Celanese Crastin Pbt Gf30 Fr Ul94v0 Sk665fr Nc010

Celanese Crastin® PBT+GF30%-FR-UL94V0 SK665FR NC010

    • Product Name: Celanese Crastin® PBT+GF30%-FR-UL94V0 SK665FR NC010
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 322373
    Density 1.63 g/cm3
    Glass Fiber Content 30 %
    Tensile Modulus 10000 MPa
    Tensile Stress At Break 120 MPa
    Tensile Strain At Break 2.0 %
    Flexural Modulus 9500 MPa
    Charpy Notched Impact Strength 23c 8 kJ/m2
    Charpy Unnotched Impact Strength 23c 40 kJ/m2
    Hdt A 1 8mpa 200 °C
    Melting Temperature 225 °C
    Flammability Ul94 V-0
    Glow Wire Flammability Index 960 °C
    Comparative Tracking Index 600 V
    Volume Resistivity >1E14 ohm·cm
    Water Absorption Saturation 0.4 %
    Molding Shrinkage Parallel 0.3 %
    Molding Shrinkage Normal 1.0 %

    As an accredited Celanese Crastin® PBT+GF30%-FR-UL94V0 SK665FR NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg bags, palletized and labeled with product identification; store sealed in a dry area.
    Container Loading (20′ FCL) 20′ FCL: palletized 25 kg bags of Celanese Crastin® PBT+GF30%-FR-UL94V0 SK665FR NC010, dry, secured, and stowed per chemical cargo standards.
    Shipping Celanese Crastin® PBT+GF30%-FR-UL94V0 SK665FR NC010 is shipped as flame-retardant, glass-fiber-reinforced PBT pellets in sealed moisture-barrier bags or octabins. It is generally non-hazardous and not regulated for transport. Keep packaging closed, store dry, avoid heat/contamination, and handle per SDS.
    Storage Store in original sealed packaging in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and moisture. Keep bags closed to prevent humidity absorption and contamination. Avoid prolonged storage above recommended temperatures; use desiccant if needed. Do not store outdoors or near oxidizing agents. Follow supplier SDS and re-dry according to processing guidance before use.
    Shelf Life Shelf life is 2 years from manufacture when stored dry in original unopened packaging below 30°C, protected from moisture and sunlight.
    Free Quote

    Competitive Celanese Crastin® PBT+GF30%-FR-UL94V0 SK665FR NC010 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Celanese Crastin® PBT+GF30%-FR-UL94V0 SK665FR NC010 is a polybutylene terephthalate injection-moulding compound reinforced with 30% by mass glass fibre and formulated with a flame-retardant package that achieves UL 94 V-0 at the thickness recorded on the supplier certification. The NC010 suffix denotes natural, unpigmented pellet feedstock. The compound is specified for dimensionally stable electrical and electronic components, connectors, relay bases, coil bobbins, and enclosures where flammability classification must be documented. Relative to unfilled PBT and non-flame-retardant PBT GF30 grades, the product has a narrower processing window, higher melt viscosity at equivalent shear rates, and modified shrinkage anisotropy because of the combined glass-fibre and flame-retardant filler package. Published data for this specific configuration is limited outside the manufacturer datasheet and lot-specific certificate of analysis.

    Thermal and Moisture Limits Define the Processing Window

    Pre-drying is mandatory for this grade. Hydrolysis of the PBT ester linkage accelerates when melt processing occurs above 240°C in the presence of more than 0.02% residual moisture by mass, resulting in reduced molecular weight, lower impact resistance, and inconsistent UL 94 test outcomes. A desiccant-bed dryer operating at 120°C for 4 hours is the standard preparation; a hopper dryer alone is not a substitute when ambient relative humidity exceeds 60%. Melt temperature measured at the nozzle should be controlled between 250°C and 270°C, with 260°C typical for balanced fibre dispersion and flame-retardant stability. Mould temperatures from 60°C to 100°C are required to develop crystallinity and surface finish; lower settings reduce heat-deflection performance and may increase post-shrinkage, while higher settings extend cycle time and increase the risk of plate-out from the flame-retardant package. Injection speed should be medium to fast to minimise premature freeze-off in thin sections. Cumulative melt residence time above 5 minutes at melt temperature should be avoided because it accelerates additive degradation, surface bloom, and volatile generation.

    Property Matrix for Comparative Material Selection

    The following representative values are based on standard conditioned test specimens and are not batch specification limits. They are intended for preliminary material comparison only and must be confirmed against the supplier’s product datasheet and the specific lot certificate of analysis.

    PropertyTest standardTypical value
    DensityISO 1183-11.65 g/cm³
    Tensile modulus, 1 mm/minISO 527-1/-210,500 MPa
    Tensile stress at break, 5 mm/minISO 527-1/-2130 MPa
    Tensile strain at breakISO 527-1/-22.0%
    Flexural modulusISO 1789,500 MPa
    Flexural strengthISO 178200 MPa
    Charpy notched impact, 23°CISO 179/1eA8 kJ/m²
    Charpy unnotched impact, 23°CISO 179/1eU45 kJ/m²
    Melting temperature, DSCISO 11357-1/-3225°C
    Heat deflection temperature, 1.8 MPaISO 75-1/-2205°C
    Vicat softening temperature, B50ISO 306215°C
    Mould shrinkage, flow directionISO 294-40.3%
    Mould shrinkage, transverse directionISO 294-40.8%
    Water absorption, saturation, 23°CISO 620.4%

    Relative to a non-flame-retardant PBT GF30 compound, SK665FR NC010 exhibits higher density because the flame-retardant package introduces higher atomic-number elements and a synergist. Tensile and flexural moduli remain close to standard PBT GF30; however, tensile strain at break and notched impact strength are lower. The V-0 classification is thickness-dependent and does not automatically transfer to sections outside the certified thickness range. The flame-retardant package can migrate under sustained thermal load, producing surface deposit on mould surfaces and on electrical contacts in enclosed assemblies. Contact compatibility in sealed relays and connectors should be evaluated with long-term condensation tests. Compared with phosphorus-nitrogen halogen-free flame-retardant PBT grades, comparative tracking index, glow-wire ignition temperature, and smoke density differ; the supplier datasheet must be consulted because publicly available data for this specific configuration is limited.

