| HS Code | 228975 |
| Polymer Type | Unreinforced polybutylene terephthalate (PBT) |
| Reinforcement | None |
| Color | Natural (NC010) |
| Density | 1.30 g/cm³ |
| Melt Volume Flow Rate 250 C 2 16 Kg | 9 cm³/10 min |
| Molding Shrinkage Parallel | 1.7 % |
| Molding Shrinkage Normal | 1.9 % |
| Tensile Modulus | 2600 MPa |
| Tensile Stress At Yield | 60 MPa |
| Tensile Strain At Yield | 4.5 % |
| Tensile Strain At Break | 30 % |
| Charpy Notched Impact Strength 23 C | 4 kJ/m² |
| Hdt At 1 8 Mpa | 50 °C |
| Hdt At 0 45 Mpa | 150 °C |
| Melting Temperature | 225 °C |
| Water Absorption At Saturation | 0.4 % |
As an accredited Celanese Crastin® Unreinforced PBT S600F10 NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Celanese Crastin® S600F10 NC010 unreinforced PBT is supplied in 25 kg moisture-barrier bags, palletized for industrial handling. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): palletized 25 kg bags of Celanese Crastin® Unreinforced PBT S600F10 NC010, shrink-wrapped and secured for export. |
| Shipping | Celanese Crastin® Unreinforced PBT S600F10 NC010 is shipped as non-hazardous polybutylene terephthalate resin pellets in sealed moisture-barrier bags or containers, typically palletized. It is not regulated for transport and requires no UN number or hazard label. Store in a cool, dry area and avoid excessive heat. |
| Storage | Store Celanese Crastin® Unreinforced PBT S600F10 NC010 in its original sealed packaging in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, moisture, and incompatible materials such as strong oxidizers. Keep containers closed to prevent contamination and moisture pickup. Avoid prolonged humid exposure; dry before processing if required, and follow the SDS and local regulations. |
| Shelf Life | Shelf life is typically 2 years from delivery when stored unopened in a dry, cool place. |
Competitive Celanese Crastin® Unreinforced PBT S600F10 NC010 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Celanese Crastin® S600F10 NC010 is an unreinforced polybutylene terephthalate (PBT) injection-molding and extrusion grade supplied as natural-color pellets. The grade code S600F10 identifies a medium-flow PBT composition; the suffix NC010 indicates the natural, uncolored appearance. Typical data measured on dry-as-molded specimens at 23°C include a melt volume-flow rate of 10 cm³/10 min under ISO 1133-1:2022 at 250°C and 2.16 kg, a density of 1.31 g/cm³ under ISO 1183-1:2019, and a tensile modulus of 2600 MPa under ISO 527-1/-2. The unfilled nature of S600F10 NC010 produces isotropic shrinkage and high elongation compared with glass-reinforced PBT, while the medium melt-viscosity range permits filling of multi-cavity tooling with wall sections from approximately 0.8 mm to 3.0 mm, depending on flow length and gate geometry.
The material is generally specified for electrical connectors, relay bobbins, switch housings, coil formers, motor brush holders, fuse holders, and appliance housings. The selection of an unreinforced PBT grade for these components rests on the combination of high crystallization rate, low equilibrium moisture absorption relative to polyamide, and good dimensional stability in controlled indoor service. In such applications, the resin is processed at melt temperatures of 250°C to 270°C and mold temperatures of 40°C to 80°C. Published processing guides require pre-drying at 120°C for 2 h to 4 h in a desiccant dryer with a dew point of -30°C or lower. The target moisture content before plastication is below 0.02% because hydrolytic degradation of the ester backbone accelerates above that threshold. The grade is classified under ISO 1043 as PBT and is normally marked as PBT on molded parts when part marking is required.
The “F10” portion of the designation is a flow indicator rather than a precise specification limit. For S600F10 NC010, the nominal melt volume-flow rate is 10 cm³/10 min at 250°C under 2.16 kg. The melt is shear-thinning across the injection-molding shear-rate range, but the grade is not formulated with hyperbranched flow modifiers; therefore spiral-flow behavior under thin-wall conditions is lower than that of high-flow PBT grades with MVR values of 20 cm³/10 min or more. This viscosity position makes S600F10 NC010 appropriate for parts with longer flow-length ratios and moderate section thickness, where excessive jetting and flash in multi-cavity tools are avoided by the higher melt pressure stability of the medium-flow resin. Barrel residence times should be kept below 8 min to 10 min at melt temperatures above 260°C; prolonged exposure to thermal stress shifts the MVR upward and reduces notch sensitivity as molecular weight decreases. Shot capacity should use 40% to 70% of the machine barrel so that plastication residence time stays within the recommended envelope.
