Celanese Crastin Toughened Pbt St820 Nc010

Celanese Crastin® Toughened PBT ST820 NC010

    • Product Name: Celanese Crastin® Toughened PBT ST820 NC010
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 396597
    Density G Cm3 approx. 1.45
    Glass Fiber Content Percent approx. 20
    Tensile Modulus Mpa approx. 6500-7000
    Tensile Stress At Break Mpa approx. 100-110
    Tensile Strain At Break Percent approx. 3
    Charpy Notched Impact Strength 23c Kj M2 approx. 9-10
    Charpy Unnotched Impact Strength 23c Kj M2 approx. 45-50
    Heat Deflection Temperature A C approx. 200-205
    Heat Deflection Temperature B C approx. 170-175
    Melting Temperature C approx. 225
    Water Absorption Percent approx. 0.2
    Molding Shrinkage Parallel Percent approx. 0.3-0.7
    Molding Shrinkage Normal Percent approx. 0.6-1.0
    Volume Resistivity Ohm M approx. 1E14
    Dielectric Constant 1mhz approx. 3.5
    Dissipation Factor 1mhz approx. 0.002

    As an accredited Celanese Crastin® Toughened PBT ST820 NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Celanese Crastin® Toughened PBT ST820 NC010 is packaged in 25 kg moisture-barrier bags, palletized and clearly labeled for safe handling and storage.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized 25 kg bags of Celanese Crastin® Toughened PBT ST820 NC010, secured and shrink-wrapped for export.
    Shipping Celanese Crastin® Toughened PBT ST820 NC010 is shipped as non-hazardous thermoplastic pellets in sealed moisture-barrier bags or octabins. It is not regulated for transport. Keep packages dry, closed, and protected from direct sunlight, heat, and damage; use normal ambient storage and handling.
    Storage Store Celanese Crastin® Toughened PBT ST820 NC010 in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers tightly closed to prevent moisture pickup and contamination. Avoid incompatible chemicals, use original packaging, follow local regulations, control dust, and rotate stock first-in, first-out.
    Shelf Life Celanese Crastin® ST820 NC010 has a typical two-year shelf life when stored unopened in original packaging, cool, dry, and away from sunlight.
    Free Quote

    Competitive Celanese Crastin® Toughened PBT ST820 NC010 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Celanese Crastin® Toughened PBT ST820 NC010 is an unfilled, impact-modified polybutylene terephthalate injection-molding grade supplied in natural color. The ST820 designation identifies a toughened PBT chemistry in which a dispersed elastomeric phase alters crack-initiation and crack-propagation behavior in the semi-crystalline polybutylene terephthalate matrix. Published typical density is 1.22 g/cm³ when measured according to ISO 1183-1, and the melt volume-flow rate is reported as 13 cm³/10 min at 250 °C/2.16 kg according to ISO 1133-1:2022. These values place the grade in the medium-viscosity range for injection molding of thin-wall and medium-flow-length parts. The NC010 suffix denotes natural color without pigmentation, which permits independent masterbatch coloring at the molding line. Because the matrix retains the ester linkages characteristic of PBT, the material exhibits rapid crystallization, low moisture absorption relative to polyamide, and resistance to many automotive and industrial oils. Unlike standard unfilled PBT grades that display Charpy notched impact energies of approximately 4–6 kJ/m² at 23 °C, ST820 NC010 is designed to shift failure from brittle crack propagation to ductile yielding under high-speed loading. The impact modifier reduces tensile modulus and lowers heat deflection temperature relative to unfilled PBT, and these trade-offs govern substitution decisions in snap-fit, clip, and connector applications.

    How Does the Toughened Phase Alter Notch-Sensitive Failure in PBT?

    When notched Charpy impact values are compared under ISO 179-1/1eA conditions, the difference between ST820 NC010 and standard PBT is not incremental. Standard unfilled PBT grades typically transition from ductile to brittle behavior near room temperature, with notched Charpy energy remaining below 10 kJ/m² and often in the 4–6 kJ/m² range. ST820 NC010 is reported by Celanese to maintain notched Charpy energy in the 60–80 kJ/m² range at 23 °C and to retain approximately 20–30 kJ/m² at −30 °C when measured with the same edgewise notch geometry and 0.25 mm notch radius. This represents a change in deformation micromechanics: the dispersed impact-modifier phase cavitates or debonds under hydrostatic tension, relieving triaxial stress ahead of the notch and permitting shear yielding of the PBT matrix. The tensile properties reflect the same compromise. Typical tensile modulus for ST820 NC010 is approximately 1900 MPa and tensile stress at yield is approximately 35 MPa per ISO 527-1/-2, while standard unfilled PBT grades commonly exhibit tensile modulus above 2500 MPa and yield stress above 50 MPa. Nominal strain at break for ST820 NC010 exceeds 50%, whereas standard PBT often fails below 30% under the same test speed. Flexural modulus is likewise lower than standard PBT, which reduces snap-fit retention force and beam stiffness. Consequently, parts designed with ST820 NC010 may require modest increases in section thickness or rib height to match the stiffness of a standard PBT part.

