Celanese Duranex Pbt Gf 3300

Celanese DURANEX® PBT+GF 3300

    • Product Name: Celanese DURANEX® PBT+GF 3300
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 600591
    Glass Fiber Content 30%
    Density 1.53 g/cm³
    Melting Point 225 °C
    Tensile Strength 140 MPa
    Tensile Elongation At Break 2.5%
    Flexural Modulus 9,500 MPa
    Charpy Notched Impact Strength 7 kJ/m²
    Heat Deflection Temperature At 1 8 Mpa 205 °C
    Water Absorption At 23 C 24 H 0.07%
    Mold Shrinkage Parallel 0.3%
    Mold Shrinkage Transverse 0.9%
    Volume Resistivity 1×10^16 Ω·cm
    Dielectric Constant At 1 Mhz 3.5
    Flammability Ul 94 HB

    As an accredited Celanese DURANEX® PBT+GF 3300 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Celanese DURANEX® PBT+GF 3300 is packaged in 25 kg moisture-resistant bags, palletized for industrial storage and transport.
    Container Loading (20′ FCL) 20′ FCL container carrying palletized Celanese DURANEX® PBT+GF 3300, securely stowed and restrained for ocean transport.
    Shipping Celanese DURANEX® PBT+GF 3300 ships as non-hazardous, glass-fiber-reinforced polybutylene terephthalate resin in sealed moisture-barrier bags or cartons. Transport as general cargo in dry, ventilated conditions; protect from moisture, heat, and direct sunlight. No special dangerous-goods labeling required under normal shipping. Store at ambient temperature.
    Storage Store Celanese DURANEX® PBT+GF 3300 in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and moisture. Keep in original sealed packaging, prevent contamination, and avoid prolonged humidity or temperature extremes. Follow the manufacturer’s SDS and local regulations, and use FIFO stock rotation.
    Shelf Life Typically indefinite when stored dry, cool, and in original unopened packaging, protected from moisture, heat, and direct sunlight.
    Free Quote

    Competitive Celanese DURANEX® PBT+GF 3300 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Celanese DURANEX® PBT+GF 3300 is an injection-molding grade of polybutylene terephthalate containing a nominal 30 % short-glass-fiber reinforcement by mass. The compound is supplied as free-flowing pellets and is specified for technical components that require higher modulus, reduced creep, and elevated heat-deflection behavior relative to unfilled PBT. Typical density is 1.53 g/cm³ per ISO 1183-1, and melt volume-flow rate is approximately 12 cm³/10 min at 250 °C and 2.16 kg load per ISO 1133-1:2022. Tensile strength at break measured on standard ISO multipurpose specimens is 130 MPa to 140 MPa per ISO 527-2, with tensile elongation at break of 2.0 % to 2.5 %. These values are characteristic for a 30 % glass-fiber-reinforced PBT and can shift with color package, regrind content, and fiber orientation in the molded part. Published data for the exact DURANEX PBT+GF 3300 designation may vary by production lot, so the applicable Celanese datasheet and lot certificate should be consulted before tooling release.

    What Does the 30 % Glass-Fiber Fraction Do to the Stiffness-Impact Balance?

    At 23 °C, flexural modulus is typically 8.5 GPa to 9.0 GPa per ISO 178, approximately 3.5 times the 2.4 GPa reported for unfilled PBT. Flexural strength is 190 MPa to 210 MPa. Notched Charpy impact is 8.0 kJ/m² to 10.0 kJ/m² per ISO 179-1/1eA. This places the grade in a moderate toughness plateau: stiffness increases more than impact resistance, so the compound is not a direct substitute for toughened PBT or PBT/PC blends when multiaxial impact, snap-fit insertion, or high-speed deformation is dominant. Heat deflection temperature at 1.8 MPa is 200 °C to 210 °C per ISO 75-2/A; unfilled PBT under the same boundary condition is approximately 60 °C. The glass-fiber network also reduces long-term creep under sustained load, but the creep resistance is anisotropic and depends on the angle between the applied stress and the prevailing fiber orientation.

    Pre-drying in a desiccant dryer with a dew point of -30 °C or lower at 120 °C to 130 °C for 4 h to 6 h is required when pellets have been exposed to ambient relative humidity above 60 %. Target residual moisture before plastication is 0.02 % or less by weight. Moisture above 0.03 % entering a reciprocating-screw injection-molding machine with an L/D of 18:1 to 22:1 can reduce molecular weight by hydrolysis; tensile strength may fall by 5 % to 15 % within ordinary barrel residence times. Screw recovery speed should maintain a recovered melt cushion of 5 mm to 8 mm and should avoid excessive fiber breakage in the compression zone. Regrind use above 20 % by mass is not recommended for critical dimensional applications because repeated heat history shortens fiber length and widens shrinkage distribution.

