Chang Chun Longlite Pbt Fr 2100 202b

Chang Chun LONGLITE® PBT-FR 2100-202B

    • Product Name: Chang Chun LONGLITE® PBT-FR 2100-202B
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 616775
    Basepolymer Polybutylene terephthalate (PBT)
    Flameretardant Yes
    Density approx. 1.50-1.55 g/cm³
    Meltflowrate approx. 10-20 g/10 min
    Moldingshrinkage approx. 0.2-0.8%
    Waterabsorption approx. 0.02%
    Tensilestrength approx. 70-100 MPa
    Elongationatbreak approx. 2-4%
    Flexuralmodulus approx. 4-7 GPa
    Notchedizodimpactstrength approx. 5-7 kJ/m²
    Heatdeflectiontemperature approx. 150-200°C at 1.82 MPa
    Ul94flamerating V-0
    Dielectricstrength approx. 20 kV/mm
    Volumeresistivity approx. 1E15 Ω·cm
    Comparativetrackingindex approx. 250-600 V

    As an accredited Chang Chun LONGLITE® PBT-FR 2100-202B factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg net moisture-proof paper bags, typically palletized, containing flame-retardant PBT resin pellets.
    Container Loading (20′ FCL) 20-foot FCL container loaded with Chang Chun LONGLITE® PBT-FR 2100-202B in 25 kg bags, palletized and secured for safe transport.
    Shipping Ship Chang Chun LONGLITE® PBT-FR 2100-202B as a non-dangerous, flame-retardant PBT molding compound in sealed moisture-barrier bags or drums. Keep dry, cool, and protected from sunlight; avoid damaged packaging. Follow the SDS, carrier requirements, and local transport regulations.
    Storage Store Chang Chun LONGLITE® PBT-FR 2100-202B in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, moisture, and ignition sources. Keep original containers tightly closed and avoid contamination with dust, water, or incompatible chemicals. Use first-in, first-out rotation, store off the floor and away from walls, protect from physical damage, maintain clear labels, and follow local regulations and SDS recommendations.
    Shelf Life Shelf life is typically two years when stored dry in sealed original packaging, away from sunlight and heat.
    Application of Chang Chun LONGLITE® PBT-FR 2100-202B

    For automotive underhood connector programmes, Chang Chun LONGLITE® PBT-FR 2100-202B is specified where the moulded part must combine UL 94 V-0 performance at 0.8 mm wall thickness, short-term thermal spike resistance, and reproducible pin retention. Tooling is typically a 24- to 32-cavity hot-runner mould with valve gates on the connector face; melt temperature is maintained at 250–260°C, and the tool surface is held at 60–80°C to balance crystallisation rate against cycle time. Pellets are dried in a dehumidifying hopper dryer with a dew point below -30°C to reach 0.02% moisture content by Karl Fischer titration; higher residual moisture hydrolyses the polybutylene terephthalate backbone and produces gas splay behind the locking lance. Hot-runner sprues are ground and re-introduced at 10–15 wt%, but for connector walls below 1.0 mm the recyclate fraction is held at 10 wt% because higher regrind levels increase filling-pressure scatter and reduce impact resistance measured under ISO 179-1. Injection speed is set between 300 mm/s and 450 mm/s for thin-wall filling; speeds above 450 mm/s generate shear heating above 280°C near the gate land, producing brown streaking and contact pin adhesion failure. Compliance is verified under USCAR-2 thermal cycling and vibration sequences, with connector housing cracks and terminal retention checked after -40°C/150°C shock in automotive harness builds. Finished parts include engine control unit connectors, body-harness connectors, and bulkhead pass-through housings.

    What Limits Continuous Operating Temperature in Relay Housings?

