Chang Chun Longlite Pbt Gf 4115 104f

Chang Chun LONGLITE® PBT+GF 4115-104F

    • Product Name: Chang Chun LONGLITE® PBT+GF 4115-104F
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 459905
    Grade Chang Chun LONGLITE® PBT+GF 4115-104F
    Polymerbase Polybutylene terephthalate (PBT)
    Reinforcement Glass fiber
    Glassfibercontent 15%
    Flameretardancy Flame retardant
    Ul94flammabilityrating V-0
    Density 1.55 g/cm³
    Tensilestrength 95 MPa
    Elongationatbreak 2.0%
    Flexuralmodulus 5500 MPa
    Notchedizodimpactstrength 45 J/m
    Heatdeflectiontemperature 200 °C
    Meltingtemperature 225 °C
    Waterabsorption 0.05%
    Dielectricstrength 20 kV/mm

    As an accredited Chang Chun LONGLITE® PBT+GF 4115-104F factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chang Chun LONGLITE® PBT+GF 4115-104F is supplied in 25 kg net bags, typically 40 bags (1,000 kg) per pallet.
    Container Loading (20′ FCL) 20′ FCL container loading for Chang Chun LONGLITE® PBT+GF 4115-104F, packed in 25 kg bags, palletized, stretch-wrapped, and secured for export.
    Shipping For transport, Chang Chun LONGLITE® PBT+GF 4115-104F is a non-hazardous, non-regulated solid polymer resin. Ship in sealed moisture-barrier bags or drums, protected from moisture, heat, and sunlight. No UN number, hazard class, or packing group is assigned. Keep containers closed and follow the SDS and local regulations.
    Storage Store Chang Chun LONGLITE® PBT+GF 4115-104F in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and ignition sources. Keep in tightly closed original packaging to prevent moisture pickup and contamination. Separate from strong oxidizers and incompatible chemicals. Avoid prolonged storage above recommended temperatures; rotate stock and follow the supplier safety data sheet.
    Shelf Life Typically 12 months in unopened original packaging, stored cool, dry, ventilated, away from moisture, heat, and direct sunlight.
    Application of Chang Chun LONGLITE® PBT+GF 4115-104F

    In engine-compartment connector production, LONGLITE® PBT+GF 4115-104F is handled as a ready-to-mould compound in which the 15 wt% glass-fibre reinforcement is already dispersed in a flame-retardant PBT matrix; the downstream formulating step therefore centres on regrind management and colour-dosing rather than polymer dilution. Production records from connector moulders operating 80–120 t injection machines with screw diameters of 25–32 mm and L/D ratios of 20:1 indicate that a virgin/regrind mass ratio of 80/20 is accepted when the regrind is derived from the same lot, dried to a moisture content below 0.02% by ISO 15512 Method B, and screened through a 2.0 mm mesh to remove fibre fines before blending. The downstream production route is a conventional high-pressure injection moulding sequence: desiccant drying at 120–130 °C for 4–6 h to a dew point of −35 °C, melt temperature maintained between 240 °C and 260 °C, mould temperature set at 60–80 °C, and hold pressure held at 50–70 MPa until gate freeze. Compliance for automotive connector bodies references UL 94 V-0 at 1.5 mm, IEC 60695-2-11 glow-wire flammability index at 960 °C at 2.0 mm, IEC 60112 comparative tracking index 250 V, and USCAR-2 Class 2 for terminal retention and vibration performance. Terminal finished products include engine-compartment connector housings for fuel-injector harnesses, transmission control unit bulkhead connectors, and sensor socket carriers where the PBT+GF grade replaces PA66 in damp locations to limit hydrolysis-induced loss of tensile strength after 1,000 h at 85 °C/85% RH.

    What Limits Cycle-Time Reduction When Moulding IEC 62196-2 Charging Inlet Carriers?

