Celanese Crastin Toughened Fr Uv Pbt St830fruv Nc010

Celanese Crastin® Toughened FR UV PBT ST830FRUV NC010

    • Product Name: Celanese Crastin® Toughened FR UV PBT ST830FRUV NC010
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 301298
    Productname Celanese Crastin® Toughened FR UV PBT ST830FRUV NC010
    Gradedesignation ST830FRUV NC010
    Polymertype Polybutylene terephthalate (PBT)
    Fillerreinforcement Glass fiber reinforced
    Glassfibercontent 30%
    Impactmodification Toughened / impact modified
    Flameretardancy Flame retardant
    Uvstabilization UV stabilized
    Color Natural (NC010)
    Processingmethod Injection molding
    Materialform Pellets
    Ul94flammabilityrating V-0
    Density 1.68 g/cm³
    Tensilemodulus 10000 MPa
    Tensilestressatbreak 100 MPa
    Elongationatbreak 2.0%
    Hdtat1 8mpa 200 °C
    Meltingtemperature 225 °C

    As an accredited Celanese Crastin® Toughened FR UV PBT ST830FRUV NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-barrier bags, Celanese Crastin® ST830FRUV NC010 is supplied as natural-color toughened FR UV PBT pellets.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of Celanese Crastin® Toughened FR UV PBT ST830FRUV NC010, shrink-wrapped and secured.
    Shipping Celanese Crastin® ST830FRUV NC010 is shipped as non-hazardous PBT resin pellets in sealed bags or octabins. It is not classified as dangerous goods for transport. Keep dry, away from direct sunlight, and avoid moisture uptake. Follow the SDS and applicable local regulations.
    Storage Store indoors in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and oxidizing agents. Keep containers or bags tightly closed to prevent moisture pickup and contamination. Maintain moderate ambient temperatures, avoid prolonged UV exposure, and follow first-in-first-out stock rotation. Consult the SDS and supplier for specific shelf-life and drying requirements.
    Shelf Life Shelf life is typically 24 months from delivery when stored dry and cool in original, unopened packaging.
    Free Quote

    Competitive Celanese Crastin® Toughened FR UV PBT ST830FRUV NC010 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Celanese Crastin® Toughened FR UV PBT ST830FRUV NC010 is an unreinforced, impact-modified, flame-retardant polybutylene terephthalate molding resin supplied in natural color. The NC010 suffix identifies the natural pellet color; ST denotes the toughening package, FR denotes the flame-retardant system, and UV denotes ultraviolet stabilization. The base resin is a semicrystalline thermoplastic polyester with a melting point near 225 °C measured by ISO 11357-1/-3. Because no glass fiber or mineral filler is present, the compound retains high elongation-to-break and a ductile failure mode, but short-term tensile creep resistance and dimensional stability are lower than those of reinforced PBT compounds. The material is classified for injection molding and is used where thin-wall flame retardance, low-temperature impact, and outdoor UV resistance must be combined. The natural-grade designation does not define the final part color; color concentrates are commonly added at the press, but colorant addition may shift the UL 94 rating and must be re-evaluated under IEC 60695-11-10.

    What Property Set Distinguishes ST830FRUV NC010 from Standard Flame-Retardant PBT?

    Standard flame-retardant PBT compounds without impact modification generally exhibit notched Charpy values in the single-digit kJ/m² range at room temperature. ST830FRUV NC010 raises room-temperature Charpy notched impact to a manufacturer-published typical value of 80 kJ/m² under ISO 179-1/1eA, while retaining tensile modulus near 2000 MPa under ISO 527-1/-2. The trade-off is a reduction in tensile modulus relative to unmodified PBT because elastomeric impact modifiers lower room-temperature modulus and increase strain at break. The published nominal strain at break of 50 % indicates ductile tensile failure, which corresponds to reduced notch sensitivity in molded snap arms, living hinges, and enclosure corners.

