Celanese Crastin Unreinforced Pbt Pc164 Nc010

Celanese Crastin® Unreinforced PBT PC164 NC010

    • Product Name: Celanese Crastin® Unreinforced PBT PC164 NC010
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 343943
    Density 1.30 g/cm3
    Melt Volume Flow Rate 250 C 2 16 Kg 8.0 cm3/10 min
    Water Absorption 23 C 24 H 0.10 %
    Water Absorption 23 C Saturation 0.40 %
    Moisture Absorption 23 C 50 Rh 0.20 %
    Tensile Modulus 2600 MPa
    Tensile Stress At Yield 55 MPa
    Tensile Strain At Yield 5.0 %
    Nominal Strain At Break >50 %
    Charpy Notched Impact Strength 23 C 5 kJ/m2
    Charpy Unnotched Impact Strength 23 C No break
    Melting Temperature 225 C
    Heat Deflection Temperature 0 45 Mpa 150 C
    Heat Deflection Temperature 1 8 Mpa 50 C
    Vicat Softening Temperature 175 C
    Coefficient Of Linear Thermal Expansion Flow 1.2E-4 /C
    Volume Resistivity >1E15 ohm*cm
    Dielectric Constant 1 Mhz 3.2
    Dissipation Factor 1 Mhz 0.002
    Ul 94 Flammability Rating HB

    As an accredited Celanese Crastin® Unreinforced PBT PC164 NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Celanese Crastin® Unreinforced PBT PC164 NC010 is packaged in 25 kg moisture-barrier bags, palletized for industrial storage and handling.
    Container Loading (20′ FCL) 20′ FCL loaded with Celanese Crastin® Unreinforced PBT PC164 NC010 in 25 kg bags, palletized, shrink-wrapped, secured, and weight-compliant.
    Shipping Celanese Crastin® Unreinforced PBT PC164 NC010 is shipped as non-hazardous thermoplastic resin pellets, typically in moisture-barrier 25 kg bags or octabins on pallets. Keep dry and protected from heat and UV; no UN hazard class or special transport labeling is required.
    Storage Store Celanese Crastin® Unreinforced PBT PC164 NC010 in its original sealed packaging/containers in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, heat, ignition sources, moisture, and humidity fluctuations. Keep containers closed when not in use, avoid prolonged high temperatures, and use first-in-first-out stock rotation. Follow supplier SDS and local regulations. Store away from incompatible substances and inspect packaging for damage.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in original unopened packaging under dry, cool conditions.
    Free Quote

    Competitive Celanese Crastin® Unreinforced PBT PC164 NC010 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Celanese Crastin® Unreinforced PBT PC164 NC010 is an unfilled, natural-colour polybutylene terephthalate injection-moulding grade. The NC010 designation identifies an uncoloured natural resin; the composition contains no glass, mineral, or impact-modifier filler. Dry-as-moulded density is 1.30 g/cm³ per ISO 1183-1, and melt volume-flow rate is approximately 19 cm³/10 min at 250 °C under 2.16 kg load per ISO 1133-1:2022. Differential scanning calorimetry per ISO 11357-1 and ISO 11357-3 records a melting endotherm near 225 °C; on cooling at 10 K/min, the crystallisation exotherm typically falls between 185 °C and 195 °C. These values place the grade in the medium-flow unfilled PBT range used for injection-moulded insulating components, connector bodies, switch parts, and small precision mechanisms.

    PBT is a semi-crystalline aromatic polyester. Under injection-moulding cooling, PC164 NC010 develops crystallinity whose level and spherulite size depend on mould temperature and cooling rate; these morphological variables influence final modulus, impact response, and solvent resistance. Consequently, the same nominal melt-flow value does not fully define the moulded part performance; mould temperature and packing pressure must be included in any realistic assessment.

    Because the grade is unreinforced, tensile behaviour is ductile rather than fibre-dominated. Tensile modulus per ISO 527-1/-2 at 23 °C is approximately 2,600 MPa; tensile stress at yield is near 55 MPa; nominal strain at break exceeds 30%. Flexural modulus per ISO 178 is approximately 2,400 MPa, with flexural strength near 80 MPa. Notched Charpy impact per ISO 179-1/1eA at 23 °C is approximately 3.0 kJ/m²; unnotched Charpy specimens usually show no break under standard laboratory conditions. Heat deflection temperature per ISO 75-1/-2 is approximately 60 °C at 1.80 MPa and near 150 °C at 0.45 MPa. Water absorption at saturation per ISO 62 is approximately 0.2%. This low moisture affinity supports electrical use in humid air but does not by itself guarantee surface tracking resistance in condensing environments.

