Barrel residence time at 260 °C should not exceed 5 min because the flame-retardant additives begin to form acidic decomposition products that cause mould deposit and reduce tracking resistance. The following compliance matrix is applied during part approval.
| Property or condition | Test standard | Acceptance criterion |
|---|---|---|
| Residual moisture after drying | ISO 15512 | < 0.02 % |
| Tensile modulus | ISO 527-2/1A | 8,500 MPa to 9,500 MPa |
| Flexural modulus | ISO 178 | 8,000 MPa to 9,500 MPa |
| Heat deflection temperature at 1.8 MPa | ISO 75-2/Af | 195 °C to 205 °C |
| Comparative tracking index | IEC 60112 | ≥ 250 V |
| Flammability at 0.8 mm | UL 94 / IEC 60695-11-10 | V-0 |
Optical and magnetic rotor-position sensor supports made from this material depend on the retention of tooth geometry after annealing and oil exposure rather than on transparency, because the grade is an opaque flame-retardant PBT. A 30 wt% glass reinforcement lifts flexural modulus into the 8,500 MPa to 9,500 MPa range per ISO 178, which reduces blade deflection at rotational speeds up to 6,000 rpm and maintains the air gap between the encoder wheel and the photoelectric pick-up. In a 16-tooth magnetic encoder hub, glass-fibre orientation becomes a process variable because fibre-rich regions create reluctance non-uniformity; process capability is verified against Hall-effect sensor thresholds on a magnetizing and back-EMF fixture, and tooth-to-tooth pitch tolerance is held to ±0.02 mm after annealing at 150 °C for 2 h per ISO 1101. Moulded hubs for resolvers and position sensors are immersed in wheel-bearing grease at 80 °C; the PBT matrix shows no significant softening after 1,000 h in standard automotive grease, but published data for this specific encoder configuration is limited. Detergent-based degreasing at pH above 11 and temperature above 70 °C attacks the ester groups and leads to surface crazing within 500 h, so neutral or hydrocarbon-based cleaning agents are specified. Service below −40 °C reduces notched impact strength in ISO 179-1/1eA Charpy testing and increases the probability of impact-related tooth chipping; spin testing at 120 % of rated speed is therefore used as the final release criterion for rotor-position sensor hubs. The processing conflict in these parts is thermal uniformity: when the mould temperature varies by more than 5 °C between the hub core and the tooth periphery, differential post-crystallization shifts tooth pitch beyond tolerance after motor heating, so conformal cooling channels are specified in high-volume tooling rather than conventional drilled lines.
Competitive Chang Chun LONGLITE® PBT+GF 4130-104F prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chang Chun LONGLITE® PBT+GF 4130-104F is a flame-retardant polybutylene terephthalate injection-moulding compound reinforced with 30 wt% glass fibre. The material is supplied as pelletised compound for electrical, electronic, and electromechanical components in which dimensional stability, stiffness, and a defined flammability classification must be maintained across high-volume production. Representative density is 1.69 g/cm³ when tested under ISO 1183-1:2019. Mould shrinkage in the flow direction is typically 0.2% to 0.5%, whereas unfilled PBT commonly shrinks 1.8% to 2.2% under comparable injection conditions. This shrinkage envelope is a consequence of the rigid glass phase and is a primary reason the grade is specified for precision connector bodies, relay bases, coil bobbins, and sensor housings. Mechanical properties are process-sensitive and depend on fibre-length retention, gate location, and local fibre orientation. Supplier technical literature values for the grade include tensile strength near 130 MPa under ISO 527-2:2012 and flexural modulus near 9,000 MPa under ISO 178:2019. Because the compound is flame-retardant, electrical tracking resistance and glow-wire behaviour must be evaluated at the exact wall thickness, regrind content, and colour used in the production tool, not on generic plaques alone.
