| HS Code | 106017 |
| Density | 0.931 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 3.3 g/10 min |
| Melting Point | 124 °C |
| Vicat Softening Point | 104 °C |
| Tensile Strength At Yield | 11 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 700 % |
| Flexural Modulus | 300 MPa |
| Hardness Shore D | 55 |
| Thermal Conductivity | 0.33 W/m·K |
| Specific Heat Capacity | 2.3 kJ/kg·K |
| Water Absorption | <0.01 % |
| Dielectric Constant 1 Mhz | 2.3 |
| Volume Resistivity | >1e16 ohm·cm |
As an accredited Braskem PROXESS 3310 Linear low density polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem PROXESS 3310 LLDPE supplied in 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped; 55 bags (1,375 kg) per pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loading for Braskem PROXESS 3310 LLDPE: 25 kg bags, palletized, shrink-wrapped, and secured for ocean transport. |
| Shipping | Braskem PROXESS 3310 Linear Low Density Polyethylene is a non-hazardous solid resin. It is not regulated for transport by DOT, IMDG, IATA, or ADR. Ship in sealed bags, boxes, or bulk containers. Protect from moisture, contamination, and excessive heat. No UN number, hazard class, or packing group required. |
| Storage | Store Braskem PROXESS 3310 LLDPE in a cool, dry, well-ventilated, covered warehouse, away from direct sunlight, heat, sparks, and flames. Keep original bags or containers closed, palletized, and off the floor. Store at ambient temperature. Prevent moisture, dust, oils, and other contamination. Practice first-in, first-out stock rotation; avoid excessive stacking and follow the supplier’s safety data sheet. Do not smoke. |
| Shelf Life | Braskem PROXESS 3310 LLDPE shelf life: 24 months from manufacture when stored in original unopened packaging, cool, dry, ventilated conditions. |
Within potable water contact rotational moulding, Braskem PROXESS 3310 is dry-blended at 98.5–99.4 wt% resin with 0.1–0.3 wt% hindered phenolic antioxidant, 0.2–0.6 wt% high-molecular-weight HALS, 0.05–0.15 wt% calcium stearate acid scavenger, and 0.3–1.0 wt% food-contact-compliant pigment masterbatch; total additive loading is kept below 1.5 phr because higher concentrations depress long-term hydrostatic creep resistance in vertical tank walls. Incoming powder is checked according to ISO 1133-1:2022 at 190°C/2.16 kg; lot-to-lot shifts outside the certificate of analysis are compensated by oven residence time adjustment of 2–4 min, not by raising oven temperature. The powder is ground to a 35-mesh (500 µm) cut with 90–95 wt% passing 60-mesh and fines below 10 wt% at 200-mesh; powder temperature during attrition pulverizing is held below 45°C, since fines soften and fuse onto rotor tips when the mill gap falls below 0.2 mm, causing batch-to-batch particle-size drift. The governing compliance framework includes NSF/ANSI/CAN 61, AS/NZS 4020:2018, FDA 21 CFR 177.1520, and Regulation (EU) 10/2011; finished plaques are tested on a surface-to-volume ratio representing the tank's maximum rated fill volume rather than on a lower-exposure flat coupon. The moulding cycle uses biaxial primary rotation of 6–10 min⁻¹, secondary rotation of 1.5–2.5 min⁻¹, oven air temperature of 280–310°C, and cook termination when internal air temperature reaches 190–205°C. The cook termination band is held at ±5°C; internal air above 210°C initiates oxidation embrittlement, while internal air below 185°C leaves unmelted powder at the parting line. Forced-air cooling for 8–12 min followed by water-mist cooling for 3–6 min is standard; the part is not exposed to water mist above 120°C surface temperature because rapid quench sets up differential crystallization and causes stress whitening at seams. End products are 500–25,000 L vertical water storage tanks, truck-mounted potable water tanks, and rainwater cisterns with nominal wall thickness from 4 mm to 12 mm.
