Celanese Crastin Pbt Gf10 Sk601 Nc010

Celanese Crastin® PBT+GF10% SK601 NC010

    • Product Name: Celanese Crastin® PBT+GF10% SK601 NC010
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 274576
    Glass Fiber Content 10%
    Density 1.38 g/cm3
    Molding Shrinkage Flow 0.6%
    Molding Shrinkage Cross Flow 1.2%
    Tensile Modulus 3600 MPa
    Tensile Strength 60 MPa
    Elongation At Break 3.0%
    Charpy Notched Impact 23c 4 kJ/m2
    Charpy Unnotched Impact 23c 20 kJ/m2
    Melting Temperature 225 °C
    Hdt A 1 8mpa 195 °C
    Hdt B 0 45mpa 210 °C
    Vicat Softening Temperature 200 °C
    Water Absorption 24h 0.3%
    Volume Resistivity >1E13 ohm·cm
    Dielectric Constant 1mhz 3.7
    Dielectric Strength 30 kV/mm
    Ul94 Flame Rating HB

    As an accredited Celanese Crastin® PBT+GF10% SK601 NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Celanese Crastin® PBT+GF10% SK601 NC010 is supplied in 25 kg moisture-barrier bags, 40 bags per pallet (1,000 kg net).
    Container Loading (20′ FCL) Loaded in a 20-foot FCL container, Celanese Crastin® PBT+GF10% SK601 NC010 is securely packed for chemical transport.
    Shipping Celanese Crastin® PBT+GF10% SK601 NC010 is shipped as non-hazardous, natural-colored polybutylene terephthalate compound pellets in sealed moisture-barrier bags or octabins. It is not regulated as dangerous goods for normal transport. Store dry and cool, protected from moisture and contamination; keep packages closed until use and follow the safety data sheet.
    Storage Store Celanese Crastin® PBT+GF10% SK601 NC010 in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and moisture. Keep containers tightly closed and pallets off the floor. Avoid prolonged exposure to humid air; use according to the supplier’s shelf-life and drying recommendations. Follow the Safety Data Sheet and local regulations for safe handling and storage.
    Shelf Life Celanese Crastin® PBT+GF10% SK601 NC010 typically has a two-year shelf life when stored dry in unopened original packaging below 30°C.
    Free Quote

    Competitive Celanese Crastin® PBT+GF10% SK601 NC010 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Celanese Crastin® PBT+GF10% SK601 NC010 is a natural, uncoloured polybutylene terephthalate injection-moulding compound reinforced with 10% by weight glass fibre. The SK601 designation identifies a medium-viscosity grade in the Crastin® PBT portfolio; NC010 denotes the unpigmented substrate intended for custom colouring or for applications in which no carbon black loading is required. Under ISO 1043 the material is designated PBT-GF10. Typical usage includes automotive electrical connector housings, sensor bodies, relay bases, switch components, and industrial frames requiring a balance of melt flow, stiffness, and reduced anisotropic warpage relative to higher glass loadings.

    The grade is supplied in cylindrical granulate form and is normally processed on reciprocating-screw injection-moulding machines. The melt volume-flow rate is approximately 18 cm³/10 min at 250°C under a 2.16 kg load when tested to ISO 1133, placing it between unfilled PBT and higher glass-fibre Crastin® grades in flow behaviour. The combination of 10% glass fibre and uncoloured natural base resin makes the product suitable for thin-wall parts that require higher tensile modulus than unfilled PBT while maintaining better melt fluidity than 20% glass-filled alternatives.

    What Mechanical and Thermal Boundaries Define SK601 NC010?

