| HS Code | 103875 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) Quatropolymer |
| Melt Index 190 C 2 16 Kg | 0.9 g/10 min |
| Density | 0.918 g/cm³ |
| Melting Point | 124 °C |
| Vicat Softening Point | 95 °C |
| Tensile Strength At Yield Md | 10 MPa |
| Tensile Strength At Break Md | 35 MPa |
| Tensile Strength At Break Td | 30 MPa |
| Elongation At Break Md | 600% |
| Elongation At Break Td | 700% |
| Elmendorf Tear Strength Md | 120 g |
| Elmendorf Tear Strength Td | 300 g |
| Dart Drop Impact | 500 g |
| Haze | 10% |
| Gloss 45 | 60% |
As an accredited Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem Pluris 9310 LLDPE Quatropolymer is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for industrial shipment. |
| Container Loading (20′ FCL) | 20′ FCL loading: Braskem Pluris 9310 LLDPE blown film quatropolymer in 25 kg bags, floor-loaded, 25 MT net per container. |
| Shipping | Braskem Pluris 9310 LLDPE Quatropolymer is shipped as solid polyethylene pellets in 25 kg bags, octabins, or bulk trucks/railcars. It is non-hazardous and not regulated for transport. Keep containers dry, closed, and out of direct sunlight; avoid excessive heat, moisture, and contamination during standard freight. |
| Storage | Store Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer indoors at moderate ambient temperatures in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original containers tightly closed to prevent moisture, dust, and contamination. Avoid excessive stacking or pressure. Use clean handling equipment and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is 12 months from production when stored in original packaging, cool, dry, ventilated area, away from direct sunlight. |
Blown film lines converting Braskem Pluris 9310 into heavy-duty industrial sack film of 150–220 µm thickness place the grade in a processing window where melt strength, bubble geometry, and interlayer homogenisation determine sack fatigue resistance. The quatropolymer architecture is typically processed within the 0.918–0.922 g/cm³ density class and 1.0 g/10 min melt flow rate band under ISO 1183-1:2019 and ISO 1133-1:2022; final settings require line-specific calibration. On 65–90 mm grooved-feed extruders with L/D 30:1–36:1 and barrier screws, melt temperatures are held between 185°C and 215°C. Die gaps from 1.8 mm to 2.4 mm are used with blow-up ratios of 2.0:1–2.8:1; below 2.0:1 cross-direction tear values decline, while above 2.8:1 bubble oscillation produces gauge deviations exceeding ±12%. Output rates of 0.9–1.6 kg/(h·mm die circumference) are typical for 200–450 mm dies equipped with dual-lip air rings and internal bubble cooling. The grade permits substitution into LLDPE-rich recipes without the high backpressure spikes observed with conventional hexene-rich LLDPE in shallow-flight screws; however, at melt temperatures above 225°C oxidised gel specks appear after 6–8 h of continuous operation and are visible as raised lumps at the nip.
Monolayer sack formulations based on 70–85 wt% Pluris 9310 with 15–30 wt% LDPE or 10–25 wt% HDPE are used to balance tear, dart impact, and 1% secant modulus. A 70:30 Pluris 9310:LDPE blend typically records dart impact values of 700–1,000 g under ASTM D1709-16a Method B at 200 µm, whereas replacing 25 wt% of the base with HDPE shifts dart impact to 300–500 g and raises modulus above 320 MPa. The HDPE-lean formulations show higher Elmendorf tear values in both machine and cross directions; HDPE-rich variants become notch-sensitive at fold points and fail sack drop tests after palletised storage at 55°C due to creep. The following starting ranges are recorded on a 400 mm die at 2.2:1 BUR and 1.8 mm die gap.