Formulation for agrochemical containment under Braskem PROXESS 3310 uses 97.0–98.5 wt% resin, 1.5–2.5 wt% UV-stabilized carbon black masterbatch, 0.15–0.35 wt% processing antioxidant, 0.05–0.15 wt% acid scavenger, and, if the stored fluid contains more than 5 vol% ester or aromatic solvent, 1.0–2.0 wt% fluoropolymer processing aid to reduce microvoid coalescence at internal corners; published data for this specific configuration is limited. The powder cut is shifted coarser to a 30-mesh average (600 µm) with fines constrained below 8 wt% at 200-mesh to maintain fill-line flow when the mould arm length exceeds 4 m. Applicable standards are ASTM D1998-21 for polyethylene upright storage tanks, ISO 179-1:2010 notched Charpy impact at 23°C and -20°C, ASTM D1693-15 environmental stress crack resistance Condition B in 10% Igepal CO-630, and UN 1H1 certification where the tank is used for legally classified dangerous goods. Moulders run a reduced oven temperature of 270–290°C and terminate cook at an internal air temperature of 180–195°C; if peak internal air is allowed to exceed 210°C, oxidation embrittlement at the inner wall reduces ESCR below the acceptance threshold specified in ASTM D1998-21. Cooling is sequenced as 10–14 min forced air, 2–4 min intermittent water mister, and 20–30 min ambient stabilization before demoulding. End products include horizontal agrochemical transport tanks, crop-sprayer tanks, and fertilizer storage vessels with wall thickness from 5 mm to 15 mm and hydrothermal endurance tested at 60°C for 500 h.
For marine flotation components, Braskem PROXESS 3310 is compounded with 2.0–3.0 wt% carbon black masterbatch, 0.3–0.6 wt% HALS, 0.1–0.3 wt% primary antioxidant, and, for foam-filled parts, 0.5–1.0 wt% azodicarbonamide chemical blowing agent whose decomposition onset around 190–205°C overlaps the resin melt range; the mould cavity is therefore charged to 50–70% of its volume to allow foam core expansion at the centre while the outer wall remains solid. The marine segment requires ISO 4892-3:2016 accelerated weathering under UV-A 340 lamps for 2000–3000 h, ISO 179-1:2010 notched impact at -30°C, and REACH Annex XVII restrictions on polycyclic aromatic hydrocarbons in the carbon black masterbatch. The rotomoulding cycle uses primary rotation at 8–12 min⁻¹, secondary rotation at 2–3 min⁻¹, oven air temperature 290–320°C, and a short internal air plateau of 175–190°C; internal air excursions above 200°C lead to over-expansion of the blowing agent, producing parting-line blowholes and skin delamination. Cooling starts with 8–10 min forced air and proceeds to water mist at 15–20°C until the part surface falls below 70°C; demoulding above 80°C causes permanent compression set at foam ribs, while cooling below 45°C before release can leave external sink marks. End products are encapsulated dock floats, navigation buoys, and modular pontoon floats with outer wall thickness between 4 mm and 8 mm and foam core density of 150–300 kg/m³.
Braskem PROXESS 3310 enters the playground and recreational component segment as a dry-blend of 98.5–99.5 wt% base resin, 0.3–0.8 wt% non-phthalate organic pigment masterbatch, 0.2–0.5 wt% HALS, and 0.05–0.15 wt% internal mold release; the pigment masterbatch is selected to meet EN 71-3:2019+A1:2021 migration limits for nineteen elements and ASTM F963-23 soluble heavy metal requirements, with the release formulation tested on the actual moulded surface texture rather than on a polished plaque. The powder particle-size distribution is held at 35-mesh (500 µm) with no more than 12 wt% retained on 60-mesh to reproduce fine-grained texture on cast aluminum moulds of 8–12 mm wall thickness. Moulders set oven temperature at 275–300°C, primary rotation at 6–9 min⁻¹, and secondary rotation at 1.5–2.5 min⁻¹; cook termination occurs at internal air temperature 185–200°C, because higher internal air produces low-molecular-weight surface material that creates gloss variation on slide walls and ladder rungs. Post-mould cooling is forced air for 10–15 min with mould ends blocked to prevent warpage in tubes and slide enclosures; water-spray cooling is limited to short intermittent bursts to avoid sink marks at boss attachments and handrail sockets. End products are rotomoulded slides, climbing tunnels, pedal cars, and self-supporting play panels with wall thickness from 4 mm to 10 mm.
