| HS Code | 863260 |
| Glass Fiber Content | 30 % |
| Flame Retardant | Yes |
| Color | Natural (NC010) |
| Density | 1.63 g/cm³ |
| Molding Shrinkage Parallel | 0.4 % |
| Molding Shrinkage Normal | 0.9 % |
| Tensile Modulus | 10000 MPa |
| Tensile Stress At Break | 120 MPa |
| Tensile Strain At Break | 2.0–2.5 % |
| Charpy Notched Impact Strength 23c | 8 kJ/m² |
| Heat Deflection Temperature 1 8mpa | 200 °C |
| Heat Deflection Temperature 0 45mpa | 215 °C |
| Melting Temperature | 225 °C |
| Ul94 Flame Rating | V-0 |
| Comparative Tracking Index | 400 V |
| Volume Resistivity | >1E14 Ω·cm |
| Dielectric Constant 1mhz | 3.6 |
| Water Absorption 24h | 0.2 % |
| Melt Temperature Range | 240–260 °C |
| Mold Temperature Range | 80–100 °C |
| Drying Condition | 120 °C / 4 h |
As an accredited Celanese Crastin® PBT+GF30%-FR SK655FR NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Celanese Crastin® PBT+GF30%-FR SK655FR NC010 is supplied in 25 kg sealed moisture-barrier bags, palletized for shipment. |
| Container Loading (20′ FCL) | 20′ FCL dry container loaded with palletized 25 kg bags of Celanese Crastin® PBT+GF30%-FR SK655FR NC010, stretch-wrapped and secured. |
| Shipping | Celanese Crastin® PBT+GF30%-FR SK655FR NC010 is a flame-retardant, 30% glass-fiber reinforced polybutylene terephthalate compound in natural color. Ship in original sealed packaging; keep dry, protect from moisture/UV, and store cool and ventilated. Handle as nonhazardous industrial thermoplastic unless the SDS states otherwise. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and open flames. Keep containers tightly closed to prevent moisture absorption and contamination. Avoid prolonged exposure to humid conditions; use first-in, first-out stock rotation. Protect from physical damage. Follow local regulations and the manufacturer’s SDS for specific handling and storage requirements. |
| Shelf Life | Shelf life is typically 24 months when stored dry in original unopened packaging, protected from moisture, heat, and UV. |
Competitive Celanese Crastin® PBT+GF30%-FR SK655FR NC010 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Celanese Crastin® PBT+GF30%-FR SK655FR NC010 is a polybutylene terephthalate compound reinforced with 30% by weight glass fiber and formulated with a halogen-free flame-retardant package. The NC010 suffix denotes natural-color virgin feedstock; the ISO 11469 designation for the compound is PBT-GF30 FR. Published supplier datasheets list a density of 1.66 g/cm³ under ISO 1183-1, a tensile modulus of 11,500 MPa under ISO 527-2/1A, a flexural modulus of 10,500 MPa under ISO 178, a notched Charpy impact value of 8.0 kJ/m² under ISO 179/1eA, and a melt volume-flow rate of 10 cm³/10 min under ISO 1133-1 at 250 °C/2.16 kg. The grade is specified for injection-molded electrical enclosures, automotive connector bodies, relay bases, terminal blocks, switch components, and battery-adjacent high-voltage parts where UL 94 V-0 at 0.8 mm and a comparative tracking index of 250 V under IEC 60112 are procurement requirements. Procurement specifications may also reference halogen content limits in IEC 61249-2-21 and RoHS Directive 2011/65/EU for halogen-free electrical components.
In thin-wall automotive connector bodies specified at 0.8 mm nominal wall, SK655FR NC010 is evaluated after thermal aging because the combination of glass reinforcement and FR additives alters weld-line retention. Mold-filling simulation with fiber orientation data is normally run before tool steel is cut; the published mold shrinkages of 0.3 % flow and 0.9 % transverse under ISO 294-4 produce anisotropic dimensional change. Multi-gate connector bodies create weld lines downstream of cores and pins; weld-line tensile strength can drop by 30–50 % relative to the bulk tensile value depending on gate location, and prototype parts are subjected to terminal insertion force testing after environmental cycling. On production tooling, hard tooling with polished gates and venting below 0.02 mm depth reduces localized burn marks from FR decomposition gases. Published data for the exact weld-line strength reduction of SK655FR NC010 under specific connector geometries is limited; tool trials with instrumented insertion forces are required.
PBT hydrolyzes at melt temperatures in the presence of moisture; drying to less than 0.02 % residual moisture is mandatory before plastication. A desiccant dryer set point of 120 °C for 4 h with an air dew point below −30 °C is typical. Incoming resin from silo or gaylord storage can vary in residual moisture after exposure above 60 % relative humidity; production facilities in high-humidity environments often extend drying time or verify moisture analyzer readings before start-up. Wet feedstock reduces molecular weight during plastication and can shift UL 94 vertical burn behavior, producing flaming drips or afterglow that are not representative of the dried compound.