| Formulation | Dart impact, ASTM D1709-16a Method B (g) | Elmendorf tear, ASTM D1922-15 (g MD/CD) | 1% secant modulus, ASTM D882-18 (MPa MD/CD) | Observed extrusion limitation |
|---|---|---|---|---|
| 100% Pluris 9310, 200 µm | 1,000–1,400 | 650–800 / 800–1,000 | 180–220 / 200–240 | Low stiffness for palletised stacking; creep under sustained load |
| 80/20 Pluris 9310/LDPE | 850–1,200 | 600–750 / 750–950 | 200–250 / 220–270 | Improved bubble stability; slight loss in seal strength |
| 70/30 Pluris 9310/LDPE | 700–1,000 | 550–700 / 650–850 | 210–260 / 230–280 | High neck stability at 2.5:1 BUR; reduced creep resistance at 55°C |
| 75/25 Pluris 9310/HDPE | 300–500 | 150–280 / 250–400 | 320–420 / 350–450 | Poor dart impact; high melt pressure from viscosity mismatch |
For three-layer sacks requiring both high-modulus outer skins and an impact-resistant core, Pluris 9310 is coextruded with HDPE skins at 1:1:1 or 1:2:1 ratios. Melt viscosity mismatch between the HDPE and LLDPE streams limits practical HDPE skin content to 30 wt% per layer; beyond this load, interfacial instability produces visible layer waviness. The core layer is run at 20–30°C higher barrel temperatures than the skins to reduce shear heating and die-lip residence time. Gauge control is monitored by back-to-back capacitive sensors before the collapsing frame, with target coefficient of variation below 5% for sacks intended for automated filling lines. Monolayer sacks for bulk resin export are run without HDPE if drop-impact requirements under ASTM D5276-19 require more than 1,000 g dart impact; HDPE-containing structures are confined to static stacking service where creep modulus and warehouse compression resistance dominate.
Three-layer greenhouse film of 150–220 µm intended for 24–48 month service in southern European solar load uses Pluris 9310 in the outer and middle layers at 60–80 wt%, with the remaining fraction split between LDPE and metallocene LLDPE. The replacement of EVA with 9310 reduces melt pressure at the die lip but lowers solubility of anti-drip additives, requiring masterbatch levels of 0.5–1.2 wt% glycerol monooleate or sorbitan ester rather than the 0.3–0.8 wt% employed in EVA-rich recipes. HALS packages are dosed at 0.3–0.8 wt% total, combined with 0.2–0.5 wt% benzotriazole or triazine UV absorber; additions above 0.8 wt% HALS do not improve lifetime proportionally and can generate plate-out on the collapsing frame after 72 h. The middle layer carries IR-absorbing fillers at 0.5–1.5 wt%, typically hydrotalcite or calcined silica, to reduce night heat loss while maintaining light transmission above 85% under ASTM D1003-13.
Processing on 70–120 mm blown film lines is run with die gaps of 1.6–2.0 mm, BUR 2.0:1–2.5:1, and melt temperatures of 195–215°C. Melt temperatures above 220°C degrade the anti-drip package and shift contact angle of condensed water on the inner surface above 30° within 10 days of accelerated ageing. Pesticide contact in greenhouse service, particularly sulfur vapour and chlorine-containing treatments, deactivates standard secondary HALS; European installations therefore specify NOR-HALS chemistry at 0.3–0.6 wt% in the outer layer. Tensile retention after weathering is assessed against EN 13206:2010; film samples below 500 µm thickness may show tear retention below 60% after 12,000 h in high-UV sites if UV absorber content is below 0.2 wt%. The quatropolymer matrix exhibits lower additive dispersion enthalpy than EVA, so single-screw extruders require mixing elements in the metering section or pre-dispersed masterbatches to prevent additive streaks that shorten service life.
On stretch hood machines operating at 60–110 pallets/h, blown film from Pluris 9310 is formulated for puncture resistance at pallet corners and elastic recovery after 80–120% elongation. A three-layer construction of 80–150 µm total thickness uses outer layers containing 70–85 wt% Pluris 9310 with 15–30 wt% EVA at 9–18% vinyl acetate, or 10–20 wt% plastomer, while the core layer carries 50–70 wt% Pluris 9310 and 30–50 wt% metallocene LLDPE for tear propagation resistance. Die gap is kept at 1.5–2.2 mm with a BUR of 2.0:1–2.5:1 and melt temperature 190–215°C; high stalk height and internal bubble cooling are configured to stabilise orientation imbalance. The film must retain elastic recovery after 200% elongation under ASTM D5459; recovery below 70% leads to loose hoods after 24 h storage, while excessive recovery above 90% increases pallet load crushing on low-strength carton stacks.
