| HS Code | 915750 |
| Density | 0.934 g/cm³ |
| Meltflowrate | 3.0 g/10 min |
| Bulkdensity | 0.35 g/cm³ |
| Particlesize | 35 mesh |
| Meltingpoint | 125 °C |
| Vicatsofteningpoint | 110 °C |
| Tensilestrengthatyield | 16 MPa |
| Tensilestrengthatbreak | 20 MPa |
| Elongationatbreak | 700% |
| Flexuralmodulus | 550 MPa |
| Escr | >1000 h |
| Armimpactstrengthatminus40c | 100 ft-lb |
| Shoredhardness | 55 |
| Uvstabilization | Yes |
As an accredited Braskem RA34U3 LLDPE Rotomolding Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem RA34U3 LLDPE Rotomolding Polyethylene is supplied in 25 kg polyethylene bags, palletized, stretch-wrapped, and labeled for secure industrial shipping. |
| Container Loading (20′ FCL) | 20′ FCL loaded with Braskem RA34U3 LLDPE rotomolding polyethylene, typically 25 kg bags on pallets, shrink-wrapped and secured for transport. |
| Shipping | Braskem RA34U3 LLDPE rotomolding polyethylene is typically shipped as non-hazardous resin pellets in moisture-barrier 25 kg bags, 500–1,000 kg bulk bags, or bulk trucks/railcars. Store in cool, dry conditions away from direct sunlight, heat, and moisture. Handle with standard material-handling equipment; no special hazard placards required. |
| Storage | Store Braskem RA34U3 LLDPE Rotomolding Polyethylene in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizers. Keep original containers or bags closed to prevent moisture, dust, and contamination. Stack pallets securely without exceeding recommended heights. Avoid prolonged UV exposure and extreme temperatures. Maintain good housekeeping; no smoking. Use first-in, first-out inventory. Store at ambient temperature. |
| Shelf Life | Typically 24 months in original, unopened packaging; store cool, dry, well-ventilated, below 50°C, away from direct sunlight and heat sources. |
Braskem RA34U3 is a linear low-density polyethylene rotomolding powder with a nominal density of 0.934 g/cm³ under ASTM D1505 and a melt flow rate of 3.0 g/10 min at 190°C under 2.16 kg load per ASTM D1238. Typical published mechanical values include tensile yield strength of 18 MPa, elongation at break above 800% under ASTM D638, and flexural modulus of approximately 550 MPa under ASTM D790. The grade is supplied in powder form; typical rotomolding powder specifications call for a 35-mesh nominal sieve size, and incoming bulk density and dry flow should be recorded because grind lot variation shifts charging behavior in carousel, shuttle, and rock-and-roll machines. Incoming powder exposed to storage above 60% RH is pre-dried at 60–70°C for 2–4 h to remove surface condensation. Absorbed water is negligible, but condensation on cold powder entering a heated tool causes steam porosity and localized pinhole defects. The grade processes within a fusion window defined by oven air temperature and peak internal air temperature; unlike injection molding, melt flow rate is not a direct predictor of rotomolding consolidation. Rotational speed ratio, cooling rate, and part wall section control the final crystallinity and residual stress state. These variables are not linear, and the optimum cycle on a large flat tank differs sharply from that on a small symmetrical float.
Rotomolded agricultural sprayer and fertigation vessels fabricated from RA34U3 require a narrow processing envelope because tank skins are typically 4–8 mm thick and must survive both hydrostatic pressure and diluted agrochemical contact. Cylindrical tanks from 800 L to 3,000 L are commonly formed on rock-and-roll machines at a major/minor axis speed ratio of 4:1; symmetrical baffled tanks may require a 3:1 ratio to avoid powder bridging at internal ribs. Oven air is held at 270–290°C, with peak internal air temperature controlled to 195–205°C. A PIAT below 190°C leaves partially sintered powder at the inner wall and lowers ASTM D638 tensile yield. A PIAT above 215°C accelerates oxidative chain scission and reduces environmental stress crack resistance. Batch-to-batch variation in melt flow rate of even ±0.2 g/10 min shifts optimum dwell by 2–4 min on production carousels; operators therefore log PIAT curves rather than fixed dwell times. Formulation for external UV service uses 2–3 wt% carbon black or UV masterbatch letdown in 100 parts RA34U3; pigment loading above 4 wt% generates local fusion viscosity mismatches and can open pinholes around spin-weld ports. Molding-in of threaded fittings and baffle anchors requires preheated inserts to create a melt pool around the boss; cold inserts produce stress concentration and microvoids that later initiate cracks. Hydrostatic testing is commonly conducted at 1.5 times service pressure with venting checks per ASTM D1998. Agrochemical compatibility is confirmed by immersion per ISO 175 for 7–30 days at 23°C and 40°C, with mass change and tensile retention recorded against the untreated control. ESCR testing under ASTM D1693 Condition A, 50°C, 10 wt% Igepal CO-630, gives a comparative indication of stress crack resistance after molding. Terminal products include tractor-mounted spray tanks, fertigation dosing reservoirs, and transport pods for drip-irrigation chemicals.