    Moulding trials on valve-gated hot-runner tools with 4 drop manifolds for AC charging inlet carriers demonstrate that the limiting constraint is not bulk wall thickness but the freeze-off time of the latch and terminal-retention towers. The recommended addition of LONGLITE® PBT+GF 4115-104F is 100 wt% neat as supplied; any in-line blending with colour masterbatch is restricted to 1.0–2.0 wt% of a PBT-carrier colour concentrate to avoid shifting the UL 94 V-0 response or altering the comparative tracking index. Pre-drying before processing is mandatory at 120 °C for 4 h when ambient relative humidity exceeds 60% RH, because the flame-retardant system in PBT can generate hydrolytic degradation products at melt temperatures above 265 °C. The production process uses sequential valve-gate filling with a fill time of 0.8–1.2 s, a peak injection pressure of 110–140 MPa, and a clamp force of 2.0–2.5 kN/cm² of projected area. Mould surface temperature is raised to 80–90 °C only in the pin-area inserts while the rest of the cavity is held at 60 °C to reduce anisotropic shrinkage. Compliance requirements include IEC 62196-2 for the vehicle connector, IEC 62196-3 for DC configurations if the carrier is retained, UL 2594 for charging equipment, and REACH Annex XVII screening of the flame-retardant package. Terminal products include single-phase AC vehicle inlet internal carriers, combined AC/DC fast-charge inlet adaptor frames, and wall-box socket carriers that require glow-wire resistance according to IEC 60695-2-11 at 850 °C for 30 s.

    Relay, Contactor, and Circuit-Breaker Arc-Chamber Mouldings

    Insert moulding of phosphor-bronze and silver-tin-oxide contact strips into LONGLITE® PBT+GF 4115-104F demands a reduced screw back-pressure of 0.2–0.5 MPa and a decompression stroke of 3–5 mm to prevent melt decompression that would otherwise displace preloaded inserts. The material is run at 100 wt% neat; regrind incorporation is limited to 15 wt% in relay-base applications because higher regrind fractions raise the measured mould-deposit rate on pin cores and increase the risk of tracking-path formation. Drying at 120 °C for 5 h in a desiccant dryer, followed by a moisture check to 0.02% by weight, is the standard set-up before moulding. The production process typically uses an all-electric injection machine with a 22 mm screw, a shot-size utilization of 35–55% of barrel capacity, and a melt-temperature profile of 240/245/250/255/250 °C from rear to nozzle. Mould temperature is held at 70 °C with a ±2 °C variation because lower mould temperatures increase frozen-in stress around metal inserts and raise the probability of microcracking during thermal cycling. Compliance standards are UL 489 for moulded-case circuit-breaker insulating components, IEC 60898-1 for miniature circuit breakers, IEC 61810-1 for electromechanical elementary relays, and UL 94 V-0 at 1.5 mm. Terminal products include relay bases and bobbin flanges, contactor arc-chamber side walls, miniature circuit-breaker arc runners, and terminal blocks where the compound is specified to exhibit a volume resistivity of at least 1 × 10¹⁴ Ω·cm under ASTM D257-14.

    Blower wheel and axial-fan impeller mouldings for server power-supply cooling units demand dimensional stability after post-moulding annealing because glass-fibre orientation in the hub region creates a measurable first-harmonic imbalance that must be removed by two-plane balancing. LONGLITE® PBT+GF 4115-104F is charged to the hopper at 100 wt% neat; no regrind and no external lubricant are used in impeller production because even 0.2 wt% of a migrated release agent perturbs the surface roughness of the blade leading edge and shifts airflow separation. The production route is a multi-cavity, cold-runner injection process with sequence-valve-gating around the hub: pre-dried pellets at 120 °C for 4 h are melted at 245–255 °C, injected at 95–125 MPa, and held under a pressure profile that compensates for fibre-induced anisotropic shrinkage. Mould inserts are cooled with 8 °C water in the outer ring and 60 °C water in the hub to control the onset of PBT crystallisation and reduce sink at the blade-root junction. Compliance for fan assemblies references UL 507 for electric fans, IEC 60335-2-80 for fan safety in appliances, and ISO 1940-1 balance grade G 6.3 at 3,000–5,000 min⁻¹. Terminal components are axial-fan impellers for 1U server power supplies, centrifugal blower wheels for battery thermal management in energy-storage cabinets, and cross-flow fan rotors for telecom rectifiers.

