| HS Code | 700253 |
| Density | 1.53 g/cm³ |
| Glass Fiber Content | 20% |
| Tensile Strength | 110 MPa |
| Elongation At Break | 2.0% |
| Flexural Modulus | 7500 MPa |
| Flexural Strength | 160 MPa |
| Notched Izod Impact Strength | 5 kJ/m² |
| Hdt At 0 45 Mpa | 205 °C |
| Hdt At 1 8 Mpa | 195 °C |
| Ul94 Flammability Rating | V-0 |
| Molding Shrinkage | 0.2–0.5% |
| Water Absorption | 0.05% |
| Volume Resistivity | 1E15 ohm·cm |
| Dielectric Strength | 20 kV/mm |
| Arc Resistance | 120 s |
As an accredited Chang Chun LONGLITE® PBT-FR 2100-200K factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chang Chun LONGLITE® PBT-FR 2100-200K is supplied in 25 kg polyethylene-lined paper bags, 40 bags per pallet (1,000 kg total). |
| Container Loading (20′ FCL) | Chang Chun LONGLITE® PBT-FR 2100-200K is loaded in a 20′ FCL container under dry conditions, palletized and secured for safe transport. |
| Shipping | Shipping description: Chang Chun LONGLITE® PBT-FR 2100-200K, flame-retardant polybutylene terephthalate resin in solid pellet form; non-hazardous and not regulated for transport. Supplied in moisture-barrier 25 kg bags or 500 kg jumbo bags on pallets. Keep dry and store away from heat and direct sunlight. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep containers or bags tightly closed to prevent moisture pickup and contamination. Avoid prolonged storage at elevated temperatures. Maintain first-in, first-out stock rotation and keep away from incompatible materials such as strong oxidizers. Follow local regulations and the manufacturer’s safety data sheet. |
| Shelf Life | Shelf life is typically 24 months when stored in original, unopened packaging under cool, dry conditions, protected from moisture and direct sunlight. |
Inside miniature circuit breaker internal insulating components, the decision to replace thermoset phenolics with LONGLITE® PBT-FR 2100-200K is controlled by abnormal heat resistance, tracking classification, and the requirement to hold UL 94 V-0 at 0.8 mm after molding. The granulate is used as a fully compounded flame-retardant PBT at 100 % of the feed for current-carrying part retention; no secondary flame-retardant masterbatch is introduced at the press because dilution shifts both flammability classification and tracking index. Regrind is limited to ≤15 wt% of dried shot weight for mechanical brackets, and is excluded from arc chamber side plates unless revalidation under IEC 60112 is completed. Predrying is conducted in desiccant dryers at 120–130 °C for 3–4 h to a residual moisture of ≤0.02 % by ISO 15512; moisture above 0.03 % accelerates hydrolytic chain scission at melt temperatures above 260 °C, producing surface splay, a measurable drop in dielectric strength, and inconsistent burn-time performance. Injection molding is run on hydraulic or hybrid machines of 80–120 t clamp force with screws of L/D 20:1 and non-return valve clearance ≤0.05 mm. Melt temperature is controlled between 250–270 °C, nozzle temperature 255–265 °C, and mold temperature 60–80 °C; two-stage fill velocities of 30–60 mm/s in plate sections and 80–120 mm/s in 0.8–1.2 mm ribs provide sufficient flow without jetting. Hold pressure is 60–80 MPa for 3–5 s, and total cycle time is 20–35 s. Compliance for residential breakers is assessed against IEC 60898-1, while industrial switchgear components are assessed under IEC 60947-2; both require creepage and clearance verification under IEC 60664-1 with material group classification from IEC 60112. End article types in this application include MCB arc barriers, contact carriers, trip-lever supports, bimetallic strip holders, and DIN-rail engagement clips. For breakers where working voltage and pollution degree 3 conditions exceed the values covered by the material datasheet, part-level glow wire and CTI validation are performed on the minimum wall thickness.