    The continuous operating temperature of relay housings moulded from PBT-FR 2100-202B is limited less by gross melting than by two slower degradation paths: volatilisation of the flame-retardant package into the contact zone and progressive tensile strength loss at terminal staking points. Power relay bases and coil formers are manufactured in multi-cavity tools where melt residence time must not exceed 5 min at 250°C; longer residence increases the concentration of low-molecular-weight condensate on the cavity surface and raises contact resistance drift. When ejection from the coil former requires external lubrication, a silicone-based release agent is added at 0.1 wt%; higher levels reduce comparative tracking index under IEC 60112 and create adhesion failure on printed circuit board terminal coatings. Regrind from rejected coil bobbins is limited to 10 wt% because repeated heat cycles lower the elongation at break measured under ISO 527-2 and create a brittle fracture risk during terminal insertion. Continuous-use temperatures are validated against IEC 61810-1 for electromechanical elementary relays, with high-temperature soak at 130°C used to measure contact resistance stability. The material is incompatible with relay designs that require long-term exposure above 150°C in sealed enclosures unless the relay manufacturer specifically accepts contact contamination from the flame-retardant system. Terminal products include automotive relay coil formers, power relay bases, and miniature PCB relay housings.

    In capacitor enclosures for appliance power boards, the material is selected when the housing must pass UL 94 V-0 at 0.8 mm, resist 850°C glow-wire ignition under IEC 60695-2-11, and maintain insulation resistance after damp-heat exposure. Insert-bearing designs with brass terminals are moulded at melt temperatures of 245–255°C and tool temperatures of 70–80°C to reduce post-mould voiding around the insert. Because wave-soldering exposes capacitor housings to 260°C for 3–5 s, the grade must be moulded at low moisture levels—0.02% maximum as measured by Karl Fischer titration—to prevent blistering at terminal bosses. The regrind fraction is restricted to 10 wt% and only from non-plated reject parts; metal-contaminated sprues from insert moulding are excluded to avoid dielectric breakdown paths. Insulation resistance is tested under IEC 60384-1 and voltage withstand under IEC 60243-1 after 48 h at 50°C/93% RH to bound end-use performance. This application includes washing-machine inverter capacitor housings, refrigerator compressor drive capacitor cans, and electronic ballast capacitor shells.

    When E-Mobility Charging Couplers Replace PBT/ASA Blends in Outdoor Enclosures

    When AC charging couplers replace PBT/ASA blends in outdoor enclosures, qualification must include ultraviolet exposure, hydrolytic stability, and tracking-index retention, because flame retardance alone does not cover degradation caused by condensation and sunlight. Coupler shells with insert-moulded pilot pins are run on hydraulically clamped injection machines with clamp force calculated at 0.5–0.6 t/cm² of projected area; melt temperature is set at 250–260°C and mould temperature at 70–80°C to control shrink around the pilot-pin boss. Weld lines are generated where melt fronts recombine around the pin; injection speed must be ramped before the weld location to maintain at least 70–80% of virgin tensile elongation under ISO 527-2. Regrind from outdoor-exposed runner systems is capped at 10 wt% because previous heat history accelerates crystallisation and increases surface chalking. Published UV ageing data for this specific black configuration under ISO 4892-2 is limited; pre-qualification at the application-specific UV dose is required before committing to exposed charging pistols. Damp-heat performance at 85°C/85% RH is inherently limited by PBT hydrolysis, so housing designs should include drainage paths rather than sealing moisture against the polymer. Compliance is verified under IEC 62196-1 for vehicle conductive charging systems and UL 2251 for plugs, receptacles, and couplers. Terminal products include AC charging plug shells, control pilot connector housings, and vehicle inlet housings.

    ApplicationPrimary standardCritical test conditionValidation output
    Automotive underhood connectorsUSCAR-2 / ISO 20860thermal shock -40°C/150°Cno housing crack, terminal retention
    Relay housingsIEC 61810-1soak 130°Ccontact resistance drift within supplier limit
    Capacitor enclosuresIEC 60384-1 / IEC 60695-2-11glow wire 850°Cno ignition
    EV charging couplersIEC 62196-1 / UL 2251weathering and dielectric withstandpass application-specific UV dose
    PV junction boxesIEC 62790 / UL 373glow wire per IEC 60695-2-11no ignition, CTI retained
    Miniature circuit breaker housingsIEC 60898-1 / IEC 60947-2glow wire per product standardno sustained flame

