| HS Code | 444606 |
| Polymertype | PBT |
| Reinforcement | Glass fiber |
| Glassfibercontent | 15% |
| Flameretardancy | UL94 V-0 |
| Density | 1.55 g/cm³ |
| Tensilestrength | 90 MPa |
| Tensileelongationatbreak | 2.5% |
| Flexuralmodulus | 5500 MPa |
| Notchedizodimpactstrength | 5 kJ/m² |
| Heatdeflectiontemperatureat1 82mpa | 195 °C |
| Meltingpoint | 225 °C |
| Waterabsorption | 0.08% |
| Moldshrinkage | 0.4-0.8% |
| Dielectricstrength | 20 kV/mm |
| Volumeresistivity | 1E15 ohm·cm |
| Meltprocessingtemperature | 240-260 °C |
| Moldtemperature | 60-90 °C |
As an accredited Chang Chun LONGLITE® PBT+GF 4115-202FV factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chang Chun LONGLITE® PBT+GF 4115-202FV is supplied in 25 kg net moisture-resistant paper bags, palletized for storage. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Chang Chun LONGLITE® PBT+GF 4115-202FV, palletized 25 kg bags, securely stowed for ocean transport. |
| Shipping | Chang Chun LONGLITE® PBT+GF 4115-202FV is shipped as dry, moisture-sensitive thermoplastic pellets in sealed moisture-barrier bags, cartons, or bulk containers under ambient conditions. Protect from heat, sunlight, punctures, and contamination. For transport classification and any UN/hazard details, follow the current SDS; normally handled as a non-hazardous solid polymer. |
| Storage | Store Chang Chun LONGLITE® PBT+GF 4115-202FV in a cool, dry, well-ventilated area away from direct sunlight, heat, moisture, and ignition sources. Keep original containers tightly closed and palletized; protect from UV, dust, physical damage, and excessive stacking. Maintain stable temperature and humidity, practice first-in/first-out rotation, and avoid prolonged outdoor storage. Do not store near strong oxidizers or open flames. |
| Shelf Life | Shelf life is two years from manufacture when stored dry, cool, and in original sealed packaging. |
Photovoltaic combiner-box terminal carriers moulded from 15% glass-fibre-reinforced flame-retarded polybutylene terephthalate are governed by tracking resistance rather than short-term mechanical strength. The creepage and clearance framework of IEC 60664-1 requires a comparative tracking index measured per IEC 60112 of at least 400 V for uncoated surfaces in pollution degree 3, but certain flame-retardant packages in PBT-GF15 may depress the result to 250–300 V; qualification therefore requires a coating or ribbed barrier design. Moulded sections of 0.8 mm achieve UL 94 V-0 only if the cavity surface temperature is held at 65–80°C; lower temperatures produce a low-crystallinity skin that fails to form the required graphitic char. The material is pre-dried in a desiccant dryer to a residual moisture content below 0.02% by weight because ester linkages hydrolyze rapidly above 0.03% moisture at melt temperature. Injection moulding with a reciprocating screw of L/D 20:1, nozzle melt temperature of 250°C, and holding pressure of 700–900 bar is standard. Long-term xenon-arc weathering data for this specific product configuration is limited; outdoor deployment without a UV-stable coating is outside the documented operational boundary.
High-voltage battery management system connector housings impose simultaneous heat-aging, electrical tracking, and terminal retention loads. The UL Relative Thermal Index for reinforced flame-retarded PBT grades is commonly reported as 130°C electrical and 120°C mechanical; the yellow-card entry for the exact 4115-202FV designation should be consulted for thickness-dependent limits. Under 85°C/85% RH conditioning per IEC 60068-2-78, hydrolytic degradation reduces terminal retention force; if pellets are not dried below 0.02% residual moisture, insertion force retention can fall below 80 N after 1,000 h in a 0.8 mm boss. The processing window is constrained: melt temperature above 265°C at the nozzle causes decomposition of the flame-retardant package and acid-catalyzed matrix hydrolysis, while melt temperature below 245°C increases glass fibre orientation and short-shot frequency in thin snap-fit walls. A four-cavity connector tool with a projected area of 220 cm² requires approximately 160 t clamp force when filling at 1,000–1,200 bar injection pressure. Contact with amine-bearing sealants or alkaline battery electrolyte residues must be avoided because residual alkalinity accelerates ester bond cleavage in the moulded boss. The track and gap distances for 800 V DC systems should be verified under IEC 60664-1 pollution degree 2 with the actual CTI value of the production lot.