For automotive 12 V and 48 V connector housings, the dominant production failure in high-cavitation tooling of 24–64 cavities is not shell shrinkage but latch-root delamination and pin retention loss caused by residual moisture in the granulate. The material is evaluated under SAE USCAR-2 and SAE USCAR-21 as a complete connector system, while material-level heat aging and chemical exposure are referenced to ISO 16750-4 from −40 °C to 125 °C. The compound is therefore predried at 130 °C for 4 h with dryer dew point not higher than −40 °C, and moisture is held at ≤0.02 % before plasticating; otherwise the melt viscosity drift exceeds ±5 % and the molecular weight loss at 270 °C transfers directly to knit-line brittleness in the connector latch. LONGLITE® PBT-FR 2100-200K is used as the 100 % first-shot resin for sealing surfaces and terminal retention regions; regrind is limited to ≤10 wt% for sealed connector bodies and ≤25 wt% for non-sealing retainers, with no additional flame retardant or impact modifier added at the press. Molding is performed on 80–200 t clamp force injection machines with sequential valve-gated hot runners and subgates of 0.8–1.2 mm. Melt temperature is 255–270 °C; mold temperature is 70–90 °C; fill speed is staged at 20–40 mm/s around the latch geometry and 50–80 mm/s through the body walls, followed by hold pressure of 55–75 MPa for 4–6 s and a cycle time of 25–45 s. The 200K black grade is suited to connector bodies, terminal position assurance devices, body control module headers, fuse box terminal blocks, sensor sockets, and actuator connectors. Operational boundaries apply: direct immersion in hot aqueous solutions above pH 10 at temperatures beyond 85 °C is not recommended without long-term hydrolysis testing, because polyester chain cleavage accelerates under strong alkaline coolant contact.
Solenoid coil bobbins for industrial pneumatic and hydraulic valve actuators present a process conflict between insert pin retention and thin flange fill that does not appear in connector molding. The bobbin is injected around preheated brass or phosphor bronze terminal pins at 120–150 °C on vertical clamping machines of 60–120 t; the insert preheat is required to prevent early skin formation that would otherwise generate radial knit lines around the pin base. LONGLITE® PBT-FR 2100-200K is processed at melt temperatures of 250–265 °C, mold temperatures of 70–90 °C, and injection speeds of 20–40 mm/s, with lower speeds preferred to avoid insert deflection. The material is used as a fully compounded flame-retardant PBT at 100 % of first-shot feed; regrind is held to ≤10 wt% for bobbin flanges thinner than 1.0 mm because knit-line strength after pin insertion is the limiting property, not tensile strength. Packing pressure is staged from 30–50 MPa for 1–2 s to 60–80 MPa for 2–3 s to reduce sink marks without shifting the insert; after demolding, the parts are annealed at 120 °C for 2 h to relax molded-in stress before epoxy potting or varnish impregnation. Compliance is assessed within IEC 61810-1 for electromechanical relays and within UL 1446 insulation-system recognition at Thermal Class 130 (B) or higher as determined by the system test. The relevant thermal endurance standard is IEC 60085, while flammability is verified to UL 94 V-0 at 0.8 mm on the molded piece. End article categories include solenoid valve bobbins, industrial relay spools, contactor magnet coil forms, and sensor coil formers where the coil winding is continuously energized and heat rise above ambient does not exceed the system class. Published data for this specific configuration at Thermal Class 155 (F) is limited; qualification therefore requires system-level aging data rather than extrapolation from the PBT datasheet.
