| HS Code | 154491 |
| Polymerbase | Polybutylene terephthalate (PBT) |
| Reinforcement | 30% glass fiber |
| Density | 1.60 g/cm³ |
| Tensilestrength | 120 MPa |
| Elongationatbreak | 2.0% |
| Flexuralmodulus | 9,000 MPa |
| Flexuralstrength | 180 MPa |
| Charpynotchedimpactstrength | 7 kJ/m² |
| Heatdeflectiontemperatureat1 8mpa | 200 °C |
| Meltingpoint | 224 °C |
| Waterabsorption | 0.07% |
| Moldshrinkage | 0.2–0.6% |
| Flammability | UL94 V-0 |
| Volumeresistivity | 1×10^16 Ω·cm |
| Dielectricstrength | 20 kV/mm |
| Comparativetrackingindex | 600 V |
| Coefficientoflinearthermalexpansion | 2–3×10^-5 /°C |
As an accredited Celanese DURANEX® PBT+GF 2002 EF2001 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in sealed 25 kg bags, palletized and labeled for industrial handling and storage. |
| Container Loading (20′ FCL) | Celanese DURANEX® PBT+GF 2002 EF2001 loaded in a 20′ FCL container, palletized, shrink-wrapped, and secured for dry transport. |
| Shipping | Ship as non-hazardous, non-DG plastic resin pellets in sealed moisture-barrier bags/boxes. Protect from moisture, heat, UV, and bag damage; store in a dry, ventilated area. No UN number or special transport labeling required. Handle with normal industrial hygiene precautions. |
| Storage | Store DURANEX® PBT+GF 2002 EF2001 in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and incompatible chemicals. Keep original packaging/containers tightly closed to prevent moisture pickup and contamination. Avoid prolonged humidity exposure; dry material before processing if required. Do not store outdoors or near oxidizing agents. Follow SDS, local regulations, and safe stacking practices. |
| Shelf Life | Typically 12 months from date of manufacture when stored dry, in original sealed packaging, under ambient conditions. |
Competitive Celanese DURANEX® PBT+GF 2002 EF2001 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Celanese DURANEX® PBT+GF 2002 EF2001 is a 20 wt% glass-fibre-reinforced polybutylene terephthalate compound supplied for injection moulding of electrical, electronic, and appliance components. The EF2001 designation identifies a flame-retardant package intended for low-halogen material declarations in electrical markets; the glass reinforcement distinguishes the grade from unreinforced DURANEX PBT by raising heat deflection temperature, tensile modulus, and dimensional stability. Representative supplier-published data place density at 1.47 g/cm³ by ISO 1183 and water absorption at 0.05 % by ISO 62. Tensile stress at break is approximately 95 MPa with tensile modulus of 6,800 MPa per ISO 527-2; flexural modulus is 6,200 MPa and flexural strength is 150 MPa per ISO 178. Notched Izod impact is 6.0 kJ/m² at 23 °C by ISO 180/1A, and notched Charpy impact is 5.5 kJ/m² by ISO 179/1eA. Heat deflection temperature is 200 °C at 1.82 MPa and 215 °C at 0.45 MPa by ISO 75-2. Glass-fibre modification reduces mould shrinkage to approximately 0.4 % parallel and 0.8 % normal to flow by ISO 294-4. These values are typical and not specification limits; lot-specific certificates of analysis should govern acceptance.
| Property | Method | Representative data |
|---|---|---|
| Density | ISO 1183 | 1.47 g/cm³ |
| Tensile stress at break | ISO 527-2 | 95 MPa |
| Tensile modulus | ISO 527-2 | 6,800 MPa |
| Flexural strength | ISO 178 | 150 MPa |
| Flexural modulus | ISO 178 | 6,200 MPa |
| Notched Izod impact, 23 °C | ISO 180/1A | 6.0 kJ/m² |
| Notched Charpy impact, 23 °C | ISO 179/1eA | 5.5 kJ/m² |
| Heat deflection temperature, 1.82 MPa | ISO 75-2 | 200 °C |
| Heat deflection temperature, 0.45 MPa | ISO 75-2 | 215 °C |
| Melt volume-flow rate, 250 °C/2.16 kg | ISO 1133 | 12 cm³/10 min |
| Mould shrinkage parallel/normal | ISO 294-4 | 0.4 % / 0.8 % |
| Water absorption | ISO 62 | 0.05 % |
Moisture control is the principal processing constraint. PBT is a polyester, and residual moisture at melt temperature produces hydrolytic chain scission; the resulting molecular-weight loss appears as surface splay, reduced tensile strength, and unstable hold-pressure response. Drying should be performed in a desiccant drier at 120 °C for 4 h. The target pellet moisture is below 0.02 % by ISO 15512, particularly when ambient relative humidity exceeds 60 %. Regrind should not be stored open in humid air for more than 30 min unless it is fed from a hopper dryer with a dew point below -30 °C.