The glow-wire end-product test of IEC 60695-2-11 applies a 750°C tip to the finished carrier for 30 s. A flame-retarded PBT-GF15 moulded at 0.8 mm can pass the test if the cavity surface temperature remains uniform between 70°C and 80°C; cold spots below 60°C produce a resin-rich amorphous layer that may ignite and drip onto tissue paper, which is the ignition criterion of the standard. The glow-wire ignition temperature measured on a 1.0 mm plaque per IEC 60695-2-13 is typically reported in the range 775–850°C for reinforced flame-retarded PBT, but the end-product test is the governing requirement because geometry, ribs, and gate weld lines alter char-forming behaviour. The coefficient of linear thermal expansion measured per ISO 11359-2 is anisotropic, approximately 40×10⁻⁶ K⁻¹ along flow and 70×10⁻⁶ K⁻¹ transverse; a 150 mm carrier can distort by more than 0.2 mm between mould temperature and operating temperature if flow orientation is not balanced with multiple gates. The material should be pre-dried at 120°C for 4 h in a desiccant dryer with a -40°C dew point; leaving pellets open to 60% RH for 30 min can raise moisture content above 0.03%.
Compliance obligations across the downstream segments are consolidated below.
| Application segment | Governing standard | Test method or clause | Typical acceptance criterion |
|---|---|---|---|
| Photovoltaic combiner terminal carrier | IEC 60664-1 | IEC 60112 | CTI ≥ 400 V for pollution degree 3 |
| EV battery management system connector | IEC 60664-1 | IEC 60068-2-78 | Terminal retention after 85°C/85% RH, 1,000 h |
| Unattended appliance terminal carrier | IEC 60695-2-11 | 750°C glow-wire end-product test | No ignition of tissue paper within 30 s |
| Automotive relay base | ISO 16750-4 | Thermal cycling -40°C to 125°C | Terminal retention shift < 15% after 1,000 cycles |
| Power tool brush holder housing | IEC 62841-1 | ISO 179-1/1eA | Notched Charpy ≥ 3 kJ/m² after conditioning |
| Frequency-converter coil bobbin | IEC 61558-1 | ISO 294-4 | Flange flatness ≤ 0.05 mm total indicator reading |
Under engine-compartment temperature cycles from -40°C to 125°C per ISO 16750-4, relay bases moulded from the 15% glass-fibre PBT show less than 15% shift in terminal insertion force after 1,000 cycles when the terminal boss wall is 1.0 mm or greater and glass orientation is radial. The bosses are filled through a sub-gate from a cold runner; when the wall falls below 1.0 mm, the solidification front advances from the tool wall at approximately 0.8 mm/s at 70°C, and short-shot incidence rises sharply. Pre-drying at 120°C for 4 h to below 0.02% residual moisture is required before combining with silicone-based terminal grease; hydrocarbon greases are generally non-reactive. Continuous exposure to aqueous glycol coolants above 100°C is outside the operational boundary, because hydrolytic degradation lowers melt viscosity and produces surface blisters after approximately 500 h. The compound is not recommended for direct contact with strong alkaline engine degreasers without validation.