In household appliance terminal blocks and current-carrying insulating bases made from LONGLITE® PBT-FR 2100-200K, the material must meet the flammability requirements of IEC 60335-1 clause 30.2, with glow wire testing carried out under IEC 60695-2-11. For unattended appliances with current-carrying connections above 0.2 A, a glow wire test temperature of 750 °C is commonly applied; if the product committee or end-product standard raises the requirement to 850 °C, validation on the final molded wall thickness is mandatory because the UL 94 V-0 datasheet classification alone does not guarantee glow wire performance at all geometries. The molding operation uses multi-cavity cold-runner tools of 8–32 cavities on hydraulic machines of 80–200 t clamp force. The compound is used at 100 % of the feed for terminal bodies that separate current paths; regrind is limited to ≤15 wt% for current-carrying components to maintain creepage resistance under IEC 60112, and can be increased to ≤25 wt% only for non-current-carrying covers. Predrying at 120–130 °C for 3–4 h to ≤0.02 % moisture is required before melt processing at 255–270 °C. Mold temperature is set at 60–80 °C to avoid post-mold warpage in long terminal strips; injection fill begins at 25–50 mm/s through thick terminal bosses and increases to 70–100 mm/s in creepage ribs of 0.8–1.0 mm. Hold pressure is 60–80 MPa for 3–5 s, with cycle times of 20–35 s. The product group includes appliance terminal blocks, washing machine and dishwasher control-panel bases, air-conditioner internal connection blocks, switch actuator supports, and motor capacitor covers. Molded parts intended for outdoor use are also verified for weather resistance under UL 746C if energized components are exposed to solar radiation.
When wall thickness at the contact retention ribs falls below 0.8 mm, the flame-retardant classification of LONGLITE® PBT-FR 2100-200K must be re-established on the actual part geometry because the datasheet certifies UL 94 V-0 at 0.8 mm only. Thin-wall lamp holder shells and LED driver terminal covers subject the flame-retardant package not only to combustion testing but also to thermal endurance under continuous conduction and contact spring load. Melt temperature is raised within the datasheet range to 260–275 °C, mold temperature to 80–100 °C, and injection fill speed to 80–120 mm/s to keep the melt front from freezing before thin ribs fill; hold pressure is 70–90 MPa for 3–5 s. The material is used at 100 % of the feed for contact-bearing and creepage-distance sections; regrind is limited to ≤15 wt% for non-current-carrying covers and is excluded from screw-shell overmolding regions because contamination affects adhesion and creates paths for arc leakage. Standards applicable to the end uses include IEC 61347-1 for lamp controlgear insulation, IEC 60598-1 for luminaire construction, and UL 8750 where the product enters North American LED markets; creepage and clearance are verified under IEC 60664-1 with material group data from IEC 60112. End article categories include LED driver terminal covers, lampholder shells, wiring compartment covers, and contact carrier plates in retrofit lamps. Continuous use above 125 °C at the contact interface is not recommended without thermal aging validation under IEC 60216-1, because the flame-retardant additive package and the PBT chain mobility both contribute to time-dependent brittle failure at elevated temperatures.
Competitive Chang Chun LONGLITE® PBT-FR 2100-200K prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chang Chun LONGLITE® PBT-FR 2100-200K is an unfilled flame-retardant polybutylene terephthalate injection-moulding compound intended for electrical insulation parts that require definition under UL 94 or IEC 60695-2-12 flammability protocols. The designation places the grade within the LONGLITE PBT portfolio: the FR prefix identifies a flame-retardant package, the 2100 sequence identifies the unfilled base-resin family, and the 200K suffix indicates a supplier-defined colour code or colour batch. In application terms, the compound is used in connectors, terminal blocks, relay sockets, coil formers, switch housings, and other moulded electrical parts where rapid crystallisation, low moisture absorption relative to polyamide, and solvent resistance are required. Compared with non-flame-retardant PBT, the flame-retardant package raises melt density and may reduce melt-volume flow rate; compared with glass-fibre-reinforced PBT-FR compounds, the unfilled grade produces less fibre-induced anisotropic shrinkage and permits thinner wall sections and smaller gate vestiges.