    The flame-retardant mechanism is balanced against the toughening phase. Flame-retardant additives generally increase stiffness and reduce impact; the toughening package compensates by distributing elastomeric domains through the semicrystalline PBT matrix. The resulting morphology is notch-ductile at room temperature but loses some ductility below the polymer beta transition. The manufacturer-published Charpy notched value at -30 °C is 15 kJ/m², which is lower than the room-temperature value but above that of brittle unreinforced PBT grades.

    The table below summarizes representative physical, mechanical, thermal, and electrical values from the supplier technical data sheet. These are typical values, not lot-specific minimum specifications.

    PropertyTest methodRepresentative published value
    DensityISO 1183-11.31 g/cm³
    Melt volume rate, 250 °C/2.16 kgISO 1133-19.0 cm³/10 min
    Tensile modulusISO 527-1/-22000 MPa
    Tensile stress at yieldISO 527-1/-238 MPa
    Nominal strain at breakISO 527-1/-250 %
    Flexural modulusISO 1781800 MPa
    Flexural strengthISO 17855 MPa
    Charpy notched impact, 23 °CISO 179-1/1eA80 kJ/m²
    Charpy notched impact, -30 °CISO 179-1/1eA15 kJ/m²
    Izod notched impact, 23 °CISO 180/1A55 kJ/m²
    Deflection temperature under load, 1.80 MPaISO 75-1/-270 °C
    Melting temperatureISO 11357-1/-3225 °C
    Dielectric strengthIEC 60243-130 kV/mm
    Comparative tracking indexIEC 60112250 V
    Volume resistivityIEC 600931E15 Ω·m
    Coefficient of linear thermal expansionISO 11359-280 ×10⁻⁶ /K

    For injection molding operations, the resin must be dried to a moisture content below 0.02 % by weight, typically achieved with a desiccant dryer supplying -40 °C dew point air at 120 °C for 4 to 8 h. Drying is not optional because residual moisture hydrolyzes ester linkages at melt temperature, reducing molecular weight and notched impact. Wet pellets stored above 60 % relative humidity require longer drying. The melt temperature is maintained between 240 and 260 °C. Barrel settings from feed to nozzle are typically 230–240 °C at the feed throat, 240–250 °C in compression, 250–260 °C in metering, and 250–260 °C at the nozzle. Mold temperature should be 40–80 °C; the upper end of the range is preferred for thin-wall parts to reduce premature solidification. Back pressure is kept low, typically 0.3–0.7 MPa, to avoid excessive shear heating of the impact modifier. Holding pressure is set to prevent sink marks without overpacking. The material exhibits shear-thinning flow; moderate-to-high injection speeds are used, but excessive shear can cause viscous heating and degradation of the elastomeric phase.

    Combination with amine-based purging compounds or mold releases is not recommended; amines can promote transesterification in the polyester backbone and reduce molecular weight. Regrind from sprues and runners may be reincorporated only after drying and verification of UL 94 performance. Long hot-runner residence times above 260 °C should be avoided because the impact modifier and flame-retardant package may separate or degrade. In multicavity hot-runner tools, ballpoint or open-tip gates with rapid fill rates reduce premature freeze-off and improve impact retention at weld lines.

    When Outdoor UV Exposure Is Combined with Thin-Wall Flame Retardance

    Ultraviolet stabilization in ST830FRUV NC010 is incorporated to preserve color, surface gloss, and impact after outdoor weathering. The grade is targeted at enclosures and structural housings that must pass UL 746C UV and water exposure protocols. The relevant accelerated laboratory method is ISO 4892-2 xenon arc with specified irradiance, black-standard temperature, and water spray cycle. Qualification should be performed on the actual molded surface because knit lines, packing, and gloss can influence crack initiation. Published data for this specific natural formulation under multi-year arid-climate exposure is limited; part-level validation is required. The UV stabilization package is not equivalent to carbon black or opaque pigmentation. Natural NC010 can still show optical surface changes during long-term exposure, although mechanical retention may remain acceptable.

