| HS Code | 482097 |
| Productdesignation | Celanese Crastin® Unreinforced FR PBT S650FR NC010 |
| Polymertype | PBT |
| Reinforcement | Unreinforced |
| Flameretardant | Yes |
| Moldingshrinkage Percent | 1.5-2.0 |
| Ul94rating | V-0 at 0.75 mm |
| Processingmethod | Injection molding |
As an accredited Celanese Crastin® Unreinforced FR PBT S650FR NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Celanese Crastin® S650FR NC010 is supplied in 25 kg moisture-resistant bags, 40 bags per pallet, totaling 1,000 kg per pallet. |
| Container Loading (20′ FCL) | 20′ FCL loading: palletized 25 kg bags of Crastin® S650FR NC010; approximately 20–22 MT net, subject to weight and stowage limits. |
| Shipping | Shipping description: Celanese Crastin® Unreinforced FR PBT S650FR NC010 is a non-hazardous, flame-retardant, unreinforced polybutylene terephthalate resin in pellet form. It is not regulated for transport; no UN number, hazard class, packing group, or marine pollutant designation. Ship dry in closed containers, protected from moisture and contamination. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers tightly closed to prevent moisture and contamination. Avoid prolonged high-temperature exposure. Use first-in, first-out stock rotation and follow the supplier’s safety data sheet for detailed handling and storage precautions. |
| Shelf Life | Shelf life: 24 months from manufacture when stored in original unopened packaging at ≤30°C and ≤65% relative humidity. |
Competitive Celanese Crastin® Unreinforced FR PBT S650FR NC010 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
In thin-wall electrical components where flame propagation must stop after two 10 s flame applications, Celanese Crastin® S650FR NC010 is specified as an unreinforced flame-retardant polybutylene terephthalate (PBT) supplied in natural pellet form. Under UL 94 the grade is rated V-0 at 0.75 mm and 5VA at 3.0 mm, according to the current Celanese product data sheet. The melt volume-flow rate under ISO 1133-1:2022 at 250 °C and 2.16 kg is approximately 18 cm³/10 min; density is reported as 1.45 g/cm³ under ISO 1183-1.
Compared with glass-filled PBT grades, the unfilled composition eliminates fiber-induced anisotropy and reduces tool wear on injection screws and check rings. Tensile modulus of S650FR NC010 is approximately 2500 MPa under ISO 527-2/1A/50, whereas glass-fiber-reinforced PBT grades can exceed 9000 MPa depending on fiber content. The lower modulus reduces notch sensitivity in thin snap arms and allows more uniform cavity filling when wall thickness drops below 1.0 mm.
PBT resins undergo hydrolytic chain scission when heated above the melting point in the presence of moisture. S650FR NC010 therefore requires pre-drying in a forced-air desiccant dryer to a maximum residual moisture of 0.02 wt.%; a drying temperature of 120 °C for 4 h at a dew point of ≤ −40 °C is the standard processing recommendation. In plants where ambient relative humidity exceeds 60%, hopper loader intervals should be kept below 20 min or the material transferred by dry-air conveying, because pellets stored in open containers can regain sufficient surface moisture to produce splay and silver streaking in parts with wall thickness below 0.8 mm.
Melt temperature should be measured at the nozzle rather than in the barrel zone set points and held between 240 °C and 260 °C. Above 265 °C decomposition of the flame-retardant package leads to surface plate-out, screw torque instability, and yellowing in the natural grade. Mold temperature is normally set between 60 °C and 90 °C; mold temperatures below 60 °C restrict crystallization and can generate out-of-plane distortion values of up to 0.5 mm per 100 mm of part length after post-mold annealing.
General-purpose screws with 20:1 to 22:1 L/D and a compression ratio of 2.5:1 to 3.0:1 are adequate for this grade. A shut-off nozzle is preferable because the melt volume-flow rate at processing temperature allows drool at open nozzles. Back pressure of 0.3–0.5 MPa improves homogenization without excessive frictional heating; higher back pressure above 0.7 MPa can increase melt temperature by more than 5 °C and should be avoided.
Residence time in the barrel should remain below 10 min at 250 °C. Shutdowns longer than 10 min require purging with a low-viscosity PBT or a commercial purging compound; direct restart without purging can transfer degraded material into the cavity as black specks. The maximum regrind addition should be limited to 25 wt.% unless mold trials verify mechanical and flammability properties, because repeated melt processing progressively reduces the UL 94 margin at 0.75 mm.
