Celanese Crastin Pbt Gf30 Super Tough Sk609 Bk851

Celanese Crastin® PBT+GF30%-Super-Tough SK609 BK851

    • Product Name: Celanese Crastin® PBT+GF30%-Super-Tough SK609 BK851
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 121001
    Productdesignation Celanese Crastin® PBT+GF30%-Super-Tough SK609 BK851
    Polymertype PBT
    Glassfibercontent 30%
    Color Black (BK851)
    Density 1.42 g/cm³
    Tensilemodulus 7500 MPa
    Tensilestressatbreak 110 MPa
    Tensilestrainatbreak 3.0%
    Charpynotchedimpactstrength23c 12 kJ/m²
    Charpyunnotchedimpactstrength23c 50 kJ/m²
    Heatdeflectiontemperaturea 205 °C
    Meltingtemperature 225 °C
    Moldshrinkageparallel 0.3%
    Moldshrinkagenormal 0.9%
    Processingmethod Injection molding
    Melttemperaturerange 240-270 °C
    Moldtemperaturerange 80-100 °C

    As an accredited Celanese Crastin® PBT+GF30%-Super-Tough SK609 BK851 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Celanese Crastin® PBT+GF30%-Super-Tough SK609 BK851 is supplied in 25 kg moisture-barrier bags, palletized and labeled with grade, lot, and safety information.
    Container Loading (20′ FCL) 20′ FCL container loading of Celanese Crastin® PBT+GF30%-Super-Tough SK609 BK851, a 30% glass-fiber reinforced black PBT resin, packed for shipment.
    Shipping Celanese Crastin® PBT+GF30%-Super-Tough SK609 BK851 is a non-hazardous, glass-fiber-reinforced PBT resin supplied as black pellets. Ship in sealed moisture-barrier bags, boxes, or octabins; not regulated for DOT/IATA/IMDG. Store dry, away from excessive heat, and handle with standard industrial precautions to minimize dust.
    Storage Store in a cool, dry, well-ventilated area in original, sealed packaging. Protect from moisture, direct sunlight, heat sources, and ignition. Keep away from incompatible chemicals and strong oxidizers. Avoid prolonged exposure to high humidity; use desiccant if condensation risk exists. Maintain stable temperature and follow local regulations and SDS recommendations.
    Shelf Life Typically 24 months from production date when stored dry, cool, and in original unopened packaging; avoid moisture and direct sunlight.
    Free Quote

    Competitive Celanese Crastin® PBT+GF30%-Super-Tough SK609 BK851 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Celanese Crastin® PBT+GF30%-Super-Tough SK609 BK851 is a 30% by weight glass-fibre-reinforced polybutylene terephthalate compound in which an elastomeric impact-modification package shifts failure response from brittle crack propagation toward ductile yielding under high-strain-rate loading. The BK851 suffix identifies the black colour formulation intended for injection-moulded components where surface appearance, dimensional stability, and low-temperature impact resistance are specified on the same part print. Before lot release, processors typically verify melt volume-flow rate under ISO 1133-1:2022 at 250°C/2.16 kg and residual moisture under ISO 15512:2019, because the elastomeric phase can widen flow variation compared with unmodified PBT-GF30.

    Material Constitution and Standard Designation

    Under ISO 1043-1, the base polymer family is polybutylene terephthalate, and the reinforcement is designated GF30. The super-tough suffix does not alter the ISO 1043 designation but signals a notched impact response above basic PBT-GF30 grades. Glass content determined by ISO 3451-1 ash testing is nominally 30% by weight, with production-lot tolerance typically ±2%. The BK851 suffix is a colour identifier rather than a separate polymer grade. Published data for the exact modifier chemistry in SK609 BK851 is limited, but impact-modified PBT-GF30 compounds of this class generally use a dispersed elastomeric phase selected for low-temperature cavitation and interfacial adhesion to the PBT matrix. Specific lot values for density, filler content, and viscosity should be confirmed against the current Celanese material datasheet and lot certificate.

    How Does the Super-Tough Modifier Shift Low-Temperature Notched Impact Response?