The fibre fraction separates the 4130-104F grade from unfilled PBT and lower-glass reinforced PBT. Table 1 compares representative mechanical properties. Values are laboratory specimen data and must be confirmed on production tooling because fibre orientation in a constant-thickness ISO specimen differs from orientation in a complex mould.
| Property | Test method | 4130-104F | Unfilled PBT | PBT+GF20 FR |
|---|---|---|---|---|
| Density | ISO 1183-1:2019 | 1.69 g/cm³ | 1.31 g/cm³ | 1.59 g/cm³ |
| Tensile strength | ISO 527-2:2012 | 130 MPa | 55 MPa | 100 MPa |
| Flexural modulus | ISO 178:2019 | 9,000 MPa | 2,300 MPa | 5,500 MPa |
| Heat deflection temperature at 1.8 MPa | ISO 75-2:2013 | 205 °C | 55 °C | 195 °C |
| Notched Charpy impact strength | ISO 179-1:2010 | 7 kJ/m² | 5 kJ/m² | 5 kJ/m² |
| Mould shrinkage, flow direction | ISO 294-4:2018 | 0.2–0.5% | 1.8–2.2% | 0.3–0.6% |
The increase in flexural modulus from approximately 2,300 MPa to 9,000 MPa is accompanied by a substantial reduction in elongation at break. That reduction limits snap-fit deflection and requires hinge geometry to be recalculated when converting from unfilled PBT. Compared with a 20 wt% glass-fibre flame-retardant PBT, the 4130-104F grade provides higher stiffness and thermal resistance but lower melt flow and higher density. That density penalty is relevant in mass-sensitive automotive connectors and portable electrical equipment. Because glass fibres orient in the flow field, transverse shrinkage can differ from flow-direction shrinkage by a factor of 2 to 3 in complex parts. Cooling-channel layout, gate position, and pack pressure profile must therefore be evaluated before a direct substitution is approved.
Injection moulding of the grade is constrained primarily by moisture, residence time, and fibre attrition. PBT is hydrolytically sensitive at melt temperature. Moisture above 0.02% causes molecular weight loss, reduced tensile strength, and lower impact resistance. The pellet should be dried in a desiccant-bed dryer at 120 °C for 4 h to 6 h, with supply air dew point below −30 °C. If ambient humidity exceeds 60% RH, unheated hopper residence time should be kept below 30 min. Barrel zones are typically set from 240 °C at the rear to 270 °C at the nozzle. Melt temperature must not exceed 270 °C; residence time above 5 min at maximum melt temperature can generate black specks and volatile decomposition products from the flame-retardant system. A screw with L/D ratio between 18:1 and 22:1 and compression ratio between 2.0:1 and 2.5:1 is preferred. Back pressure is often held between 0.3 MPa and 0.5 MPa to maintain melt homogeneity without excessive glass-fibre attrition. Mould surface temperature between 60 °C and 100 °C controls crystallisation rate and post-mould shrinkage. Regrind content above 25 wt% should trigger re-evaluation of comparative tracking index and UL 94 classification because repeated heat exposure changes fibre length distribution and flame-retardant efficacy. Production-scale experience with this material class shows that inconsistent regrind particle size is a more frequent cause of screw-feeding variation than pellet colour variation.
PBT is not typically specified for continuous immersion in hot water above 60 °C because ester hydrolysis accelerates rapidly above that threshold. The 30 wt% glass reinforcement does not eliminate hydrolysis; it mainly reduces the dimensional component of water uptake relative to glass-reinforced polyamide. Saturated moisture uptake in PA66-GF30 can reach 1.5% to 2.5% by mass, while PBT-based grades generally remain below 0.5%. For dry-heat exposure, continuous use of PBT GF30 FR is commonly limited to 130 °C, with intermittent excursions to 200 °C permitted only at low mechanical load. The flame-retardant package may be sensitive to strong bases, certain amine environments, and prolonged contact with aggressive lubricants or sealants. Chemical exposure should be screened under ISO 175:2010, and published data for this specific grade under combined chemical and thermal load is limited. Validation programs should include tensile retention after ageing at the upper use temperature and at the expected relative humidity of the application environment.
