| HS Code | 337006 |
| Grade Name | Celanese DURANEX® PBT+GF 3316 ED3002 |
| Polymer Type | Polybutylene terephthalate (PBT) |
| Glass Fiber Content Percent | 30 |
| Flame Retardant | Yes |
| Ul94 Rating | V-0 |
| Density G Cm3 | 1.58–1.60 |
| Tensile Modulus Mpa | 9000–10000 |
| Tensile Strength Mpa | 120 |
| Elongation At Break Percent | 2.0 |
| Flexural Modulus Mpa | 8500–9000 |
| Flexural Strength Mpa | 180 |
| Charpy Notched Impact Strength Kj M2 | 7–8 |
| Hdt At 1 8 Mpa C | 200–210 |
| Melting Point C | 225 |
| Water Absorption Percent | 0.1 |
| Molding Shrinkage Percent | 0.2–0.8 |
| Volume Resistivity Ohm Cm | >1E15 |
| Dielectric Strength Kv Mm | 20 |
As an accredited Celanese DURANEX® PBT+GF 3316 ED3002 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Celanese DURANEX® PBT+GF 3316 ED3002 is packaged in 25 kg moisture-barrier bags, palletized and stretch-wrapped for shipment. |
| Container Loading (20′ FCL) | 20′ FCL container loading: palletized Celanese DURANEX® PBT+GF 3316 ED3002, evenly distributed and secured, protected from moisture and contamination. |
| Shipping | Celanese DURANEX® PBT+GF 3316 ED3002 is normally shipped as non-hazardous thermoplastic resin pellets in sealed moisture-barrier bags, packed in fiberboard drums, octabins, or palletized bags. Keep dry, away from direct sunlight and heat, and avoid moisture pickup. It is not regulated as dangerous goods for transport under standard DOT/ADR/IMDG/IATA rules. |
| Storage | Store Celanese DURANEX® PBT+GF 3316 ED3002 in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep in original sealed containers, protected from moisture, dust, and contamination; reseal after use. Avoid prolonged high-humidity exposure. Prevent static buildup, label clearly, keep away from incompatible materials, inspect containers regularly, and follow local regulations and SDS guidance. |
| Shelf Life | Typically 12 months from delivery when stored dry, cool, and in unopened original packaging; confirm with Celanese datasheet. |
Competitive Celanese DURANEX® PBT+GF 3316 ED3002 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Celanese DURANEX® PBT+GF 3316 ED3002 is an injection-molding-grade polybutylene terephthalate based on 30% by weight short-glass-fiber reinforcement and a black color/stabilizer package identified by the ED3002 suffix. In specimens conditioned according to ISO 291, the grade exhibits anisotropic mold shrinkage with flow-direction values in the 0.2% to 0.4% range and cross-flow values near 1.0% when measured by ISO 294-4. The compound is specified for power window motor housings, HVAC actuator gears, relay bobbins, sensor bodies, electrical connectors, and underhood brackets. It is not an impact-modified PBT; low-temperature notched impact remains below rubber-toughened PBT grades, but tensile modulus and heat deflection temperature are higher than unfilled PBT and 15% glass-filled PBT.
The grade is differentiated from standard unfilled PBT by an increase in tensile modulus from approximately 2,600 MPa to 10,000 MPa and by an increase in HDT/A at 1.8 MPa from approximately 60°C to 205°C. Compared with PBT-GF15, the 30% fiber loading raises flexural modulus and reduces elongation at break, but also increases melt viscosity and mold wear. The ED3002 suffix should not be used interchangeably with natural or white versions of the same 3316 base without re-qualification, because carbon black affects dielectric properties, laser marking behavior, and UL 94 classification.
The principal processing boundary is hydrolytic degradation. Residual moisture above 0.02 wt% at melt temperatures above 250°C leads to random ester cleavage, molecular weight reduction, splay, loss of notched Charpy impact, and intermittent screw feeding. A closed-loop desiccant dryer with a dew point of −40°C to −30°C and airflow of 3.7 m³/h per kg/h throughput is specified. Dry-as-molded containers should be dried at 120°C for 4 h; containers open for more than 2 h at 50% RH require 6 h drying. Hopper residence above 4 h at 120°C can cause oxidative yellowing. Airflow must be measured at the hopper inlet, not the dryer outlet.
Melt temperature at the nozzle is 250–270°C. Barrel profiles typically are 240°C, 250°C, 260°C, and 260°C from feed to nozzle. Mold temperature is 60–80°C; lower values reduce cycle time but yield lower crystallinity and larger post-mold shrinkage. Injection pressure is 70–120 MPa; hold pressure is 50–80% of injection pressure. Back pressure should be 1–5 MPa to avoid excessive fiber breakage. Screw surface speed is 0.2–0.4 m/s; shot mass should be 40–70% of barrel capacity. These parameters are typical for 30% glass-filled PBT on hydraulic toggle machines with clamp force of 5–8 kN/cm² projected area. At 270°C, total barrel residence time above 10 min should be avoided; dark specks, gloss variation, and loss of viscosity indicate local dead spots.
Regrind handling requires additional controls. Processors recirculating sprues and runners should maintain regrind below 25% and re-dry regrind before introduction. Glass fiber sizing degradation in regrind can reduce weld-line tensile strength by 15–30% relative to virgin compound. Production-scale experience on hydraulic injection presses shows that brittle weld lines in connector housings often trace to regrind moisture, not base resin molecular weight loss.