Drying validation should use a dew-point meter at the dryer outlet and a Karl Fischer moisture analyzer. Lot-to-lot moisture in original bags should be confirmed below 0.05 wt.% before processing; if above 0.05 wt.%, drying time should be extended to 6 h at 120 °C. Store in sealed original bags at 20–30 °C; opened bags should be consumed within 24 h or resealed under dry-air purge.
Injection speed should be profiled to maintain a melt-front velocity of approximately 200–300 mm/s at the gate; if the melt front slows below 100 mm/s before the end of fill, premature crystallization can cause weld-line weakness. Peak injection pressure on a direct sprue-gated connector housing is typically 80–120 MPa melt pressure; back pressure not exceeding 0.5 MPa and screw decompression of 3–5 mm minimize gas entrapment at the feed throat.
Gates should be located in the thick-wall section and not beyond a length of 25 mm to avoid jetting. For multi-cavity tools, artificially balanced runners with primary diameter of 4.0 mm and secondary diameter of 3.0 mm are typical for unfilled PBT with this melt viscosity. Cold slug wells should have a diameter of at least 3.0 mm; vent depths of 0.02–0.03 mm at the end of fill prevent burn marks and improve shear heating at the vent edges.
Representative tested values for unfilled Celanese Crastin® S650FR NC010 are summarized below. These are not guaranteed lot-release limits; current Celanese quality certifications and the material’s UL Yellow Card should be consulted for specific batch data.
| Property | Test standard | Representative value / condition |
|---|---|---|
| Density | ISO 1183-1 | 1.45 g/cm³ |
| Molding shrinkage | ISO 294-4 | 1.5–2.0% |
| Melt volume-flow rate | ISO 1133-1:2022 | 18 cm³/10 min at 250 °C, 2.16 kg |
| Tensile modulus | ISO 527-2/1A/50 | 2500 MPa |
| Tensile stress at break | ISO 527-2/1A/50 | 42 MPa |
| Tensile strain at break | ISO 527-2/1A/50 | 8% |
| Flexural modulus | ISO 178 | 2400 MPa |
| Charpy notched impact | ISO 179-1/1eA | 4 kJ/m² at 23 °C |
| Melting temperature | ISO 11357-1/-3 | 225 °C |
| Deflection temperature | ISO 75-2/Af | 65 °C at 1.8 MPa |
| Comparative tracking index | IEC 60112 | 250 V |
| Volume resistivity | IEC 62631-3-1 | >1E13 Ω·m |
| Surface resistivity | IEC 62631-3-2 | >1E15 Ω |
| UL 94 vertical burn | UL 94 | V-0 at 0.75 mm |
| UL 94 5VA | UL 94 | 5VA at 3.0 mm |
Rheological data for this grade at processing shear rates show shear-thinning behavior typical of PBT. At a shear rate of 1000 s⁻¹ and 250 °C, apparent viscosity is reported in the range of 50–80 Pa·s depending on capillary or rotational instruments; this supports filling of thin walls with moderate injection pressures. Molders should not interpret the high MVR as an indication of low melt strength; ribbon-like hot-runner drool and stringing can still occur if the hot-runner system is not sealed.
When hot-runner systems are used, externally heated manifolds with melt channel diameters of 3.0–4.0 mm are suitable for shot weights below 100 g. Dead spots in valve gates and manifold corners retain material; periodic purging of the hot runner at 250 °C prevents black spec formation. Needle shut-off nozzles with wear-resistant coatings are preferred because the flame-retardant additive may be abrasive to gate surfaces.
Because the use of regrind is limited by thermal history and contamination, processors should meter regrind with a loss-in-weight blender rather than volumetric mixing. Re-ground material should be dried to the same moisture specification as virgin pellets. Repeated extrusion cycles can slightly reduce UL 94 performance at the minimum thickness, so the 25 wt.% regrind limit should not be exceeded without re-qualification of the finished part.
Under UL 94 vertical burn, a V-0 classification permits total flaming combustion time of no more than 10 s per specimen, no flaming drips, and no afterglow beyond 30 s. For S650FR NC010, the flame-retardant system promotes char formation and retards gas-phase combustion, but a V-0 material does not automatically pass larger-scale tests such as the needle-flame test of IEC 60695-11-5 or the glow-wire end-product test of IEC 60695-2-11 without validation on the finished part.
