Celanese Crastin Hydrolytic Pbt Hr5330hf Nc010

Celanese Crastin® Hydrolytic PBT HR5330HF NC010

    • Product Name: Celanese Crastin® Hydrolytic PBT HR5330HF NC010
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 422058
    Material Type PBT-GF30
    Hydrolytic Stabilization Yes
    Density 1.53 g/cm³
    Tensile Modulus 10000 MPa
    Tensile Stress At Break 140 MPa
    Tensile Strain At Break 2.5%
    Charpy Notched Impact Strength 23c 9 kJ/m²
    Deflection Temperature 1 8mpa 205 °C
    Melting Temperature 225 °C
    Water Absorption 24h 0.25%
    Molding Shrinkage Parallel 0.3%
    Molding Shrinkage Normal 0.9%
    Flammability Rating UL94 HB
    Processing Method Injection molding

    As an accredited Celanese Crastin® Hydrolytic PBT HR5330HF NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Celanese Crastin® Hydrolytic PBT HR5330HF NC010 is supplied in 25 kg moisture-barrier bags, palletized and labeled with grade, lot, and safety details.
    Container Loading (20′ FCL) Celanese Crastin® Hydrolytic PBT HR5330HF NC010 loaded in a 20-foot FCL container, palletized, secured, and protected from moisture during transport.
    Shipping Celanese Crastin® Hydrolytic PBT HR5330HF NC010 is shipped as non-hazardous thermoplastic resin pellets in sealed bags or containers. It is not regulated for transport under DOT, IMDG, or IATA. Store in a dry, cool, ventilated area, protected from moisture, direct sunlight, and contamination.
    Storage Store Celanese Crastin® Hydrolytic PBT HR5330HF NC010 in a cool, dry, well-ventilated area, away from direct sunlight, heat, moisture, and ignition sources. Keep containers tightly closed and protected from humidity, strong acids, bases, and oxidizing agents. Avoid dust generation and follow the SDS and local regulations for safe handling and storage.
    Shelf Life Shelf life is 24 months from delivery when stored unopened in original packaging, dry, at temperatures not exceeding 30°C.
    Free Quote

    Competitive Celanese Crastin® Hydrolytic PBT HR5330HF NC010 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Celanese Crastin® HR5330HF NC010 is an unfilled, hydrolysis-resistant polybutylene terephthalate (PBT) injection-molding grade. The suffix “HR” identifies a hydrolytic stabilizer package; “HF” identifies high-flow melt rheology developed for thin-wall, multi-cavity tooling; “NC010” denotes natural, uncolored pellets without carbon black or pigment loading. The grade is specified where a semi-crystalline polyester must retain tensile properties and impact after exposure to hot humid environments. Representative density per ISO 1183-1 at 23 °C is 1.31 g/cm³. Melt volume-flow rate per ISO 1133-1:2022 at 250 °C/2.16 kg is published as 38 cm³/10 min, subject to lot-specific variation and sample preparation. Tensile modulus per ISO 527-2 at 1 mm/min is 2500 MPa; tensile stress at break at 50 mm/min is 55 MPa; Charpy notched impact strength per ISO 179-1/1eA at 23 °C is 4.0 kJ/m². The melting peak determined by differential scanning calorimetry per ISO 11357-3 at 10 K/min is near 225 °C. Heat deflection temperature under 1.8 MPa per ISO 75-2/A is 65 °C, and comparative tracking index per IEC 60112 is 600 V. These dry as-molded values place the product in the general-purpose unfilled PBT range; differentiation from standard PBT appears under hydrolytic aging rather than in short-term tensile data.

    Representative datasheet properties for Crastin® HR5330HF NC010
    PropertyStandardConditionRepresentative value
    DensityISO 1183-123 °C1.31 g/cm³
    Melt volume-flow rateISO 1133-1:2022250 °C/2.16 kg38 cm³/10 min
    Tensile modulusISO 527-21 mm/min2500 MPa
    Tensile stress at breakISO 527-250 mm/min55 MPa
    Charpy notched impact strengthISO 179-1/1eA23 °C4.0 kJ/m²
    Melting peakISO 11357-310 K/min225 °C
    Heat deflection temperatureISO 75-2/A1.8 MPa65 °C
    Comparative tracking indexIEC 60112Solution A600 V

    What separates hydrolytic stabilization from conventional PBT formulations?

    In unmodified PBT, ester linkages undergo chain scission when water is present above the glass-transition temperature. The reaction is accelerated by carboxyl end groups, acidic residues, and processing-induced thermal history. The hydrolytic stabilizer package in Crastin® HR5330HF NC010 is designed to reduce the concentration of active chain ends available for hydrolysis and to buffer local pH during service. This mechanism is measurable through accelerated aging per ISO 22088-3 or OEM-specific protocols such as VW PV 1200 and USCAR-2 Class 4. Published comparative data for this specific grade are limited; however, hydrolysis-stabilized PBT grades typically retain 80–90% of initial tensile strength after 1000 h at 85 °C and 85% RH, whereas unmodified PBT of comparable initial tensile strength may fall below 50% under the same conditions. The performance boundary is not indefinite: polyester hydrolysis still occurs at high pH, at steam temperatures above 120 °C, and in continuous immersion with high acid content.