Compounding of this type of 30% glass-filled PBT is normally performed on a co-rotating twin-screw extruder with L/D 40:1 and side-fed glass at a downstream barrel zone to minimize fiber attrition. Fiber length distribution after injection molding typically has a number-average fiber length below 300 µm; excessive back pressure, high-compression-ratio screws, and gates narrower than 1.0 mm reduce fiber length further and lower tensile modulus.
Unfilled PBT mold shrinkage by ISO 294-4 is often 1.5–2.0% in both flow and cross-flow directions, while a 30% glass-reinforced PBT exhibits 0.2–0.4% in flow and 0.8–1.2% cross-flow. This anisotropy is caused by glass fiber orientation in the frozen layer. Differential shrinkage between thick bosses and thin walls drives warp; maintaining mold temperature at 80°C rather than 40°C reduces post-mold shrinkage after underhood exposure at 150°C from approximately 0.3% to below 0.1%. Post-mold annealing at 120°C for 2 h in forced-circulation air is used where close-tolerance pin spacing is critical. Published data for this specific configuration is limited, so dimensional capability studies should be performed on production tooling.
Gate placement for warp control should account for fiber orientation. Edge gates create highly oriented flow-direction skins and low-orientation cores; center gates produce radial orientation patterns and local shrinkage differences. Mold-filling simulation inputs should use measured melt volume rate, specific heat, and thermal conductivity from the current lot rather than generic PBT values.
Connector applications require comparative tracking index and dielectric strength under humidity aging. Typical PBT-GF30 grades are tested according to IEC 60112 and IEC 60243-1; published CTI for 30% glass-filled PBT is often 250 V to 300 V, and dielectric strength at 2.0 mm is 20–25 kV/mm. The ED3002 black package may reduce tracking resistance compared with unfilled PBT by increasing surface carbon content. UL 94 classification for PBT-GF30 without halogenated flame retardants is frequently HB at 0.75 mm; V-0 is not expected unless a specific flame-retardant masterbatch or retarded grade is used. High-voltage and creepage-sensitive designs should confirm the UL yellow card for the exact ED3002 color.
In molded connector bodies after 85°C/85% RH aging for 1,000 h, pin-retention force can decline when mold temperature is below 60°C. This behavior is attributed to incomplete crystallization. Molding at 80°C and annealing at 120°C for 2 h typically restores retention force. Glass-fiber-rich surfaces on valve gates or hot runners can cause insulation resistance drop after damp heat storage; gate freeze-off speed and local shear rate should be reduced to limit surface resin depletion.
| Property | Test Method | Representative Value |
|---|---|---|
| Density | ISO 1183-1 | 1.53 g/cm³ |
| Melt volume rate, 250°C, 2.16 kg | ISO 1133-1 | 16–22 cm³/10 min |
| Tensile stress at break | ISO 527-2 | 130–145 MPa |
| Tensile modulus | ISO 527-2 | 10,000 MPa |
| Flexural modulus | ISO 178 | 9,000 MPa |
| Flexural strength | ISO 178 | 200 MPa |
| Notched Charpy impact, 23°C | ISO 179-1/1eA | 8 kJ/m² |
| HDT/A, 1.8 MPa | ISO 75-2 | 205°C |
| Mold shrinkage, flow | ISO 294-4 | 0.3% |
| Mold shrinkage, transverse | ISO 294-4 | 1.0% |
These values are representative for 30% glass-filled PBT and are not specification limits. Lot-specific certificate of analysis and the current Celanese datasheet govern production qualification.
On hardened tool steel inserts, 30% glass-filled PBT generates wear rates higher than unfilled PBT. Vent depths greater than 0.030 mm can produce flash, while insufficient venting below 0.010 mm leads to burn marks and short shots. Molders typically specify hardened cores and ejector pins with nitriding or PVD coating when cumulative shot counts exceed 250,000.
Under coolant or hot water contact, the limiting property is not dry HDT/A but hydrolytic stability. PBT homopolymer with 30% glass fiber slowly loses tensile strength in pressurized hot water above 80°C. Published data for continuous coolant exposure on this exact ED3002 grade is limited; specific hydrolysis-resistant PBT or PBT/ASA blends should be benchmarked against this material for water-pump, thermostat, and cooling-system housings. In dry heat below 120°C, the grade retains useful mechanical properties, but UL RTI values must be taken from the exact color and thickness.
| Regulatory Standard | Status |
|---|---|
| REACH (EC) No 1907/2006, Article 33 | No SVHC intentionally added above 0.1% w/w |
| RoHS 2011/65/EU as amended by (EU) 2015/863 | Lead, mercury, hexavalent chromium, PBB, PBDE, DEHP, BBP, DBP, DIBP each <0.1%; cadmium <0.01% |
| UL 94 | Confirm specific ED3002 color; typical PBT-GF30 non-flame-retardant: HB at 0.75 mm |
| FDA 21 CFR 177.1660 | Food-contact status is not automatically conferred; confirm specific pigment and glass sizing |
In failure analysis of underhood bracket warpage after six months at 120°C dry air, dimensional movement has been traced to residual internal stress from packing pressure gradients rather than thermal degradation. Reducing hold pressure from 80 MPa to 50 MPa after gate freeze reduced post-mold warpage without sacrificing tensile modulus. This field observation confirms that processing history, not just glass loading, governs the dimensional stability of the ED3002 product in continuous-use automotive modules.