Moisture control is the first release point. PBT undergoes hydrolytic ester cleavage in the melt, and hydrolysis rate increases with temperature and residence time. Residual moisture above 0.02 wt% by ISO 15512 can cause molecular-weight loss, splay streaking, loss of notched impact resistance, and reduced flame-retardant performance at the part surface. A desiccant dryer with supply air at 120 °C and dew point ≤ −30 °C for 4 h to 6 h is typical. During production, the hopper should be blanketed with dry air and the granulate should not remain in an open feed throat at ambient humidity above 60 % RH. If wet granulate is reintroduced after line stoppage, the impact failure pattern at gate regions is typically brittle, and gate staining can appear on textured surfaces. Regrind addition to unfilled flame-retardant PBT should be limited because repeated thermal residence degrades both the base resin and the flame-retardant package.
Thin-wall ignition resistance is not a single property but a combination of additive loading, char formation, anti-dripping behaviour, and wall-thickness-dependent UL 94 classification. For unfilled flame-retardant PBT grades, the UL 94 V-0 rating is valid only at the thickness and colour listed in the UL yellow card; transferring a V-0 certification from 1.6 mm natural to 0.8 mm black or pigmented versions without additional verification can be invalid. In thin-wall connectors below 0.75 mm, unfilled FR-PBT may exhibit improved flow length but also lower flame-front resistance because less material is available for char formation. Comparative tracking index according to IEC 60112 on moulded plaques can drop when wetting agents, antistatic additives, or heavy colour pigmentation are used. The user should obtain the grade-specific CTI and UL 94 thickness certification for the production colour, not from generic PBT-FR literature.
Injection-moulding process settings for unfilled flame-retardant PBT must balance flame-retardant additive degradation against crystallinity and surface finish. Barrel temperature profiles typically start at 230 °C in the rear zone and rise to 245–260 °C at the nozzle. Melt temperatures above 270 °C can degrade the flame-retardant package and create mould plate-out on vent channels. Mould temperatures from 60 °C to 90 °C are used; the upper end is preferred for parts requiring high crystallinity, dimensional stability, and low post-mould shrinkage. On a reciprocating screw with 18:1 to 22:1 L/D and 2.5:1 compression ratio, back pressure in the 0.3–0.5 MPa range is typical. High injection speed above 100 mm/s may generate shear heating and surface burns at the gate, while very low speed below 30 mm/s can cause premature freeze-off in thin ribs. Gate-seal time should be established by weight variation studies; hold pressures from 50 % to 70 % of peak injection pressure are normal starting points. Screw rotation should be kept below 100 min⁻¹, and cushion stability should be held within 1 mm to avoid residence-time variability.
PBT-FR 2100-200K is differentiated from glass-fibre-reinforced PBT-FR compounds primarily by modulus, impact resistance, and shrinkage. A glass-fibre-reinforced PBT-FR grade may have flexural modulus above 6,000 MPa, whereas unfilled flame-retardant PBT typically falls below 3,000 MPa; published data for this specific configuration should be verified against the supplier datasheet because brominated and phosphinic FR packages differ in modulus retention. The unfilled grade allows finer pin holes and more stable guide-wall positions because glass-fibre orientation does not create anisotropic shrinkage. However, it cannot provide the load-bearing stiffness required in structural circuit-breaker frames or high-current switchgear mounting plates. Halogen-free PBT-FR grades can be selected when end-user specifications restrict brominated additives, but halogen-free systems may require higher additive loadings, leading to lower tensile strength and different mould-deposit behaviour. The choice between LONGLITE PBT-FR 2100-200K and other grades should be based on flatness after conditioning at 80 °C/60 % RH, not on a single datasheet comparison.
The flame-retardant package is also relevant to tool steel corrosion and mould maintenance. Halogenated systems can release acidic decomposition products when thermal degradation occurs, causing pitting on unprotected mould vents and ejector sleeves if condensation and repeated plate-out are not removed. Vent channels should be cleaned at intervals derived from shot counts rather than calendar hours. A production-scale observation from connector moulds running unfilled FR-PBT is that initial dark spots at the end of a hot-runner manifold often indicate degraded additive or resin trapped in a dead zone, not colour contamination. Replacing the hot-runner tip or reducing manifold temperature can resolve the defect. The use of corrosion-resistant tool steel or hard-chrome plating on vent areas is common when flame-retardant PBT grades are processed continuously.