On production lines, field failures include gate blush, splay, brown streaks, and delamination. Splay on the part surface typically indicates moisture above 0.02 wt.% or screw decompression that draws air into the melt. Brown streaks are associated with residence time above 10 min or hot spots above 265 °C. Reducing screw decompression to 3–5 mm and reducing melt temperature by 5 °C often resolves these defects without changing cavity fill.
In a 16-cavity relay bobbin tool with a cold runner and tunnel gates of 1.0 mm diameter, typical cycle times in unfilled PBT with wall thickness 1.5 mm fall between 10 s and 15 s at mold temperatures of 80 °C. Published data for this specific configuration is limited; molders should run a design-of-experiments over injection speed and holding pressure to establish the process window.
When S650FR NC010 replaces a 20 wt.% glass-fiber-reinforced FR PBT, the tensile modulus drops from the reinforced range of 9000–12000 MPa to approximately 2500 MPa under ISO 527-2/1A/50. Deflection temperature under 1.8 MPa similarly falls from values above 200 °C to a range of 60–70 °C by ISO 75-2/Af. Mold shrinkage becomes more isotropic: unreinforced S650FR NC010 exhibits flow and transverse shrinkage of approximately 1.5%–2.0% by ISO 294-4, whereas glass-filled grades typically shrink 0.3%–0.7% in the flow direction and 0.8%–1.2% transverse. This shrinkage pattern reduces warpage in flat connector bodies and bobbin flanges when cavity dimensions are adjusted accordingly.
Relative to a general-purpose unfilled PBT without flame retardant, the primary difference is flammability classification. Non-FR unfilled PBT normally carries a UL 94 HB rating or no rating at thin sections, while S650FR NC010 achieves V-0 at 0.75 mm. The flame-retardant package also reduces tensile strain at break and notched impact: S650FR NC010 typically falls between 3 kJ/m² and 5 kJ/m² notched Charpy at 23 °C under ISO 179-1/1eA, compared with approximately 5–10 kJ/m² for unfilled non-FR PBT. For snap-fit beams, the lower allowable strain should be used in finite-element models; a strain limit of 1.5% is a conservative starting value for design.
Within the Celanese Crastin portfolio, the FR designation indicates flame-retardant behavior; the NC010 suffix indicates natural color. S650FR NC010 differs from reinforced FR grades in that it contains no glass fiber; ash content is typically below 5% under ISO 3451-1. It differs from impact-modified grades in that notched Charpy is not raised by elastomer domains; therefore, press-fit and snap-fit insertion must consider lower ductility.
Electrical applications include relay bobbins, connectors, switch housings, fuse holders, and motor brush holders specified under IEC 60335-1 or UL 1446. In these components the combination of comparative tracking index above 250 V and volume resistivity above 1E13 Ω·m supports creepage distances calculated from IEC 60664-1. For parts exposed to high humidity, a post-mold annealing cycle of 4 h at 100 °C may be necessary to stabilize dimensions and remove molded-in stress, particularly around metallic inserts.
Continuous service temperature is not a single value; UL RTI ratings from the UL Yellow Card should be consulted. Long-term exposure to automotive coolants, alkaline cleaners, or strong acids should be tested under ISO 175 or ASTM D543 because PBT undergoes chain scission in hydrolytic environments, especially above 60 °C. The grade should not be assembled with adhesives that release amines or with lubricants containing esters that may plasticize the surface.
No compound containing phosphorus-based flame retardant should be assumed halogen-free. Celanese Crastin® S650FR NC010 may contain halogenated flame-retardant components; users must verify compliance with Directive 2011/65/EU and Regulation EC 1907/2006 from the current Celanese regulatory datasheet. In plants that require PFAS-free or halogen-free materials, published performance data for this specific configuration is limited, and alternative PBT grades should be screened under the same UL 94 and IEC 60112 protocols.
The NC010 natural grade is translucent to off-white; adding masterbatch can reduce flammability performance if the carrier resin is incompatible. Any colored variant must be UL 94 re-qualified at the final wall thickness because pigments can act as nucleation sites and alter burn extinguishing time. Carbon black above 0.5 wt.% can reduce CTI and dielectric strength under IEC 60243-1; UL Yellow Card recognition may be voided unless the colored compound is certified.