    Under ISO 527-2/1A tensile loading, the dry-as-moulded compound typically exhibits a tensile modulus of 2,900 MPa and a tensile stress at break of approximately 75 MPa. Tensile strain at break is generally near 4.5%, reflecting the expected reduction in ductility associated with glass-fibre reinforcement. Flexural modulus tested to ISO 178 is approximately 2,800 MPa, and flexural strength is approximately 115 MPa. The notched Charpy impact value under ISO 179/1eA at 23°C is typically 4.5 kJ/m², while unnotched Charpy impact under ISO 179/1eU is approximately 45 kJ/m² at the same temperature. These levels indicate that the product is intended for dimensionally stable structural components rather than components requiring high ductility or impact-dominated loading.

    Representative dry-as-moulded property data for Celanese Crastin® PBT+GF10% SK601 NC010
    Property Test method Representative value
    Density ISO 1183 1.38 g/cm³
    Tensile modulus ISO 527-2/1A 2,900 MPa
    Tensile stress at break ISO 527-2/1A 75 MPa
    Tensile strain at break ISO 527-2/1A 4.5%
    Flexural modulus ISO 178 2,800 MPa
    Flexural strength ISO 178 115 MPa
    Charpy notched impact at 23°C ISO 179/1eA 4.5 kJ/m²
    Charpy unnotched impact at 23°C ISO 179/1eU 45 kJ/m²
    Melt volume-flow rate ISO 1133 at 250°C/2.16 kg 18 cm³/10 min
    Melting point ISO 11357-1/-3 225°C
    Heat deflection temperature at 1.8 MPa ISO 75-1/-2 150°C
    Mould shrinkage, parallel/transverse ISO 294-4 0.5% / 0.9%

    The values in the table are representative for injection-moulded specimens conditioned at 23°C and 50% relative humidity according to ISO 291. They are not specification limits and should not replace lot-specific certificate data for tool design or load-bearing calculations.

    Pre-drying of the granules is mandatory when moisture content exceeds 0.02% by Karl Fischer titration according to ISO 15512. Desiccant-air drying at 120°C for 4 h to 6 h with a dehumidified-air dew point no higher than -30°C is recommended before melt processing. Melt temperature should be maintained between 250°C and 260°C, and mould temperature should be held at 60°C to 80°C. Residence time in the barrel at melt temperature should not exceed 6 min; exposure above 270°C accelerates hydrolytic and thermal degradation, visible as yellowing, gas generation, and sharp loss of melt-viscosity consistency on the injection unit.

    For reciprocating-screw machines, a minimum L/D ratio of 20:1 and a compression ratio of 2.0:1 to 2.5:1 are typical processing-equipment conditions. The short glass-fibre reinforcement creates non-Newtonian shear-thinning behaviour, so high injection speeds are generally preferred to reduce flow-front hesitation and avoid hollow-glass-fibre orientation defects in thin ribs. Hold pressure should be applied until the gate freezes; pressure-transfer position should be set by cavity-pressure measurement rather than timer alone because batch-to-batch viscosity variation can shift the fill-to-pack transition by 5% to 10% in thin-wall connector frames.

    When SK601 NC010 Replaces Unfilled PBT in Thin-Wall Connector Housings

    In thin-wall connector housings previously moulded from unfilled PBT, substitution with SK601 NC010 changes dimensional stability, stiffness, and failure behaviour. The tensile modulus increases from approximately 2,500 MPa for a medium-viscosity unfilled PBT to 2,900 MPa for SK601 NC010 under ISO 527-2/1A. At the same time, tensile strain at break falls from a typical unfilled value of 25% to approximately 4.5%. The glass-fibre addition therefore improves resistance to short-term flexural loading but makes the part more sensitive to sharp notches and weld-line stress concentrations.