| Standard | Method or condition | Application in rotomolded agricultural vessels |
|---|---|---|
| ASTM D638 | Tensile testing, 50 mm/min, 23°C | Tensile yield strength and elongation at break |
| ASTM D1693 | Condition A, 50°C, 10 wt% Igepal CO-630 | Environmental stress crack resistance of molded sidewall |
| ASTM D1998 | Upright polyethylene tank specification | Workmanship, wall thickness, fittings, pressure rating |
| ISO 175 | Immersion in agrochemical fluid, 7–30 days | Chemical compatibility and tensile property retention |
| ISO 4892-2 | Xenon arc exposure, method A | UV resistance for outdoor exposure |
When the target wall section exceeds 6 mm, as in large irrigation and fire reserve tanks, the principal conflict is between complete inner-wall sintering and outer-wall oxidative degradation. Oven air temperatures above 280°C accelerate outer skin degradation before the inner surface reaches 200°C; lower oven settings of 260–275°C combined with longer dwell reduce this gradient but increase cycle time. Peak internal air temperature is held at 200–210°C for wall sections of 6–12 mm. After the sintering plateau, cooling must remove heat through the tool surface without creating abrupt thermal contraction at the parting line. Forced air is applied until the part surface falls below 80°C; water mist is introduced only after this point to avoid internal stress whitening and flange distortion. Large flat panels and baffled tank ends are particularly sensitive to non-uniform cooling; production-scale carousel machines with asymmetric tooling often show wall thickness variation of ±15% unless tool rotation is slowed or internal air circulation is improved. Formulation is 100 parts RA34U3 for buried or indoor tanks; exterior above-ground tanks use 2 wt% UV masterbatch. Potable water service is not automatically granted for any rotomolding resin; the finished tank must be tested for migration under applicable national or local drinking-water standards, and the fabrication plant must verify whether the specific lot carries the necessary third-party certification. Structural design of upright tanks references ASTM D1998 for workmanship, wall thickness, fittings, and pressure rating; above-ground chemical storage may also fall under EN 13575:2012. Terminal components include rainwater harvesting cisterns, fire reserve reservoirs, and irrigation buffer tanks where chemical contact is incidental.
Chemical containment shells, secondary bund liners, and acid dosing skid modules manufactured from RA34U3 are usually validated through a combination of immersion testing and mechanical retention testing because the polymer is compatible with many aqueous salt solutions, weak acids, and alkalis but is not suitable for concentrated oxidizing acids, aromatic hydrocarbons, or halogenated solvents. Continuous service above 40°C with aggressive media accelerates environmental stress cracking at molded-in inserts and weld seams. Parts are typically rotationally molded on shuttle or carousel machines at 5–8 mm wall thickness, with a speed ratio of 4:1 for rectangular bunds and 8:1 for sump bodies. Peak internal air temperature is maintained at 195–210°C; because chemical containment parts often include metal inserts for pump mounts and level sensors, the insert must be preheated to within 40°C of the mold cavity surface before charging. Cold inserts create a quench zone that remains underfused and initiates stress cracks under thermal cycling. Formulation uses 100 parts RA34U3 with 2.0–2.5 wt% carbon black masterbatch for outdoor bunds; recycled or reprocessed powder from unknown molding history is not added without revalidation of ASTM D1693 ESCR and ASTM D638 elongation on molded plaques. Chemical compatibility is screened by ISO 175 immersion for at least 30 days at the maximum service temperature; acceptance criteria commonly include mass change below 1%, no visible blistering, and tensile elongation retention above 70%. Where published data for a specific chemical mixture is limited, a full-scale lined or unlined service trial with periodic thickness and hardness logging is used. Terminal parts include double-wall acid dosing cabinets, secondary bund liners for battery electrolyte storage, and sump reservoirs for water treatment skids.
