| HS Code | 148320 |
| Polymertype | Polybutylene terephthalate (PBT), hydrolytically stabilized |
| Reinforcement | 15% glass fiber |
| Color | Natural (NC010) |
| Density | 1.41 g/cm³ |
| Tensilemodulus | 5200 MPa |
| Tensilestressatbreak | 95 MPa |
| Strainatbreak | 2.5% |
| Charpynotchedimpactstrength23c | 5 kJ/m² |
| Charpyunnotchedimpactstrength23c | 35 kJ/m² |
| Hdtat1 8mpa | 200 °C |
| Meltingtemperature | 225 °C |
| Moldingshrinkageparallel | 0.4% |
| Moldingshrinkagenormal | 0.9% |
| Waterabsorption24h | 0.4% |
| Flammabilityrating | HB |
As an accredited Celanese Crastin® Hydrolytic PBT HR5315HF NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Celanese Crastin® Hydrolytic PBT HR5315HF NC010 is supplied in 25 kg moisture-resistant bags, palletized for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized, shrink-wrapped 25 kg bags of Celanese Crastin® Hydrolytic PBT HR5315HF NC010, secured for transport. |
| Shipping | Celanese Crastin® Hydrolytic PBT HR5315HF NC010 is supplied as dry thermoplastic polyester pellets in sealed moisture-barrier bags, boxes, or octabins. It is not classified as dangerous goods for transport. Ship and store in a cool, dry, ventilated area, protected from moisture, contamination, and direct sunlight. |
| Storage | Store Celanese Crastin® Hydrolytic PBT HR5315HF NC010 in its original, sealed packaging in a cool, dry, well-ventilated area, away from direct sunlight, heat, moisture, and contaminants. Keep containers closed to prevent humidity ingress. Avoid prolonged exposure to elevated temperatures; if moisture absorption is suspected, dry the resin according to the manufacturer’s recommendations before processing. |
| Shelf Life | Shelf life is 24 months when stored in sealed, moisture-proof packaging under dry, cool conditions (10–30°C), away from sunlight. |
Competitive Celanese Crastin® Hydrolytic PBT HR5315HF NC010 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Celanese Crastin® HR5315HF NC010 is an unfilled, hydrolytically stabilized polybutylene terephthalate injection-molding grade supplied in natural color. The grade is formulated for thin-walled electrical and electronic parts that must retain mechanical and dielectric integrity in hot, humid service conditions. The product designation identifies the core attributes: HR denotes hydrolysis resistance, HF denotes high flow, and NC010 denotes natural color. Under ISO 11469, the resin is identified as PBT-HI. The high-flow character is defined by a melt volume-flow rate typically reported in the 20–35 cm³/10 min range under ISO 1133-1:2022 at 250 °C and 2.16 kg. Tensile properties are assessed on ISO 527-2/1A bars, impact resistance by notched Charpy under ISO 179-1/1eA, and heat distortion by ISO 75-2. The grade belongs to the semi-crystalline polyester family; differential scanning calorimetry under ISO 11357-3 typically places the melting peak at 220–225 °C. The glass transition is generally measured in the 45–60 °C range by ISO 11357-2, which has practical implications for humid aging because chain mobility increases above that temperature.