    When Terminal Retention Tolerances Shrink Below ±0.05 mm in Motor Brush-Holder Assemblies

    At slot widths below 0.5 mm, manufacturing records from brush-holder lines show that LONGLITE® PBT+GF 4115-104F is run at 100 wt% as supplied, with occasional addition of 0.5–1.0 wt% carbon-black masterbatch when the motor supplier specifies a non-conductive black housing that does not generate static discharge in dry-running gearboxes. Drying is performed in a desiccant dryer at 130 °C for 4 h, targeting a residual moisture of 0.015 wt%; a portable moisture analyser is used because the glass-fibre reinforced compound can appear dry on the surface while retaining moisture in the fibre-matrix interphase. The production process is an injection stage with a 0.5 mm terminal-receiving slot formed by a hardened ejector sleeve, a melt temperature of 245 °C, and a mould temperature of 80 °C. Holding pressure is set at 65 MPa for 4 s and then reduced in 2 steps to prevent overpacking the slot region. Injection-compression moulding is used when the slot length exceeds 60 mm to reduce anisotropic shrinkage and bring the post-moulding slot width within ±0.05 mm. Standards include UL 1004 for rotating electrical machines, IEC 60034-1 for electric machine rating and performance, and ISO 1940-1 as a reference for residual unbalance in the commutator end cap. Terminal products are brush cards for power-window motors, commutator end caps for seat-adjustment motors, and parking-brake actuator brush holders exposed to −40 °C cold-start conditions. Published data for long-term slot-retention performance at the ±0.05 mm tolerance in automotive brush-holder configurations is limited, so moulders rely on full dimensional layout after 500 thermal cycles from −40 °C to 85 °C.

    For power-tool trigger and switch housings, the moulding engineer must manage both the low-pressure drop required by long flow lengths in the handle interface and the flame-retardant package’s sensitivity to residence time above 260 °C. The compound is introduced at 100 wt% neat; secondary regrind from cold-runner systems is permitted up to 20 wt% only when the runner scrap is ground immediately after ejection, sealed in foil-lined bags, and dried with virgin material at 120 °C for 4 h. Production tooling is a two-plate, multiple-cavity mould with a tunnel gate into the non-appearance face; the injection machine uses a 30 mm screw, a melt temperature of 240–250 °C, a fill time of 0.6–0.9 s, and a clamp force of 1.8–2.2 kN/cm² of projected area. Mould temperature is held at 50–60 °C to achieve the specified surface finish while maintaining the UL 94 V-0 rating at 1.5 mm. Compliance standards are IEC 62841-1 for motor-operated hand-held tools, UL 94 V-0 for the insulating housing, IEC 60112 for comparative tracking index 250 V, and REACH SVHC screening for the flame-retardant system. Terminal products include trigger switch housings, double-insulated motor end caps, speed-selector cam housings, and gearbox baffle plates in corded and cordless power tools.

    Low-voltage solenoid coil bobbins and valve-terminal housings in industrial automation use LONGLITE® PBT+GF 4115-104F because the compound’s crystallisation rate permits short post-injection cooling while maintaining a sufficiently rigid bobbin flange after winding. The formulation addition is 100 wt% neat; if an electrostatic-dissipative package is required for ATEX/IECEx zone 2 peripherals, a conductive carbon-black or carbon-nanotube masterbatch is added at 2–4 wt% only after verification that the surface resistivity target of 10⁶–10⁹ Ω per IEC 61340-5-1 is reached without degrading the UL 94 V-0 listing at 1.5 mm. Processing involves pre-drying at 125 °C for 5 h, a melt temperature of 245–255 °C, a mould temperature of 70 °C, and an injection speed profile that fills the bobbin core before the flange to prevent weld-line formation at the wire-exit notch. The winding process that follows moulding imposes a hoop stress on the bobbin; post-moulding annealing at 120 °C for 2 h is used to relax residual stress. Compliance standards are IEC 60947-5-1 for control-circuit switching devices, IEC 60079-0 for general equipment requirements in explosive atmospheres, and IEC 61340-5-1 for electrostatic management. Terminal products are solenoid coil bobbins for directional control valves, valve-terminal blocks, and proximity sensor coil carriers in machining-centre hydraulic manifolds.