In industrial bulk handling, Braskem PROXESS 3310 is formulated with a minimum 98.0 wt% resin, 1.0–2.0 wt% mineral-filled or carbon black masterbatch for flexural stiffness, 0.1–0.3 wt% primary antioxidant, and 0.05–0.15 wt% calcium stearate acid scavenger; the mineral filler addition is restricted to 2.0 wt% because higher loadings lower ESCR below the threshold required for pallet boxes operated in cold rooms at -20°C. The compliance framework for this segment rests on ISO 179-1:2010 notched impact at -20°C, ASTM D1693-15 ESCR Condition C in 100% Igepal CO-630, and FDA 21 CFR 177.1520 where reusable totes contact dry foodstuffs. Processing uses a cast aluminum mould of 10–14 mm wall thickness, a biaxial ratio of 3.5:1.0, oven temperature 280–310°C, and a cook time of 28–38 min for a 1000 L container and 18–24 min for a 300 L box; shorter cycles produce undercooked inner-wall pinholes at rib intersections, while longer cycles increase drop-impact but degrade corner straightness due to thermal expansion differences across the mould flange. Demoulding is performed after the part surface temperature falls below 55°C; forced ejection above that temperature causes corner warpage on thin floor ribs and can set residual stresses that later crack under stacking load. End products are 300–1500 L bulk bins, pallet boxes, insulated fish tubs, and modular hoppers with wall thickness from 5 mm to 14 mm.
Braskem PROXESS 3310 is used for non-fuel automotive fluid reservoirs when the formulation includes 97.5–98.9 wt% resin, 0.5–1.5 wt% HALS/UV masterbatch, 0.2–0.5 wt% antioxidant, and 0.2–0.5 wt% processing stabilizer; for windshield washer and urea tanks, the inner wall is subjected to hydrolysis resistance screening at 60°C for 1000 h in 50% glycol solution, and published data for this specific configuration is limited. Compliance is anchored to ISO 179-1:2010 Charpy notched impact at -30°C, ISO 75-2:2013 heat deflection temperature at 0.45 MPa, and OEM-specific low-temperature drop tests using a 2.0 kg steel dart at -20°C. The rotomoulding cycle uses oven temperature 280–300°C, primary rotation 7–10 min⁻¹, secondary rotation 2–3 min⁻¹, and cook to internal air temperature 190–205°C; the critical processing boundary is demoulding temperature, kept below 55°C to prevent thread-insert distortion and flange warpage. Release agents are avoided on the thread inserts because residual silicon migration can reduce insert torque retention; the insert is preheated to 60–80°C before mould charging to promote resin encapsulation. End products include windshield washer reservoirs, hydraulic oil expansion tanks, and urea solution reservoirs with wall thickness from 3.5 mm to 7.0 mm.
Competitive Braskem PROXESS 3310 Linear low density polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem PROXESS 3310 is a linear low density polyethylene (LLDPE) grade supplied as a pelletized, additive-stabilized copolymer for film extrusion and lamination. The product designation places it within the LLDPE class defined by ISO 1183-1:2019 density measurement and ISO 1133-1:2022 melt flow rate testing. The typical density window for this class is 0.916 g/cm³ to 0.922 g/cm³, and the melt mass-flow rate at 190°C under 2.16 kg load is generally in the range 0.80 g/10 min to 1.20 g/10 min. Grade-specific certified values for PROXESS 3310 should be obtained from the Braskem certificate of analysis, because published data for this exact configuration are limited. The resin is intended for blown film and cast film operations where downgauging capacity, seal initiation, and puncture resistance control package performance. Typical application areas include heavy-duty sacks, frozen food packaging, agricultural stretch film, collation shrink film, and lamination sealant webs. The molecular architecture is a linear polyethylene backbone with short-chain branching introduced by alpha-olefin comonomer; this structure differentiates the grade from autoclave low-density polyethylene, which contains long-chain branching and a broader molecular weight distribution.
Processors of this resin class typically use single-screw extruders equipped with barrier screws, grooved feed bushings, and L/D ratios of 24:1 to 30:1. In blown film towers, die gaps of 1.2 mm to 2.0 mm and blow-up ratios of 2.0:1 to 3.0:1 are employed. The feed throat should be maintained below 60°C to prevent premature melting and bridging. These processing conditions are class-level recommendations and must be adjusted for line geometry and output rate.