Brush holder housings in hand-held power tools operate at intermittent surface temperatures up to 160°C near the carbon brush seats. The housing enclosure requirements of IEC 62841-1 force the design to retain impact resistance after thermal ageing; a notched Charpy impact of 3–4 kJ/m² per ISO 179-1/1eA for GF15 flame-retarded PBT is lower than unreinforced PBT, so snap-fit arms and screw bosses must avoid weld lines. A single edge gate produces a weld line on the opposite side of the boss where tensile strength measured per ISO 527-2 can drop by more than 40% relative to the flow-parallel value. The brush pockets should be fed by a flash gate of 0.8 mm thickness on the rear face, producing radial orientation and reducing visible glass bundles on the seating surface. Injection speed of 60–100 mm/s, holding pressure of 700–900 bar, and screw back pressure of 50–80 bar are typical; back pressure above 100 bar increases shear heating and may expose the flame-retardant package to temperatures above 265°C in the metering zone.
Directly after moulding, coil bobbins for frequency-converter inductors must maintain flange flatness within 0.05 mm total indicator reading for automated winding at 12,000 rpm. The anisotropic shrink of 15% glass-fibre PBT is measured per ISO 294-4; typical values are 0.3% parallel to flow and 0.8% transverse, and uneven cooling across the flange increases dogleg warpage. A differential of 10°C between the fixed and moving tool halves adds approximately 0.03 mm of flange runout in a 60 mm flange, which is sufficient to cause winding tension variation. Mould designers specify a three-plate tool with a film gate around the core to distribute glass orientation and minimize weld-line exposure to the winding channel. Hot-runner manifolds should be held at 240–250°C with no stagnation zones; residence times above 5 min at 260°C produce brown streaking and a decline in UL 94 V-0 performance on thin bobbin flanges. Electrical safety compliance for reinforced insulation is evaluated under IEC 61558-1, with creepage distances maintained after winding and impregnation; the limiting property is generally the comparative tracking index rather than flammability.
Competitive Chang Chun LONGLITE® PBT+GF 4115-202FV prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Within the Chang Chun LONGLITE injection-molding portfolio, LONGLITE® PBT+GF 4115-202FV is a flame-retardant polybutylene terephthalate compound containing 15 wt% chopped glass fiber. The pelletized material is supplied for thin-wall electrical and electronic components in which UL 94 V-0 performance, moderate stiffness, and confined shrinkage are specified. The FV designation is associated with flame-retardant V-0 certification; the current supplier UL Yellow Card defines the certified wall thickness, color range, and minimum thickness. Typical published density is 1.52 g/cm³. Relative to unfilled PBT, the glass fiber raises flexural modulus from approximately 2.5 GPa to approximately 5.5 GPa, while reducing elongation at break to 2–3%. The material also shows higher heat deflection temperature, lower mold shrinkage, and increased melt viscosity.
Table 1 summarizes typical injection-molded specimen data reproduced from supplier technical literature and polymer databases. These values are not design maxima; weld lines, moisture absorption, regrind content, and fiber orientation will reduce molded-part performance.
| Property | Typical value | Test standard |
|---|---|---|
| Density | 1.52 g/cm³ | ISO 1183-1:2019 |
| Molding shrinkage, flow direction | 0.4–0.6% | ISO 294-4:2018 |
| Molding shrinkage, transverse direction | 0.8–1.1% | ISO 294-4:2018 |
| Tensile stress at break | 85 MPa | ISO 527-1/-2:2012 |
| Elongation at break | 2.5% | ISO 527-1/-2:2012 |
| Flexural modulus | 5.5 GPa | ISO 178:2019 |
| Flexural strength | 130 MPa | ISO 178:2019 |
| Charpy notched impact strength | 3.5 kJ/m² | ISO 179-1/1eA:2010 |
| Heat deflection temperature, HDT/A at 1.8 MPa | 205 °C | ISO 75-2:2013 |
| Comparative tracking index | 250 V | IEC 60112:2020 |
| Volume resistivity | 1.0E+15 Ω·m | IEC 62631-3-1 |
| Dielectric strength | 20 kV/mm | IEC 60243-1:2013 |
| UL 94 flammability | V-0 at 0.75 mm | UL 94 |
The comparative tracking index of 250 V places the grade in the IEC 60112 PLC category used for connector and relay barriers, although it is below the 600 V CTI values available in some halogen-free or mineral-filled grades. The dielectric strength of 20 kV/mm is typical for a 15% glass-fiber polyester measured on standard test plaques; parts with thinner walls, sharp electrodes, or internal voids will show lower values. HDT/A of 205 °C reflects the glass-fiber reinforcement and flame-retardant package rather than long-term chemical resistance at elevated temperatures. Density of 1.52 g/cm³ is higher than unfilled PBT at approximately 1.31 g/cm³ and lower than a typical 30% glass-fiber PBT at approximately 1.65 g/cm³.