In marine buoyancy and flotation chamber production, the cooling segment of the cycle, not the oven dwell, frequently controls impact performance. Sealed air chambers or foam-filled shells are rotationally molded in two-piece aluminum tools at wall thicknesses of 4–6 mm, with major/minor axis ratios from 8:1 to 10:1 for spherical or oval float geometries. Oven air at 270–290°C and PIAT of 195–205°C are standard, but the cooling ramp after demolding determines low-temperature impact behavior. Slow air cooling to 70°C before tool separation reduces residual stress and improves drop-impact resistance at −20°C; rapid water quench can increase impact strength in some sections but creates differential shrinkage at parting lines and threaded port areas. Rotational speeds below 8:1 on asymmetric floats cause powder accumulation at the deepest cavity, visible as thick equatorial bands and thin polar walls; instruments tracking internal air temperature alone will not detect this distribution error. Finished floats are pressure-tested at 0.2–0.3 bar compressed air and subjected to instrumented impact per ISO 6603-2 or puncture testing per local buoyancy standard. The RA34U3 formulation is normally 100 parts natural, with UV-stabilized compounds only if the float shell remains exposed above water; foam filling with closed-cell polyurethane is done after molding and does not require solvent bonding. Terminal products include navigation buoy hulls, dock flotation units, aquaculture cage collars, and removable marine survey floats.
Underground septic chambers and access risers molded from RA34U3 demand a different validation sequence because the part carries soil load and occasional vehicle load far below the resin’s normal room-temperature stress envelope. Wall thickness is typically 6–10 mm, with ribbed sidewalls and corrugated profiles molded into the tool to increase section modulus without raising resin mass. The molding process uses oven air at 280–300°C and a PIAT of 200–210°C; the higher oven setpoint compensates for heat absorbed by large mold mass and structural ribs. Finished parts are evaluated for brittleness temperature per ASTM D746, where typical values below −75°C indicate sufficient low-temperature toughness for cold-climate installation, and for impact strength after molding per ASTM D2444 or ISO 179-1. Thick ribbed walls must be cooled slowly to 60–80°C before demolding; ejection at higher temperature causes warped riser threads and stress whitening at corrugation roots. Installed load-bearing capacity is not derived from resin tensile strength alone; structural design is governed by soil modulus, burial depth, and the specified wheel load, commonly AASHTO H-25 or equivalent, with finite element verification of ribbed shell deflections. Threaded access riser sections are often molded with sacrificial aluminum thread inserts that are removed after cooling; reused inserts must be coated with release agent and preheated, or thread surface tearing increases scrap. The formulation is 100 parts RA34U3; UV masterbatch is added only in above-ground vent and lid components because buried shells are not exposed. Terminal products include septic tank bodies, pump chamber risers, leach field inspection ports, and underground cistern extensions.
Outdoor furniture shells and playground panels are rotationally molded from the same grade in 1.5–3.0 mm wall stock; the key requirement is UV retention under ISO 4892-2, and no additional reinforcement or formulation change is required beyond 2 wt% UV masterbatch.
Competitive Braskem RA34U3 LLDPE Rotomolding Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem RA34U3 LLDPE Rotomolding Polyethylene is a linear low density polyethylene powder supplied for biaxial rotational molding of hollow parts such as agricultural chemical tanks, recreational components, outdoor water tanks, and industrial containers. The grade is specified by a density of 0.934 g/cm³ measured in accordance with ASTM D792 and a melt flow rate of 3.4 g/10 min measured at 190°C/2.16 kg in accordance with ASTM D1238. These values place the material in the medium-density segment of the rotomolding polyethylene family, between lower-density flexible grades and high-density stiff grades. The resin is typically supplied as a ground powder with a controlled particle size distribution and dry-flow character; the current supplier certificate of analysis is the binding source for sieve retention, bulk density, and moisture content.
Laboratory property values alone do not guarantee end-use performance. Rotational molding introduces residual stress, corner thinning, and cooling-rate gradients that cannot be reproduced on compression-moulded test plaques. A production-scale tool must therefore be used to qualify the interaction between RA34U3 and the intended mould geometry before serial production begins.