    What Distinguishes PC164 NC010 From Glass-Fibre Reinforced Crastin PBT in Moulded Assemblies?

    The primary difference is reinforcement content. PC164 NC010 has no glass fibre. A 30 wt% glass-fibre PBT typically increases density to approximately 1.53 g/cm³ and tensile modulus to 9,500–11,000 MPa, but reduces nominal strain at break to 2.5–3.0%. The unfilled grade is selected when the design can accept lower stiffness and instead requires ductility, low warpage, lower tool wear, and surface finish without fibre prominence. Table 1 compares typical dry-as-moulded values.

    PropertyPC164 NC010 unreinforced30 wt% glass-fibre PBTTest method
    Density1.30 g/cm³1.53 g/cm³ISO 1183-1
    Tensile modulus2,600 MPa9,500–11,000 MPaISO 527-1/-2
    Tensile stress at yield55 MPa135 MPaISO 527-1/-2
    Nominal strain at break>30%2.5–3.0%ISO 527-1/-2
    Flexural modulus2,400 MPa9,000 MPaISO 178
    Notched Charpy impact, 23 °C3.0 kJ/m²8–10 kJ/m²ISO 179-1/1eA
    Heat deflection temperature, 1.80 MPa60 °C200 °CISO 75-1/-2
    Mould shrinkage, flow direction1.8–2.0%0.3–0.5%ISO 294-4

    The difference extends beyond stiffness. E-glass fibre has a modulus near 70 GPa, but fibre orientation during injection moulding makes shrinkage anisotropic in glass-filled grades. In PC164 NC010 the melt is less viscous and less abrasive; injection moulds can use smaller gates, and reciprocating screw tips and check rings experience lower wear than with glass-fibre compounds. Shot-to-shot pressure variation in small connector moulds is usually lower because the melt has no fibre bundles to orient and break during plastication.

    The melt volume-flow rate of approximately 19 cm³/10 min under 2.16 kg places PC164 NC010 in a higher-flow part of the unfilled PBT spectrum than higher-viscosity general-purpose PBT grades. This flow level supports thin-wall filling but reduces melt strength; it is not intended for extrusion blow moulding or sheet extrusion. As an unmodified PBT, PC164 NC010 has lower notched impact resistance than impact-modified PBT grades used for connector latches and snap-fit housings. Impact-modified PBT may contain elastomeric modifiers that increase notched Charpy impact by a factor of two or more but reduce tensile modulus and HDT. PC164 NC010 retains higher tensile modulus, high CTI, and better chemical resistance than many impact-modified grades; when a snap-fit design requires repeated flexure at low temperature, prototype testing is required because the unreinforced grade at 3.0 kJ/m² notched Charpy may be marginal under high-speed snap engagement.

    Before melt feeding into a 40 mm, 20:1 L/D general-purpose injection screw, PC164 NC010 must be dried in a closed-loop desiccant dryer. Drying at 110–120 °C for 4–6 h with inlet-air dew point at or below -30 °C is typical; residual pellet moisture should be below 0.02% by weight before moulding. In high-humidity plants, regeneration air with dew point below -40 °C provides drying margin. A three-zone screw with compression ratio between 2.0:1 and 2.5:1 and a back-flow check valve is usually sufficient; high-shear barrier mixing sections are unnecessary and may locally raise melt temperature above 270 °C, causing discoloration and molecular weight loss. Melt temperature measured at the nozzle should be held at 240–260 °C. Mould wall temperature should be maintained between 40 °C and 80 °C; higher mould temperature near 80 °C increases crystallinity, improves surface appearance, and reduces post-mould shrinkage, while lower mould temperature near 40 °C shortens cooling time but can increase residual stress and later dimensional change.

    For hot-runner valve-gate systems, manifold and nozzle setpoints should not exceed 260 °C to limit residence-time degradation. Shear heating can raise local melt temperature by 10–20 K above setpoint, so external thermocouple readings are not sufficient; purge-temperature checks are recommended after grade or colour changes. Total melt residence time in the barrel and hot runner at 250 °C should be kept below 5 min to avoid viscosity increase and impact-strength loss in thin-wall sections. On production lines, inadequately dried material produces silver streaking, nozzle drool, and reduced tensile elongation; the splay is caused by steam expanding at the flow front. Overdrying above 120 °C or beyond 6 h may discolour the natural resin and should be avoided unless verified by melt-flow or colour measurement.