PBT degradation in humid conditions follows an autocatalytic chain-scission mechanism. Water attacks the ester carbonyl linkage, producing hydroxyl and carboxylic acid end groups; the carboxylic acid groups then catalyze further ester hydrolysis. The degradation rate is therefore not constant but accelerates as the concentration of acid end groups rises. Heat and absorbed moisture control the rate. The hydrolysis reaction is most severe when parts are exposed to temperatures above the glass transition, around 45–60 °C, and relative humidity above 80 %. Hydrolytic stabilization for HR5315HF NC010 interrupts this autocatalytic cycle. Published industrial data for hydrolytically stabilized PBT grades indicate that stabilization is generally achieved through control of carboxylic acid end-group concentration and incorporation of acid-scavenging or end-group-capping chemistry. The exact stabilizer composition is not disclosed in standard technical literature for this grade. The practical effect is a shift in molecular-weight retention during hot-humid aging: tensile strength, elongation, and notched impact strength are retained for longer exposure windows than with general-purpose PBT. Stabilization is not permanent protection. At sufficiently high temperature and steam pressure, all PBT ester linkages undergo hydrolysis regardless of additive package. The material is therefore not recommended for continuous pressurized steam service or repeated autoclave sterilization above 121 °C. The rate of property retention also depends on wall thickness, because thicker sections retain absorbed moisture for longer periods and increase the internal acid concentration gradient.
Molecular weight retention is commonly monitored by melt viscosity or solution viscosity after aging. A drop in solution viscosity under ISO 1628-5 methods indicates chain scission before tensile failure occurs. In molded parts, the first mechanical indicators are usually reductions in notched impact strength and elongation at break, while tensile modulus may remain nearly constant because the crystalline structure retains short-term stiffness. This property sequence is important for inspection programs: if a hydrolytically aged connector retains modulus but loses terminal retention force, the root cause is often surface embrittlement and microcracking at terminal insertion points. Moisture conditioning prior to processing should be avoided, even at room temperature, because absorbed surface moisture can produce splay and reduce weld-line strength.
Residual moisture must be reduced to 0.02 wt% or less before melting to prevent processing-induced hydrolysis. Desiccant-bed drying at 110–120 °C for 4–6 h is conventional, with drying air supplied at a dew point of −30 °C or lower. Closed-loop material handling from dryer to feed throat is specified in high-humidity molding environments. Water absorption at saturation is typically measured at 0.2–0.5 wt% under ISO 62; this seemingly low level is sufficient to degrade PBT at melt temperature, which is why closed-loop drying is mandatory. The material is processed at melt temperatures of 240–260 °C and mold temperatures of 60–100 °C. The lower mold-temperature range permits short cycle times in thin-wall parts, while the upper range improves surface finish, weld-line strength, and crystalline uniformity in sections above 2 mm. Because HR5315HF NC010 is a high-flow grade, it commonly permits a 20–40 % reduction in peak injection pressure relative to general-purpose unfilled PBT at identical melt temperature. This viscosity advantage also increases the risk of flash if clamp force is insufficient or parting-line maintenance is poor. Cavity pressure in thin-wall electronic parts is commonly held below 500–600 bar, but exact values must be established from flow simulation and mold trials. Melt residence time at upper melt-temperature settings should remain below 8–10 min. Prolonged residence, especially with moisture ingress, accelerates chain scission and reduces notched impact strength before visible color shift occurs. Nozzle temperature should follow the front-zone set point, and a shut-off nozzle is favored for large shot sizes to reduce drooling in high-flow PBT.
Screw geometry and check-ring condition influence melt quality. A general-purpose polyolefin screw is unsuitable because PBT has a sharper melting transition and lower melt strength; a low-shear nylon/PBT screw with a compression ratio near 2.5:1 and an L/D ratio of 18:1–22:1 is typically used. Shot size should fill 50–70 % of barrel capacity to limit residence time. Back pressure in the 0.3–0.7 MPa range is sufficient for homogenization; higher back pressure can generate shear heating and cause flashing on low-viscosity high-flow grades. Injection speed is dictated by wall thickness and surface appearance, with high-speed filling used for thin-wall sections below 1 mm to prevent premature gate freeze, and profiled speed reduction near the end of fill to avoid gas traps and weld-line voids.
Recycled regrind of HR5315HF NC010 can be used, but the recommended regrind ratio should not exceed 20–30 % by weight in critical electrical parts unless validated by aging tests. Repeated drying and remelting consumes the hydrolytic stabilizer and reduces the safety margin in hot-humid service. Sprues, runners, and rejected startup parts should be kept clean, dry, and free of mineral oil or release-agent contamination. Contaminated regrind is a documented cause of delamination in molded parts because low-molecular-weight material migrates to the flow front and weakens weld lines.
