Celanese Crastin Unreinforced Pbt S610sf Nc010

Celanese Crastin® Unreinforced PBT S610SF NC010

    • Product Name: Celanese Crastin® Unreinforced PBT S610SF NC010
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 460989
    Density 1.20 g/cm³
    Melt Volume Flow Rate 15 cm³/10 min (250 °C/2.16 kg)
    Tensile Modulus 2100 MPa
    Tensile Stress At Break 45 MPa
    Tensile Strain At Break 50%
    Charpy Notched Impact Strength At 23 C 10 kJ/m²
    Charpy Unnotched Impact Strength At 23 C 100 kJ/m²
    Melting Temperature 225 °C
    Vicat Softening Temperature 165 °C
    Heat Deflection Temperature At 0 45 Mpa 150 °C
    Heat Deflection Temperature At 1 8 Mpa 55 °C
    Water Absorption 0.4%
    Molding Shrinkage 1.5–2.0%
    Volume Resistivity >1E13 Ω·cm

    As an accredited Celanese Crastin® Unreinforced PBT S610SF NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Celanese Crastin® Unreinforced PBT S610SF NC010 is packaged in 25 kg moisture-resistant bags on pallets.
    Container Loading (20′ FCL) 20′ FCL loading: Celanese Crastin® Unreinforced PBT S610SF NC010 supplied in 25 kg bags, palletized and securely stowed for transport.
    Shipping Celanese Crastin® S610SF NC010 is an unreinforced polybutylene terephthalate resin supplied as natural-color pellets in moisture-barrier bags or octabins. It is non-hazardous for transport, requires no special temperature control, and should be shipped dry, protected from moisture, contamination, and direct sunlight in standard trucks or containers.
    Storage Store Celanese Crastin® Unreinforced PBT S610SF NC010 in a cool, dry, well-ventilated area in original sealed containers. Keep away from direct sunlight, heat sources, moisture, and contamination. Leave packages closed until use to prevent moisture pickup. Avoid contact with strong oxidizers and incompatible chemicals, and follow the manufacturer’s safety data sheet.
    Shelf Life Shelf life is typically 24 months from manufacture when stored dry in original unopened packaging under recommended conditions.
    Free Quote

    Competitive Celanese Crastin® Unreinforced PBT S610SF NC010 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Celanese Crastin® S610SF NC010 is an unreinforced, natural-colour polybutylene terephthalate (PBT) injection-moulding grade within the Crastin® semicrystalline polyester family. The material is supplied without short-glass, mineral, or carbon-fibre reinforcement. That compositional choice removes the anisotropic shrinkage, abrasive screw wear, and surface roughness commonly associated with hard fillers, but it also reduces tensile modulus and long-term creep resistance relative to glass-filled PBT. Manufacturer-published representative data for this specific grade include a density of 1.31 g/cm³ measured per ISO 1183-1:2019, a melt volume-flow rate of approximately 30 cm³/10 min at 250 °C under 2.16 kg load per ISO 1133-1:2022, and a melting endotherm peak near 225 °C per ISO 11357-3:2018. The low-viscosity melt is intended for thin-wall sections, high-cavitation tooling, and reduced injection-pressure demand; the unreinforced structure nevertheless limits continuous temperature capability compared with reinforced PBT grades.

    PropertyTest methodRepresentative value
    DensityISO 1183-1:20191.31 g/cm³
    Melt volume-flow rateISO 1133-1:202230 cm³/10 min at 250 °C, 2.16 kg
    Tensile modulusISO 527-2:20122,600 MPa
    Tensile stress at yieldISO 527-2:201260 MPa
    Nominal strain at breakISO 527-2:201220 %
    Flexural modulusISO 178:20192,400 MPa
    Charpy notched impact strength at 23 °CISO 179-1:20233.0 kJ/m²
    Heat deflection temperature at 1.8 MPaISO 75-2:201360 °C
    Heat deflection temperature at 0.45 MPaISO 75-2:2013150 °C
    Flammability at 0.8 mmUL 94HB

    High-flow character in this unfilled grade is not a simple viscosity reduction. The modification alters gate freeze time, pressure drop across cold-runner channels, and weld-line morphology. In multi-cavity tools with runner diameters below 2.5 mm, S610SF NC010 normally requires lower injection pressure than a standard-flow unfilled PBT, but it can also exhibit more pronounced jetting if gate velocity is left uncontrolled. Published data for this specific runner configuration is limited; initial tool trials should therefore include short-shot studies and cavity-pressure transducer records rather than relying solely on fill simulation libraries.

    Why does residual moisture above 0.02 % govern the processing window of this unfilled PBT grade?

    PBT is hydrolytically unstable in the melt phase. Ester linkages in the polybutylene terephthalate backbone react with absorbed water at processing temperatures, producing chain scission, molecular-weight reduction, melt-viscosity drift, and volatile evolution. For bulk material stored in ambient conditions above 50 % relative humidity, a closed-loop desiccant-bed dryer with a supply-air dew point of -30 °C or lower and an inlet air temperature of 120 °C over 4 h is specified. The target residual moisture is below 0.02 % by mass, typically verified by Karl Fischer titration or ISO 15512:2019. Drying longer than 8 h at 120 °C can cause thermal yellowing and a measurable loss of flow. Production-scale experience with damp regrind introduced at a 20 % reuse level has shown intermittent silver streaking, gate-area splay, weak weld lines, and short shots in sections below 1.0 mm. The condition is not recoverable by raising melt temperature; higher barrel temperatures accelerate the degradation reaction and increase evolution of butanediol-derived volatiles.