For automotive and telecom connector bodies with wall thicknesses between 0.6 mm and 1.2 mm, the grade is processed on standard reciprocating-screw injection-molding machines. Hot-runner valve-gate tooling is preferred for multi-cavity molds because glass fibers can freeze at small edge gates and create surface streaking or gate blush. In relay bases, coil bobbins, and switch housings, the 15 wt% fiber loading reduces post-molding warpage relative to unfilled PBT when gates are placed away from thin-wall transitions. The compound is also used in connector bodies for appliance controls, industrial sensors, and motor brush holders, where V-0, rigidity, and electrical tracking resistance are evaluated under thermal cycling rather than raw-material datasheet values. For connector latch retention and terminal insertion force, published data for this specific configuration is limited; OEM validation procedures derived from USCAR-2 should be run on molded components rather than on standardized plaques. Terminal retention force is influenced by mold temperature and cooling rate; a shift from 60 °C to 100 °C mold temperature alters crystallinity and therefore extraction force. Batch-to-batch variation in glass fiber length distribution can shift flow length by 5–10%; incoming lot acceptance should include melt viscosity and fiber content checks.
PBT is highly sensitive to moisture-induced hydrolysis. Before molding, LONGLITE® PBT+GF 4115-202FV must be dried to residual moisture below 0.02 wt%. Supplier processing guidance specifies 4 h at 120 °C in a dehumidifying dryer with dew point ≤ −30 °C. Drying beyond 6 h at this temperature should be avoided because discoloration can occur. In production aisles above 60% relative humidity, exposed pellets can regain sufficient moisture within 30–40 min to produce silver streaks and reduced surface finish. The degradation mechanism is autocatalytic chain scission of the butylene terephthalate ester linkage, which lowers melt viscosity and weld-line strength.
Table 2 gives starting machine settings used on production equipment with a general-purpose screw.
| Processing parameter | Recommended starting range |
|---|---|
| Drying temperature | 120 °C |
| Drying time | 4 h |
| Dryer dew point | ≤ −30 °C |
| Melt temperature range | 250–270 °C |
| Mold temperature range | 60–100 °C |
| Barrel profile | rear 240–250 °C, center 250–260 °C, front 255–270 °C, nozzle 260–270 °C |
| Back pressure | 0.5–1.0 MPa |
| Holding pressure | 40–70 MPa |
| Injection speed | 100–200 mm/s |
| Screw L/D ratio | 18:1–22:1 |
| Compression ratio | 2.5:1 |
| Regrind content | maximum 20 wt% |
Equipment selection should account for glass fiber abrasion. Bimetallic barrel and screw flights are recommended for annual production volumes above 100,000 cycles. Back pressure above 1.0 MPa can raise melt temperature sufficiently to degrade the flame-retardant package, producing brown streaks and free carbon deposits. Injection speed should be medium-high to fill thin walls before freeze-off; screw forward speeds of 100–200 mm/s are typical starting points. Holding pressure must be optimized on the specific mold because excessive holding can increase parallel-shrinkage difference and stress concentration at the gate. A cushion of 3–6 mm should be maintained to prevent fiber separation and to sustain consistent packing. Running a hot-runner system with dead spots or sharp right-angle turns is not recommended for flame-retardant grades; additive decomposition products can accumulate in stagnant zones and later release as black specks. Externally heated manifolds with smooth transitions and no dead corners should be used.