The unfilled, high-flow profile of HR5315HF NC010 places it between general-purpose unfilled PBT and reinforced PBT compounds. The absence of glass fiber or mineral filler preserves high elongation, fine surface detail, and low anisotropic shrinkage, but it lowers tensile modulus and heat deflection temperature. The following table compares typical property ranges for hydrolytically stabilized unfilled high-flow PBT, standard unfilled PBT, and 30 wt% glass-fiber-reinforced PBT.
| Property | Test Method | HR5315HF NC010 nominal range | Standard unfilled PBT nominal range | 30% glass-fiber PBT nominal range |
|---|---|---|---|---|
| Density | ISO 1183-1:2019 | 1.30–1.32 g/cm³ | 1.30–1.32 g/cm³ | 1.52–1.56 g/cm³ |
| Tensile modulus | ISO 527-2/1A | 2400–2600 MPa | 2400–2800 MPa | 9000–10000 MPa |
| Tensile stress at break | ISO 527-2/1A | 50–60 MPa | 50–65 MPa | 130–150 MPa |
| Notched Charpy impact at 23 °C | ISO 179-1/1eA | 4–6 kJ/m² | 3–6 kJ/m² | 8–12 kJ/m² |
| Heat deflection temperature 0.45 MPa | ISO 75-2/B | 150–165 °C | 150–165 °C | 210–220 °C |
| Melt volume-flow rate at 250 °C / 2.16 kg | ISO 1133-1:2022 | 20–35 cm³/10 min | 10–20 cm³/10 min | 8–15 cm³/10 min |
| Flammability at 0.75 mm | UL 94 | HB | HB | HB |
| Coefficient of linear thermal expansion flow direction | ISO 11359-2 | 80–120 × 10⁻⁶ /K | 80–120 × 10⁻⁶ /K | 25–35 × 10⁻⁶ /K |
Values are nominal ranges assembled from public industrial datasheets and should not be used as lot-specific release limits. The key differentiation of HR5315HF NC010 is not visible in dry-room mechanical data but in retained properties after hydrolytic aging. General-purpose unfilled PBT can lose more than 50 % of initial tensile strength after 1,000 h at 85 °C and 85 % relative humidity, whereas hydrolysis-resistant PBT is formulated to retain a substantially higher proportion of initial properties under the same conditions. Published data for this specific grade under every OEM-specific aging protocol is limited; production qualification must use application-defined test conditions and molded test specimens. Flame-retardant PBT variants are selected when UL 94 V-0 at thin wall is required; HR5315HF NC010 is typically documented as UL 94 HB at common molded thicknesses.
HR5315HF NC010 differs from standard unfilled PBT primarily in hot-humid aging response. In dry mechanical properties, the two materials are similar. The difference appears in retained tensile strength and retained notched impact after accelerated hydrolytic aging. A component that is never exposed to moisture gains little from the HR grade; a component exposed to water, condensation, or humid air at elevated temperatures may gain substantially longer service life. Design engineers should evaluate the actual humidity exposure, because selecting a hydrolysis-resistant grade without hot-moist service does not improve dry heat aging or UV stability. Additional UV stabilizers are needed for direct outdoor exposure. Compared with PBT/PET blended resins, HR5315HF NC010 retains the faster crystallization rate of PBT, which yields shorter molding cycles but lower surface gloss; PET-rich blends are sometimes used for smooth surfaces and lower warpage but can require higher mold temperatures and longer holding pressure.