    The impact-modifier phase in super-tough PBT-GF30 has a glass transition below −40°C. Under ISO 179-1:2010 notched Charpy conditions at 23°C, the dispersed rubber particles cavitate and initiate multiple shear bands in the PBT matrix before fibre-matrix debonding becomes the dominant crack path. Unmodified PBT-GF30 typically exhibits notched Charpy values of 6–9 kJ/m² at 23°C under ISO 179-1/1eA, whereas super-tough PBT-GF30 compounds commonly reach 12–20 kJ/m². At −30°C, the unmodified class can fall below 5 kJ/m², while impact-modified systems frequently retain 8–10 kJ/m². The toughness increase is accompanied by a measurable reduction in stiffness: unmodified PBT-GF30 under ISO 527-2:2012 shows tensile modulus values of 8000–10000 MPa, while the super-tough class generally ranges from 5500–7500 MPa. For SK609 BK851, published datasheet-specific values should be retrieved before final design calculations.

    When Pre-Drying and Melt Temperature Deviate from the Recommended Envelope

    On a 100-tonne hydraulic injection moulding machine with a 25 mm general-purpose screw, the barrel profile is set rear 240–250°C, middle 250–260°C, front 250–260°C, and nozzle 250–265°C. Mould surface temperature is maintained at 60–100°C using a closed-loop water or oil temperature control unit. For wall sections below 1.5 mm, the upper half of this range is preferred to avoid premature skin freezing and flow-line formation. Holding pressure is typically 50–70% of actual peak injection pressure, and gate freeze time for a 2.0 mm wall section is 3–6 s. Back pressure is held at 0.3–0.7 MPa to homogenise glass distribution without excessive fibre attrition. Pre-drying is performed at 120°C for 4 hours in a desiccant dryer until residual moisture falls below 0.02% by weight. If ambient relative humidity exceeds 60%, pellet containers should remain sealed and hopper residence time should be limited to 30 minutes. Moisture above 0.03% at melt temperature accelerates hydrolytic chain scission in PBT, reducing intrinsic viscosity and causing silver streaking and loss of weld-line strength within 10 minutes of barrel residence time.

    In automotive engine-compartment connector applications, the material is selected where snap-fit latch arms are subjected to assembly impact loads at −40°C. In production-scale moulding trials, unsupported latch arms with a root radius of 0.8 mm and a wall thickness of 2.0 mm have shown reduced fracture when moulded with a fast injection speed of 120–150 mm/s and a mould temperature of 80°C. The lower modulus of the super-tough grade distributes strain more uniformly than standard PBT-GF30. For power distribution housings, shrinkage anisotropy measured under ISO 294-4:2018 is lower than unfilled PBT, but tools developed for standard PBT-GF30 still require gate and runner rebalancing because the impact modifier reduces thermal diffusivity and can increase differential shrinkage in thick sections.

    Difference in Shrinkage, Warpage, and Tool Design Relative to Standard PBT-GF30

    Compared with standard PBT-GF30, the super-tough package reduces moulded-in stress but can increase total in-plane shrinkage by 0.1–0.3 percentage points. ISO 294-4:2018 measurements on 60 mm × 60 mm × 2 mm plaques generally show parallel shrinkage near 0.3–0.5% and perpendicular shrinkage near 0.5–0.8% for impact-modified PBT-GF30, while unmodified PBT-GF30 tends toward parallel shrinkage of 0.2–0.4% and perpendicular shrinkage of 0.4–0.6%. The amorphous elastomer phase flattens the crystallisation exotherm under ISO 11357-3:2018, so the material can be moulded with lower mould temperatures than a high-flow PBT but reaches peak crystallinity more slowly. For tooling, ejection pins should be placed closer to deep-draw sidewalls, and core pins should have a minimum draft angle of 0.5–1.0° to compensate for the lower flexural modulus. Spiral flow and mould-filling simulation should use class-typical melt viscosity near 100–200 Pa·s at 250°C and 1000 s⁻¹ for 30% glass-filled PBT; impact modification tends to raise low-shear viscosity while reducing shear sensitivity. Gate sizing should account for higher pressure drop in gates below 1.5 mm diameter. A round gate diameter of at least 1.0 mm per 1.5 mm wall section is typically specified to avoid jetting and excessive shear heating.

