Celanese Crastin Unreinforced Pbt S600f40 Nc010

Celanese Crastin® Unreinforced PBT S600F40 NC010

    • Product Name: Celanese Crastin® Unreinforced PBT S600F40 NC010
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 660054
    Density 1.30 g/cm³
    Melting Temperature 225 °C
    Tensile Modulus 2600 MPa
    Tensile Stress At Yield 55 MPa
    Tensile Strain At Yield 4.0%
    Nominal Strain At Break >50%
    Charpy Notched Impact Strength At 23 C 4 kJ/m²
    Charpy Notched Impact Strength At 30 C 3 kJ/m²
    Hdt At 1 8 Mpa 50 °C
    Hdt At 0 45 Mpa 150 °C
    Vicat Softening Temperature 175 °C
    Water Absorption At Saturation 0.4%
    Water Absorption At Equilibrium 23 C 50 Rh 0.2%
    Molding Shrinkage Parallel 1.8%
    Molding Shrinkage Normal 1.8%
    Melt Volume Rate At 250 C 2 16 Kg 40 cm³/10 min
    Processing Melt Temperature 240-260 °C
    Mold Temperature 60-100 °C

    As an accredited Celanese Crastin® Unreinforced PBT S600F40 NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Celanese Crastin® Unreinforced PBT S600F40 NC010 is supplied in 25 kg sealed moisture-barrier bags, palletized for industrial handling.
    Container Loading (20′ FCL) 20′ FCL loading for Celanese Crastin® Unreinforced PBT S600F40 NC010: palletized 25 kg bags, dry, secure stowage for sea freight.
    Shipping Celanese Crastin® Unreinforced PBT S600F40 NC010 ships as a non-hazardous, solid thermoplastic polyester resin in sealed moisture-barrier bags or boxes. Keep dry, cool, and protected from contamination and direct sunlight. No special transport hazard classification; follow local regulations and the manufacturer’s SDS.
    Storage Store Celanese Crastin® Unreinforced PBT S600F40 NC010 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and moisture. Keep containers tightly closed to prevent contamination and moisture pickup. Avoid dust generation and contact with incompatible substances. Follow local regulations and the manufacturer’s safety data sheet for detailed handling and storage recommendations.
    Shelf Life Celanese Crastin® S600F40 NC010 typically has a 24-month shelf life from manufacture when stored dry, cool, and unopened.
    Free Quote

    Competitive Celanese Crastin® Unreinforced PBT S600F40 NC010 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Celanese Crastin® S600F40 NC010 is an unreinforced polybutylene terephthalate (PBT) injection-molding grade supplied in natural color. The material is designated PBT under ISO 1043, and the NC010 suffix identifies an unpigmented base resin without carbon black, permitting press-side masterbatch coloring. The grade is distinguished within the Crastin PBT portfolio by a melt volume-flow rate of 40 cm³/10 min measured at 250 °C under a 2.16 kg load in accordance with ISO 1133-1. This high-flow rheology targets thin-wall, high-cavitation molds where lower-flow unreinforced PBT grades generate excessive injection pressure and incomplete packing.

    PropertyTest methodValue
    DensityISO 1183-11.31 g/cm³
    Melt volume-flow rate, 250 °C, 2.16 kgISO 1133-140 cm³/10 min
    Tensile modulusISO 527-1/-22600 MPa
    Tensile stress at yieldISO 527-1/-257 MPa
    Nominal strain at breakISO 527-1/-2>50%
    Flexural modulusISO 1782400 MPa
    Flexural stress at 3.5% strainISO 17880 MPa
    Charpy notched impact, 23 °CISO 179-1/1eA4.0 kJ/m²
    Heat deflection temperature, 1.8 MPaISO 75-1/-260 °C
    Heat deflection temperature, 0.45 MPaISO 75-1/-2160 °C
    Vicat softening temperature, 50 °C/h, 50 NISO 306215 °C
    Melting pointISO 11357-3225 °C
    Comparative tracking indexIEC 60112600 V
    Dielectric strength, 2.0 mmIEC 60243-125 kV/mm
    FlammabilityUL 94HB at 0.75 mm
    Molding shrinkage, flow/transverseISO 294-41.9–2.1% / 1.9–2.1%

    S600F40 NC010 exhibits a tensile modulus of 2600 MPa and a tensile stress at yield of 57 MPa under ISO 527-1/-2. The yield strain is approximately 4%, after which cold drawing and orientation produce a nominal strain at break above 50%. Flexural modulus under ISO 178 is 2400 MPa, and flexural stress at 3.5% strain is 80 MPa. These values place the grade in the conventional unfilled PBT stiffness range, below glass-filled alternatives but adequate for snap-fit applications when the clip arm is designed with generous radii and reduced strain concentration. Unreinforced structure removes fiber-induced notch sensitivity but exposes knit lines and gate transitions as crack-initiation sites; sharp corners and direct gate frost lines should be radiused or relocated away from load-bearing areas.

    Charpy notched impact at 23 °C is 4.0 kJ/m² under ISO 179-1/1eA. At subzero temperatures, unfilled PBT embrittles, and molded-in stress can reduce impact further. Process-induced hydration, excessive melt residence time, and rapid cooling from high mold-temperature settings can shift the ductile-to-brittle response toward higher temperatures. For high-speed assembly operations using snap fits, the lower notched impact value of this high-flow unfilled grade requires evaluation under end-use strain rate and temperature conditions rather than supplier datasheet values alone.

    What limits melt residence time in thin-wall injection molding of natural NC010?

