Cabot Cabelec Ca4918 Ldpe Conductive Compound

Cabot CABELEC® CA4918 LDPE, Conductive Compound

    • Product Name: Cabot CABELEC® CA4918 LDPE, Conductive Compound
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 270066
    Density 1.08 g/cm³
    Melt Flow Rate 6.0 g/10 min (190°C/2.16 kg)
    Carbon Black Content 30%
    Volume Resistivity 100 ohm·cm
    Tensile Strength 15 MPa
    Elongation At Break 200%
    Hardness Shore D 55
    Vicat Softening Temperature 90°C
    Brittleness Temperature -70°C
    Melting Point 110°C
    Moisture Content <0.1%

    As an accredited Cabot CABELEC® CA4918 LDPE, Conductive Compound factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Cabot CABELEC® CA4918 LDPE Conductive Compound is supplied in 25 kg (55 lb) polyethylene bags, palletized for shipping.
    Container Loading (20′ FCL) Standard 20′ FCL container loaded with Cabot CABELEC® CA4918 LDPE, Conductive Compound, palletized, shrink-wrapped, evenly distributed, and secured for transport.
    Shipping Cabot CABELEC® CA4918 LDPE, Conductive Compound is shipped as non-hazardous thermoplastic pellets in sealed moisture-barrier bags, boxes, or octabins on pallets. Store dry, away from heat and contamination. No UN number or dangerous goods classification required for transport. Handle with care; avoid puncturing packaging. Maintain clean, dry conditions during transit.
    Storage Store Cabot CABELEC® CA4918 LDPE Conductive Compound in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original containers tightly closed, palletized, and protected from moisture, dust, and contamination. Maintain ambient temperatures, avoid excessive stacking, and follow first-in, first-out inventory practices. Consult the safety data sheet for specific local requirements.
    Shelf Life Typically 24 months from manufacture when stored unopened in original packaging, dry, below 30°C, away from direct sunlight.
    Application of Cabot CABELEC® CA4918 LDPE, Conductive Compound

    Thermoformed matrix trays and wafer shipping carriers for semiconductor and PCB assembly lines are produced from Cabot CABELEC® CA4918 LDPE conductive compound by first extruding sheet of 0.5–3.0 mm thickness, followed by plug-assist forming at sheet surface temperatures of 120–150 °C and mold temperatures of 20–40 °C. The applicable ESD compliance framework is ANSI/ESD S20.20 in conjunction with IEC 61340-5-1; surface resistance is tested to IEC 61340-2-3 or ANSI/ESD STM11.11 at 12% ±3% RH and 23 °C, with a concentric ring probe at 10 V or 100 V depending on the resistance decade. The compound is loaded with a conductive carbon black network in LDPE, so the standard processing ratio is 100% neat resin without dilution; if sheet stiffness must be raised by blending with virgin LDPE, the addition ratio of CABELEC CA4918 should not fall below 80 wt% unless production trials have mapped the non-linear rise in surface resistance. Production problems in this segment concentrate in draw-ratio uniformity: deep thermoformed pockets with draw ratios above 3:1 can fracture the carbon black network enough to push local surface resistance from below 1×106 Ω into the dissipative-to-insulative transition, so post-forming testing should sample the corners, sidewalls, and bottom simultaneously. Sheet extrusion on 60–90 mm single-screw extruders with 24:1–30:1 L/D, a melt pump, flat die, and chill-roll stack is the preferred route; barrel zones from 170 °C to 210 °C are typical, but the melt should not exceed 230 °C to avoid polymer matrix degradation, carbon black plate-out, and processing odour. Finished parts include wafer shipping trays, PCB handling trays, component matrix trays, and stackable dunnage trays used in wafer fabs, PCB assembly, and third-party test houses.