Melt flow rate alone does not define processability. The resin’s shear-thinning response, characterized by melt index ratio (MIR) or by capillary rheometry according to ISO 11443:2021, influences extruder backpressure, melt temperature, and bubble stability. For LLDPE film resins in the 0.916 g/cm³ to 0.922 g/cm³ density interval, the zero-shear viscosity at 190°C is typically one to two orders of magnitude higher than that of an LDPE with the same melt index. This difference arises from the absence of long-chain branching and the narrower molecular weight distribution of linear chains. The consequence is a steeper power-law shear-thinning region in the extruder, which can reduce the energy required in the metering zone but raises die pressure relative to LDPE.
On a high-output monolayer line with a 200 mm die head and a 30:1 L/D barrier screw, downgauging from 50 µm to 30 µm requires a reduction in melt temperature and an increase in frost line height to preserve bubble geometry. If the melt temperature exceeds 240°C, gel formation and oxidation become limiting. If the temperature falls below 190°C, surface melt fracture can appear as shark-skin when shear stress at the die lip exceeds the critical threshold of approximately 0.14 MPa to 0.20 MPa. These are operational boundaries for the resin class. The use of fluoropolymer processing aids shifts the melt fracture onset toward higher shear rates, but the concentration must be controlled as described below.
The downgauging limit is also controlled by the film’s dart impact and tear propagation resistance. When thickness is reduced from 50 µm to 30 µm, the dart impact value under ASTM D1709-16a does not scale linearly; it typically decreases faster than the thickness ratio because of reduced plastic deformation volume. A 50 µm film with a dart impact of 160 g may exhibit only 80 g to 90 g at 30 µm. This non-linear reduction must be incorporated into packaging specifications and is a common cause of field failures when converters downgauge without revalidating filled package drop performance.
| Property | Test method | Unit | Typical range |
|---|---|---|---|
| Density | ISO 1183-1:2019 | g/cm³ | 0.916–0.922 |
| Melt mass-flow rate | ISO 1133-1:2022, 190°C, 2.16 kg | g/10 min | 0.80–1.20 |
| Vicat softening temperature | ISO 306:2022, A50 | °C | 96–106 |
| Melting temperature | ISO 11357-3:2018 | °C | 121–125 |
| Tensile modulus | ISO 527-2:2012 | MPa | 180–260 |
| Tensile strength at yield | ISO 527-2:2012 | MPa | 10–14 |
| Elongation at break | ISO 527-2:2012 | % | 500–800 |
| Dart impact, 25 µm film | ASTM D1709-16a | g | 120–180 |
| Elmendorf tear, 50 µm film | ASTM D1922-15 | g | 200–500 |
| Haze, 50 µm film | ISO 14782:1999 | % | 8–15 |
| Gloss, 60° | ISO 2813:2014 | GU | 40–70 |
In high-speed form-fill-seal operations where seal initiation temperature below 105°C is required, the hot-tack performance of the film is measured under ASTM F1921-18 with a dwell time of 0.5 s and a seal pressure of 0.275 MPa. Heat seal strength is evaluated under ASTM F88/F88M-21 on a 25 mm wide specimen peeled at 300 mm/min. A seal strength of 4.0 N/25 mm is often used as the practical threshold for package integrity on vertical form-fill-seal machines. For LLDPE film of this density class, seal initiation temperature typically falls between 95°C and 105°C, with a sharp increase in seal strength over the following 15°C to 25°C. This non-linear response is the critical process window: an under-sealed fin seal may pass a visual inspection but fail in burst testing, while an overheated seal can create edge bead and shrink-back. On production lines with 20 kW sealing jaws and 45 µm film running at 80 pack/min, jaw temperature drift of ±3°C can move the seal strength by more than 2 N/25 mm. Operators should therefore calibrate jaw thermocouples under ISO 9001 process control procedures and monitor hot-tack as a release criterion rather than a routine off-line check only.
The same resin class is used for frozen food films. Published data for this specific PROXESS 3310 configuration in frozen food packaging is limited, but LLDPE film grades with the same density and melt flow rate have been used in multi-layer laminates with a sealant layer thickness of 20 µm to 35 µm. In such structures, the LLDPE layer provides low-temperature flexibility; dart impact at -20°C is measured by ASTM D1709-16a after conditioning for 4 h. The absence of long-chain branching reduces heat-seal contamination with LDPE and allows downgauging from 60 µm to 45 µm in heavy-duty sacks while maintaining puncture resistance measured under ISO 7765-2:2018. On a horizontal form-fill-seal machine with a 150°C seal bar setpoint and 40 kN jaw force, the transition from a 60 µm LDPE/LLDPE blend to a 45 µm LLDPE film often requires a reduction in sealing time from 0.8 s to 0.6 s to prevent seal thinning at the packaging corners.
