| HS Code | 603989 |
| Product | Celanese Crastin® PBT+GF20%-FR-LW LW9020FR BK851 |
| Polymerbase | Polybutylene terephthalate (PBT) |
| Reinforcement | 20% glass fiber |
| Flameretardant | Yes |
| Color | Black (BK851) |
| Processingmethod | Injection molding |
| Density | 1.52 g/cm³ |
| Moldingshrinkageparallel | 0.3 % |
| Moldingshrinkagenormal | 0.8 % |
| Tensilemodulus | 7600 MPa |
| Tensilestressatbreak | 105 MPa |
| Tensilestrainatbreak | 2.5 % |
| Charpynotchedimpactstrength23c | 6 kJ/m² |
| Charpynotchedimpactstrengthminus30c | 5 kJ/m² |
| Deflectiontemperatureunderload1 8mpa | 200 °C |
| Meltingtemperature | 225 °C |
| Ul94flammabilityrating | V-0 |
| Waterabsorption | 0.4 % |
As an accredited Celanese Crastin® PBT+GF20%-FR-LW LW9020FR BK851 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Celanese Crastin® PBT+GF20%-FR-LW LW9020FR BK851 is supplied in 25 kg moisture-resistant bags, 40 bags per pallet (1,000 kg total). |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Celanese Crastin® PBT+GF20%-FR-LW LW9020FR BK851 is palletized, shrink-wrapped, and secured inside a 20-foot FCL for export. |
| Shipping | Celanese Crastin® PBT+GF20%-FR-LW LW9020FR BK851 is shipped as solid thermoplastic resin pellets in moisture-barrier bags or octabins. It is generally non-hazardous for transport; keep dry, avoid heat, and follow the supplier SDS and local shipping regulations. |
| Storage | Store Celanese Crastin® PBT+GF20%-FR-LW LW9020FR BK851 in original, sealed packaging in a cool, dry, well-ventilated area, protected from moisture and direct sunlight. Keep away from heat, sparks, flames, and oxidizing materials. Avoid dust generation and static buildup. Maintain recommended storage temperature per the SDS, observe first-in/first-out, and keep containers closed when not in use. |
| Shelf Life | Shelf life is two years from delivery when stored in original unopened packaging, dry, at temperatures not exceeding 30°C. |
Competitive Celanese Crastin® PBT+GF20%-FR-LW LW9020FR BK851 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Celanese Crastin® PBT+GF20%-FR-LW LW9020FR BK851 is a polybutylene terephthalate injection-moulding grade that combines a nominal glass-fibre reinforcement level of 20%, a flame-retardant package, and a low-warpage filler system. The product designation identifies the base PBT chemistry, 20% glass-fibre content, flame-retardant performance, low-warpage modification, and BK851 black colour concentrate. It is supplied as black pellets for use in tight-tolerance electrical and electronic components where post-mould flatness and a UL94 V-0 rating must be maintained across multi-cavity production.
Typical use areas include multi-pin connectors, terminal blocks, relay sockets, miniature circuit-breaker housings, and automotive electrical interfaces. These applications share long flow lengths, densely packed metal inserts, thin wall sections, and stringent dimensional checks. The material is generally considered when unfilled PBT cannot meet stiffness requirements and when standard glass-filled PBT grades show unacceptable part distortion.
Glass-fibre orientation in a filling cavity restrains shrinkage parallel to the fibre axis more strongly than transverse shrinkage. In a standard 20% glass-fibre PBT, this differential can produce out-of-flatness in parts with length-to-width ratios above 4:1. The LW9020FR BK851 low-warpage package is formulated to reduce the shrinkage anisotropy rather than to eliminate all mould shrinkage. On ISO 294-4 plaque specimens, published representative data for reinforced flame-retardant PBT of this class typically place flow-direction shrinkage in a range of 0.3% to 0.4% and transverse shrinkage in a range of 0.7% to 0.8%; conventional non-low-warpage grades can display transverse shrinkage above 1.0%. Lot-specific values must be confirmed on the production tool because the black colour concentrate and regrind content can shift shrinkage slightly.
The low-warpage behaviour is most repeatable when the mould temperature is held at 80°C or above. At a mould temperature below 60°C, crystallisation is suppressed and the part may continue to change dimension after ejection; above 100°C, cycle time rises without a proportional flatness gain. Production experience on multi-cavity connector tools shows that cavity-to-cavity coolant temperature variation should be controlled within ±2°C, and water circuits should be balanced so that the pressure drop across parallel circuits is within 10% of the mean. Otherwise the low-warpage package cannot compensate for uneven heat removal.