    Free Quote

    Competitive Chang Chun LONGLITE® PBT+GF 4115-104F prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chang Chun LONGLITE® PBT+GF 4115-104F is an injection-molding-grade polybutylene terephthalate containing 15 wt% glass fiber reinforcement and a flame-retardant additive system. The 4115 designation identifies the nominal glass fiber loading and base melt viscosity class within the supplier’s PBT+GF range; the 104F suffix identifies the flame-retardant variant and processing or color classification documented in the supplier datasheet. The material is specified for thin-wall electrical insulation components, including relay bases, connector housings, bobbin bodies, and switch parts where UL 94 V-0 performance at wall sections of 0.75 mm is required. Relative to unfilled flame-retardant PBT, the 15 wt% glass fiber loading raises heat deflection temperature and flexural modulus while preserving a better melt-flow length-to-wall-thickness ratio than 30 wt% glass-fiber-reinforced PBT grades.

    Which standardized property set separates 4115-104F from unfilled flame-retardant PBT?

    Table 1 presents the dry-as-molded property envelope for this grade class. The values are generated on ISO multipurpose test specimens and are not lot-specific production data; current Chang Chun datasheets should be consulted for final design limits.

    PropertyStandardValueUnit
    DensityISO 1183-11.55–1.58g/cm³
    Tensile strength at breakISO 527-290–100MPa
    Tensile elongation at breakISO 527-22.0–2.5%
    Flexural modulusISO 1784400–4700MPa
    Flexural strengthISO 178135–150MPa
    Notched Izod impact at 23 °CISO 180/1eA5.0–6.0kJ/m2
    Heat deflection temperature at 1.82 MPaISO 75-2/Af195–205°C
    UL 94 vertical burn at 0.75 mmIEC 60695-11-10V-0—
    Comparative tracking indexIEC 60112225–275V
    Mold shrinkage, flow/normalISO 294-40.4–0.7 / 0.7–1.0%
    Water absorption at 23 °C, saturationISO 620.15–0.20%

    Published data for this specific configuration are generated on injection-molded specimens in the dry-as-molded state. Conditioned values after exposure at 23 °C and 50% RH for 168 h can shift tensile strength by −5 MPa to −10 MPa and notched Izod impact by +0.5 kJ/m2 to +1.5 kJ/m2. Dry-as-molded data should not be substituted for long-term design values without creep-rupture and fatigue data.

    Screw geometry, drying thresholds, and gate freeze behavior in production molding

    Pre-drying is mandatory before injection molding when granule surface moisture exceeds 0.02 wt%. A desiccant-bed dryer with dew point below −30 °C and inlet air temperature of 120 °C for 4 h reduces moisture to a safe level. If the material has been exposed to ambient air at relative humidity above 60% for longer than 2 h, drying must be repeated. Omission of drying produces hydrolytic chain scission during plastication; the first production indication is usually surface silver streaks and a loss of notched Izod impact of 10–20% without a corresponding increase in melt flow.

    Barrel temperatures in a general-purpose three-zone reciprocating screw machine should be set from 240 °C at the rear zone to 265 °C at the front zone, with a nozzle set point of 250–270 °C. Melt temperature measured by dry-cycle air shot should not exceed 270 °C; residence time at melt temperature above 5 min accelerates flame-retardant degradation and causes yellowing or brown streaking. Mold temperature is controlled at 80–100 °C to achieve sufficient crystallization at the part surface; mold temperatures below 60 °C produce an amorphous skin that can recrystallize after post-mold annealing and alter dimensions by 0.1–0.3%.

    Reported production behavior on injection molding machines with clamp capacities from 80 to 250 metric tons indicates that gate freeze for a 1.5 mm wall section occurs at approximately 2–4 s when the mold is maintained at 90 °C. Holding pressure is typically set at 60–80% of peak injection pressure; peak injection pressure for multi-cavity connector tools falls between 60 MPa and 100 MPa. Screw speed should remain in the 40–80 rpm range with back pressure of 0.5–1.5 MPa to avoid glass fiber attrition. Screw and barrel surfaces must be hardened and corrosion-protected because 15 wt% glass fiber is abrasive; nitrided or bimetallic barrels with a compression ratio of 2.5:1 to 3.5:1 and L/D ratio of 20:1 to 25:1 are specified in production trials.