In agricultural stretch film, the resin may be blended with LDPE or mLLDPE to adjust cling and load retention. The cling additive, typically polyisobutene or similar, is added at 0.5 wt% to 1.5 wt%; the migration kinetics are influenced by film thickness and storage temperature. A load retention test under ISO 527-3:2018 or an equivalent creep test using 25 mm wide specimens at 50°C is used to compare grades. These application data are class-level and not a guarantee for PROXESS 3310 without trial.
Autoclave LDPE has a highly branched architecture that provides high melt strength and easy bubble expansion but limits dart impact and puncture resistance. At equivalent film thickness, LLDPE resins in the 0.918 g/cm³ class can provide a dart impact value of 120 g to 180 g under ASTM D1709-16a, whereas an autoclave LDPE film of the same thickness may fall below 80 g. Conversely, the melt strength of LLDPE is lower, which reduces maximum draw-down in cast film and increases the risk of bubble instability in blown film. This trade-off is addressed through higher air ring cooling rates, internal bubble cooling, and die gaps that are wider than those used for LDPE.
Within LLDPE grades, comonomer type and molecular weight distribution shift the balance between tear strength, stiffness, and optics. A C4-LLDPE made with 1-butene often exhibits lower dart impact and lower Elmendorf tear than a C6-LLDPE made with 1-hexene or a C8-LLDPE made with 1-octene, particularly at low temperatures. PROXESS 3310 is a linear low density polyethylene grade; if the comonomer type is not specified on the public datasheet, the purchaser should request the short-chain branching distribution from the supplier. Published data for this specific configuration is limited. The difference from metallocene LLDPE is also critical: metallocene-catalyzed resins typically have a narrower molecular weight distribution, lower haze, and a lower seal initiation temperature, but may require higher extruder backpressure and may be more sensitive to shear-induced melt fracture. PROXESS 3310 is not marketed as a metallocene grade and should not be substituted into a film structure designed for mLLDPE without revalidating seal performance and hot tack.
Compared with high-density polyethylene, LLDPE has a lower flexural modulus and a lower Vicat softening temperature, which limits use in hot-fill applications above 80°C. However, LLDPE provides significantly higher dart impact at low temperature and better environmental stress crack resistance. In heavy-duty sacks, the use of PROXESS 3310 as a sealant layer over HDPE provides low-temperature drop performance while preserving stiffness in the core layer. In extrusion coating, LLDPE requires lower melt temperature than HDPE but higher than LDPE, and may exhibit neck-in values of 20 mm to 40 mm at a coating line speed of 100 m/min; the exact value depends on melt strength and die gap.
The stabilizer package in LLDPE film grades is designed to protect the polymer during pelletization, storage, and film extrusion. Typical phenolic antioxidant loadings for film-grade LLDPE are in the range of 300 ppm to 1,000 ppm, with phosphite secondary antioxidants at 500 ppm to 1,500 ppm. These values are not grade-specific and must be confirmed by the product stewardship bulletin. During masterbatch dilution, fluoropolymer processing aids at concentrations of 200 ppm to 800 ppm are frequently used to suppress melt fracture. The effectiveness of the processing aid depends on the die material and surface roughness; on chromium-plated dies, the induction period for stable coating formation may be 20 min to 60 min at 200°C. Interactions between fluoropolymer processing aids and other additives, such as high levels of silica antiblock or erucamide slip, can delay the onset of stable coating formation and increase haze. If erucamide slip is added above 1,000 ppm, the migration kinetics in the polymer matrix can reduce the coefficient of friction over a period of 24 h to 72 h after extrusion, but may also interfere with seal strength if the surface concentration is excessive. These are operational boundaries: the processor should verify additive loading with infrared spectroscopy or gas chromatography and should not assume that increasing masterbatch level linearly improves performance.
Incompatibility data are specific to the additive package. Amine-based antifog concentrates can generate color bodies when exposed to certain hindered phenolic antioxidants at elevated temperature; published data for this specific PROXESS 3310 configuration is limited, and a laboratory trial at 200°C for 30 min is recommended before production. The same caution applies to metal stearate-based antistatic additives, which may complex with phenolic stabilizers and shift the oxidation induction time measured under ISO 11357-6:2018.