Connector bodies, sensor housings, and electronic module enclosures in automotive underhood and cabin locations are subjected to combined thermal and humidity loads that accelerate PBT hydrolysis. Qualification programs for such components frequently reference ISO 16750-4:2010 climatic load sequences, including high-humidity heat soak at 85 °C and 85 % relative humidity, followed by low-temperature exposure and power-temperature cycling. In these applications, HR5315HF NC010 is used where terminal retention force, dimensional stability, and surface insulation resistance must survive extended moisture exposure. The material’s high flow permits thin-wall connector face plates and dense pin arrays, but tool design must compensate for high-flow characteristics with adequate venting and precision parting-line fit. Because the grade is unfilled, its coefficient of linear thermal expansion is isotropic and lower than unfilled polyolefins, but higher than glass-filled PBT. This thermal expansion behavior should be considered when metal terminals are inserted after molding. The hydrolytic stabilization does not prevent degradation in direct contact with strongly alkaline battery electrolytes, hot concentrated acids, or aggressive amine-containing sealants; such combinations should be avoided during design review.
Terminal retention force is often evaluated per USCAR-21 or OEM-specific pull-out procedures. Because PBT can undergo minor post-molding shrinkage, retention force may rise over time as the polymer locks around inserted terminals, but embrittlement from uncontrolled hydrolysis creates the opposite failure mode: terminal back-out due to cracking. The high-flow grade’s low melt viscosity enables molding around terminals with less insertion-side deformation, but insert tooling must maintain stable pin alignment to avoid short shots in thin sections. In automotive connector validation, specimens are often exposed to multiple cycles of hot-humid soak, cold shock at −40 °C, and power-temperature cycling. The material must not exhibit surface cracking, insulation resistance drop, or terminal retention loss below the OEM limit. Hydrolytically stabilized PBT is also used in exterior electrical enclosures where solar heating and condensation cycles occur. The grade’s natural color can be laser-marked in many final-part configurations, but marking contrast must be validated with the actual masterbatch because pigment packages change laser absorption and tracking performance.
Thin-wall filling behavior in HR5315HF NC010 is determined by high melt volume-flow rate and rapid crystallization. Multi-cavity electrical connector tools with pin counts above 40 can be filled using gate diameters of 0.5–1.0 mm per cavity when melt temperature is held near 250 °C. Because PBT crystallizes rapidly, gates must freeze quickly but not before the packing phase is complete; valve-gated hot-runner systems with independently controlled nozzle tips are specified on many high-density tools. The material’s low melt viscosity under shear permits flow length-to-wall-thickness ratios above 150:1 in unfilled PBT at pressures below 1,000 bar, although exact values depend on mold temperature and gate geometry. Cavity tooling should be hardened to HRC 48–52 if the production run exceeds 500,000 cycles because unfilled PBT at high injection speed can produce gate wear. The absence of abrasive glass fibers reduces screw and barrel wear, but the high flow does not eliminate the need for a properly sized check-ring assembly to maintain shot-to-shot consistency. Splay, silver streaking, and gate blush are observed in production when moisture content exceeds the drying limit or when melt temperature exceeds 260 °C; these defects are addressed by lowering melt temperature, reducing injection velocity, or verifying dew point in the drying system.
HR5315HF NC010 is available as a natural-color resin that can be color-compounded or masterbatched to meet OEM aesthetic specifications. Under the ISO 1043-1 marking system, the material is identified as PBT-HI. Compliance is commonly assessed against the European Union REACH regulation, RoHS 2011/65/EU, and the end-of-life vehicle directive 2000/53/EC when relevant. The material is not marketed as a food-contact grade; design engineers requiring food-contact compliance should verify specific migration limits under EU Regulation 10/2011 or FDA 21 CFR for the final article rather than assume compliance from the base resin. Flammability evaluation is typically performed under UL 94 on molded thicknesses relevant to the application; electrical and electronic parts may require additional tracking resistance evaluation under IEC 60112 and dielectric strength testing under IEC 60243-1. Surface insulation resistance after humidity exposure is often measured under IEC 62631-3-2, and comparative tracking index values for unfilled PBT are commonly in the 500–600 V range, but exact values depend on color and formulation additives.