    Verification pointStandard / methodMeasurement conditionInstrument / electrode
    Surface resistance of tray materialIEC 61340-2-312% ±3% RH, 23 °CConcentric ring probe, 10 V / 100 V
    Surface resistance of planar sheetANSI/ESD STM11.1112% ±3% RH, 23 °CCylindrical 5 lb electrodes
    Volume resistanceIEC 61340-2-3 or ASTM D257-14500 V DC, 60 s electrificationGuarded electrode / picoammeter
    Static decayIEC 61340-2-1±1000 V, 10% cut-offStatic decay analyser

    What Limits Drop Impact Resistance in Blow Molded Conductive Containers for Solvent Transfer?

    Because charge accumulation during solvent transfer is a fire and explosion hazard, blow molded conductive jerrycans and narrow-mouth drums made from CABELEC CA4918 LDPE conductive compound are used in solvent dispensing and flammable powder handling. The primary compliance path is IEC 61340-5-1 for ESD control, with surface resistance measured to IEC 61340-2-3 at 12% ±3% RH; in classified hazardous areas, the end user applies IEC 60079-32-2 for electrostatic hazard assessment. The formulation addition ratio is normally 100% neat compound because dilution with virgin LDPE at as little as 15 wt% can increase surface resistance by several orders of magnitude and must be validated before production. The downstream process is extrusion blow molding on an accumulator-head machine, typically fed by a 65–75 mm grooved-barrel extruder with L/D 25:1–28:1, using a die gap of 1.5–3.0 mm, parison melt temperature of 190–210 °C, mold temperature of 10–30 °C, and blow pressure of 0.5–0.8 MPa; the melt must retain sufficient strength during parison hang without drawing down under its own weight. Process conflicts arise between melt temperature, carbon black dispersion, and drop impact. At a melt temperature below 180 °C, carbon black agglomerates may remain as process-induced defects that reduce low-temperature impact strength; at a melt temperature above 220 °C, parison drawdown lowers wall thickness consistency, and weld lines at the pinch-off zone can show localized surface resistance spikes. Drop impact is tested to ASTM D5276-19 or a customer-specific container drop test; low-temperature brittleness is compared using ASTM D746-14. Terminal products include 5–25 L conductive jerrycans, narrow-neck reagent bottles, and 20–60 L conductive drums for solvent transfer and groundable flammable-powder containers.

    At screw speeds above 120 min-1 during injection molding of CABELEC CA4918 LDPE conductive compound, the combination of shear heating and high carbon black loading can shift the melt temperature beyond the target range and alter the conductive network in stackable tote boxes and bins for ESD-protected electronics assembly. The applicable standard for end-user ESD control is ANSI/ESD S20.20 or IEC 61340-5-1, and surface/volume resistance is characterized to IEC 61340-2-3; surface resistance measurements use 10 V and 100 V constant voltage under 12% ±3% RH. The formulation addition ratio is 100% neat compound; if post-industrial regrind is added, the maximum regrind level should be kept at 15–20 wt% and the regrind must be sieved to remove degraded carbon black fines. Processing on hydraulic injection molding machines with clamping force from 2,500 kN to 8,000 kN is typical because wall thicknesses of 3.0–5.0 mm generate long flow lengths in tote-box tooling. Melt temperature is controlled at 190–220 °C, mold temperature at 15–40 °C, and injection speed at low to moderate to avoid frictional shear that orients carbon black and raises surface resistance. The main process failure mode occurs at knit lines: when multiple gates fill a tote-box base, the recombining flow fronts can produce a discrete band of higher resistance. Tooling should be configured with single sequential valve gates or post-mold surface resistance mapping of knit-line regions. Finished parts include stackable tote boxes, ESD bins, component transport boxes, and conductive KANBAN containers used in electronics assembly, repair, and logistics centers.