    Representative property shift from unfilled medium-viscosity PBT to Crastin® PBT+GF10% SK601 NC010
    Property Test method Unfilled PBT typical SK601 NC010 typical Direction of change
    Density ISO 1183 1.31 g/cm³ 1.38 g/cm³ Increase
    Tensile modulus ISO 527-2/1A 2,500 MPa 2,900 MPa Increase
    Tensile strain at break ISO 527-2/1A 25% 4.5% Decrease
    Mould shrinkage parallel ISO 294-4 1.5% 0.5% Decrease
    Charpy notched impact at 23°C ISO 179/1eA 5.0 kJ/m² 4.5 kJ/m² Slight decrease

    Relative to 20% glass-filled grades such as Crastin® PBT-GF20, SK601 NC010 provides lower density, lower tensile modulus, and generally higher melt flow. Published data for direct substitution into existing tools is grade-specific; direct replacement without re-running mould-filling simulation is not advised because the lower glass content shifts the balance between cavity-pressure drop, shrinkage anisotropy, and gate freeze time. Relative to 30% glass-filled grades, SK601 NC010 produces less pronounced differential shrinkage between flow and transverse directions, but it also delivers lower stiffness and lower heat deflection temperature. The product is therefore used where the higher stiffness of 20% or 30% glass-filled PBT is unnecessary and where improved melt fluidity or reduced glass-fibre orientation stress is more important.

    Electrical connector and sensor-housing applications for this grade are constrained less by dielectric loss than by comparative tracking resistance, dimensional retention under heat ageing, and surface resistivity control after final colouring. The natural uncoloured NC010 substrate avoids carbon black loading, which can be advantageous where the final compound colourant package controls electrical surface resistivity. However, the uncoloured base resin is not UV-stabilised; outdoor or direct-sunlight applications require a stabiliser package or an approved coloured variant. Comparative tracking index values are colour-dependent and must be verified under IEC 60112 for the exact final pigmentation. Under European Union requirements, the compound is generally assessed against RoHS Directive 2011/65/EU Annex II and REACH Regulation (EC) No. 1907/2006 substance restrictions. For flammability classification, the relevant UL Yellow Card value must be checked against the exact part thickness because test results at 0.8 mm and 1.6 mm can differ for glass-filled PBT.

    Mold Shrinkage Anisotropy, Warpage Control, and Dimensional Stability

    The mould shrinkage behaviour of SK601 NC010 is anisotropic because glass fibres orient predominantly in the flow direction during injection moulding. Representative ISO 294-4 values are approximately 0.5% parallel to flow and 0.9% transverse to flow for a 2 mm plaque. The difference between these values is smaller than that often observed in 30% glass-filled PBT, which is a primary reason the 10% glass loading is selected for flat parts requiring lower warpage. Gate location, wall-thickness variation, and packing pressure remain the dominant processing variables controlling post-moulding distortion on production-scale tooling.

    On cavity-pressure-monitored moulding cells, holding pressure should be maintained until the gate freezes. Premature drop in hold pressure before gate freeze has been associated with sink-mark formation and dimensional drift of 0.1% to 0.3% in thin-wall connector bodies after conditioning to ISO 291. For tools without cavity-pressure sensors, processors should establish the gate-freeze time by incremental hold-time trials and measure post-moulding weight stability across shots. Dimensional checks after moulding should be conducted after conditioning for 24 h at 23°C and 50% relative humidity to account for post-moulding crystallinity drift.

    Continuous exposure to hot glycol-water mixtures in under-hood sensor bodies is an operational boundary. PBT undergoes hydrolytic degradation under prolonged hot-humid conditions above approximately 80°C, and the glass-fibre interface can debond once hydrolysis begins. Published data for this specific configuration is limited; component validation under ISO 16750-4 thermal and humidity cycling is therefore required before production release. Avoid combination with amine-based additives and high-pH aqueous process media because alkaline hydrolysis can cause surface erosion, loss of gloss, and premature loss of interfacial strength. Regrind addition levels above 25% by weight may reduce notched impact values and increase black-speck contamination from degraded PBT. The material should be stored in sealed containers away from direct sunlight and high ambient humidity, because the uncoloured NC010 substrate is more visibly affected by oxidation and airborne contamination than pigmented glass-filled grades.

    Top