    Glow-Wire and Hot-Wire Ignition Testing for Photovoltaic Junction Box Interiors

    Glow-wire and hot-wire ignition testing for photovoltaic junction box interiors subjects the material to sustained heat from bypass diodes and high-current busbars while requiring outdoor service life. Junction box bases and lids are injection-moulded with wall thickness 1.2–2.0 mm around cable glands, using melt temperatures of 245–255°C to avoid premature volatilisation of the flame-retardant package. Mould temperature is set at 70–80°C; after demoulding, bases are placed on vacuum cooling fixtures for 30–60 s to prevent warp that would open the lid seal. The regrind fraction is limited to 10–15 wt% and only from uncontaminated post-industrial runner material from the same lot, because mixed virgin/reprocessed material creates visible knit lines and reduces tracking resistance under IEC 60112. Compliance is tested under IEC 62790 for junction boxes for photovoltaic modules and UL 373 for photovoltaic junction boxes; glow-wire conditions follow IEC 60695-2-11 with severity selected by product standard. Because PBT absorbs moisture, boxes assembled in humid environments are pre-dried at 80°C for 2–4 h before potting to prevent interface blistering around the polyurethane encapsulant. Terminal products include PV module junction boxes, diode housings, and combiner box interiors.

    In miniature circuit breaker housings, PBT-FR 2100-202B is used where the arc-quenching chambers require controlled melt front progression through 1.0–1.5 mm walls around the fixed and moving contact pins. Material preparation uses dehumidifying dryers at 120°C to reach 0.02% moisture; moulding is carried out at melt temperatures of 250–260°C and tool temperatures of 70–80°C. Flow is deliberately staged with low initial injection speed to prevent jetting and weld-line formation at the arc splitter plates; after flow fronts rejoin, velocity is increased to pack the narrow arc chamber ribs. Regrind is held below 15 wt% and must be free of metal shavings from secondary machining operations because conductive contaminants reduce dielectric strength under IEC 60243-1. Tracking resistance is verified under IEC 60112, and glow-wire performance is tested under IEC 60695-2-11 at the severity referenced by IEC 60898-1 for household circuit-breakers or IEC 60947-2 for industrial switchgear. Finished parts include miniature circuit breaker housings, residual current device bases, and switch disconnector covers.

    Free Quote

    Competitive Chang Chun LONGLITE® PBT-FR 2100-202B prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chang Chun LONGLITE® PBT-FR 2100-202B is a flame-retardant polybutylene terephthalate injection-moulding compound specified for thin-wall electrical connectors, relay bases, circuit-breaker internal frames, and power-distribution housings where self-extinguishing behaviour under vertical burn conditions is the decisive acceptance criterion. The material belongs to the unreinforced PBT-FR classification; published class values for density fall between 1.44–1.46 g/cm³ when measured according to ISO 1183-1, and typical tensile stress at break ranges from 50–60 MPa under ISO 527-2 at 5 mm/min. Grade-specific values for the 2100-202B designation must be extracted from the current manufacturer’s UL yellow card and technical datasheet because additive package, colour concentrate, and regrind fraction can shift mechanical and flammability results. The compound is not a general-purpose polybutylene terephthalate; the flame-retardant package alters crystallisation rate, melt viscosity, and post-moulding shrinkage relative to unfilled non-FR PBT.

    Flame-Retardant Classification Under UL 94 Vertical Burn Protocol

    UL 94 V-0 classification for LONGLITE® PBT-FR 2100-202B is assessed using bar specimens of 125±5 mm length and 13±0.5 mm width, conditioned for 48 h at 23°C and 50% RH before two consecutive 10 s flame applications with a 50 W methane burner. The V-0 requirement permits no single afterflame time greater than 10 s, a total afterflame time no greater than 50 s across ten flame applications, and no cotton-indicator ignition from flaming drips. The grade is typically certified at 0.75 mm or 1.5 mm depending on the colour masterbatch and regrind content; wall thickness below the certified rating must not be inferred from thicker-section data. The flame-retardant mechanism in this compound operates through condensed-phase char promotion and gas-phase radical trapping, which suppresses dripping and reduces heat release. Because char formation competes with thermoplastic flow, the additive package shifts the melt solidification front slightly outward compared with non-FR PBT, and tool shrinkage factors derived from unfilled PBT should be corrected using ISO 294-4 shrinkage measurements on the actual compound.

