Celanese Crastin Pbt Gf15 Fr Sk642fr Bk851

Celanese Crastin® PBT+GF15%-FR SK642FR BK851

    • Product Name: Celanese Crastin® PBT+GF15%-FR SK642FR BK851
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 521764
    Polymertype Polybutylene terephthalate (PBT)
    Fillerreinforcement 15% glass fiber
    Flameretardant Yes
    Color Black (BK851)
    Density 1.55 g/cm³
    Moldingshrinkageparallel 0.4 %
    Moldingshrinkagenormal 1.0 %
    Tensilemodulus 7000 MPa
    Tensilestressatbreak 95 MPa
    Tensilestrainatbreak 2.5 %
    Charpynotchedimpactstrength23c 5 kJ/m²
    Hdt A 200 °C
    Hdt B 215 °C
    Meltingtemperature 225 °C
    Ul94rating V-0 at 0.75 mm
    Waterabsorption 0.3 %

    As an accredited Celanese Crastin® PBT+GF15%-FR SK642FR BK851 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaging description: Celanese Crastin SK642FR BK851 is supplied in sealed 25 kg moisture-barrier bags, palletized at 1,000 kg per pallet.
    Container Loading (20′ FCL) 20′ FCL loaded with Celanese Crastin® PBT+GF15%-FR SK642FR BK851, palletized in sealed bags, evenly distributed and secured for ocean shipment.
    Shipping Celanese Crastin® PBT+GF15%-FR SK642FR BK851 ships as a flame-retardant, 15% glass-fiber-reinforced PBT molding compound in sealed moisture-barrier bags or octabins. Handle as a non-hazardous industrial resin under normal conditions; store dry and avoid heat, moisture, and contamination. Confirm SDS and local transport regulations before shipment.
    Storage Store Celanese Crastin® PBT+GF15%-FR SK642FR BK851 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and oxidizing materials. Keep containers closed and use original packaging to prevent moisture pickup and contamination. Avoid dust generation and static buildup; observe local regulations and manufacturer’s safety data sheet.
    Shelf Life Shelf life is typically 24 months when stored dry, cool, and protected from moisture in original unopened packaging.
    Free Quote

    Competitive Celanese Crastin® PBT+GF15%-FR SK642FR BK851 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Celanese Crastin® PBT+GF15%-FR SK642FR BK851 is a black, 15% glass-fibre-reinforced flame-retardant polybutylene terephthalate moulding compound. The grade is supplied for injection-moulded electrical and electronic components where a UL 94 V-0 rating at 0.75 mm wall thickness is required and where unfilled PBT lacks sufficient stiffness. Published data for the grade typically list a density of 1.53–1.55 g/cm³ according to ISO 1183-1, a tensile modulus of approximately 6800–7200 MPa according to ISO 527-2, and a notched Charpy impact value of approximately 3.5–4.5 kJ/m² at 23°C according to ISO 179-1eA. The BK851 designation identifies a black colour concentrate; the compound is intended for engineering applications requiring stiffness, flame retardancy, and dimensional stability rather than general-purpose PBT parts.

    What separates SK642FR BK851 from unfilled PBT FR and PBT GF30 FR?

    Within the Crastin PBT portfolio, SK642FR BK851 occupies a middle position between unfilled flame-retardant PBT and 30% glass-filled flame-retardant PBT. Unfilled PBT FR grades typically show tensile modulus values of 2500–2800 MPa and heat-deflection temperature under 1.8 MPa of 75–90°C according to ISO 75-2. PBT GF30 FR grades generally reach tensile modulus values of 9000–10000 MPa and HDT/A values above 200°C. SK642FR BK851, with its 15% glass fibre, provides tensile modulus near 7000 MPa and HDT/A near 195–205°C. These differences are significant in connector substitution programmes, but the 15% glass content produces lower out-of-plane warpage and lower density than 30% glass. The lower glass fraction also reduces melt viscosity relative to 30% glass-filled PBT, which can improve filling of thin-wall sections below 0.8 mm, although weld-line strength remains lower than in unfilled PBT.

    Representative published property comparisons for the grade family are shown below. Exact lot-specific values should be taken from the manufacturer’s certificate of analysis because flame-retardant lot-to-lot variation can alter impact by 5–10%.