    In electrical enclosure production, the material is processed with hot-runner systems and multicavity tooling. Gate geometry should avoid constrictions below 1.0 mm for direct edge gates; pinpoint gates require fast fill rates. Weld lines in thin ribs reduce impact strength disproportionately. For connectors and terminal housings, the comparative tracking index of 250 V under IEC 60112 supports use in circuits where surface contamination may be present. The current UL Yellow Card and IEC 60695 glow-wire data should be consulted for each wall thickness because the rating is thickness-dependent and colorant-dependent.

    Heat Aging Effects Are Evaluated Under Two Distinct Failure Modes

    Thermal aging of ST830FRUV NC010 follows two failure modes: hydrolytic degradation under hot-moist conditions and oxidative embrittlement in dry air. The continuous-use temperature for unreinforced flame-retardant PBT is usually limited by impact retention rather than tensile strength. In dry air, oxidation of the impact modifier causes surface cracking and loss of elongation before the semicrystalline PBT backbone fails. In humid environments, hydrolysis targets ester bonds and reduces molecular weight, which is measurable as a drop in melt volume rate and notched Charpy. Molded bars aged under ISO 188 in air at 120 °C often show a rapid reduction in Charpy notched impact before tensile yield changes. Because the compound contains a flame-retardant package, aging can also shift flame performance and alter char formation. Published data for this specific blend after 1000 h thermal aging is limited; validation should be performed on the final part. The UL Yellow Card may list relative thermal index values for electrical, mechanical, and impact categories, and those values control long-term thermal exposure limits.

    Comparative Limitations Against Glass-Filled PBT and Non-Toughened FR Grades

    ST830FRUV NC010 is not a direct substitute for glass-filled PBT. The tensile modulus of 2000 MPa under ISO 527-1/-2 is lower than that of a 30 % glass-filled PBT, which typically exceeds 9000 MPa. The heat deflection temperature at 1.80 MPa is 70 °C; glass-filled PBT grades often exceed 200 °C at the same stress. Therefore, the toughened flame-retardant grade should be selected when impact and flame retardance dominate, not when creep, heat sag, or dimensional stability is the limiting criterion. Against a non-toughened flame-retardant PBT, ST830FRUV NC010 provides higher notched impact but lower tensile modulus and lower stiffness. The UV package differentiates it from flame-retardant PBT grades without UV stabilization, which may chalk, surface-crack, or lose gloss in outdoor use. The polyester backbone is also hydrolytically attacked by hot alkaline solutions and concentrated oxidizing acids; motor oils and aliphatic hydrocarbons are generally acceptable at ambient temperature, but stress-cracking resistance for specific geometries should be evaluated under ISO 22088-3.

    RequirementStandard or controlling documentVerification position
    FlammabilityIEC 60695-11-10 / UL 94UL Yellow Card controls thickness and colorant
    Outdoor ultraviolet exposureUL 746Cf1/f2 rating per UL Yellow Card
    Accelerated weatheringISO 4892-2Part-level validation required
    Comparative tracking indexIEC 60112Supplier certificate controls lot values
    Restriction of hazardous substancesRoHS Directive 2011/65/EUSupplier declaration and SDS
    REACH SVHC disclosureRegulation EC 1907/2006Supplier safety data sheet

    For outdoor enclosures, retention of impact after UV exposure is the controlling acceptance criterion. Component-level testing per ISO 4892-2 with 0.51 W/m² irradiance at 340 nm, black-standard temperature 65 °C, and a water spray cycle is recommended to benchmark surface cracking after 1000 h. Because natural NC010 is unpigmented, surface haze may increase before structural failure. Molded parts that must maintain UL 94 V-0 at thin sections should be inspected after weathering, because surface degradation can alter the char formation mechanism during vertical burn testing.

    Top