The primary difference is the absence of glass-fiber reinforcement. In S600F10 NC010, the tensile modulus of 2600 MPa is closer to the amorphous PBT matrix response, whereas 30 wt% glass-reinforced PBT grades typically exhibit tensile moduli of 9500 MPa to 11000 MPa. This lower modulus reduces notch sensitivity and permits higher elongation at break, but it also limits the use of the unfilled grade in creep-limited structural parts. Under 1.8 MPa flexural load, the heat deflection temperature of S600F10 NC010 is approximately 60°C, compared with 200°C to 210°C for reinforced PBT. The lower heat deflection temperature is not an indication of melting-point change; the crystalline melting point of PBT remains at approximately 225°C under ISO 11357-1/-3. Instead, the unfilled grade softens at lower service temperatures because the matrix alone carries the applied load without the rigid fiber network.
| Property | Test method | S600F10 NC010 | 30 wt% GF PBT reference range |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 1.31 g/cm³ | 1.52–1.55 g/cm³ |
| Tensile modulus | ISO 527-1/-2 | 2600 MPa | 9500–11000 MPa |
| Tensile stress at yield | ISO 527-1/-2 | 58 MPa | 130–140 MPa |
| Nominal strain at break | ISO 527-1/-2 | >50% | 2.5–3.5% |
| Charpy notched impact at 23°C | ISO 179-1/1eA | 4.0 kJ/m² | 8.0–10.0 kJ/m² |
| Heat deflection temperature at 1.8 MPa | ISO 75-1/-2 | 60°C | 200–210°C |
| Heat deflection temperature at 0.45 MPa | ISO 75-1/-2 | 160°C | 220–225°C |
| Molding shrinkage, parallel/normal | ISO 294-4 | 1.5% / 1.8% | 0.2% / 0.5% |
The unfilled grade offers practical advantages in tool wear, surface finish, and dimensional isotropy. Glass-filled grades produce anisotropic mold shrinkage, typically 0.2% parallel and 0.5% normal to flow in 2 mm plaques, while S600F10 NC010 exhibits shrinkage in the range of 1.5% to 1.8% with much lower anisotropy. Thus, the unfilled material is preferred when flatness, roundness, and uniform post-mold shrinkage dominate design requirements, provided the mechanical loads remain below the creep threshold of unreinforced PBT. In drive couplings, pump impellers, or brackets exposed to torsional or flexural stress, the unfilled grade is generally unsuited unless stiffness and creep resistance are augmented by geometric ribs and thicker sections. Compared with flame-retarded PBT grades, S600F10 NC010 also retains higher comparative tracking index and better weld-line strength because no flame-retardant filler or reactive additive disrupts the matrix, but it is not a UL 94 V-0 material.
For injection molding, standard three-zone reciprocating screw machines with general-purpose screws of 20:1 to 25:1 L/D and compression ratios between 2.5:1 and 3.5:1 are suitable. A non-return valve of the ring or ball type is recommended to maintain shot consistency at back pressures of 2 MPa to 5 MPa. The feed throat should be cooled to prevent pellet bridging, and the hopper should be blanketed with dry air if ambient relative humidity exceeds 60%. Melt temperature measured by air shot or infrared pyrometry should be held at 250°C to 270°C; the nozzle temperature should be set near the upper end to prevent freeze-off at the sprue bushing. Mold temperatures below 40°C reduce surface gloss and crystallinity, producing parts with lower chemical resistance and higher post-mold shrinkage. Mold temperatures above 80°C extend hold time and may cause sticking in deep-draw cores if the part is not adequately drafted.
Screw speed and injection velocity are set to avoid melt fracture at the gate and to minimize shear heating. For thin-wall connectors with wall stock of 0.8 mm, injection velocities of 150 mm/s to 300 mm/s and holding pressures of 60 MPa to 90 MPa are typical starting points in production trials. For thicker sections above 3.0 mm, the velocity is reduced to prevent jetting and gas entrapment; pack pressure is held until gate freeze is confirmed by short-shot weight plateau measurements. Venting depths of 0.01 mm to 0.02 mm on the parting line are used because unfilled PBT does not generate volatiles at a high rate, but moisture or degraded regrind can generate volatile decomposition products and blistering if vents are blocked. Hot-runner systems are allowed provided the manifold and drops are individually controlled, with no dead spots exceeding the recommended residence-time limits. In multi-cavity connector and relay-bobbin tooling, the unfilled grade is often selected over glass-filled alternatives to reduce abrasion on gate inserts and core pins, particularly in tools running more than 1 × 106 cycles. The absence of glass fibers lowers tool maintenance frequency, but the molder must compensate for higher mold shrinkage and lower ejector temperature stiffness.