    To avoid latent hydrolysis during melt processing, closed-loop moisture control is required. Pellets should be dried to a residual moisture content below 0.02% using a desiccant-bed dryer with dew point not higher than −30 °C, hopper temperature 120 °C, and drying time 4–6 h. Melt temperature at the nozzle should be held between 250 °C and 270 °C, with the lower half of the range preferred in machines where residence time exceeds 5 min; mold temperature from 40 °C to 80 °C produces adequate crystallinity and surface release in unfilled PBT. On a reciprocating-screw injection machine with an L/D 20–24 general-purpose screw and compression ratio 2.5:1–3.0:1, the high-flow melt permits filling of 0.4 mm wall sections at hydraulic pressure values normally below 120 MPa, but cavity pressure should be measured directly because machine-specific pressure loss varies with nozzle tip, hot-runner geometry, and gate design. Holding pressure should be adjusted to gate-seal time determined by part mass stabilisation, not by arbitrary timer values.

    Thin-wall filling pressure and the high-flow envelope

    The high-flow designation in HR5330HF NC010 corresponds to a melt volume-flow rate approximately 60% higher than standard unfilled PBT grades in the same product family, although exact values are lot-specific and must be verified from the certificate of analysis. In production-scale connector tools with sub-gate diameters of 0.6 mm and wall thickness below 0.5 mm, this flow increase permits shorter filling time and lower injection pressure than standard-flow PBT; exact pressure reduction must be derived from mold-filling simulation because hot-runner shear heating and gate freeze time are geometry-dependent. The rheological benefit is temperature-sensitive: for every 10 °C increase above 250 °C, apparent melt viscosity declines by 8–12%, but prolonged exposure to 270 °C increases thermal degradation risk. Mold-filling simulation with Cross-WLF viscosity model parameters is recommended before tool construction; generic PBT material cards without HR-specific degradation kinetics overpredict flow length after prolonged hot-runner residence.

    In engine-compartment connector applications, the resin is selected for the combination of a 600 V comparative tracking index per IEC 60112, a melting peak near 225 °C per ISO 11357-3, and hydrolysis resistance under temperature-humidity cycling. For connectors exposed to 85 °C/85% RH for 1000 h, retention of tensile strength and elongation is a more reliable acceptance criterion than dry as-molded impact, because standard PBT can pass short-term mechanical tests and still fail late-stage durability after moisture uptake. The grade is also used in power distribution housings where UL 94 HB is typical for the natural unfilled state; UL 94 V-0 requires a flame-retardant formulation or additive masterbatch. Natural grade NC010 is intended for internal parts or for colouring at the molding facility with masterbatch systems compatible with PBT.

    When hot humid aging exceeds 1000 hours, tensile retention becomes the decisive metric

    Long-term component testing at 85 °C and 85% RH is common for automotive interior and underhood connectors. The relevant failure mode is not initial yield, but the drop in tensile strain at break after moisture-induced chain scission. Hydrolysis-stabilized PBT such as HR5330HF NC010 slows the time to 50% tensile-strength loss relative to unmodified PBT; the exact ratio depends on initial carboxyl end-group concentration, part thickness, and exposure period. In a comparative aging program, tensile bars per ISO 527-2 should be conditioned for 500 h, 1000 h, and 2000 h at 85 °C/85% RH. Published data for this specific grade’s retention curve are limited, so end-users should commission a grade-specific aging verification before design freeze. The test should include welded or snap-fit regions because molded-in stress and weld lines accelerate hydrolysis.

    Design verification and regulatory compliance matrix
    AssessmentStandard or regulationCondition or clause
    Restriction of hazardous substancesEU 2011/65/EU + (EU) 2015/863Annex II threshold values
    REACH SVHC declarationRegulation (EC) No 1907/2006Article 33 communication
    Comparative tracking indexIEC 60112600 V
    Flame classification, natural unfilledUL 94HB at specified wall thickness
    Hydrolytic agingISO 22088-385 °C/85% RH, 500–2000 h

    Because polyester hydrolysis is pH-dependent, the high-flow variant is not recommended for continuous contact with strong alkaline solutions, hot mineral acids, or amine-based coolants above 80 °C unless component testing demonstrates sufficient retention of molecular weight. Molded parts with residual stress from gating or weld lines show earlier brittle failure even in hydrolysis-stabilized grades; annealing or gate relocation may be required. Regrind addition above 20% shifts melt viscosity and reduces hydrolytic aging resistance unless the regrind is dried to the same moisture specification as virgin pellets.

    For thin-wall sensor housings with overmolded elastomer seals and metallic inserts, insert temperature and mold tempering must be validated because the high-flow resin can generate visible weld lines at gate junctions and insert boundaries. Gas counterpressure and dynamic mold temperature control are used in production tools to reduce weld-line depth at critical sealing surfaces, but process validation must be performed on the actual tool and injection machine.

    Top