    Comparative property ranges for 30% glass-fibre-reinforced PBT systems; values are class-typical from ISO specimen testing and not lot guarantees.
    PropertyTest methodUnmodified PBT-GF30Super-tough PBT-GF30 class
    DensityISO 1183-1:20191.50–1.55 g/cm³1.31–1.42 g/cm³
    Tensile stress at breakISO 527-2:201290–110 MPa60–80 MPa
    Tensile modulusISO 527-2:20128000–10000 MPa5500–7500 MPa
    Flexural modulusISO 178:20196500–8500 MPa4500–6500 MPa
    Charpy notched impact, 23°CISO 179-1:20106–9 kJ/m²12–20 kJ/m²
    HDT-A, 1.8 MPaISO 75-2:2013195–210°C180–205°C

    Compared with a PA66-GF30 impact-modified grade in the same connector family, SK609 BK851 absorbs less moisture under ISO 62:2008. PBT typically exhibits 24-hour water absorption below 0.1%, while PA66-GF30 can reach 1.2–1.6% at 23°C. This leads to more stable electrical insulation resistance after humidity ageing; however, PBT-GF30 has a lower continuous use temperature under mechanical load than PA66-GF30 and is more sensitive to alkaline hydrolysis. Designers substituting SK609 BK851 for PA66-GF30 should verify maximum service temperature against the application’s heat-deflection requirement, using ISO 75-2:2013 for short-term screening and UL 746B relative thermal index for long-term ageing. Published data for SK609 BK851 under UL 746B is limited; the current Celanese UL yellow card should be consulted before specification.

    Before Component Release, Regulatory Screening Demands REACH and RoHS Traceability

    Under EU REACH, Regulation (EC) No 1907/2006, moulders must request from the material supplier confirmation of SVHC content in accordance with Article 33. Under Directive 2011/65/EU, Annex II, lead, mercury, hexavalent chromium, PBB, and PBDE must each remain below 0.1% w/w in homogeneous material, with cadmium below 0.01% w/w. A typical non-flame-retarded PBT-GF30 compound does not intentionally contain these substances, but carbon black and glass-fibre sizings require lot-level documentation. The grade is not inherently flame-retarded; if a UL 94 V-0 or VTM-0 classification is required, a flame-retarded PBT-GF30 grade must be specified. Food-contact status under FDA 21 CFR 177.1660 or EU Regulation 10/2011 is not automatically granted for this filled grade; end-use migration testing with the actual food simulant is required before use.

    Regulatory screening matrix for injection-moulded PBT-GF30 components.
    CriterionReferenceTypical obligation for SK609 BK851
    EU REACH SVHC candidate listRegulation (EC) No 1907/2006, Article 33Supplier confirmation required for each lot; no SVHC above 0.1% w/w expected
    RoHS restricted substancesDirective 2011/65/EU, Annex IILead, cadmium, mercury, hexavalent chromium, PBB, PBDE below 0.1% w/w; cadmium below 0.01% w/w
    Flammability classificationIEC 60695-11-10HB class typical for non-FR PBT-GF30; V-0 requires flame-retarded grade
    Continuous use temperatureUL 746BYellow-card value required for final component rating

    Immersion testing under ISO 22088-1 or ASTM D543 in common automotive fluids shows resistance to aliphatic hydrocarbons, mineral oils, and most glycol coolant mixtures at temperatures up to 60°C. Strong acids and bases, especially hot aqueous sodium hydroxide above pH 10, attack PBT ester linkages; steam autoclaving above 100°C should be avoided. Methanol and other polar solvents can swell the impact-modifier phase, reducing weld-line strength after exposure. Parts should not be solvent-welded or cleaned with chlorinated solvents. Stress-cracking risk is highest at moulded-in stress concentrations; annealing at 150°C for 2 hours in an air-circulating oven after moulding can reduce internal stress and improve chemical resistance. For moulding shops running multi-material production, line purging should use a general-purpose PBT or low-viscosity polyethylene purge compound, and any PVC or acetal residue must be removed before charging SK609 BK851 to the hopper.