    HS Code 489659
    Polymer Base PBT
    Glass Fiber Reinforcement 30%
    Flame Retardant Yes
    Color Natural
    Density 1.68 g/cm³
    Tensile Modulus 10000 MPa
    Tensile Stress At Break 125 MPa
    Tensile Strain At Break 2.5%
    Charpy Notched Impact Strength At 23 C 9 kJ/m²
    Heat Deflection Temperature At 1 8 Mpa 200°C
    Heat Deflection Temperature At 0 45 Mpa 215°C
    Melting Temperature 225°C
    Ul94 Flammability Rating V-0
    Molding Shrinkage Parallel 0.3%
    Molding Shrinkage Normal 0.7%

    As an accredited Celanese Crastin® PBT+GF30%-FR SK645FR NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Celanese Crastin® PBT+GF30%-FR SK645FR NC010 supplied in 25 kg moisture-resistant bags, palletized for industrial handling and storage.
    Container Loading (20′ FCL) Loaded into a 20′ FCL: palletized 25 kg bags of Celanese Crastin® PBT+GF30%-FR SK645FR NC010, shrink-wrapped, labeled, and secured for export.
    Shipping Celanese Crastin® PBT+GF30%-FR SK645FR NC010 is shipped as dry, flame-retardant, glass-fiber-reinforced PBT pellets in sealed moisture-barrier bags—typically 25 kg bags or octabins on pallets. Handle as non-hazardous industrial resin under normal conditions; keep dry and avoid moisture, heat, and contamination. Follow the SDS and local transport regulations.
    Storage Store Celanese Crastin® PBT+GF30%-FR SK645FR NC010 in original, sealed packaging in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and moisture. Protect from contamination and incompatible chemicals. Keep containers closed, maintain stable temperature and humidity, follow first-in/first-out rotation, use clean, dry handling equipment, and dry opened material before processing if required, in accordance with local regulations.
    Shelf Life For Celanese Crastin® PBT+GF30%-FR SK645FR NC010, shelf life is typically two years in original unopened packaging below 30°C, protected from moisture.
    Free Quote

    Competitive Celanese Crastin® PBT+GF30%-FR SK645FR NC010 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Celanese Crastin® PBT+GF30%-FR SK645FR NC010 is a flame-retardant polybutylene terephthalate injection-moulding compound reinforced with a nominal 30% by weight glass-fibre loading. The NC010 suffix identifies the natural, uncoloured colour package. The material is normally specified where a component must combine stiffness, creep resistance at elevated temperature, and self-extinguishing behaviour under IEC 60695-11-10 without relying on an external flame-retardant coating. The base polymer is semicrystalline; the glass-fibre network reduces mould shrinkage and raises heat-deflection temperature compared with unreinforced PBT, but it also reduces tensile elongation at break and increases melt viscosity. Properties are typically reported at 23°C and 50% relative humidity after conditioning to ISO 291:2008. All grade-specific values should be checked against the current Celanese product datasheet because flame-retardant PBT compounds vary from lot to lot in filler length distribution, stabiliser concentration, and moisture uptake. Published data for this specific configuration is limited in open literature for electrical tracking and long-term hydrolytic ageing; therefore electrical design should use tested values from the grade-specific file rather than general PBT-GF30 literature.

    In terms of composition, the PBT matrix provides fast crystallisation during cooling and a sharp melt-to-solid transition. The 30% glass-fibre content is typically verified by ash or gravimetric methods based on ISO 3451-4:1998. Density measured under ISO 1183-1:2019 for filled flame-retardant PBT grades generally lies between 1.60 g/cm³ and 1.75 g/cm³; the exact value depends on the flame-retardant package and glass sizing. Melt volume-flow rate determined by ISO 1133-1:2022 at 250°C under 2.16 kg is typically set low enough to maintain fibre length but high enough for thin-wall fill; the datasheet value should be used for mould-filling simulation. The natural NC010 colour package contains no carbon black, which permits self-colouring but also means UV exposure and colour stability must be managed by the moulder. Lot certifications normally include batch-level data for melt flow rate, ash content, residual moisture, and tensile modulus under the Supplier Quality Agreement.

    What Distinguishes SK645FR NC010 from Unfilled PBT and Halogen-Free PBT-GF30?

    The primary difference versus unfilled flame-retardant PBT is the sharp increase in tensile modulus and the corresponding loss of elongation. Unfilled PBT has a tensile modulus commonly below 3 GPa under ISO 527-2:2012, whereas 30% glass-filled PBT grades typically reach 9 GPa to 11 GPa. Strain at break moves from a ductile value above 10% in unreinforced PBT to roughly 1.5% to 2.5% in the filled grade. This trade-off is not an indicator of lower durability; it is a consequence of load transfer to the glass fibres and is exploited in connector housings, relay bases, and terminal blocks.