    When Blown Film Bubble Stability Governs ESD Protective Packaging

    Blown film lines used for ESD protective packaging made from CABELEC CA4918 LDPE conductive compound operate within a narrow bubble-stability window because the carbon black level that produces surface resistance below 1×106 Ω/sq also reduces melt extensibility. Formulation addition ratio is 100% neat compound; if the film must be heat-sealed to a non-conductive LDPE inner layer, the conductive layer is typically a coextruded skin or the compound is laminated to a carrier, not dry-blended. The downstream production process is tubular film extrusion on a single-screw extruder with L/D 25:1–30:1, a spiral die of 150–300 mm diameter, blow-up ratio 2.0:1–2.8:1, and die gap 0.8–1.5 mm; melt temperature is held at 190–210 °C to maintain carbon black dispersion while avoiding bubble flapping. Because the carbon black network is shear-sensitive, an increase in screw speed above 100 min-1 can transfer excessive shear energy and raise local melt temperature, leading to thin spots that fail surface-resistance uniformity. The industry compliance framework for packaging is IEC 61340-5-1 and ANSI/ESD S20.20; verification uses IEC 61340-2-3 for surface resistance and IEC 61340-2-1 for charge decay on film specimens. Terminal products include ESD bags, moisture-barrier conductive shrouds, component retainer films, and interleave films for PCB kitting. Published data for this specific configuration is limited; therefore, film extrusion parameters and antistatic testing must be validated on production-scale lines, not transferred directly from compression-moulded plaque values.

    Profile Extrusion of Conductive Component Rails and Edge Protectors

    In SMT lines and ESD-protected workstations, conductive component rails, edge protectors, and PCB transport guides are profile-extruded from CABELEC CA4918 LDPE conductive compound. The applicable compliance standards are IEC 61340-5-1 and ANSI/ESD S20.20, with surface resistance measured by IEC 61340-2-3 on the extruded profile at 12% ±3% RH and 23 °C. The compound is processed neat at 100%; because profile extrusion uses long die lands and back pressure, the addition of virgin LDPE to improve surface finish is not recommended without re-qualification of the conductive network. Downstream process conditions on a 45–65 mm single-screw extruder with L/D 24:1–28:1 include barrel temperature profiles from 160 °C near the feed zone to 200–210 °C at the die; vacuum sizing is preferred over pressure calibration because carbon black-loaded LDPE has lower melt strength than unfilled LDPE. The principal process bottleneck is die drool: carbon black and process-aid decomposition products can build at the die exit after 8–16 h of continuous production, leading to surface defects and inconsistent resistance along the profile. Periodic wiping with copper-brass tooling and avoiding zinc stearate-based cleaning compounds are common production measures. Terminal products include grounded PCB transport guides, SMT component rails, edge protectors for ESD benches, and snap-on conductive covers used in electronics manufacturing and optoelectronics assembly.

    Free Quote

    Competitive Cabot CABELEC® CA4918 LDPE, Conductive Compound prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Cabot CABELEC® CA4918 is introduced as a pelletized low-density polyethylene compound containing a pre-dispersed conductive carbon black network. The product is positioned as a ready-to-use conductive polyolefin rather than a masterbatch, which means the carbon black structure and the electrical percolation network are established during compounding before the material reaches the converting line. In extrusion and thermoforming operations, this formulation strategy shifts the burden of dispersion control from the processor to the compound supplier. The compound is typically evaluated for extruded sheet, thermoformed trays, and profiles where static-dissipative or conductive surface resistivity is required under IEC 61340-5-1 conditions. Supplier documentation should be consulted for exact melt flow rate, density, tensile properties, and resistivity values; Cabot has published application-specific data for the CABELEC product family, but grade-specific public values for CA4918 remain limited outside the manufacturer’s current technical datasheet. The LDPE base polymer provides lower flexural modulus and easier heat-sealing than conductive polypropylene or polycarbonate compounds, a distinction that becomes important in high-draw ratio packaging and flexible ESD-protective formats.