High-density rotomolding grades commonly occupy a density range of 0.945 g/cm³ to 0.950 g/cm³ and offer higher flexural modulus but lower environmental stress-crack resistance at equivalent wall thickness. RA34U3, at 0.934 g/cm³, shifts the property balance toward longer survival under wetting-agent contact and improved low-temperature ductility, while reducing room-temperature stiffness. The lower density corresponds to lower crystallinity and generally increases the population of tie molecules that bridge crystalline lamellae, retarding slow crack growth under continuous stress. In practice, this makes the grade appropriate for tanks that must withstand repeated chemical contact, flexural loading from sloshing liquid, and outdoor temperature cycling.
| Property | Test method | Published value |
|---|---|---|
| Density | ASTM D792 | 0.934 g/cm³ |
| Melt flow rate | ASTM D1238, 190°C/2.16 kg | 3.4 g/10 min |
| Environmental stress-crack resistance | ASTM D1693, 100% Igepal, F50 | > 1000 h |
For tank designers, the selection logic is not based on a single property but on the dominant failure mode. If the part is likely to fail by stress cracking at a corner radius or insert, RA34U3 is preferred over many higher-density grades. If the part is panel-like and deflection-controlled, the lower modulus of RA34U3 may require a thicker wall than an HDPE alternative. Deflection calculations should use flexural modulus data generated in accordance with ASTM D790 and finite element analysis of the actual part geometry.
In a rotationally moulded chemical tank, stress-crack resistance frequently determines service life more than short-term burst strength. The molded tank is typically evaluated with the actual stored chemical because ESCR values obtained in standard Igepal solutions do not reproduce every detergent, surfactant, or agrochemical formulation. Cracks often initiate at microvoids near the inner surface, at sharp corner radii, or around metallic inserts. The use of generous radii, controlled cooling, and post-mould annealing can reduce residual stress concentrations and improve the observed ESCR of the finished part.
The polymer is classified as linear low density polyethylene because the short-chain branches introduced by an alpha-olefin comonomer interrupt the crystallizable ethylene sequences without eliminating them. In rotomolding, this molecular architecture yields a melt that coalesces into a bubble-free wall at peak internal air temperatures of 190°C to 210°C, while retaining sufficient zero-shear viscosity to prevent excessive sag on thick sections. The powder is produced by grinding the pelletized resin to a controlled particle size distribution; typical rotomolding powders are specified with a top size below 35 mesh (500 µm). Bulk density and dry-flow values vary with grinding equipment and ambient humidity and must be taken from the certificate of analysis.
Particle size distribution influences pinhole formation, inside-wall surface finish, and powder flow into deep ribs. A broader distribution can improve pack density in complex tooling but may segregate when the mould is rotated at low speed. RA34U3 should not be transferred directly from bulk railcar to mould without screening because handling can alter the particle size distribution supplied by the producer. Central hoppers, sifters, and dry-air conveying are used to preserve flowability in large rotomolding plants.
Rotomolded parts used in cold districts, agricultural sprayer reservoirs, and recreational cargo boxes are often specified by instrumented puncture tests at -20°C or -40°C. The lower density and higher comonomer content of RA34U3 generally provide greater ductility at sub-zero temperatures than high-density homopolymer grades, but the mould cooling history is decisive. Slow cooling from the melt increases lamellar thickness and reduces low-temperature impact; an unfavourable tool can therefore erase part of the resin’s inherent ductility.
Impact evaluations are conducted with ISO 6603-2 or ASTM D3763 instrumented puncture methods on specimens cut from production mouldings. The test reports total energy, peak force, and failure mode. A ductile failure under low-temperature impact is often a prerequisite for outdoor service. When published data for a specific configuration is limited, the moldmaker should produce a prototype tool insert and run process mapping before committing to full-scale cavity sets.
Processing of RA34U3 in shuttle, carousel, or rock-and-roll machines follows the conventional four-stage cycle: charging, heating, cooling, and unloading. Oven air temperature is typically set between 260°C and 320°C. The peak internal air temperature is the controlling process variable for this grade; a range of 190°C to 210°C is used for wall thicknesses up to 6 mm, but thicker sections may require slower heat-up to avoid surface oxidation. Mold rotation ratios are commonly 4:1 for simple tanks, with primary-axis speed between 2 rpm and 5 rpm depending on mould diameter.
Cooling rate controls shrinkage and low-temperature impact. Forced-air cooling is used for general purpose parts; water mist cooling shortens cycle time but increases the risk of warpage at abrupt wall-thickness transitions. Warpage is corrected by reducing cooling rate, adjusting rotation ratio, or moving the parting line, not by increasing oven temperature alone. If the powder is stored in a cold warehouse and introduced into a warm mould area, condensation can create surface porosity; pre-drying at 60°C for 2 h is a standard corrective action when the bulk powder temperature is below shop-floor dew point.