    Compared with a non-flame-retardant PBT+GF30, the FR package generally reduces impact toughness and can narrow the processing window. Whether SK645FR NC010 is regarded as halogen-free depends on the supplier’s compliance declaration and the specific formulation version; the grade designation alone does not confer halogen-free status. If a halogenated FR package is present, the melt can release acidic decomposition products when overheated or held too long; if a phosphorus- or nitrogen-based system is used, high melt residence time may still produce colour shift and plate-out. The moulder should therefore use the safety data sheet and UL Yellow Card for the actual grade rather than generic PBT-GF30 FR guidance.

    Compared with halogen-free PBT-GF30 FR alternatives, materials of this class are often selected where low FR addition is required to achieve V-0 at thin wall and where mechanical retention after wet conditioning is advantageous. However, halogen-free alternatives may offer better comparative tracking index under IEC 60112 or lower smoke density in certain applications. Final selection must be made on the basis of end-product flammability testing at the actual wall thickness, not on raw-material V-0 ratings alone. For safety-critical components, the effect of pigments on flame retardancy must also be verified because some organic colorants can reduce the V-0 margin.

    Property or performance areaStandard methodTypical parameter measuredDesign relevance
    DensityISO 1183-1:2019g/cm³part mass calculation
    Tensile modulus and strengthISO 527-2:2012MPasnap-fit and housing stiffness
    Charpy notched impactISO 179-1:2010kJ/m²fastener and drop performance
    Heat-deflection temperatureISO 75-2:2013°C at 1.8 MPashort-term temperature resistance
    FlammabilityIEC 60695-11-10class at thicknessfire-safety compliance
    Comparative tracking indexIEC 60112Vcreepage path design
    Melt volume-flow rateISO 1133-1:2022cm³/10 min at 250°C, 2.16 kgmould-filling simulation

    Another differentiating factor is flow behaviour. The GF30 network adds significant reinforcement at the expense of flow; the melt volume-flow rate is usually lower than that of the equivalent unfilled FR grade, so filling thin walls below 0.5 mm requires proper gate placement and possibly higher injection pressure. In multi-cavity tools for terminal blocks, cavity-to-cavity variation in fibre orientation is a more important driver of dimensional variation than material lot changes. A 30% glass-fibre grade raises tensile modulus compared with a 20% glass-fibre grade, but may reduce weld-line strength and spiral flow length.

    Processing-Window Constraints in Injection Moulding and Hot-Runner Systems

    Before processing, pellets are dried in a desiccant dryer with a supply air dew point no higher than -30°C. A drying schedule of 120°C for 4 h is typical for PBT-GF30 FR grades, but the target residual moisture content is normally below 0.02%, measured by ISO 15512. Inadequate drying produces splay, loss of surface gloss, and a reduction in tensile strength at the weld line. Filled flame-retardant compounds are more sensitive to moisture-induced degradation than unfilled PBT because glass sizing and FR additives can hydrolyse at processing temperature.

    Melt temperature measured at the nozzle is usually maintained between 250°C and 270°C. The lower bound is set by the need to minimise glass-fibre attrition and ensure uniform dispersion; the upper bound is controlled by the thermal stability of the flame-retardant package. A general-purpose high-wear screw with an L/D ratio of 18:1 to 22:1 and a compression ratio of 2.0:1 to 2.5:1 is acceptable for many applications, but a low-shear or matched-and-mated screw may better preserve fibre length in thin-wall moulding. Back pressure is commonly limited to 2 bar to 5 bar hydraulic to avoid frictional heating and fibre fracture. The non-return valve and screw tip should be specified with wear-resistant chromium-alloy construction because glass-filled melts are abrasive.

    Mould temperature is controlled between 40°C and 80°C. At the lower end, surface finish and dimensional stability improve in fast-cycling tools but crystallinity may be insufficient to meet heat-deflection requirements. At the upper end, crystallinity increases, but cycle time lengthens and post-mould shrinkage becomes more significant. The glass-fibre network reduces isotropic shrinkage; typical in-plane mould shrinkage for PBT+GF30 is direction-dependent, with values often in the region of 0.2% to 0.5% along flow and 0.5% to 1.0% transverse to flow. Gate land length, gate area, and venting depth must be checked on a case-by-case basis because flame-retardant additives can generate volatiles that deposit on cavity surfaces.

    Mould-filling simulation for PBT+GF30 FR should use temperature-dependent shear-viscosity curves obtained by capillary rheometry under ISO 11443. Wall-slip and fibre-migration effects in thin walls can create core-skin morphology differences that standard Cross-WLF data for unfilled grades do not capture. In production-scale hot-runner assemblies, internal runner surface temperatures should be balanced to avoid local overheating. Maximum melt residence time at the upper temperature should be kept below 8 min to 10 min unless purge studies demonstrate acceptable colour stability. If splay, brown streaking, or plate-out appears after cycle interruptions, the machine should be purged with a clean PBT or dedicated commercial purge compound; abrasive purge agents should be avoided because they can score check rings and screw surfaces.