Process reproduction from a glass-filled PBT mould to unfilled FR-PBT without recalculation of shot volume and injection profile often results in flash or short shots. Because glass-fibre-reinforced PBT and unfilled FR-PBT differ in melt density and compressibility, the shot size must be corrected, and the switchover point from injection to hold should be re-established. Transferring glass-filled PBT settings can lead to over-pack in the unfilled grade, causing gate blush and ejection sticking. Unfilled PBT typically exhibits mould shrinkage in the range 1.4 % to 2.0 %, while glass-fibre-reinforced PBT may shrink 0.3 % to 0.5 % in the flow direction; transverse shrinkage can be higher. Published data for this specific compound should be obtained from the supplier’s ISO 294-4 certificate. Tool dimensions calculated for glass-filled PBT are frequently unsuitable for unfilled FR-PBT because the unfilled grade contracts more uniformly but more substantially.
For electrical performance validation, grade-specific values should be requested for dielectric strength IEC 60243-1, volume resistivity IEC 62631-3-1, and surface resistivity IEC 62631-3-2. Flame-rated PBT compounds may show moisture-dependent volume resistivity; parts conditioned at 23 °C/50 % RH before testing per ISO 291 give lower values than dry-as-moulded parts. The material is generally suitable for low-voltage insulation where creepage and clearance distances dominate, but live-metal contact and hot-wire ignition limits must be confirmed with the final wall thickness. The UL 746B relative thermal index may impose an upper continuous-use temperature below the short-term HDT, and the electrical RTI can differ from mechanical with and without impact because flame-retardant additive extraction and polymer oxidation are time-dependent.
| Method/Standard | Property | Typical test condition | Notes for grade selection |
|---|---|---|---|
| ISO 1183-1 | Density | 23 °C | Flame-retardant additives raise density above unfilled non-FR PBT; use supplier value for shot weight calculation. |
| ISO 527-2 | Tensile strength and elongation | 5 mm/min, type 1A specimen | Grade-specific values required for load-bearing snap-fit evaluation. |
| ISO 178 | Flexural modulus | 2 mm/min | Unfilled FR-PBT is below glass-fibre-reinforced grades; verify modulus for latch deflection. |
| ISO 75-2/A | HDT under 1.8 MPa | edgewise position | Short-term heat deflection; not a continuous-use temperature. |
| IEC 60112 | Comparative tracking index | solution A | Use production colour because pigmentation can lower tracking resistance. |
| UL 94 | Flammability class | thickness and colour listed on UL yellow card | V-0 certification is thickness- and colour-specific; obtain current card for production grade. |
| IEC 62631-3-1 | Volume resistivity | conditioned 23 °C/50 % RH | Moisture reduces resistivity; report conditioning per ISO 291. |
| ISO 294-4 | Moulding shrinkage | parallel and normal to flow | Unfilled grade has higher and more isotropic shrinkage than glass-filled PBT; tool dimensions must be recalculated. |
Regulatory compliance for the specific flame-retardant package should be obtained from the supplier declaration. REACH SVHC and RoHS recast 2011/65/EU with Annex II exemptions are frequently required for electrical components. A UL yellow card is a certification document, not a general statement of resistance: it lists minimum thickness, colour, RTI, and any elevated-temperature performance. The pre-selection of this product should include a request for the current UL provisional file and the supplier’s processability certificate for the actual production colour.
In terminal-block production with moulded-in brass inserts, cracking around inserts after thermal cycling is a known failure mode. Unfilled FR-PBT grades must be designed with adequate boss thickness and insert preheating; insert moulding at ambient tool temperature can induce residual stress that combines with flame-retardant additive notch sensitivity. Validation should follow IEC 60512-1 mechanical tests for connector housing contact retention and insert retention after thermal cycling between −40 °C and 105 °C. The product is best considered for electrical parts where a balance of processability, UL 94 certification, and lower anisotropic distortion is required within the PBT thermal-ageing boundary.