    When the Moulding Line Changes Over from Standard PBT GF30 or Unfilled PBT

    Tooling and process parameters require systematic adjustment. The 30% glass-fibre content produces anisotropic shrinkage: fibre orientation along the flow direction reduces shrinkage in that axis and increases shrinkage transverse to flow. Warpage is influenced by gate location, wall thickness, and packing pressure. Mould temperatures at the upper end of the 60°C–100°C range improve crystallinity and reduce post-mould shrinkage in service. Screws with low compression ratios and wear-resistant coatings are preferred because glass fibre is abrasive relative to unfilled resin; replacement intervals should be determined from shot count and maintenance inspection rather than a universal value. Needle shut-off nozzles and thermal-gate systems may accumulate residue from the flame-retardant package; cleaning schedules are more aggressive than for unfilled PBT. If the tool has polished surfaces, venting depth may need to be increased in small increments to avoid gas burn marks from flame-retardant decomposition products at the last-filled areas; vent depths beyond 0.02 mm for PBT can produce flash.

    Melt viscosity of SK665FR NC010 is higher than that of unfilled PBT at typical shear rates, and the glass fibres produce a pronounced shear-thinning response. During filling, fibres align parallel to the melt front, creating a shell-core morphology: the outer layer is fibre-rich and oriented, while the core is resin-rich and less oriented. This morphology generates differential shrinkage between the shell and core, which can produce warpage in flat components such as cover plates. Gate placement that creates long, converging flow fronts should be avoided; a centrally located gate with balanced radial flow reduces fibre orientation gradients. Packing pressure must be sufficient to maintain fibre-matrix contact during crystallisation; inadequate packing produces sink marks and internal voids at thick sections. For parts with wall thicknesses between 1.0 mm and 3.0 mm, packing pressures from 40 MPa to 80 MPa hydraulic are commonly evaluated, but final values depend on part geometry and runner design. The material crystallises rapidly, so long holding times are not normally required; however, premature gate freeze must be avoided by using gates with adequate diameter, typically at least 0.8–1.0 mm for small parts and larger for thicker sections. Hot-runner systems with valve gates are preferred when the gate mark must be hidden, but the flame-retardant system may leave deposits in unheated cold sprues if the melt cools too rapidly.

    Flame-Retardant Chemistry and Compatibility Limits

    The flame-retardant system used in this product is not fully disclosed in public literature; the grade achieves UL 94 V-0 by use of a halogenated additive package typical for PBT compounds of this class. Processing and end-use conditions must avoid combination with strongly basic or amine-based additives, because these can accelerate dehydrohalogenation of the flame-retardant package and produce premature colour shift, mould deposit, and loss of flame performance. Contact with copper or copper-alloy inserts at sustained temperatures above 120°C may induce catalytic degradation; such combinations require long-term ageing studies. The material is not recommended for direct contact with hot concentrated alkaline solutions, ketones, or aromatic hydrocarbons under stress, because stress-cracking resistance is lower than that of polyolefins.

    Which Standards Verify Flammability, Electrical Performance, and Regulatory Status?

    The following checklist identifies the principal test and documentation categories for release and end-use qualification. Numerical values from lot certificates should be used for production acceptance.

    RequirementStandard or regulationCondition or reported value
    Flammability classificationUL 94V-0 at certified thickness
    Comparative tracking indexIEC 60112Test condition A, supplier reported value
    Dielectric strengthIEC 60243-1Short-time test, supplier reported value
    Volume resistivityIEC 62631-3-123°C, 50% RH
    Surface resistivityIEC 62631-3-223°C, 50% RH
    Melt volume-flow rateISO 1133-1:2022Supplier reported condition and value
    RoHS restriction2011/65/EUSupplier certificate required
    REACH SVHC communicationRegulation (EC) No 1907/2006Article 33 communication required above 0.1% w/w

    Storage should be in sealed moisture-barrier packaging at ambient temperatures below 40°C. Opened bags should be re-dried before use if exposure exceeds 30 minutes in high-humidity environments; production records should include dryer dew point and exit moisture. Regrind usage is possible only after validation because regrinding reduces glass-fibre length and can alter flame-retardant distribution; the UL 94 V-0 classification of the finished part must be reconfirmed if regrind content exceeds the proportion recommended by the supplier. Lot-to-lot control should include melt volume-flow rate per ISO 1133-1:2022, glass-fibre content, and flammability testing according to UL 94. Where electrical properties are critical, comparative tracking index and volume resistivity should be tested on the production part, because results from test plaques do not always transfer to complex geometry. If the application can tolerate a halogen-free system or if chemical exposure to alkaline solutions is severe, an alternative grade may be required. If the tool runs an unfilled PBT grade, dimensional changes are likely because mould shrinkage in SK665FR NC010 is lower and anisotropic; cores, ribs, and bosses may require revised clearances. If the tool runs a conventional PBT GF30, the main adjustments are drying, melt-temperature control to reduce plate-out while maintaining fibre wetting, and periodic cleaning of vents and hot-runner components.

    Top