    The primary processing constraint for S600F40 NC010 is hydrolytic degradation in the melt. Supplier processing guidance specifies pre-drying at 120 °C for 4 h in a dehumidifying or desiccant dryer to reach a pellet moisture content below 0.02 wt%. At melt temperatures above 250 °C, residual moisture cleaves the ester linkages of PBT, causing molecular-weight loss, a reduction in melt viscosity, and surface splay on molded parts. On production-scale reciprocating-screw injection machines, this degradation is observed as an increase in flash at the parting line and a drop in tensile elongation measured on molded plaques. The effect is accelerated in NC010 natural color because yellowing appears in the sprue and gate area before dimensional or mechanical degradation is detected.

    Barrel temperature profiles of 235 °C to 250 °C are used in practice, with a mold temperature of 60 °C to 80 °C to balance crystallization and dimensional stability. For thin-wall sections, mold temperatures up to 100 °C are permissible but can extend cycle time because the unreinforced resin has a heat deflection temperature of 60 °C at 1.8 MPa under ISO 75-1/-2. Screw L/D ratios in the range of 18:1 to 22:1 with a conventional general-purpose screw are adequate; high-compression screws are not required because the resin is not compounded with fiber and excessive shear can accelerate yellowing of NC010. Back pressure should be limited to 2–5 MPa to avoid shear heating, and screw recovery speed should be set so that melt residence time is minimized without introducing unmelted solids into the shot.

    Residence time at melt temperature should be kept below 10 min for natural NC010. In hot-start molding trials on thin-wall connector tools, yellowing in the sprue and gate area appeared when the melt cushion exceeded 5 mm and cycle interruptions extended barrel residence time beyond 8 min. This is an operational boundary for unpigmented resin; black or colored versions may mask yellowing but do not arrest molecular-weight loss. Published data for this specific trial configuration is limited, but the observation is consistent with PBT hydrolysis chemistry. For open hopper systems in ambient relative humidity above 60%, dried pellets can regain moisture quickly; a closed hopper dryer or direct suction feed from a desiccant dryer is necessary to prevent intermittent splay defects. Unopened bags should be stored in a dry area below 50% RH; opened bags must be resealed or transferred to a hopper dryer.

    Electrical insulation performance of S600F40 NC010 is governed by a comparative tracking index of 600 V under IEC 60112, which supports use in low-voltage connectors and terminal blocks. The dielectric strength at 2.0 mm is listed as 25 kV/mm under IEC 60243-1. These properties are not sufficient for high-voltage insulation or for designs requiring UL 94 V-0; the grade is classified UL 94 HB at 0.75 mm in natural color. End-product evaluation under IEC 60695-2-11 glow-wire requirements remains mandatory for appliance and electrical applications because the base resin does not provide flame-retardant behavior. Typical injection-molded components include low-profile connector housings, relay covers, sensor bodies, switch actuators, appliance control panels, and automotive interior electrical parts. In thin-wall connector applications, the high melt volume-flow rate permits filling of wall sections below 1 mm on multi-cavity tools when gate location and melt temperature are optimized. Mold-filling simulation should be used to verify shear heating, pressure requirements, and weld-line position because published data for exact part geometries is limited.

    When glass-fiber reinforcement is removed: shrinkage, warpage, and mechanical stiffness

    Relative to a 30 wt% glass-fiber-reinforced PBT, S600F40 NC010 reduces density from approximately 1.50–1.60 g/cm³ to 1.31 g/cm³ under ISO 1183-1. Tensile modulus decreases from the typical 9000–10000 MPa range for glass-filled grades to 2600 MPa under ISO 527-1/-2. Heat deflection temperature at 1.8 MPa falls from roughly 200 °C for glass-filled PBT to 60 °C for the unreinforced grade. These reductions are offset by more uniform mold shrinkage of approximately 1.9–2.1% in flow and transverse directions under ISO 294-4, lower warpage in flat parts, and the absence of fiber-rich weld lines that can reduce tensile strength at knit lines in complex geometries. The isotropic shrinkage response is particularly relevant in connector bodies and sensor housings where differential flow/transverse shrinkage in filled grades causes post-molding dimensional drift.

    Compared with lower-flow unreinforced PBT grades such as S600F10 NC010, S600F40 NC010 has a higher melt volume-flow rate and lower melt viscosity. In production-scale thin-wall molding, this reduces fill pressure but also lowers notched impact strength because high-flow PBT grades typically have lower molecular weight than lower-flow unreinforced equivalents. The trade-off is acceptable where the part is stiffness-critical or geometry-limited rather than impact-critical. For thick-wall parts with sections above 3 mm, lower-flow unreinforced PBT may provide better process control because the higher melt viscosity reduces jetting and helps pack out large bosses without gas entrapment. In such thick sections, the high-flow grade may require lower injection speed and higher hold pressure to prevent sink marks and vacuum voids at the intersection of ribs and nominal wall.

    Flame-retardant PBT grades can achieve UL 94 V-0 at 0.75 mm but may contain halogenated or halogen-free flame-retardant additives that can reduce comparative tracking index or promote plate-out and mold corrosion. S600F40 NC010 is halogen-free by base chemistry but rates only HB under UL 94. Selection of this grade for electrical parts therefore assumes that end-product flammability requirements can be met by enclosure design or that the final assembly does not require a V-0 resin. For UL 94 V-0 requirements, a flame-retardant Crastin grade must be specified instead. Regulatory compliance for S600F40 NC010 is documented by the supplier for RoHS 2011/65/EU and REACH SVHC obligations. Food-contact and medical grades are not covered by the NC010 natural specification unless separate certifications are obtained. UL recognition is for natural color at listed thicknesses; colored masterbatch formulations require separate end-product testing.

    Top