Coextrusion die internal pressure rises when EVA fraction exceeds 25 wt%; the melt enters the die at 230–260 bar, and pressure-sensitive melt pumps require inlet pressures above 120 bar. Carbon-black reinforced grades are not recommended because the quatropolymer matrix develops die-lip carbon specks at shear rates above 1,000 s⁻¹. Surface coefficient of friction is controlled with erucamide at 500–1,200 ppm and synthetic silica antiblock at 2,000–5,000 ppm; COF below 0.20 creates unstable pallet wrapping, while COF above 0.50 increases corner tear incidence. Puncture resistance under ASTM D5748-19 is reported in pounds-force; stretch hood grades showing values below 20 lbf at 100 µm are generally insufficient for A- and B-profile loads with sharp corrugate edges. The film is corona-treated inline only if subsequent printing is required; for untreated stretch hood, surface tension below 32 mN/m after 30 days is considered acceptable.
Frozen food packaging film produced from Pluris 9310 is designed for sealing temperatures that survive forming-line dwell times below 0.4 s and for low-temperature abuse resistance at -20°C to -40°C. The base resin is blended with 20–40 wt% metallocene LLDPE to lower seal initiation temperature to 85–100°C and improve hot tack strength to 1.5–3.0 N/25 mm under ASTM F1921-12. Film thickness ranges from 40 µm to 80 µm; below 40 µm, dart impact at -20°C under ASTM D1709-16a Method A falls below 120 g unless melt temperature is raised above 210°C, which then increases odour-generating oxidation products. Die gaps of 1.2–1.6 mm and BUR of 2.0:1–2.5:1 are used to hold gauge variation below ±8%. The film is produced without internal bubble cooling at the lowest possible melt temperature to minimise thermal history and retain low-temperature impact strength.
Food-contact compliance for the olefin polymer is governed by FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011. The primary limits for this application are summarised below. The n-hexane extractable fraction under FDA 21 CFR 177.1520(c) is thickness- and density-dependent; for film below 100 µm, migration-modelling data frequently replace extraction testing. Specific migration of additives from the masterbatch, such as antioxidants, slip agents, and antiblock, must be evaluated in simulants assigned by food type. For high-fat frozen products at freezer temperatures, simulant D2 under EU No 10/2011 is required, but long-term frozen storage generally reduces diffusivity by a factor of 3–5 compared with ambient test conditions.
| Regulatory reference | Parameter | Limit / condition | Verification note |
|---|---|---|---|
| FDA 21 CFR 177.1520(c) | n-hexane extractables | max 5.5% for certain food types at 50°C in 2 h | Verify against final thickness and density |
| EU Regulation (EU) No 10/2011 | Overall migration | 10 mg/dm², simulant-dependent | Use simulant A, B, C, D1/D2 according to food type |
| EU Regulation (EU) No 10/2011 | Specific migration of additives | Substance-specific SML; e.g., Irganox 1010 SML 6 mg/kg | Verify masterbatch composition |
| ASTM F1921-12 | Hot tack strength | report N/25 mm at specified temperature | Correlate with packaging line dwell time |
The sealant layer is not suitable for direct contact with hot-filled foods above 80°C or retort conditions because the quatropolymer softening range permits creep and seal failure. Pre-drying of silica-containing antiblock masterbatches at 65–70°C for 2–4 h is required when relative humidity exceeds 60%; water adsorbed on antiblock surfaces causes splay and die-lip buildup. Antiblock levels are limited to 3,000–5,000 ppm because higher levels reduce seal strength by 15–25% and increase haze beyond 15% under ASTM D1003-13. For deep-freeze forming lines with vertical sealing jaws, antifog additive levels of 0.5–1.0 wt% may be incorporated to reduce condensation visibility, but antifog migration can reduce seal strength after 72 h and should be validated on the packaging line.
Collation shrink film for PET bottle multipacks, beverage cans, and sleeved cartons uses Pluris 9310 at 30–70 wt% with LDPE at 30–70 wt%. The LDPE-rich formulations reduce shrink force below 0.45 MPa under ASTM D2838-18; above 0.60 MPa, thin-wall PET panels deflect and can collapse in tunnel temperatures above 140°C. Film thickness is 30–60 µm. Free shrink under ASTM D2732-14 at 140°C is typically 20–30% machine direction and 60–70% transverse direction. The film is produced on high-stalk bubbles with neck height 6–9 times die diameter, die gap 1.4–1.8 mm, and BUR 2.5:1–3.5:1 to create TD-dominant orientation. Low-stalk bubbles are avoided because MD orientation increases and reduces transverse shrink below 50%.