    Moisture control is the first processing boundary for PBT-FR 2100-202B. Polybutylene terephthalate undergoes hydrolytic chain scission above the glass transition temperature when moisture exceeds <0.02% by weight. Pre-drying in a desiccant dryer is required at 120°C for 4–6 h, with a hopper-air dew point no higher than −30°C. Hopper residence time should not exceed 8 h at temperature because prolonged heat exposure can oxidise the flame-retardant package and darken the melt. On production-scale injection lines with heated hopper loaders, moisture breakthrough is frequently detected as splay on gate lands, reduced notched impact, and a downward shift in tensile stress at break. When ambient relative humidity exceeds 60% RH, desiccant beds should be regenerated more frequently and moisture analysis should be performed on granulate taken directly from the machine throat rather than from sealed bags.

    What Limits Regrind Ratio in Thin-Wall Electrical Housings?

    The regrind fraction in LONGLITE® PBT-FR 2100-202B is limited by thermal and hydrolytic degradation accumulated during multiple melting cycles. In thin-wall connector mouldings with wall sections between 0.4 mm and 1.0 mm, the recommended regrind addition is kept at or below 20% unless the specific UL 94 listing permits a higher fraction. Recycled granulate produced with a screen diameter of 4–6 mm is preferred because larger regrind particles create melt-temperature heterogeneity and can produce unmelted agglomerates in small shot sizes. The first consequence of regrind elevation is a reduction in notched impact; ISO 180/A values can fall by several kilojoules per square metre after three processing passes. The second consequence is a change in flammability response, because degraded flame-retardant additive disperses unevenly and char formation becomes less reproducible. Moulders producing circuit-breaker housings often maintain first-generation regrind segregated from mixed-colour post-industrial scrap because pigmented regrind alters the quench rate and can move the UL 94 rating from V-0 to V-1 at identical wall thickness.

    Injection-moulding conditions for the compound should follow a rising barrel-temperature gradient to limit residence time in the rear feed zone. A typical profile is 240/250/260/260°C from feed to nozzle, with nozzle temperature held at 250–260°C and mould temperature controlled between 60°C and 90°C. Screw L/D ratio should be at least 20:1, with a compression ratio of 2.5:1 to 3.0:1. Back pressure of 5–10 bar hydraulic is used to improve melt homogenisation without excessive shear heating. Melt temperature must not exceed 270°C because the flame-retardant system begins to evolve corrosive acidic volatiles at higher temperatures, and barrel residence time should be kept below 10 min. Injection speed is set according to flow-length-to-wall-thickness ratio; for thin-wall connectors, filling speeds sufficient to prevent premature freeze-off are required, but excessive shear can raise local melt temperature at the gate above the degradation threshold.

    Electrical property requirements for power-distribution applications are evaluated using comparative tracking index and dielectric strength protocols. The flame-retardant additive can reduce comparative tracking index relative to unfilled PBT; compliance is therefore verified per IEC 60112 using platinum electrodes and 0.1% ammonium chloride electrolyte. Surface resistivity is measured per IEC 62631-3-2, and dielectric strength is assessed per IEC 60243-1 at 2 kV/s ramp. Published data for this specific configuration is limited for all colour-matched production lots, so converter qualification should include a minimum of three independently moulded plaques per colour. The product differs from non-flame-retardant LONGLITE® PBT 2100-series grades primarily in UL 94 classification, melt flow stability, and tensile elongation. Non-FR PBT typically exhibits higher elongation at break and is rated HB, while the FR compound exhibits slightly higher density and a narrower processing window.

    When Halogen-Free FR PBT Alternatives Are Compared in Connector Applications

    A comparison with halogen-free flame-retardant PBT compounds shows the design trade-off in electrical and thermal performance. Halogen-free PBT-FR grades that use nitrogen-phosphorus or metal-hydrate mechanisms often show lower smoke density but may require thicker walls to meet V-0, and their comparative tracking index can be affected by the hygroscopic nature of the phosphorus package. LONGLITE® PBT-FR 2100-202B is selected where thin-wall 0.75 mm self-extinguishing behaviour and high flow length are the primary requirements. Glass-fibre-reinforced FR PBT grades, in contrast, provide flexural modulus values commonly between 7000–9000 MPa under ISO 178, but introduce anisotropic shrinkage and surface roughness that are undesirable in small-pitch connectors. The unreinforced FR compound therefore occupies a processing niche where dimensional tolerance and surface quality are more critical than maximum heat deflection temperature.