On shuttle machines using cast aluminium moulds of 6 mm to 10 mm thickness, the internal air temperature typically lags the oven air temperature during the first half of the heating cycle. Operators use the time required to reach a stable peak internal air temperature as an indicator of heat transfer into the mould. Fabricated steel moulds have higher thermal mass and may require longer oven residence than aluminium tools of the same wall thickness. These cycle-time differences must be determined by thermocouple mapping of the actual mould because tool mass, parting-line area, and corner radii all affect heat transfer.
Compared to conventional high-density rotomolding grades with density 0.945 g/cm³ to 0.950 g/cm³, RA34U3 requires careful attention to wall-thickness design because its lower flexural modulus increases deflection under identical hydrostatic load. The compensating advantage is a longer time to stress-crack failure under contact with surfactants and agricultural chemicals. In processing terms, the 3.4 g/10 min melt flow rate is positioned for medium-thick walls; grades below 1 g/10 min require longer oven dwell and may provide better long-term creep, while grades above 6 g/10 min fill thin ribs more easily but may show lower ESCR. These differences are not linear and must be mapped for each mould geometry.
Regrind incorporation is permitted only after evaluation of particle size, melt flow rate, and oxidation stability. The use of high levels of regrind can shift the melt flow rate and lower ESCR. Polypropylene contamination must be excluded because incompatible dispersed domains can delaminate within the moulded wall. Oxidative stability is monitored by oxidation induction time in accordance with ASTM D3895 when regrind levels are increased or when long oven cycles are used.
Regulatory conformity for RA34U3 must be verified against the application. Polyethylene homopolymers and copolymers intended for food contact may be evaluated under FDA 21 CFR 177.1520; however, the supplier’s food-contact certification is batch-specific and should be requested for the exact grade and lot. REACH registration for the polymer applies in the European Union. RoHS does not apply to the base polyolefin resin unless functional fillers or additives containing restricted heavy metals are incorporated. The resin should be stored away from strong oxidizing agents, chlorinated solvents, and aromatic hydrocarbons, particularly at elevated temperatures.
UL 94 flammability testing of polyolefin materials commonly gives a classification of HB at specified thicknesses, but certification requires testing of the final moulded part at production wall thickness because flame spread depends on part shape and thickness. No statement in this technical note substitutes for part-specific regulatory testing.
| Standard | Property or scope |
|---|---|
| ASTM D1238 | Melt flow rate at 190°C/2.16 kg |
| ASTM D792 | Density by displacement |
| ASTM D1693 | Environmental stress-crack resistance |
| ASTM D638 | Tensile properties of plastics |
| ASTM D790 | Flexural properties |
| ISO 6603-2 / ASTM D3763 | Instrumented puncture impact |
| FDA 21 CFR 177.1520 | Olefin polymer food-contact compliance |
For thin-walled parts with complex parting lines, the processing window at peak internal air temperature is narrow. Under-fusion at the parting line produces pinholes and weak knit lines; over-heating oxidizes the inner air-exposed surface and can shift color in natural or light-tinted parts. A change of even a few degrees in peak internal air temperature can alter the failure mode of a cold-impact specimen from ductile to brittle when the tool has high heat-transfer contrast between massy corners and thin panels. Process engineers therefore control the oven setpoint, the residence time, and the demolding temperature as a single interacting set of variables, not as independent settings.
The use of internal air temperature probes is recommended for production-scale validation. The probe is mounted inside the mould and attached to a rotary transmitter. The recorded heating curve identifies the time at which the melt reaches a stable temperature plateau, which is the earliest point at which full fusion can be considered complete. For RA34U3, plateau stability is often achieved between 190°C and 210°C; continued heating beyond the plateau improves bubble release only marginally while increasing oxidative degradation. Cooling is then initiated when the wall is fully fused and the desired surface finish has developed.
Typical failure modes observed on production rotomolding lines include pinhole clusters at vent locations, particulate contamination from unclean filling areas, and linear cracking at the weld line between successive powder layers. RA34U3 does not differ from other polyolefin powders in requiring clean-room discipline for high-quality tanks. Static charges on dry powder can attract dust and lint; ionizing air or grounded conveying lines are used to reduce contamination in critical applications. The chemical resistance of the base polymer does not compensate for defects created by contaminated powder or dirty mould surfaces.