Gate placement remains important. A single end gate on a long connector body creates highly oriented unidirectional flow and can concentrate warp at the opposite end. Central or dual-gate layouts reduce the flow path but introduce weld lines that can disturb fibre orientation and reduce flatness near the pin plane. For parts above 150 mm in flow length, published mould-filling data specific to this grade are limited; tool trials should map fill time, switch-over point, and holding pressure against pin-plane coplanarity measurements.
The mechanical property profile is established on ISO moulded specimens. The values in the table are representative ranges from the manufacturer’s current published data for this grade family; they are not maximum or minimum release limits.
| Property | Test method | Representative range or value |
|---|---|---|
| Density | ISO 1183 | 1.52–1.58 g/cm³ |
| Tensile stress at break | ISO 527-1/-2 | 90–105 MPa |
| Tensile modulus | ISO 527-1/-2 | 6.5–7.5 GPa |
| Flexural modulus | ISO 178 | 6.0–6.8 GPa |
| Charpy notched impact, 23°C | ISO 179/1eA | 3.0–4.5 kJ/m² |
| Heat deflection temperature, 1.8 MPa | ISO 75-2/A | 195–205°C |
| Flammability | IEC 60695-11-10 | V-0 at 0.8 mm |
| Comparative tracking index | IEC 60112 | 250 V |
The tensile modulus places the material well above unfilled PBT, which is commonly reported between 2.4 and 2.8 GPa under ISO 527-1/-2. The notched Charpy impact value is lower than most unfilled PBT grades, and snap-fit arms should be designed with a minimum radius and an end-use temperature safety factor. Creep and fatigue data specific to the BK851 colour code are limited; users should not transfer long-term data from natural-colour or non-flame-retardant grades without validation.
For electrical properties, volume resistivity is measured under IEC 62631-3-1 or IEC 60093, and dielectric strength under IEC 60243-1. The presence of carbon black in BK851 can reduce surface resistivity in some formulations, but the volume resistivity of the base grade remains in the high-insulation range. Comparative tracking index data are discussed with the flame-retardant package below.
Insert moulding adds another dimensional variable. When brass or tin-plated pins are incorporated, the insert temperature should be maintained at 80–120°C before injection to reduce early quench and shrinkage-induced stress around the pin root. Cold inserts can cause sink marks and increase the risk of cracking around the insert, particularly in a 20% glass-fibre PBT with low elongation at break. The holding pressure profile should be adjusted so that the glass fibres pack around the insert without creating excessive residual stress at the gate. After ejection, parts should be placed on a flat cooling fixture if the part length exceeds 120 mm; uncontrolled cooling on a wire rack can reintroduce warpage even in a low-warpage grade.
The flame-retardant system is qualified by the manufacturer to provide a UL94 V-0 rating at 0.8 mm when tested under IEC 60695-11-10. The rating is not a material property alone; it is a specimen-thickness-dependent result that must be re-established on moulded parts because weld lines, gas traps, gloss variations, and regrind content can change ignition response. For wall sections below 0.5 mm, published data for this specific black grade are limited, and the material should not be treated as a guaranteed thin-wall flame-retardant compound without end-part testing.
The comparative tracking index under IEC 60112 is reported as 250 V. This places the grade outside the high-CTI category that begins near 400 V. Designers who intend to reduce creepage distances through a higher CTI should compare mineral-filled or dedicated high-CTI PBT grades instead of LW9020FR BK851. Glow-wire testing is generally carried out under IEC 60695-2-11; the glow-wire ignition temperature and flammability index for this grade depend on thickness and should be taken from the certified UL Yellow Card or from a test report for the finished part.
The flame-retardant additive package imposes an upper processing temperature of 270°C. Above this boundary, the package can decompose and produce acidic by-products. The first visible sign is often surface splay or a brownish gate blush, but tensile strength and UL94 V-0 reproducibility can decline before the visual defect becomes obvious. Mould steel in the gate, runner, and vent regions should be corrosion resistant or protected when the material is processed for long campaigns, because flame-retardant decomposition by-products can attack unprotected tool steel during extended production runs.
PBT hydrolyses at melt temperature, so moisture control is the first processing boundary. The material is dried in a desiccant-bed dryer with a dew point of -30°C or lower at 120°C for 4 h to 6 h when the original packaging has been opened. The maximum recommended moisture content before processing is 0.02%. Wet pellets produce not only surface splay but also a loss of tensile stress at break and inconsistent flame-retardant performance. Drying hoppers should be sized for the full shot-mass consumption rate, and return-air temperature should be monitored because glass-filled PBT can generate fines that reduce dryer efficiency.