    PropertyTest StandardTypical Class Range for Unreinforced FR PBTRelevance
    DensityISO 1183-11.44–1.46 g/cm³shot weight and regrind separation
    Tensile stress at breakISO 527-250–60 MPasnap-fit and latch design
    Flexural modulusISO 1782400–2800 MPaconnector housing stiffness
    Notched Izod impact at 23°CISO 180/A3–5 kJ/m²drop-impact performance
    Heat deflection temperature at 1.82 MPaISO 75-2/A60–70°Cunreinforced grade limitation
    Water absorption, 24 hISO 620.2–0.4%moisture uptake before drying

    Compliance Assessment Against EU and International Regulatory Schemas

    Regulatory compliance for PBT-FR 2100-202B is verified through a supplier-level material declaration and selective laboratory screening. The compound is subject to the hazardous substance restrictions defined in Directive 2011/65/EU Annex II, with test methods drawn from IEC 62321 series. The specific brominated flame retardant used in the formulation must be distinguished from restricted polybrominated biphenyls and polybrominated diphenyl ethers, which are subject to maximum concentration limits of 1000 ppm by weight in homogeneous materials. Substance evaluation under Regulation (EC) No 1907/2006 requires review of the candidate list for substances of very high concern, and converters are advised to request a REACH Article 33 declaration for each production lot. The UL 94 yellow card is the authoritative flammability document and lists the minimum certified thickness, pigment families, and allowed regrind content.

    Regulatory SchemaCitationTest or Verification MethodAcceptance Limit
    RoHS Directive2011/65/EU, Annex IIIEC 62321-5, IEC 62321-4, IEC 62321-7-11000 ppm per homogeneous material for Pb, Hg, Cr(VI), PBB, PBDE; 100 ppm for Cd
    REACH SVHC1907/2006, Articles 33 and 57Supplier declaration, GC/MS screeningNotification required above 0.1% w/w per article
    UL 94 flammabilityUL 94, 7th edition, Section 7Vertical burn testV-0 at certified minimum thickness
    Material designationISO 1043-1Polybutylene terephthalate base with flame-retardant codeMarking on part surface when specified

    Processing incompatibilities must be considered before using this compound in multi-material moulding. The flame-retardant package may catalyse hydrolysis in hygroscopic semi-aromatic polyamides if co-moulded at elevated temperature without effective purge separation. High levels of alkaline or amine-based colour concentrates should be avoided unless explicitly approved by the manufacturer because they can interfere with the acid-sensitive flame-retardant chemistry and reduce melt stability. Barrel purging after processing should use a low-viscosity polyolefin or dedicated PBT purging compound at a temperature not exceeding 260°C, followed by a sealed hopper purge if the machine will stand idle for more than 30 min. The compound should not be combined with polycarbonate-rich regrind streams because transesterification between polycarbonate and polybutylene terephthalate can produce inconsistent crystallinity and lower chemical resistance in the finished moulding.

    Differences from glass-fibre-reinforced PBT grades are most evident in post-moulding dimensional stability. The unreinforced flame-retardant compound exhibits higher linear mould shrinkage, typically 1.2–2.0% in the flow direction depending on part geometry and holding pressure, whereas 30% glass-fibre-reinforced FR PBT commonly shrinks less than 0.4–0.6% in the flow direction but with significant transverse anisotropy. Connector sockets with closely spaced contact pins therefore favour the unreinforced grade because uniform volumetric shrinkage reduces pin-retention variation across the cavity. When flatness and heat distortion become dominant requirements, process engineers shift to glass-reinforced grades and accept higher tool abrasion and surface roughness. In relay bases and terminal blocks, the unreinforced FR grade is selected for consistent flow through narrow gate land lengths and for reduced gas-jetting at vent pins under fast injection.

    Top