Electrical and electronic components produced from 4130-104F are often evaluated for flammability, tracking resistance, and water absorption. Table 2 summarises commonly reported electrical and conditioning parameters. The data are not substitutes for lot-specific certificates and should be verified against the actual colour and regrind level.
| Parameter | Test standard | Typical value/rating | Application note |
|---|---|---|---|
| UL 94 vertical burn classification | UL 94 | V-0 at 0.75 mm | Regrind and colour may affect rating |
| Comparative tracking index | IEC 60112:2003 | 250 V | Lower than unfilled PBT |
| Water absorption, 24 h at 23 °C | ISO 62:2008 | 0.05% | Dimensional baseline for humid storage |
| Heat deflection temperature at 1.8 MPa | ISO 75-2:2013 | 205 °C | Short-term thermal benchmark |
| Melt mass-flow rate at 250 °C, 2.16 kg | ISO 1133-1:2022 | approximately 15 g/10 min | Confirm against incoming QC lot |
The comparative tracking index of 250 V is a significant design boundary. Unfilled PBT frequently exhibits CTI values above 600 V, but flame-retardant additives can reduce resistance to tracking. When electrical spacing is based on CTI, the lower value must be incorporated into creepage and clearance calculations. The UL 94 V-0 classification at 0.75 mm is not automatically transferable to regrind-containing mouldings or to parts with weld lines, highly polished surfaces, or local glass-rich regions. Parts that require glow-wire resistance should be tested according to IEC 60695-2-12:2021 at the exact wall thickness used in production. Published data for this specific grade under glow-wire ignition temperature testing are limited; component-level validation is required.
The 4130-104F grade is not a direct substitute for unfilled PBT in snap-fit designs or for PA66-GF30 in moisture-sensitive applications. It is more correctly specified where the design envelope includes both a flammability requirement and a narrow post-mould tolerance. Typical application contexts include relay bases, circuit breaker housings, terminal blocks, appliance control connectors, and motor brush holders. In such components, wall thickness is often between 0.8 mm and 2.5 mm, and conformance to UL 94 V-0 at 0.75 mm is a mandatory design input. When dimensional stability is the primary driver but flammability is secondary, a non-FR PBT GF30 may offer slightly higher tensile strength and better tracking resistance but will not provide the same V-0 classification. Conversely, where flammability is the primary driver and stiffness can be reduced, a PBT GF15 FR grade may reduce density while still meeting V-0.
Tooling trials for connector housings indicate that gate location and packing time affect post-mould flatness more than minor barrel temperature variation. If flatness is evaluated after 24 h conditioning at 23 °C and 50% RH under ISO 291:2008, parts moulded with short pack time below gate seal are more likely to show warpage from anisotropic shrinkage. Closed-loop injection control with cavity pressure transducers is recommended for critical dimensions. Press selection should be based on melt pressure and projected area with a clamp-force safety margin of 15% to 20%. Incoming QC checks generally include density under ISO 1183-1:2019, melt flow under ISO 1133-1:2022, and ash content to confirm glass loading. Glass-fibre length after moulding is governed more by screw geometry and back pressure than by pellet glass content.
Storage of 4130-104F should be in moisture-resistant packaging, and material exposed to uncontrolled ambient air beyond 2 h should be re-dried before use. The grade is not suitable for continuous hot-water immersion, strong alkaline environments, or repeated steam sterilisation. For electrical components with closely spaced terminals, the reduced CTI relative to unfilled PBT must be incorporated into the electrical safety review. For load-bearing parts with snap-fit retention, the lower elongation at break must be addressed through hinge thinning and reduced deflection. For components exposed to automotive under-hood thermal cycling, dimensional change after cycling should be measured on production parts, not derived from dry-as-moulded laboratory specimens. These boundaries define the operational envelope more reliably than a single mechanical property value.