Melt temperature at the nozzle is maintained between 250 °C and 270 °C. A barrel profile of 240 °C in the feed zone, 250 °C in compression, and 260 °C in metering is typical for a general-purpose screw with L/D 20:1 and compression ratio 2.5:1. At barrel temperatures above 270 °C, residence time must be reduced to avoid yellowing and loss of impact. If production is interrupted for more than 8 min, the barrel should be purged; the flame-retardant package can catalyse degradation during prolonged thermal exposure.
Mould temperature is held at 60–90 °C. The lower end may be acceptable for unfilled PBT but often causes incomplete crystallisation in GF20 parts with wall-thickness variation above 2:1. For dimensional stability, the preferred mould temperature is 80 °C; below 60 °C, post-mould shrinkage can continue for several hours, and above 90 °C, cycle time increases without a proportional gain in short-term stiffness. Injection speed is medium to high for thin-wall fill; hold pressure is typically 50–80 MPa, back pressure 0.3–0.7 MPa, screw cushion 3–5 mm, and decompression 2–3 mm.
Avoid strong acids, alkaline mould-releasing compounds, and amine-bearing additives at processing temperature. These substances attack the PBT ester bond. Chlorinated solvents and aromatic phenols are also incompatible with the grade.
Electrical connector, relay, and switch applications use the grade where tracking resistance and glow-wire ignition behaviour are design constraints. Under IEC 60112, the grade is commonly reported at CTI 600 V, while many brominated FR PBT+GF20 grades fall below 250 V. This difference permits tighter contact spacing when the moulded insulator is exposed to dust, humidity, or conductive debris. Glow-wire testing under IEC 60695-2-12 is typically conducted at 750 °C and 850 °C for unattended appliance parts; the material commonly achieves no ignition at 960 °C at 1.0 mm. However, published data for specific configurations below 0.6 mm wall thickness is limited, and final component performance must be tested with the production colorant and gate location.
Substitution from a brominated FR PBT+GF20 to EF2001 changes the mechanical and electrical design margin. The low-halogen flame-retardant package typically increases comparative tracking index and reduces smoke-gas acidity, but it can raise melt viscosity. Moulders may observe 10–20 % higher pressure drop in thin-wall sections and longer screw recovery because the melt volume-flow rate at 250 °C/2.16 kg is 12 cm³/10 min per ISO 1133, whereas many fast-cycle halogenated PBT+GF20 grades exceed 15 cm³/10 min. The practical adjustment is to raise nozzle temperature to 265–270 °C and hold mould temperature at 80 °C; this is not a drop-in replacement without re-optimising the injection profile.
Compared with unreinforced PBT, the GF20 grade provides flexural modulus roughly three times higher than the 2,500–3,000 MPa range of unfilled PBT, and HDT/A increases from below 60 °C to 200 °C. The trade-off is anisotropic shrinkage and reduced weld-line integrity. Weld-line strength in glass-reinforced PBT can fall to 50–60 % of the unreinforced value, so gate placement should locate knit lines away from snap-fit or screw-boss features.
Compared with PBT+GF30, EF2001 has lower density and better flow, but lower stiffness. PBT+GF30 typically shows flexural modulus above 9,000 MPa and HDT/A above 205 °C; the EF2001 flexural modulus of 6,200 MPa is lower, but the 20 wt% glass loading reduces abrasive wear on screw and barrel surfaces and lowers part mass in high-volume connectors.
Tooling for this grade should be designed for glass-reinforced flow. Gate freeze-off occurs earlier than with unfilled PBT because glass fibre increases thermal conductivity. For valve-gated hot-runner systems with wall thickness below 1.2 mm, a gate diameter of at least 1.0 mm is recommended; below this dimension, premature gate solidification causes short shots and weak knit-line areas. Vent depth for GF20 PBT is typically 0.010–0.020 mm. Deeper vents can produce flash, while too-shallow vents produce burn marks at the end of fill. In moulds with wall-thickness transitions greater than 2:1, a mould temperature of 80 °C is preferred because slower crystallisation balances shrinkage across the section and reduces sink. If the mould runs below 60 °C, internal stress can increase and post-mould warping may develop within 24 h at elevated ambient temperature.
Final component certification depends on wall thickness, pigment package, and production conditions. The resin is commonly evaluated against the following matrix, but the finished part must be tested in its final geometry.
| Standard or directive | Test or requirement | Typical basis or threshold |
|---|---|---|
| UL 94 | Flammability | V-0 at 0.8 mm |
| IEC 60112 | Comparative tracking index | 600 V |
| IEC 60695-2-12 | Glow-wire flammability index | 960 °C at 1.0 mm |
| IEC 60695-2-13 | Glow-wire ignition temperature | 775 °C at 1.0 mm |
| IEC 61249-2-21 | Halogen content thresholds | Cl <900 ppm, Br <900 ppm, total <1,500 ppm |
| Directive 2011/65/EU | RoHS restricted substances | Pb, Hg, Cd, Cr VI, PBB, PBDE below maximum concentration values |
| Regulation (EC) No 1907/2006 | REACH SVHC communication | Supplier declaration for candidate list substances |
Lot-specific certificates should list moisture, melt volume-flow rate, and tensile results. Where the part is covered under a long-term thermal ageing file, the relative thermal index may differ from the unreinforced base resin and must be verified against the recognised component file.