Vent depth in the mold should be 0.01–0.02 mm; deeper vents can flash, shallower vents trap gas and cause burn marks. Cold-runner gate designs should avoid pinpoint gates smaller than 1.0 mm for glass-filled PBT because fiber accumulation can cause gate freeze-off and jetting. Tab, fan, or full-round gates are preferred. For thin-wall connectors, velocity-controlled fill is typically switched over at 95–98% fill volume to prevent flash and improve packing. If short shots occur in walls below 0.8 mm, raising mold temperature to 100 °C is more effective than increasing barrel temperature, which risks additive degradation. Regrind above 20 wt% can reduce tensile strength and invalidate UL 94 certification unless the part is requalified under production conditions.
Substitution of unfilled LONGLITE PBT with 4115-202FV changes both tool design and part performance. Unfilled PBT has a flexural modulus near 2.5 GPa and an HDT/A near 60 °C; the 15 wt% glass-fiber grade raises these to 5.5 GPa and 205 °C. The trade-off is lower elongation and increased notch sensitivity, particularly at sharp corners, weld lines, and molded-in inserts. Against a 30 wt% glass-fiber PBT, 4115-202FV has lower density, lower flexural modulus, and somewhat easier thin-wall flow, but less maximum stiffness and lower creep resistance. The 15% reinforcement also produces less tool wear than 30% reinforcement and can often be processed at lower barrel temperatures, reducing energy input and additive degradation risk.
End-use UL 94 V-0 certification is thickness-dependent and does not transfer automatically to thinner sections. A component molded at 0.5 mm may fail vertical burning even when the resin supplier’s Yellow Card lists V-0 at 0.75 mm. Conversely, thick sections do not require a separate lower-thickness certification, but electrical and mechanical relative thermal index values still depend on the thickness and formulation listed in the UL file. For parts thinner than the certified rating, additional end-use burning tests are required; the result can be influenced by color, aging, mold temperature, regrind content, and weld-line placement. The presence of glass fiber at 15 wt% can produce a wick effect that reduces droplet formation during burning but may also create surface roughness that alters flame spread. Published data for this specific configuration is limited below 0.75 mm; direct verification on the molded geometry is required.
For regulatory documentation, the compound is generally evaluated under the EU RoHS Directive 2011/65/EU recast and REACH Regulation 1907/2006. A UL Yellow Card is required for end-use UL 94 V-0 claims; certification is thickness-, color-, and grade-specific. Because flame-retardant PBT may contain halogenated additives, OEMs requiring IEC 61249-2-21 halogen-free limits must confirm halogen content separately. The published data for this specific configuration does not replace lot-level verification in safety-critical electrical insulation. For production-scale traceability, retain the supplier lot number, drying log, and the UL Yellow Card revision in the part qualification file.
Because the 15% fiber loading sits between unreinforced and 30% glass-filled PBT, it is selected when a balance of flow and stiffness is required. Shrinkage anisotropy is lower than with 30% reinforcement but higher than unfilled PBT; mold designers typically use parallel shrinkage of 0.4–0.6% and transverse shrinkage of 0.8–1.1%. Weld-line locations with 15% glass fiber may retain only 50–65% of the unfilled matrix tensile strength, so gates should be placed to move weld lines away from snap-fit retention features and terminal insertion regions. Compared with a flame-retardant unfilled PBT, the glass-filled grade improves load-bearing capability but reduces flow length; mold-filling simulation should be run with fiber orientation data rather than isotropic viscosity assumptions. Dimensional measurements after demolding should be conditioned according to ISO 291:2008 because post-molding crystallization can shift dimensions by 0.05–0.15% over several hours.
Storage life is limited by moisture absorption. Unopened sealed bags should be stored below 30 °C and used within 6 months; opened bags should be dried before use. The material is not recommended for continuous exposure to hot water, strong acids, or strong bases because hydrolytic degradation accelerates rapidly above 80 °C in wet environments. Avoid blending with amine-based additives or recycled polyamide, which can induce transesterification and viscosity drift. Purging after processing should use a mineral-filled or cast-acrylic purge compound; nylon-based purge compounds may cause ester–amide interchange. Weld-line strength, flame-retardant certification, and electrical tracking resistance are thickness-dependent; parts below the certified UL 94 wall thickness require additional end-use burning tests.