    Rheological profile and melt-processing boundaries

    The grade is intended for processing at melt temperatures of 240–260 °C measured at the nozzle, with an upper practical limit near 270 °C to minimise thermal degradation during prolonged residence. Mould temperature is normally held at 60–100 °C, with 80 °C as a typical starting point for dimensional stability and crystallinity development. Lower mould temperatures reduce crystallinity and can freeze the melt before complete pack, increasing warp and lowering mechanical strength. Capillary-rheometry data for this specific grade should be obtained from the current Celanese technical datasheet for gate and runner sizing; high-flow unfilled PBT generally exhibits pseudoplastic behaviour at processing shear rates above 1,000 s⁻¹, but the exact viscosity curve depends on moisture content, lot-to-lot molecular-weight distribution, and thermal history.

    Processing parameterRecommended starting range or condition
    Pre-drying120 °C for 4 h, desiccant-bed dryer, dew point -30 °C or lower
    Residual moisture targetBelow 0.02 %
    Melt temperature at nozzle240–260 °C, maximum 270 °C
    Mould temperature60–100 °C, typical 80 °C
    Injection speedMedium to high; fill time 1.0–2.5 s for walls 0.8–1.5 mm
    Back pressure0.3–0.5 MPa hydraulic; excessive back pressure causes shear heating
    Screw design20:1–25:1 L/D, compression ratio 2.5:1–3.0:1
    Hot-runner manifold and nozzle250–260 °C maximum; avoid dead spots

    Field observations on high-cavitation thin-wall connector tooling indicate that the grade is sensitive to gate vestige quality when hot-runner tip temperature exceeds the melt-temperature upper limit. Cavity-pressure sensors and post-gate freeze-pressure measurements are preferable to timer-based hold settings because the low-viscosity melt can overpack small gates if hold pressure is not reduced early. When mould temperature is raised to 80–90 °C for crystallinity, cycle time may increase by approximately 10–15 % depending on wall thickness; this thermal penalty must be balanced against warp and impact-strength requirements.

    If hot-runner dwell times exceed five minutes, which process changes become measurable?

    Extended hot-runner residence progressively degrades PBT through thermal and thermo-oxidative pathways. In manifold systems held above 260 °C, prolonged hold time can cause yellowing, an apparent increase in melt flow due to initial chain scission, and generation of tetrahydrofuran and other low-molecular-weight degradation products. The embrittlement threshold depends on manifold volume, shear history, and temperature uniformity across the hot-runner circuit. A practical operational boundary is to keep total melt residence time in hot-runner systems below 5–6 min when the manifold is at 260 °C; higher manifold temperatures require shorter hold times. In valve-gated tools, stagnant melt pools around the valve pin often show discolouration earlier than flow channels, so pin withdrawal and manifold cleaning schedules should be aligned with actual residence-time measurement rather than fixed production-hour intervals.

    The high-flow formulation also differs from standard-flow unfilled PBT in gate-freeze response. Because the melt solidifies quickly once injection stops, gates may freeze before full pack if gate diameter is oversized or if mould temperature is low. This is the reverse of the common failure mode in high-viscosity PBT, where short shots dominate. Runner balancing in multi-cavity tools should be adjusted for lower melt viscosity, and cold-runner diameters below 2.5 mm should be evaluated for pressure drop at the grade’s actual melt temperature rather than using generic PBT curves.

    Comparative behaviour is measurable in tensile modulus, weld-line strength retention, and heat distortion.

    Compared with a 30 % short-glass-filled PBT, S610SF NC010 has a tensile modulus of roughly one-third to one-half the reinforced value, a lower heat deflection temperature, and reduced retention of tensile strength in weld-line regions. The unreinforced grade is therefore not appropriate for structural supports requiring high stiffness at elevated temperature. Its advantages appear in thin-wall flow, surface finish, dimensional isotropy, and reduced screw and barrel wear. Compared with standard-flow unfilled PBT, the S610SF NC010 grade permits shorter filling times and lower injection pressure in walls as low as 0.5 mm, but it requires tighter control of gate geometry and hot-tip temperature to prevent stringing and drool.

    Application evaluations for unreinforced S610SF NC010 typically include relay bases, sensor housings, connector bodies, bobbin insulation, and mechanical clips. In such uses, the material is assessed for dielectric strength under IEC 60243-1:2013, comparative tracking index under IEC 60112:2020, and glow-wire ignition under IEC 60695-2-13:2021. Unfilled PBT formulations of this physical form often exhibit a comparative tracking index around 600 V; however, the specific UL Yellow Card and current Celanese datasheet values must be confirmed because additive and colour packages can alter tracking behaviour and glow-wire performance.

    Regulatory and electrical performance boundaries

    When evaluated at 0.8 mm thickness, the natural grade is rated HB under UL 94. This rating is not a V-0 classification and should not be substituted where a higher flammability rating is required without additional flame-retardant formulation. The grade does not contain intentional halogenated flame retardants in its natural form; published data for this specific unfilled formulation should be referenced from the current Celanese material safety and regulatory documentation for REACH, RoHS, and any food-contact status. Electrical performance is typical of dry PBT, with high volume resistivity and good tracking resistance in clean moulded parts, but absorption of polar solvents or contamination from mould-release agents can degrade comparative tracking index and dielectric strength.

    Chemical resistance is generally consistent with semicrystalline PBT: satisfactory for aliphatic hydrocarbons, glycols, and dilute mineral acids at room temperature. The material is not recommended for continuous immersion in hot water above 60 °C, strong alkaline solutions, concentrated oxidising acids, phenols, or ketones under mechanical stress. Environmental stress-cracking data for this specific grade is limited, so chemical-exposure validation should be performed on moulded components under actual load and thermal conditions. In production of clip geometries and snap-fit features, mould-temperature uniformity, moisture control, and hot-runner residence time are the controlling variables most likely to shift lot-to-lot part performance.

    Top