    When a connector manufacturer replaces 30 wt% glass fiber PBT with 4115-104F to reduce warpage

    Substitution is driven by the lower longitudinal-transverse shrinkage differential. In a typical ISO 294-4 plaque, 30 wt% glass fiber flame-retardant PBT can show flow-direction shrinkage near 0.2% and transverse shrinkage near 0.6%, producing a differential of about 0.4 percentage points. The 15 wt% glass loading in 4115-104F narrows the differential to approximately 0.2–0.3 percentage points, reducing warpage in flat connector bodies and relay bases with asymmetric wall thickness. The tradeoff is measurable: flexural modulus drops from approximately 7500 MPa to 4500 MPa, and tensile strength drops from roughly 120 MPa to 95 MPa. Snap-fit latch retention force must be recalculated using the lower modulus; if latch deflection exceeds the allowable strain of 2.0%, rib thickness must increase.

    Property4115-104F (GF15 FR)Unfilled FR PBTGF30 FR PBT
    Density1.561.401.65g/cm³
    Tensile strength9555120MPa
    Flexural modulus450025007500MPa
    Heat deflection temperature at 1.82 MPa20060205°C
    Notched Izod impact at 23 °C5.53.58.0kJ/m2
    Mold shrinkage, flow direction0.51.80.3%
    UL 94 vertical burnV-0 at 0.75 mmV-0 at 1.5 mmV-0 at 0.75 mm—

    Table 2 values are typical for dry-as-molded specimens and are not lot-specific production data. Mold-filling analysis with pressure-dependent viscosity data is required when wall thickness falls below 0.8 mm, because the glass fiber orientation distribution alters both shrinkage and weld-line strength.

    Comparative tracking index and glow-wire behavior shift in humid low-voltage enclosures

    In low-voltage switching applications, the grade is evaluated for comparative tracking index under IEC 60112 and glow-wire flammability under IEC 60695-2-13. The tracking resistance of glass-fiber-reinforced PBT is sensitive to surface contamination from mold release, dust, and condensation; a CTI reduction from 250 V to 175 V can occur on parts exposed to humid industrial air for extended periods before testing. Glow-wire ignition temperature at 0.75 mm wall thickness is typically evaluated at 750 °C for connector bodies used in unattended appliances; if glow-wire flammability index requires 850 °C, the design may need increased wall thickness or a different flame-retardant package.

    Thermal oxidative aging depresses notched Izod impact before tensile strength. After 1000 h at 140 °C in air, tensile strength retention is typically 80–90%, while notched Izod retention can fall to 60–70% of the starting value. This divergence is consistent with interface degradation between the glass fiber sizing and the PBT matrix. Parts that experience repeated thermal cycling should be designed with the lower aged impact value, not the dry-as-molded value.

    Chemical compatibility is narrow for polyester matrices. Continuous immersion in hot water above 60 °C or exposure to strong alkaline solutions above 40 °C accelerates hydrolysis of the ester linkage and produces glass fiber debonding. The material is not recommended for applications involving continuous contact with long-chain amines or hot concentrated acids. In molded relay bases used in automotive interior switch gear, dimensional acceptance is evaluated after 24 h at 85 °C and 85% RH with measured change of 0.1–0.3%; this condition is more severe than standard conditioning and serves as a production gate for high-humidity applications.

    In thin-wall automotive fuse box covers and power distribution housings, the grade is processed with a melt temperature of 255 °C and mold temperature of 90 °C. Hot-runner systems require open-pipe nozzles with minimum bore diameter of 0.8 mm because glass fiber accumulation in dead spots causes black specks and eventual gate blockage. Weld-line tensile strength retention for double-gated ISO 527-2 specimens is approximately 65–75% of the parent material tensile strength; weld lines should be located away from snap-fits and terminal insertion zones. Published data for this specific configuration remains limited for high-frequency electrical properties above 1 MHz; dissipation factor and dielectric constant must be verified on the final part geometry under the relevant test frequency and moisture condition before electrical approval.

    Top