    PropertyTest methodSK642FR BK851Unfilled PBT FRPBT GF30 FR
    DensityISO 1183-11.53–1.55 g/cm³1.45 g/cm³1.65 g/cm³
    Tensile modulusISO 527-26800–7200 MPa2500–2800 MPa9000–10000 MPa
    Notched Charpy 23°CISO 179-1eA3.5–4.5 kJ/m²4.0–5.0 kJ/m²7.0–8.0 kJ/m²
    HDT/AISO 75-2195–205 °C75–90 °C200–210 °C
    Flame retardancyUL 94V-0 @ 0.75 mmV-0 @ 0.75 mmV-0 @ 0.75 mm
    Comparative tracking indexIEC 60112250 V250 V250 V

    Relative to non-flame-retardant PBT GF15, the FR system in SK642FR BK851 lowers unnotched impact and reduces tensile elongation at break, but it adds the UL 94 V-0 rating required for electrical enclosures. Flame-retardant additives also raise melt viscosity slightly and can form plate-out on mould vents over extended runs; vent cleaning every 5000–10000 cycles is common on production equipment.

    When melt temperature exceeds 260°C during high-speed injection moulding

    Processing boundaries are governed by the flame-retardant package rather than by the PBT melting point. Melting temperature measured by differential scanning calorimetry according to ISO 11357-3 is approximately 225°C, but the recommended melt temperature for SK642FR BK851 is 240–260°C. If the melt-temperature setting exceeds 270°C or if hold-up time at 260°C exceeds 8–10 min, flame-retardant degradation may produce black specks, surface splay, and loss of UL 94 V-0 performance. On production machines with L/D ratios of 20–24 and three-zone screws, screw speeds are typically held between 50 and 120 rpm; back pressure is set at 0.3–0.7 MPa. High shear heating from screw speeds above 150 rpm can push melt temperature beyond the barrel set point by 5–15°C. For thin-wall connectors, injection velocity should be medium-to-fast, but gate diameters below 1.0 mm can cause jetting and glass-fibre bloom. Hydraulic holding pressure is normally set at 40–70 MPa until gate freeze is reached; packing time is adjusted by cavity-pressure sensors rather than by stroke alone.

    Mould temperature should be maintained at 60–100°C. For semi-crystalline PBT, the upper half of this range increases crystallinity and improves dimensional stability and chemical resistance, but cycle time increases. Mould temperatures below 60°C produce an amorphous skin that may reduce HDT/A and increase post-mould shrinkage. Draft angles of 0.5–1.0° per side are recommended for glass-filled grades because fibre-filled PBT exhibits higher ejection friction than unfilled PBT.

    Short shots in SK642FR BK851 are often corrected by increasing mould temperature rather than melt temperature. Elevating the mould from 60°C to 90°C improves filling of thin ribs by delaying solidification of the glass-filled melt; raising the melt temperature beyond 260°C is less desirable because the FR additive package degrades faster. For hot-runner systems, manifold temperature should be set between 240°C and 255°C, and unscrewing tips are preferred over valve-gate designs that generate high shear in the glass-fibre compound.

    Before melt processing, residual moisture is lowered to below 0.02% by weight. A desiccant dryer operated at 120°C for 4 h is the standard preparation for sealed containers, and the drying air dew point should be at or below -30°C. If the granulate is exposed to ambient relative humidity above 60% for more than 2 h, re-drying or hopper-dryer installation is required. Moisture determination by Karl Fischer titration according to ISO 15512 is preferred over weight-loss drying because black glass-filled PBT can release adsorbed surface moisture inconsistently. Hydrolysis of PBT at melt temperature reduces molecular weight and causes silver streaks, reduced tensile strength, and irregular flame-retardant behaviour. Dryer hopper residence should not exceed 6 h at 120°C because prolonged exposure can degrade the FR additive package.

    Electrical performance and comparative tracking index under IEC 60112

    In low-voltage switchgear and control equipment, SK642FR BK851 is specified for connector bodies, relay sockets, terminal blocks, coil formers, sensor housings, and power-supply covers. The UL 94 V-0 rating at 0.75 mm is a critical requirement for components mounted in unattended electrical appliances. Comparative tracking index measured according to IEC 60112 is typically 250 V, placing the grade in tracking class IIIa. Under IEC 60664-1, a CTI of 250 V generally requires larger creepage distances than materials with CTI above 600 V; therefore, product designs should verify clearance and creepage against the overvoltage category and pollution degree of the final equipment. Volume resistivity is typically above 1×1013 Ω·m and surface resistivity above 1×1015 Ω according to IEC 60093. Dielectric strength according to IEC 60243-1 is typically in the range 15–25 kV/mm for 2.0 mm specimens; exact values depend on specimen conditioning and electrode geometry.