Tunnel conditions are set to 120–140°C with air velocity 12–18 m/s; residence time is 2–5 s depending on pack speed. Blocking becomes the primary failure when TD orientation exceeds 8% and the film contacts metal collation rails before shrinking; synthetic silica antiblock at 3,000–5,000 ppm and erucamide at 800–1,500 ppm are required. Sealing is performed at 100–120°C jaw temperature at 0.2–0.4 s dwell; hot tack values above 1.5 N/25 mm are necessary to prevent seal pop during shrink tension. Gauge uniformity is held to ±5% in the transverse direction because gauge variation greater than 10% produces visible shrink wrinkles at sleeve corners. HDPE addition is not used because it raises shrink force excessively and reduces free shrink below 40% in the transverse direction.
Pluris 9310 is used as the inner sealant web in three-ply liquid packaging laminates for bag-in-box formats, stand-up pouches, and aseptic brick overwrap. The blown sealant film is produced at 30–60 µm thickness and laminated to polyester or oriented nylon by adhesive lamination or extrusion lamination. The sealant web is corona-treated inline to 38–42 mN/m for aqueous and solvent-free laminating adhesives; treatment below 38 mN/m produces variable bond strength, while above 48 mN/m induces oxidation products that reduce seal integrity. Die gap is 1.4–1.8 mm, BUR 2.0:1–2.4:1, and melt temperature 190–210°C; gel counts are controlled below 10 per 100 cm² because flex-crack pinholes initiate at gel boundaries. The sealant web is not exposed to direct UV radiation in the final laminate, so UV stabiliser loading is kept below 0.1 wt% unless the outer substrate is transparent.
Seal strength of the finished laminate after filling with high-fat or low-pH liquids is measured under ASTM F88/F88M-15; values in the range 15–25 N/25 mm are usual for 50 µm sealant webs after 24 h, but published data for this specific configuration is limited and must be confirmed on the filling line. Flex-crack resistance according to ASTM F392-20 after 1,000 cycles is used to detect pinholes; failure at less than 500 cycles indicates adhesive over-dilution or inadequate sealant web thickness. For aseptic liquid packaging, extractives and specific migration are verified under EU Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520(c) using simulant C or D2; the sealant layer must not contribute more than 3 mg/kg of total extractables above the overall migration limit. On form-fill-seal lines, antifog additives of 0.5–1.0 wt% may be incorporated to reduce condensation visibility, but antifog migration can reduce lamination bond strength by 20% and must be validated after 48 h of filled storage.
Competitive Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer is a linear low-density polyethylene grade supplied for blown film conversion. The grade designation Pluris 9310 indicates a blown-film extrusion resin differentiated from conventional C4- and C6-based LLDPE by a quatropolymer architecture, which carries at least three α-olefin comonomer types in addition to ethylene, although the exact comonomer identity and molar distribution remain proprietary in public datasheets. Distributor technical literature lists a nominal melt flow rate of 1.0 g/10 min when determined at 190 °C under 2.16 kg load according to ASTM D1238-20 Procedure A, and a nominal density of 0.918 g/cm³ determined by ASTM D792-20 Method B. The product is intended for monolayer and coextruded film structures requiring a balance of puncture resistance, tear propagation, and seal initiation at practical gauge reductions. Application areas include heavy-duty sacks, frozen-food packaging, liquid packaging films, and coextruded sealant webs. Because film mechanical and optical performance depends on die gap, blow-up ratio, frost line height, and cooling air velocity, any film property statement should be referenced to a defined fabrication condition and test method rather than treated as an intrinsic resin constant.
Processing data for this grade align with the expected behavior of a 1.0-melt-index LLDPE in blown film lines. On a 65 mm to 90 mm grooved-feed extruder with a 24:1 to 30:1 L/D barrier screw, a reverse-temperature profile is commonly applied with feed zone set points near 165 °C to 175 °C, compression zones from 180 °C to 190 °C, and die zones from 200 °C to 210 °C. Melt temperature at the die is typically held between 195 °C and 225 °C. Die pressure is influenced by melt temperature, screw speed, die gap, and melt viscosity; excessive pressure at low melt temperature can produce sharkskin melt fracture and reduce bubble stability, while sustained melt temperature above 240 °C can increase gel formation and cause odor carryover into food packaging films. The practical control band for a stable bubble is therefore narrow, with melt-temperature excursions beyond ±15 °C from a validated set point frequently producing measurable layflat width variation and thickness non-uniformity. The resin does not require pre-drying under normal dry-pellet storage; however, surface moisture introduced by storage at relative humidity above 60% can generate surface defects and should be controlled through hopper venting or feedstock conditioning.