Barrel temperatures from rear to front are normally set between 250 °C and 270 °C, with nozzle temperature maintained at 260–270 °C. Mold temperature is controlled between 60 °C and 100 °C; the upper end improves crystallinity and HDT but extends cycle time. Residence time at melt temperature should not exceed 5 min; hot-runner dead spots, undersized screw channels, or overheated barrel zones above 280 °C can degrade the FR package and generate mold deposits. On production machines, hydraulic injection pressure at the gate is often above 60 MPa for wall sections below 0.8 mm, and clamp force is calculated from projected area and packing pressure; glass-filled PBT transmits substantial packing stress through the gate. General-purpose screws with L/D 18–22 and compression ratio 2.5:1 are used for glass-filled PBT. Back pressure between 0.3 MPa and 0.7 MPa maintains melt homogeneity without excessive shear heating; higher back pressure can accelerate fiber attrition. Regrind usage above 25 % by weight is not generally recommended unless the regrind is dried and the re-molded parts pass UL 94 and mechanical strength checks. Scrap generated from wet material or high-temperature residence should be segregated because molecular weight is already reduced. Batch-to-batch variation in feedstock moisture is a recognized cause of intermittent UL 94 vertical burn failures on production shifts.
The table below consolidates typical values from public supplier documentation. Values are not design minimums; specimen geometry, conditioning, and color can influence results.
| Property | Typical published value | Test method |
|---|---|---|
| Density | 1.66 g/cm³ | ISO 1183-1 |
| Molding shrinkage, flow | 0.3 % | ISO 294-4 |
| Molding shrinkage, transverse | 0.9 % | ISO 294-4 |
| Tensile modulus | 11,500 MPa | ISO 527-2/1A |
| Tensile stress at break | 125 MPa | ISO 527-2/1A |
| Flexural modulus | 10,500 MPa | ISO 178 |
| Flexural stress at break | 190 MPa | ISO 178 |
| Notched Charpy impact | 8.0 kJ/m² | ISO 179/1eA |
| Unnotched Charpy impact | 45 kJ/m² | ISO 179/1eU |
| Melt volume-flow rate | 10 cm³/10 min | ISO 1133-1, 250 °C/2.16 kg |
| Melting temperature | 225 °C | ISO 11357-3 |
| Heat distortion temperature HDT/A | 210 °C | ISO 75-2/A, 1.8 MPa |
| Heat distortion temperature HDT/B | 220 °C | ISO 75-2/B, 0.45 MPa |
| Flammability rating | V-0 | UL 94, 0.8 mm and 1.6 mm |
| Comparative tracking index | 250 V | IEC 60112 |
The 250 V comparative tracking index under IEC 60112 is critical for creepage-distance calculation. The UL 94 V-0 rating at 0.8 mm supports thin-wall electrical housings, but the rating is thickness- and color-dependent and must be confirmed from the UL Yellow Card for the specific production color. The HDT/A of 210 °C under 1.8 MPa is derived from a flatwise flexural specimen; injection-molded parts with residual stress or weld lines may exhibit lower retained HDT. The notched Charpy value of 8.0 kJ/m² indicates limited ductility; snap-fit latches should incorporate large radii and should be prototype-tested at the lowest service temperature because glass-fiber orientation at knit lines can reduce local impact resistance. Long-term thermal aging data under UL 746A and relative thermal index values are not supplied in the short-form datasheet and must be obtained from the UL Yellow Card for the intended thickness and color.
Substitution of a non-FR PBT-GF30 with SK655FR NC010 changes density, melt viscosity, and post-molding deposit behavior. A standard 30% glass-filled PBT without flame retardant is often specified at 1.53–1.56 g/cm³; the SK655FR NC010 density of 1.66 g/cm³ increases part mass and may alter snap-fit closing force and hinge stress. The melt volume-flow rate of 10 cm³/10 min under ISO 1133-1 at 250 °C/2.16 kg is lower than many high-flow non-FR PBT-GF30 grades; thin sections below 0.8 mm may require melt temperatures near 270 °C and higher injection velocity to prevent short shots at the end of fill. Compared with unfilled FR PBT, the 30% glass reinforcement raises the tensile modulus, lowers shrinkage, and improves creep resistance under connector terminal loads, but it produces anisotropic warpage and higher melt viscosity.
Compared with brominated flame-retardant PBT-GF30 grades, the halogen-free package eliminates antimony trioxide synergism and reduces halogen acid release during combustion or recycling, but published direct tracking-resistance comparisons under identical specimen geometry are limited. Brominated systems may achieve higher comparative tracking index values in some formulations; end-product clearance calculations must use the CTI of the specific grade and not assume parity. The halogen-free FR system in SK655FR NC010 may produce slightly higher mold deposit on hot-runner gates; cleaning intervals should be validated on the production tool. If the application requires laser marking, NC010 natural is generally markable with 1064 nm Nd:YAG lasers, but contrast is lower than black and should be confirmed at production cycle speed.
In power distribution terminal blocks certified to IEC 60947-7-1, the comparative tracking index of 250 V under IEC 60112 places SK655FR NC010 in material group IIIa for creepage calculation under IEC 60664-1. At pollution degree 2, creepage distances for working voltages above 250 V must be increased or insulating barriers added. Terminal screw torque retention and snap-fit engagement after thermal cycling from −40 °C to 150 °C require end-use testing because glass-filled PBT loses impact strength at low temperature and can stress-crack under excessive insert hoop stress. The material is not intended for continuous immersion in hot aqueous acids or strong alkaline solutions above 60 °C; hydrolytic degradation of the PBT backbone reduces stress-cracking resistance. Published data for long-term exposure to specific automotive coolants and battery coolant media for the exact SK655FR NC010 configuration is limited; end-use testing is required before release.