Melt temperature is maintained at 250–270°C. The nozzle is typically set at 255–265°C, and the front zone near 260°C. A typical barrel profile for a three-zone screw is hopper 230–240°C, compression 240–255°C, metering 250–260°C, and nozzle 250–260°C. In hot-runner systems, manifold and nozzle temperatures should remain inside this band. During interruptions longer than 5 min, barrel temperatures should be lowered or the material purged to avoid static residence. The screw design is preferably a 20:1 to 24:1 L/D general-purpose screw with a compression ratio between 2.0:1 and 2.5:1; deeper flights and polyolefin screws are not recommended because they can break glass fibres unevenly and produce variable melt quality. Back pressure is set between 0.3 and 0.7 MPa to homogenise glass distribution without excessive fibre attrition.
Injection velocity is a compromise. A medium fill speed is usually selected to prevent jetting and to allow the flow front to advance uniformly. High shear near the gate can increase melt temperature locally and change fibre orientation, which directly affects the low-warpage result. The holding pressure profile should be set to maintain a stable gate freeze time; premature gate freeze produces sink marks and pitch errors, while excessively long holding times increase cycle time without improving flatness. Regrind use up to 20% is common if the regrind is kept dry and dust-free, but the exact limit must be validated for the finished-part flammability and dimensional requirements.
The practical processing window is not set solely by the melting point of PBT, which is near 225°C under ISO 11357-3. The upper limit is set by the flame-retardant package. At melt temperatures above 270°C, and especially above 280°C, the residence time must be kept to less than 3 min because degradation kinetics accelerate rapidly. Production experience on hot-runner connectors shows that a blocked hot-tip or a delayed mould change can expose the same melt volume to repeated shear and heat, producing black specks, splay, and a measurable drop in notched impact strength.
Heat deflection temperature under 1.8 MPa is generally reported in the range 195–205°C by ISO 75-2/A. This value is influenced by fibre content, annealing, and mould temperature. The material should not be used continuously at the HDT value; the HDT test is a short-time thermal-mechanical benchmark, not an end-use continuous-service temperature. Long-term thermal ageing data for this specific BK851 grade are not part of the typical short-term datasheet. If the application requires relative thermal index values, the UL Yellow Card is the controlling reference.
Batch-to-batch variation in glass-fibre length and flame-retardant dispersion can affect mechanical properties more than colour variation. Incoming-material control should therefore check melt volume-flow rate under ISO 1133-1, ash content, and tensile modulus rather than relying only on infrared resin identification. The moisture content of each incoming lot should also be measured with a calibrated moisture balance, because the hydrolysis threshold is low.
The grade differs from unfilled PBT in stiffness, mould shrinkage, and creep response. Tensile modulus increases from roughly 2.5 GPa to the 6.5–7.5 GPa range, while elongation at break falls below 3%. The low elongation means that snap-fit designs must use larger strain-relief geometry than unfilled PBT and must not expect post-yield ductility. The material also has higher notch sensitivity; sharp corners, weld lines, and moulded-in inserts deserve radius optimisation.
Compared with standard 20% glass-fibre flame-retardant PBT without the low-warpage package, LW9020FR BK851 is chosen when pin-plane coplanarity and flatness are the controlling dimensional criteria. The tradeoff is that the low-warpage filler system may reduce melt-flow length at the same injection pressure. Published data for this specific configuration are limited, but tooling trials generally show that thin-wall sections below 0.8 mm require additional gates or higher holding pressure. Compared with 30% glass-fibre PBT, the 20% grade provides lower melt viscosity and lower density, while accepting a reduction in tensile modulus and heat deflection temperature. Compared with high-CTI flame-retardant PBT grades, the 250 V CTI value should not be used where regulatory creepage standards require a higher tracking category.
Chemical incompatibility must also be considered. PBT is sensitive to hot water, strong alkaline environments, and certain polar solvents at elevated stress. The material is not recommended for continuous exposure to hot ethylene glycol at elevated temperature and high stress levels, nor for direct contact with strong inorganic acids or high-pH cleaning agents. For applications with such exposure, alternative base polymers or stress-crack-resistant PBT blends should be evaluated under ISO 22088 or an equivalent solvent-stress-cracking protocol.