    When Pre-Drying and Melt-Temperature Control Are Layered into the Extrusion Window

    For a carbon black-loaded LDPE pellet, the practical drying question is not governed solely by the water absorption of the polyethylene matrix. Low-density polyethylene is not strongly hygroscopic, but carbon black surfaces can adsorb moisture during outdoor storage or prolonged hopper residence in a non-conditioned plant. Under relative humidity > 60%, pre-drying at 70 °C for 2 h to 4 h in a desiccant dryer with a dew point of ≤ -30 °C reduces the risk of surface defects in thin-gauge sheet. If an unvented single-screw extruder is used, the feed throat should remain water-cooled to prevent pellet bridging, and the screw should have an L/D ratio of 24:1 to 30:1 with a compression ratio near 3:1. A grooved-feed section is not essential for LDPE-based compounds, but barrel temperature profiles are typically set to rise from 150 °C in the feed zone to 200 °C in the metering zone. Melt temperatures above 230 °C can initiate polyethylene chain scission and may also alter the carbon black surface chemistry enough to raise resistivity after repeated extrusion. Melt temperatures below 180 °C can leave the conductive carbon black network insufficiently relaxed, producing visible agglomerates or rough sheet edges. The compound should be bracketed in 5 °C barrel-zone increments during trial runs, and the extruder should be held at steady state for 20 min before sampling for resistivity testing.

    Because surface resistivity on a filled polyolefin is sensitive to conditioning history, measurements made immediately after extrusion rarely predict the final ESD-protective performance after thermoforming. A guarded ring electrode or concentric ring probe should be used according to IEC 62631-3-2:2023 or ASTM D257, with specimens conditioned at 23 °C and 50% RH for 48 h under ISO 291 class 2 atmospheres. Readings taken after 60 s of electrification reduce the effect of capacitive charging and provide better repeatability. Carbon black-loaded conductive polyolefins typically exhibit surface resistivity from 10¹ Ω to 10⁵ Ω, while dissipative compounds occupy the higher span up to 1 × 10¹¹ Ω; the applicable pass-fail limit must be drawn from the specific ESD control plan or packaging standard, not from the material classification alone. The electrical percolation threshold in LDPE depends on carbon black structure and loading. High-structure grades with dibutyl phthalate absorption above 120 cm³/100 g tend to form conductive networks at lower loadings than low-structure grades, but they also raise viscosity more sharply. In thermoformed parts, draw ratios exceeding 3:1 can generate localized surface-resistivity drift because the carbon black interparticle gaps increase under large plastic deformation. For this reason, the final electrical test should be performed on the formed article, not only on the incoming sheet.

    What Separates CA4918 from a Carbon Black Masterbatch Dilution at the Converting Line?

    In a masterbatch-based conductive LDPE system, the processor receives a carbon black concentrate and natural LDPE; the final network is only formed after the letdown mixture is melt-blended. That configuration requires precise gravimetric feeder calibration, often to ±0.5% of setpoint, and the final resistivity is directly sensitive to screw geometry, throughput, and residence-time distribution. A ready-to-use compound such as CA4918 moves the carbon black dispersion step to the supplier, where high-intensity mixing equipment can produce a more reproducible network than a simple single-screw dilution. The operational difference appears most clearly when production schedules shift between screw geometries or when a feeder is serviced. A masterbatch dilution may require full revalidation of resistivity after a screw change, while a supplied compound primarily requires revalidation of melt temperature and residence time. However, this does not imply that CA4918 is insensitive to processing. If run through a hot-runner injection mold or an extruder with excessive shear, the conductive network can be mechanically degraded just as it would in a masterbatch. The practical advantage is the elimination of letdown weighing errors and the associated lot-to-lot compositional drift. When compared with general-purpose carbon black-loaded LDPE compounds, CA4918 is expected to show a tighter surface-resistivity distribution across a multi-station thermoforming line, although published grade-specific statistical capability data is limited. The LDPE base also gives lower heat-seal initiation than conductive polypropylene; LDPE seal initiation typically occurs near 95 °C to 110 °C. For applications requiring continuous service above 80 °C under mechanical load, the LDPE matrix is generally unsuitable because of creep, and a conductive polypropylene or engineering thermoplastic should be selected instead.