    Clamp-force estimation follows projected area and peak cavity pressure. For connector and relay bodies, peak cavity pressure at the end of fill commonly lies between 350 bar and 600 bar; the clamp requirement is then derived from the projected area. A 100 t machine may be adequate for a multi-cavity connector tool if the projected area and cavity-pressure calculation demonstrate a clamp margin of at least 15%. Venting depths for PBT are usually 0.01 mm to 0.03 mm, but with volatile FR decomposition, peripheral vents and vent inserts should be cleaned more frequently than with unfilled grades.

    The weld-line region of a PBT+GF30 FR part is the most common failure location because glass fibres align parallel to the weld interface and do not cross it. Injection speed, gate location, and melt temperature should be set to raise weld-line strength; however, flame-retardant additives reduce local ductility at the weld line compared with the bulk. Weld-line tensile strength can be 40% to 60% of the bulk value when measured by ISO 527-2 on a double-gated plaque. This is a critical design constraint for relay housings exposed to snap-fit assembly or ultrasonic welding.

    If Long-Term Thermal and Humidity Ageing Are Required, Which Failure Modes Must Be Evaluated?

    PBT is susceptible to hydrolytic degradation in hot-humid environments because water attacks ester linkages. In a 30% glass-filled FR grade, hydrolysis reduces molecular weight, which then lowers tensile strength and impact resistance before visible cracking appears. Ageing trials should be performed at the upper service temperature and high relative humidity using tensile bars per ISO 527-2:2012 and notched Charpy specimens per ISO 179-1:2010. Retention after 1000 h at 85°C and 85% relative humidity is commonly specified for automotive and appliance applications, but the grade-specific file must contain the tested values.

    Thermal-oxidative ageing under hot air, for example 1000 h at 150°C, is used to verify long-term heat resistance. Failure modes include surface chalking, loss of glass-fibre sizing, and embrittlement near the skin. Because flame retardants can migrate to the surface during ageing, comparative tracking index under IEC 60112 and dielectric strength under IEC 60243-1 should be measured after heat ageing, not only on as-moulded specimens. For printed circuit board connectors, the material must also survive reflow or wave-soldering thermal profiles; the heat-deflection temperature under 1.8 MPa per ISO 75-2:2013 is only a first indication because soldering exposes the part for shorter times but at higher local temperature.

    Hot-humid ageing protocols should include mechanical retention after conditioning and possibly a post-ageing flammability check. Flame-retarded materials can pass flame tests as moulded but fail after hydrolysis because degraded polymer releases fuel more readily or because FR additives have migrated. For safety-related components, designers often require 70% retention of tensile strength after 1000 h at 85°C/85% RH, but the specific acceptance limit must be set by the application standard, not by the polymer supplier. Salt-spray or coolant environments, especially in underhood electrical centres, require additional testing under ISO 16750-5 or OEM-specific standards.

    If the component is used in contact with alkali or hot water, stress-cracking resistance should be evaluated using a constant-strain fixture with actual moulded parts. The combination of glass-fibre orientation, weld lines, and flame-retardant degradation can accelerate environmental stress cracking. Published data for this specific configuration is limited in this area; therefore application-specific testing is required before serial production. PBT is not inherently resistant to strong alkaline solutions, and prolonged contact with hot organic solvents can degrade glass sizing. The recommended upper continuous-use temperature is not a single material constant; it depends on mechanical load, environmental moisture, and wall thickness.

    Electrical and electronic applications dominate the grade’s use: connector bodies, relay bases, terminal blocks, circuit-breaker internal supports, coil formers, and switch housings. In connectors, the combination of 30% glass fibre and flame retardancy provides dimensional repeatability over 0.4 mm to 1.6 mm wall sections, but the moulder should verify that the selected wall thickness corresponds to the approved flame rating for the grade. The natural NC010 colour is suited to self-colouring in dark shades; if high electrical tracking resistance is required, pigment selection must be validated because some colourants degrade tracking performance under IEC 60112.

    Compared with polyamide 30% glass-fibre FR compounds, PBT-GF30 FR generally offers lower moisture absorption and better dimensional stability in humid environments, but lower notched impact strength. Compared with mineral-filled PBT, the glass-filled grade provides higher stiffness and resistance to creep, but also more anisotropic shrinkage and a more pronounced weld-line weakness. These differences make the grade less suitable for thick-wall impact-critical enclosures unless design features such as ribs and radii are carefully evaluated. Regrind content should be controlled by the application-specific specification, commonly up to 25%, but the relevant UL component recognition may limit or prohibit regrind unless the moulder is certified under the appropriate follow-up service procedure. Uncontrolled addition of non-FR regrind reduces flame retardancy and may change tracking and hot-wire ignition behaviour.

    The grade is normally supplied with a statement of conformity to the RoHS Directive 2011/65/EU and REACH Regulation EC 1907/2006; however, these are regulatory documents and do not replace application-specific performance testing. If an end product must satisfy the fire-safety requirements of IEC 60335-1, the appliance standard’s glow-wire and needle-flame clauses require testing on the finished part rather than relying only on raw-material flammability classification. Colour matching should be performed on the final formulation because flame-retardant additives can shift colour during heat ageing, and some pigments may interact with phosphorus- or halogen-based FR systems.