    Dielectric constant at 1 MHz is typically around 3.5–4.0 and dissipation factor around 0.015–0.025 according to IEC 60250; these values change with moisture and temperature. Because PBT is polar, dielectric loss is higher than in polyolefins, but the glass reinforcement reduces thermal expansion mismatch in metal-insert designs.

    With respect to chemical-regulatory requirements, the grade is normally assessed against RoHS Directive 2011/65/EU and REACH Regulation 1907/2006 SVHC disclosure obligations. Flame-retardant PBT compounds may contain brominated flame retardants and antimony synergists; therefore, the supplier’s safety data sheet and UL Yellow Card should be checked before use in applications with restricted halogen content. The material is not typically certified for food-contact use under FDA 21 CFR 177.1660 or EU Regulation 10/2011, and it should not be specified for hot-water contact because PBT hydrolyzes at prolonged high-temperature moisture exposure. For outdoor or UV-exposed applications, the black pigmentation provides some surface stabilization, but long-term weathering data for this specific compound is limited; UV stabilization should be requested from the manufacturer if exposure exceeds indoor electrical-equipment service conditions.

    Under sustained load, 15% glass fibre reinforcement reduces creep strain relative to unfilled PBT, but creep-test data according to ISO 899 for SK642FR BK851 is less commonly published than short-term tensile data. In the absence of grade-specific long-term data, design calculations should not extrapolate short-term tensile strength beyond a continuous-use temperature range of approximately 120–130°C for electrical retention and 90–110°C for impact-loaded mechanical retention unless the UL Yellow Card RTI for this grade confirms otherwise. At temperatures above the glass-transition temperature of the amorphous PBT phase, the material retains a useful portion of stiffness up to roughly 150°C, but notched impact becomes more sensitive to moisture and fibre orientation.

    Linear mould shrinkage values for SK642FR BK851 measured according to ISO 294-4 are approximately 0.3–0.5% in flow direction and 0.6–0.9% transverse to flow. This anisotropy is lower than 30% glass fibre PBT, which commonly shows a wider flow/transverse differential and higher warpage in flat connector housings. The coefficient of linear thermal expansion according to ISO 11359-2 is approximately 40×10-6/K in flow direction and 80×10-6/K transverse, compared with 80–100×10-6/K for unfilled PBT. These values are relevant for metal-insert designs and snap-fit mating components.

    The primary operational limitation is the combination of a brittle failure mode at high strain rates and reduced flow length compared with unfilled PBT. The notched Charpy value of approximately 4 kJ/m² means that snap-fit designs should use generous radii and avoid high insert loads. Glass-fibre orientation at weld lines can reduce local strength by 20–40% relative to bulk values; gate placement should be set to move weld lines away from impact-bearing areas. Thin sections below 0.5 mm may require high-speed injection and elevated mould temperatures, but the flame-retardant package may limit the maximum flow length at these thicknesses.

    Published melt volume-flow rate data for SK642FR BK851 is limited in public datasheets, and processors should obtain the current certificate of analysis because FR package variations shift the MVR by more than 10% between lots. In comparable PBT GF15 FR grades, MVR values at 250°C/2.16 kg commonly fall between 10 and 20 cm³/10 min under ISO 1133-1. Viscosity shear thinning is significant because the glass-fibre network breaks down under shear, which supports filling of thin walls but complicates prediction of gate freeze.

    Glass-fibre reinforcement requires wear-resistant screw and barrel surfaces. Bimetallic barrels and hardened screw tips are recommended because 15% glass fibre produces measurable barrel abrasion over 100000–200000 cycles. Mould inserts should be hardened to HRC 52–56 in gate and flash areas. Vent depths should not exceed 0.02–0.03 mm to prevent flash while allowing volatiles to escape; glass-filled FR materials often require wider vents than unfilled PBT.

    Regrind use in flame-retardant PBT is limited because the FR additive distribution and glass-fibre length are affected by multiple heat histories. Typical production practice allows 20–30% regrind from clean sprue/runner systems, but the exact proportion must be validated for UL 94 V-0 at the final wall thickness. Regrind from parts exposed to oil, grease, or metal fines should be excluded. If a production line uses closed-loop recycling with 100% regrind, the flame-retardant V-0 rating and tensile modulus should be re-qualified because glass-fibre attrition shifts the reinforcement aspect ratio.

    Top