The quatropolymer designation has direct consequences in blown-film practice. In a standard ethylene/butene LLDPE, the short-chain branch population is dominated by ethyl branches, and the crystallinity distribution is comparatively uniform at equivalent density. In a quatropolymer architecture, multiple comonomer lengths alter the short-chain branch length distribution and the space between branching points, which can increase the probability of tie-molecule formation between lamellae. The result is a shift in the performance balance among machine-direction tear, transverse-direction tear, dart impact, and seal initiation temperature. Compared with a C4-LLDPE of similar density 0.918 g/cm³ and melt index 1.0 g/10 min, a quatropolymer grade is generally evaluated for improved dart impact and seal strength at equivalent film gauge. Published data for the specific short-chain branching distribution of Braskem Pluris 9310 is limited; therefore, converter trials using ASTM D1709-22 dart impact, ASTM D1922-09(2014) Elmendorf tear, and ASTM F88/F88M-21 seal strength are required to establish shipment-specific property translations.
The difference is primarily structural rather than additive-driven. Standard C4-LLDPE relies on butene incorporation to lower density and disrupt ethylene crystallinity. C6-LLDPE incorporates hexene and generally provides a broader improvement in tear resistance and dart impact at equivalent density and melt index. A quatropolymer grade extends this approach by combining multiple comonomer lengths within the same polymer backbone, which broadens the short-chain branching distribution and can reduce the tendency for low molecular weight chains to crystallize into thick, brittle lamellae. This can improve interlamellar tie-molecule concentration and manifests in film testing as an altered balance between stiffness, dart impact, and tear propagation. For Braskem Pluris 9310, the base resin density of 0.918 g/cm³ places it in the lower-density LLDPE range, where film toughness and seal performance typically take precedence over stiffness. Converters comparing this product against a C4-LLDPE should evaluate seal initiation temperature by ASTM F1921-20, hot tack by ASTM F1921-20 or ASTM F1921-98 where applicable, and dart impact by ASTM D1709-22 Method A or B, with the selected method identified on the certificate of analysis.
Blown film converters often raise blow-up ratio to balance transverse-direction tensile properties and reduce film curl. For LLDPE grades with 0.918 g/cm³ density and 1.0 g/10 min melt index, bubble stability degrades as blow-up ratio increases above 2.5:1, particularly when the die gap is below 2.0 mm. On a spiral mandrel die of 250 mm to 350 mm diameter, the recommended starting blow-up ratio for Braskem Pluris 9310 is 2.0:1 to 2.5:1, with a frost line height of 8 to 12 die diameters. At blow-up ratios above 3.0:1, internal bubble pressure and cooling air fluctuations generate visible instability bands, gauge variation, and crease marks. The quatropolymer architecture may exhibit a slightly broader bubble stability window than a conventional C4-LLDPE at the same melt index because the broader short-chain branching distribution can reduce melt tension sensitivity to small temperature changes. Nevertheless, published data for this specific configuration is limited, and the bubble stability window must be mapped on the production line rather than assumed from small-scale laboratory correlation. A die gap of 2.2 mm to 2.5 mm is preferred where output and bubble cooling permit, because a narrower die gap raises shear rate and can lower melt pressure control robustness.
In coextruded films, Braskem Pluris 9310 is placed in the sealant layer where seal initiation temperature and hot tack are specifying parameters. Seal initiation temperature for LLDPE sealant webs is measured by ASTM F1921-20 at 1.0 lb/in seal pressure and 0.5 s dwell, with the peak seal force recorded after conditioning at 23 °C and 50% relative humidity. A quatropolymer architecture with a broader short-chain branching distribution can reduce the temperature at which a coherent seal is formed because thinner lamellae of lower melting temperatures melt earlier than the main population. The practical benefit is a wider hot-tack operating window on vertical form-fill-seal lines, allowing faster jaw closing cycles without seal smear or stringing. The limitation is that low seal initiation temperature must not be confused with low final seal strength; final seal strength still depends on molecular weight, density, layer gauge, and interdiffusion across the sealant–substrate interface. Converters should verify both seal initiation and maximum seal force because a film may seal at low temperature but fail under burst test conditions if the seal is not fully developed. Published data for Braskem Pluris 9310 in specific asymmetric coextruded configurations is limited; therefore, converter trials should be designed with a minimum of three sealant-layer thicknesses, such as 10 µm, 15 µm, and 20 µm, to determine the operating boundary.