    Incoming Inspection, Conditioning Methods, and the Test-Method Matrix for ESD Packaging Compliance

    RequirementStandard / MethodOperational Relevance
    Melt mass-flow rateISO 1133-1:2022Confirms extrusion consistency after storage
    DensityISO 1183-1:2019Supports feed rate and yield calculations
    Surface resistivityIEC 62631-3-2:2023Primary ESD-protective function
    Tensile elongation at breakISO 527-2:2012Thermoforming integrity after draw
    Conditioning atmosphereISO 291 class 2Establishes repeatable test baseline

    Rheologically, a conductive LDPE compound is non-Newtonian. At shear rates near 100 s⁻¹ the carbon black network reduces apparent viscosity, but at low shear the compound may show yield-like behavior and higher viscosity than unfilled LDPE. Consequently, the extruder should not be started from a cold state at high screw speed; a staged screw ramp allows the conductive network to soften without excessive melt-pressure overshoot. For LDPE-based conductive compounds, melt temperatures in the 190 °C to 210 °C range are common on production-scale single-screw lines. Oscillatory rheometry at 10 rad/s can distinguish network quality by tracking storage modulus; a sharp drop in storage modulus between 0.1 s⁻¹ and 100 s⁻¹ is characteristic of a structured carbon black network. If the storage-modulus curve resembles that of unfilled LDPE, the conductive network may have been overworked or the loading may be below the percolation threshold. This type of measurement is more informative than melt flow rate alone because melt flow rate does not detect network continuity.

    Extrusion of CA4918 into thin-gauge sheet for thermoformed ESD trays places simultaneous demands on melt strength and conductive-network retention. On a 60 mm single-screw extruder operating at 1.2 m/min line speed, melt temperatures in the 190 °C to 210 °C range are common for LDPE conductive compounds. Higher line speeds can increase melt temperature through viscous dissipation, and the operator should monitor resin pressure at the breaker plate; excursions above 300 bar may indicate excessive screen-pack blockage from carbon black agglomerates. Melt filtration with 60/80/60 mesh screen packs is acceptable if the screen area is sufficient to avoid pressure spikes. In thermoforming, sheet surface temperature should be maintained between 120 °C and 140 °C for LDPE-based materials; outside this window, webbing and wall thinning increase, and the conductive network may be further disrupted by non-uniform draw. If regrind is incorporated, the addition should be limited to 10 wt% per pass unless the surface resistivity of the formed part is revalidated, because the carbon black network is progressively fractured through each heat history. For deep-draw cavities, local thinning can reduce the probability of the conductive network remaining continuous, even though the sheet remains mechanically intact.

    Production-Scale Failure Modes Trace Back to Carbon Black Network Overwork and Thermal Nonuniformity

    On production-scale extrusion lines, three defects recur with conductive LDPE compounds: edge weld lines in sheet, pinholes in thermoformed cavities, and surface-resistivity streaks oriented in the machine direction. These defects generally indicate carbon black network overwork in the metering zone, insufficient back pressure, or uneven melt temperature across the die lip. If edge weld lines appear, the die temperature is often raised by 5 °C to 10 °C; however, this correction may lower melt viscosity and allow carbon black agglomerates to align before the sheet freezes. A more stable correction is to increase screen-pack density from 40/60/40 to 60/100/60 mesh and to verify that the die gap is uniform within ±0.02 mm. Surface-resistivity streaks in the machine direction are frequently caused by a worn screw or damaged barrel surface; a screw root-diameter variation above 0.1 mm can produce periodic temperature gradients that affect carbon black distribution. Pinholes in deep-draw thermoformed parts are frequently associated with local draw ratios above 3:1. At these ratios, the LDPE matrix may thin to the point where the carbon black network cannot maintain a continuous conductive path, even though the overall part remains mechanically intact. To separate formulation failure from process failure, processors typically cut sheet samples before and after the forming station and compare surface resistivity using a concentric ring probe after 48 h conditioning at 23 °C and 50% RH. If the resistivity shift is greater than one order of magnitude after forming, the draw ratio or sheet temperature is the more likely cause. The operational boundary is therefore not only the melt-temperature window but also the mechanical deformation profile. Published data for high-draw configurations specific to CA4918 is limited, so forming trials should map the resistivity response across the full part geometry before release to production.