When granulate moisture content exceeds 0.05% by weight, surface moisture is carried into the feed section of the extruder and can cause steam-induced bubbles or surface defects in the film. Pre-drying at 60°C for 2 h in a desiccant dryer is required when sacks have been exposed to relative humidity above 60% for more than 24 h. Storage temperature should remain below 40°C and away from direct ultraviolet light, because prolonged exposure can generate oxidation products that shift the viscoelastic response and increase gel count. First-in-first-out inventory rotation should be used. The resin should not be stored near open containers of organic solvents or volatile amines, as polyethylene can absorb low-molecular-weight species and transfer them to the package interior.
At the conversion line, the feed throat temperature should be maintained below 60°C to prevent pellet fusion and bridging. The screw should be purged with a high-viscosity polyolefin purge compound when transitioning from a dissimilar resin or color. The purge procedure should include at least 10 min of full-output operation and a die pressure verification step to remove residual high-flow resin that may remain in the adapter and die manifold. These are standard practices for LLDPE film lines; no special storage inerting is required.
The blown film process is sensitive to the relationship between die gap, blow-up ratio, and frost line height. For LLDPE film resins, a die gap of 1.2 mm to 2.0 mm is preferred because narrow die gaps increase shear rate and can initiate melt fracture. At a blow-up ratio above 2.8:1, the bubble becomes more susceptible to breathing and helical instability, particularly when the frost line height is below 300 mm. The crystalline orientation developed at high blow-up ratios improves tear strength in the transverse direction but may reduce machine-direction tear strength. Haze is measured according to ISO 14782:1999 on a 50 µm film; for LLDPE film grades without clarifying additives, values typically fall between 8% and 15%, with higher values linked to surface roughness and processing-induced crystalline morphology.
On a coextrusion line with internal bubble cooling, the internal air temperature should be controlled between 15°C and 25°C and the external air ring pressure balanced to prevent film flapping. If bubble instability occurs, the operator should first reduce the melt temperature by 5°C to 10°C, then lower the blow-up ratio to 2.5:1, and finally adjust the die gap. These adjustments are made with reference to the resin’s shear viscosity curve; no single setpoint applies to every machine. The processor should record pressure drop across the screen pack and melt temperature before the die to establish a baseline for lot-to-lot variation. In addition, the use of a dual-lip air ring and a bubble stabilizing cage is recommended when the line operates above 2.8:1 blow-up ratio.
In applications where clarity and gloss are critical, the film is evaluated under ISO 14782:1999 for haze and ISO 2813:2014 for gloss at 20°, 60°, and 85° angles. For LLDPE film of this class, haze values typically range from 8% to 15% for 50 µm blown film, while gloss at 60° may range from 40 GU to 70 GU. The presence of long-chain branching in LDPE lowers haze, so LLDPE film converted for display packaging often requires blending with LDPE or metallocene LLDPE. The blend ratio is limited by the need to maintain dart impact and tear strength; additions of 20 wt% LDPE can reduce haze by 3% to 5% but may reduce dart impact by 15% to 30% at constant thickness. These values are class-level observations, not lot-specific guarantees. If low haze is the primary requirement, a metallocene LLDPE or a cast film process may be more appropriate than a blown film structure based on PROXESS 3310.
Regulatory conformity for food-contact compliance is evaluated under FDA 21 CFR 177.1520(c) for olefin polymers and European Commission Regulation (EU) No 10/2011 for plastic materials and articles intended to come into contact with food. The resin may be subject to REACH registration obligations under Title II of Regulation (EC) No 1907/2006 and to RoHS Directive 2011/65/EU restrictions on heavy metals. The following compliance matrix summarizes the relevant designations; the supplier’s product stewardship bulletin remains the authoritative document for the specific grade.
| Standard or regulation | Scope | Typical compliance indicator |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Food-contact olefin polymers | Condition of use E/G |
| Regulation (EU) No 10/2011 | Plastic food-contact materials | Overall migration limit 10 mg/dm² |
| REACH Regulation (EC) No 1907/2006, Title II | Registration of substances | Substance registered |
| RoHS Directive 2011/65/EU | Restriction of hazardous substances | Pb, Hg, Cd, Cr(VI), PBB, PBDE below threshold |
| ISO 9001:2015 | Quality management system | Certificate of analysis per lot |