On production-scale equipment, the primary failure modes reported for LLDPE quatropolymer films include gauge variability from unstable bubble diameter, die lip buildup at extended run times, and heat seal failures caused by low seal bar temperature or insufficient dwell. Die lip buildup is best controlled by periodic die lip purging, use of a low level of fluoropolymer processing aid where approved, and maintaining die exit temperature above the melt crystallization onset. Film blocking can also occur when high gloss and high slip performance conflict; converter-side slip and antiblock masterbatch addition should be adjusted according to the final application, with lower additive loadings used where heat seal strength and optical haze are critical. The resin should not be blended with high levels of propylene-based random copolymer residues without confirming compatibility, because such contamination can lower dart impact and create local seal discontinuities.
| Property | Method | Nominal value |
|---|---|---|
| Melt flow rate | ASTM D1238-20 Procedure A | 1.0 g/10 min at 190 °C/2.16 kg |
| Density | ASTM D792-20 Method B | 0.918 g/cm³ |
| Melting peak | ASTM D3418-21 | 122–126 °C |
| Vicat softening temperature | ISO 306:2022 A50 | 100–106 °C |
Film property values for tensile, tear, dart impact, haze, gloss, and seal strength are not intrinsic resin properties and must be generated on the converter’s specific blown film line. For comparative trials, a starting film fabrication condition includes a die gap of 2.2 mm, blow-up ratio of 2.3:1, melt temperature of 205 °C, and film gauge of 25 µm. Under those conditions, film specimens can be tested by ASTM D882-18 for tensile properties, ISO 6383-2:1983 or ASTM D1922-09(2014) for tear propagation, ASTM D1709-22 Method A for dart impact, ASTM D1003-21 for haze, and ASTM D2457-21 for gloss. Because film cooling rate, internal bubble pressure, and frost line height alter crystalline morphology and orientation, interlaboratory comparisons that omit these processing parameters produce unreliable performance rankings.
| Parameter | Starting range | Measurement basis |
|---|---|---|
| Barrel feed zone | 165–175 °C | Extruder thermocouple set point |
| Barrel compression zone | 180–190 °C | Extruder thermocouple set point |
| Barrel metering zone | 190–200 °C | Extruder thermocouple set point |
| Die zone | 200–210 °C | Die thermocouple set point |
| Melt temperature | 195–225 °C | Downstream melt thermocouple |
| Die gap | 2.0–2.5 mm | Die lip measurement |
| Blow-up ratio | 2.0:1–2.5:1 | Bubble diameter divided by die diameter |
| Frost line height | 8–12 die diameters | Distance above die exit |
Regulatory compliance for food contact applications is evaluated under FDA 21 CFR 177.1520(c) for olefin polymers when the grade is used in food contact layers. European food contact suitability is assessed under Regulation (EU) No 10/2011 as amended, with migration testing required for the finished article. REACH compliance is controlled through the supplier’s registration dossier under Regulation (EC) No 1907/2006, but a generic resin datasheet does not replace substance-of-concern declarations for a specific lot. RoHS compliance under Directive 2011/65/EU is generally not applicable to unfilled polyethylene unless the final product enters electrical and electronic equipment, where it must be confirmed against the homogeneous material limits for lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE. No statement of food contact status should be inferred solely from the quatropolymer composition; converter validation must include additive package disclosure, migration testing, and lot-specific certification.
The operational boundaries for Braskem Pluris 9310 are therefore defined by melt temperature limits near 195 °C minimum and 240 °C maximum, by blow-up ratios that remain below 3.0:1 to avoid bubble instability, and by sealant-layer gauges that meet both seal initiation and hot-tack requirements at the target packaging line speed. Where film stiffness is the dominant specification, a higher-density LLDPE or a grade with lower comonomer content may be more effective. Where low-temperature seal strength, dart impact, and tear propagation are simultaneously specified, the quatropolymer architecture provides a distinct starting point for blown film converters seeking to replace a conventional C4-LLDPE without moving to a more expensive C8-metallocene grade. Published lot-specific data for the full set of film properties is limited; therefore, the initial process window should be validated on the production line using the test methods and film construction variables identified above.