    Electrical Insulation Behaviour and Creepage Current Resistance After Humid Ageing

    At 23 °C and 50% RH, PC164 NC010 exhibits a comparative tracking index of 600 V per IEC 60112, dielectric strength near 20 kV/mm per IEC 60243-1, and volume resistivity above 1 × 10¹³ Ω·m per IEC 62631-3-1. Dielectric constant at 1 MHz is approximately 3.2 per IEC 60250. These values support use in connectors, terminal blocks, coil formers, and low-voltage switch parts. The data are dry-condition values; mould release, condensed moisture films, and conductive dust can reduce creepage strength. The grade is not fire-retarded; UL 94 classification is typically HB at 1.6 mm. Applications requiring V-0, V-2, or glow-wire compliance should use a flame-retardant Crastin PBT grade or validate the completed assembly by the relevant end-product standard.

    When Warpage or Anisotropic Shrinkage Limits Glass-Fibre PBT in Miniature Connector Housings

    Mould shrinkage in PC164 NC010 is higher than in glass-fibre PBT but more uniform in orthogonal directions. On plaques per ISO 294-4, flow-direction shrinkage is approximately 1.8–2.0%, and transverse shrinkage is approximately 1.7–1.9%. A 30 wt% glass-fibre PBT may shrink only 0.3–0.5% in the flow direction but exhibits greater directionality due to fibre orientation. In miniature connector housings with closely spaced pin arrays, glass-fibre orientation around core pins can produce flatness deviation, pin-position drift, and flash. PC164 NC010 is therefore used when dimensional uniformity and low moulded-in stress are more important than tensile modulus. The unfilled grade also reduces abrasive wear on gate inserts, ejector pins, and parting lines, making it suitable for high-cavitation tools requiring consistent cavity-to-cavity fill.

    In multi-cavity connector tools, flow balancing and gate freeze-off are different with unfilled PBT than with glass-fibre compounds. PC164 NC010 typically permits shorter holding-pressure time because the absence of glass fibres lowers melt viscosity and increases effective packing length. Moulders should still validate gate dimensions by short-shot progression; the gate must freeze after packing but before screw recovery ends. A gate land thickness below 0.5 mm on a 1.5 mm wall may solidify too early and increase sink marks. For small connector walls between 0.8 mm and 2.5 mm, flow simulation using actual MVR data from ISO 1133-1:2022 is recommended before tool steel is cut.

    Compared with flame-retardant unfilled PBT grades, PC164 NC010 has a higher comparative tracking index and lower melt viscosity, but it does not provide V-0 performance. Many flame-retardant PBT compounds contain halogenated or phosphorus/nitrogen systems that reduce CTI to between 250 V and 400 V and may increase mould deposit on polished cavities. PC164 NC010 avoids those additive-related issues; it is used where UL 94 HB is acceptable and electrical tracking resistance is the dominant requirement. It is not a direct replacement for halogen-free flame-retardant PBT in unattended appliance circuits where the end-product standard requires glow-wire ignition temperature compliance.

    Above 60°C in Humid Service, Hydrolysis Controls Impact Strength Retention

    Continuous exposure to hot water or steam above 60 °C is an operational boundary for unfilled PBT. Polybutylene terephthalate is an ester polymer; moisture-driven hydrolysis reduces molecular weight, and standard stabilizers do not eliminate this mechanism. A part aged at 85 °C and 85% RH may initially retain dimensions, but notched Charpy impact per ISO 179-1/1eA and tensile elongation per ISO 527-1/-2 can decline before visible cracking occurs. Published data for this specific PC164 NC010 configuration under continuous hot-water immersion is limited; designers should not treat the unfilled grade as hydrolysis-stabilized or hot-water resistant. If chemical exposure includes aromatic solvents, concentrated acids, strong bases, or certain chlorinated hydrocarbons, stress cracking and ester attack are possible; short-term contact with aliphatic hydrocarbons, mineral oils, greases, and dilute acids at room temperature is generally less aggressive. The grade should not be melt-compounded with amine-based additives or strongly basic flame retardants because alkaline conditions accelerate ester hydrolysis and reduce molecular weight during processing.