    When Barrel Residence Time Exceeds Seven Minutes in Hot-Runner Tooling

    Melt temperature in the barrel is normally 250 °C to 270 °C. Above 270 °C, the polyester backbone undergoes progressive thermal degradation; tetrahydrofuran liberation and carboxylic acid chain-end formation are accelerated when residual moisture is present. For hot-runner systems with unheated gate bushes, long manifold channels, or valve-gate sequencing, total melt residence time should be kept below 7 min at 260 °C. If color changes or interruptions push residence time beyond 10 min, the material should be purged and the first 10 to 15 shots discarded until melt flow, gate-seal pressure, and surface appearance return to baseline. Glass-fiber attrition is more severe when back pressure exceeds 0.7 MPa to 1.0 MPa, when screw speed exceeds 0.3 m/s peripheral velocity, or when barrel temperature is raised to compensate for thick bosses. Fiber length reduction below 200 µm can measurably lower tensile strength and flexural modulus even if the molded parts pass visual inspection; published data for this specific configuration is limited, so process-capability studies using short-shot rheology and retention-time trials are required before serial production.

    Production-scale components molded from this grade are specified for automotive low-voltage connector bodies, sensor housings, relay bobbins, and structural brackets operating in dry or intermittent hot-air conditions. The grade is selected because dimensional change under load between -40 °C and 120 °C is smaller than unfilled PBT. Linear shrinkage in the flow direction is typically 0.3 % to 0.5 %, while cross-flow shrinkage is 0.8 % to 1.2 %; this anisotropy must be compensated by gate location and wall-section symmetry. Electrical volume resistivity is approximately 1.0 × 10¹⁶ Ω·cm per IEC 62631-3-1, and dielectric strength at 3.0 mm thickness is approximately 20 kV/mm per IEC 60243-1. The non-flame-retarded GF30 PBT version is typically classified UL 94 HB; where a V-0 rating is required, a flame-retarded PBT grade must be substituted and the UL file verified for the specific color and thickness.

    Comparative Mechanical, Thermal, and Electrical Data Against Unfilled and 20 % Glass-Fiber PBT

    Property Test method PBT+GF 3300 Unfilled PBT PBT-GF20 reference
    Density ISO 1183-1 1.53 g/cm³ 1.31 g/cm³ 1.45 g/cm³
    Tensile strength at break ISO 527-2 135 MPa 55 MPa 100 MPa
    Flexural modulus ISO 178 8.8 GPa 2.4 GPa 5.5 GPa
    Notched Charpy impact ISO 179-1/1eA 8.5 kJ/m² 4.0 kJ/m² 6.5 kJ/m²
    Heat deflection temperature at 1.8 MPa ISO 75-2/A 205 °C 60 °C 195 °C
    Volume resistivity IEC 62631-3-1 1.0 × 10¹⁶ Ω·cm 1.0 × 10¹⁶ Ω·cm 1.0 × 10¹⁶ Ω·cm

    Compared with a 20 % glass-fiber PBT, the 30 % variant raises flexural modulus by roughly 50 % and heat deflection temperature by 5 °C to 10 °C, but it lowers spiral-flow length and may increase cross-flow shrinkage anisotropy. Compared with a 40 % glass-fiber PBT compound, the 30 % grade typically retains a wider injection-molding processing window and lower barrel pressure drop; published data for 40 % glass-filled DURANEX grades show flexural modulus above 11 GPa, but notch sensitivity and fiber orientation effects are more pronounced. The choice between these grades should be driven by wall thickness, gate geometry, and the direction of the primary tensile stress relative to flow.

    Process Control Ranges for Desiccant Drying, Barrel Settings, and Tool Temperature

    Parameter Recommended range Measurement or equipment boundary
    Drying temperature 120 °C to 130 °C Desiccant dryer, dew point ≤ -30 °C
    Drying time 4 h to 6 h From ambient storage
    Residual moisture ≤ 0.02 % Karl Fischer or moisture analyzer
    Melt temperature 250 °C to 270 °C Melt pyrometer, nozzle check
    Mold temperature 60 °C to 100 °C Thermolator or oil temperature-control unit
    Back pressure 0.5 MPa to 1.0 MPa Hydraulic injection unit
    Injection pressure 80 MPa to 120 MPa Machine hydraulic pressure or specific pressure
    Hold pressure 60 % to 80 % of injection pressure Gate-seal study
    Screw speed 0.1 m/s to 0.3 m/s peripheral velocity Reciprocating screw, L/D 18:1 to 22:1
    Screw cushion 5 mm to 8 mm Injection machine position transducer

    Chemical resistance boundaries are defined by the PBT ester linkage. Continuous exposure to hot water above 60 °C, steam autoclave cycles, strong mineral acids, or alkaline glycol fluids can reduce molecular weight, soften the matrix, and expose glass fiber at the surface. Solvent resistance to hydrocarbons and alcohols is acceptable at room temperature, but phenolic or cresol-based mold-release agents and cleaning solvents should be avoided. Storage in unopened poly-lined bags below 30 °C and 70 % relative humidity is recommended. If material is stored outside these limits, drying time should be extended and a melt-flow verification test per ISO 1133-1 should be performed before production. RoHS Directive 2011/65/EU and REACH EC 1907/2006 conformity should be confirmed against the current supplier declaration, because pigment and additive packages vary by grade and color.

    Top