    Selected published typical property values for Celanese Crastin® Toughened PBT ST820 NC010
    PropertyTest methodPublished typical value
    DensityISO 1183-11.22 g/cm³
    Melt volume-flow rate, 250 °C/2.16 kgISO 1133-1:202213 cm³/10 min
    Tensile modulusISO 527-1/-21900 MPa
    Tensile stress at yieldISO 527-1/-235 MPa
    Nominal strain at breakISO 527-1/-2>50%
    Charpy notched impact strength, 23 °CISO 179-1/1eA60–80 kJ/m²
    Charpy notched impact strength, −30 °CISO 179-1/1eA20–30 kJ/m²
    Melting temperatureISO 11357-1/-3225 °C
    Heat deflection temperature, 0.45 MPaISO 75-1/-2105 °C
    Heat deflection temperature, 1.8 MPaISO 75-1/-250 °C
    Molding shrinkage, parallel / normalISO 294-41.8% / 1.9%
    FlammabilityUL 94HB

    The low-temperature response of ST820 NC010 is particularly relevant for automotive interior and exterior clips that experience impact at subzero temperatures. In laboratory Charpy tests, the transition from high-energy ductile failure to low-energy brittle failure is shifted downward relative to standard PBT, although the material does not exhibit the full subzero ductility of low-density polyethylene. At the same time, the impact modifier reduces the continuous-use temperature under load because the amorphous phase softens at elevated temperatures. Heat deflection temperature under 1.8 MPa is reported near 50 °C, which is in the same range as standard unfilled PBT but lower than filled PBT grades. The grade therefore is not a direct substitute for glass-fiber-reinforced PBT in structural underhood components requiring high-temperature creep resistance.

    Molding of ST820 NC010 requires closed-loop desiccant drying at 110–120 °C for 4 h, with a maximum drying temperature of 130 °C, to achieve residual moisture below 0.02%. Hydrolysis of the polybutylene terephthalate ester linkages is kinetically significant above the melting point; if pellets containing moisture above 0.04% are melted, visible splay, reduced screw recovery consistency, and Charpy impact losses of up to 30% can occur on conventional 110-ton hydraulic reciprocating-screw machines. Barrel temperature profiles normally range from 230 °C at the feed zone to 255 °C at the nozzle, with melt temperature held between 240 °C and 260 °C. At melt temperatures above 265 °C, polymer degradation generates free acid species that accelerate further hydrolysis, and residence time should not exceed 8 min. Mold temperature is specified between 40 °C and 80 °C; lower mold temperatures may quench the surface before the impact-modified phase can fully relax, producing variable Charpy values and lower elongation at break. Higher mold temperatures improve crystallinity and reduce internal stress but extend cooling time. Injection speed should be medium to fast to prevent premature freeze-off in thin sections. Recommended screw back pressure is low, typically 0.3–0.7 MPa, because higher back pressure increases shear heating without improving color. Machines with 20:1 L/D general-purpose screws and compression ratios of 2.5:1 are adequate; vented barrels are not required when drying is adequate. On a 110-ton hydraulic reciprocating-screw machine with a 25 mm diameter, 20:1 L/D screw, stable operation is obtained with a cushion between 2 mm and 4 mm and screw decompression of 3–5 mm. At ambient relative humidity above 60%, pellet drying in a hopper dryer without desiccant is insufficient; the drying air dew point should be −40 °C or lower, and airflow should be at least 3–4 m³/h per kg/h of resin throughput. Molding shrinkage is approximately 1.8% parallel and 1.9% normal as measured by ISO 294-4; the low anisotropy relative to glass-filled PBT simplifies gate location and rib design. Published data for specific equipment configurations is limited, and processors should establish in-house shrinkage values for multi-gated tools.

    When Glass-Fiber-Reinforced PBT Is Replaced by ST820 NC010

    Substitution of glass-fiber-reinforced PBT with ST820 NC010 is justified only when the failure mode is impact fracture rather than high-temperature creep. Reinforced PBT grades provide flexural modulus typically above 8000 MPa and heat deflection temperatures above 200 °C at 0.45 MPa, whereas ST820 NC010 provides flexural modulus below 2000 MPa and heat deflection temperature near 105 °C at 0.45 MPa. In connectors, sensors, fasteners, and interior trim clips, the lower modulus is often acceptable because the part is designed as a compliant beam or snap-fit. The high elongation of ST820 NC010 permits deeper undercut engagement without fracture; a cantilever snap latch with a 2 mm section and 0.8 mm deflection typically operates at lower surface strain than the yield strain of ST820 NC010. The unfilled impact-modified material also eliminates glass-fiber skin effects, reduces tool wear in high-cycle molds, and lowers molded-in anisotropy. Its lower density of approximately 1.22 g/cm³ compared with 1.53 g/cm³ for typical 30% glass-filled PBT reduces part mass.

    Because the material is unfilled and impact-modified, it is used in injection-molded automotive interior clips, cable and wire bundling clips, electrical connector bodies, sensor housings, appliance door latches, and pneumatic fitting sleeves. These applications exploit the combination of chemical resistance to hydrocarbons and lubricants with ductile snap-fit assembly. The material should not be selected for continuous load-bearing gears or structural brackets where creep rupture and fatigue under high load are governing failure modes. The grade is not suited for exposure to hot water or steam above 60 °C for extended periods because hydrolysis of the PBT ester linkage reduces molecular weight. Chemical compatibility with strong acids, strong bases, and some amine-containing additives is limited; amine-based additives can catalyze ester aminolysis and should be avoided. Ultraviolet stabilization is not present in natural ST820 NC010; outdoor load-bearing parts require UV-stabilized black or custom formulations. The grade is supplied with regulatory documentation indicating compliance with 2011/65/EU RoHS and REACH SVHC disclosure obligations as of the date of supply. Flammability is classified as UL 94 HB, so applications requiring V-2 or V-0 performance must use flame-retardant PBT grades instead. Published data for the specific ST820 NC010 electrical configuration is limited; safety-critical connector designs should use verified measurements from the final tool and not generic PBT electrical data.

    Top