Regrind addition up to 25 wt% is permissible when the material is dry, free of fines, and generated from well-stabilized S600F10 NC010 sprues and short shots. Above that fraction, the principal limitation is the cumulative thermal-oxidative history of the regrind. Each additional heat history reduces the number-average molecular weight of the polybutylene terephthalate chain, leading to an increase in melt volume-flow rate and a measurable loss in elongation at break and Charpy notched impact. In production trials with similar medium-flow unreinforced PBT grades, MVR shifts of 15% to 25% have been observed at 40 wt% regrind, but published data for this specific S600F10 NC010 configuration at that high regrind level is limited. The degradation mode is autocatalytic hydrolysis of ester linkages; moisture introduced by improper drying attacks the polymer backbone, generating carboxyl end groups that accelerate further chain scission. The resulting molded parts may exhibit silver streaks, reduced weld-line strength, and an increase in brittleness at low ambient temperatures. For critical electrical or safety-related components, regrind use above 10 wt% is not recommended unless the end-use specification explicitly permits recycled content and the molder can demonstrate consistent MVR, tensile elongation, and impact performance on each lot. Dryers should be cleaned of fines and dust before regrind is reintroduced; contaminated fines can carbonize at melt temperatures above 260°C and produce black specks in natural-color parts.
S600F10 NC010 is an unfilled, non-flame-retarded PBT; the UL 94 rating is typically HB at 1.6 mm thickness. It is not designed to replace V-0-rated flame-retarded PBT in appliance or electrical parts where a UL 94 V-0 classification at 0.8 mm or 1.6 mm is required. The absence of halogenated or phosphorus-based flame-retardant additives preserves higher comparative tracking index and mechanical properties relative to many flame-retarded compounds. For electrical insulating parts, the volume resistivity is typically on the order of 1 × 1015 ohm·cm when measured under IEC 60093, and the surface resistivity is correspondingly high. The dielectric strength of mold-grade PBT is typically 20 kV/mm to 25 kV/mm under IEC 60243-1 for 2 mm specimens, but actual values depend on specimen thickness, conditioning, and electrode geometry. The comparative tracking index is commonly reported at 600 V under IEC 60112, which places unfilled PBT in the higher tracking class for unfilled thermoplastics. These electrical values support use in connectors, switches, and relay bodies where moderate voltage stress and intermittent arcing may occur. The resin is not recommended for high-voltage cable accessories or outdoor insulators exposed to continuous UV and moisture without additional stabilization.
Regulatory status should be confirmed from the current Celanese product data sheet and regulatory statement. The grade is generally supplied without intentionally added lead, cadmium, mercury, hexavalent chromium, polybrominated biphenyls, or polybrominated diphenyl ethers above the thresholds in Directive 2011/65/EU as amended by (EU) 2015/863. REACH compliance under Regulation (EC) No 1907/2006 depends on the article and regional supply; the manufacturer’s statement should be consulted for substances of very high concern. Food-contact uses are not assumed: FDA clearance under 21 CFR 177.1660 applies only to specific polymer compositions and end-use conditions, and unfilled natural PBT may be altered by additives, processing aids, or regrind. Therefore, a food-contact authority statement is required before any application involving food or beverage contact.
In connector and relay-bobbin tooling, the unfilled grade is often selected over glass-filled alternatives to reduce abrasion on gate inserts and core pins, particularly in multi-cavity tools running more than 1 × 106 cycles. The absence of glass fibers lowers tool maintenance frequency, but the molder must compensate for higher mold shrinkage and lower ejector temperature stiffness. For thin-wall connector bodies, mold temperatures at the upper end of the recommended range (80°C) improve surface definition and reduce frozen-in orientation. For thick bobbin flanges, lower mold temperatures (40°C to 50°C) shorten cycle time but may increase void formation if packing pressure is terminated before gate freeze. The processing window narrows when hot-runner manifold temperatures exceed 270°C, because degradation of unstabilized resin at dead spots produces surface splay and weakens weld lines. Thus, the grade is best deployed in tools designed with generous venting, minimal hot-runner dead volume, and no long residence-time paths.