Braskem Pluris 9300 Lldpe Blown Film Extrusion Polyethylene Quatropolymer

Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer

    • Product Name: Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 483552
    Density 0.930 g/cm³
    Melt Index 0.9 g/10 min (190°C/2.16 kg)
    Melting Point 125 °C
    Vicat Softening Point 110 °C
    Tensile Strength At Yield 12 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 600%
    Flexural Modulus 500 MPa
    Dart Drop Impact 300 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 350 g
    Haze 10%
    Gloss 80%

    As an accredited Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem Pluris 9300 LLDPE is typically supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for secure transport and storage.
    Container Loading (20′ FCL) Loaded in 20-foot FCL: Braskem Pluris 9300 LLDPE quatropolymer, blown film extrusion polyethylene; palletized bags, dry container, ambient, securely stowed.
    Shipping Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer ships as non-hazardous polyethylene resin pellets. Standard packaging: 25 kg bags, octabins, or bulk containers. Store dry, cool, away from sunlight, heat, and contamination. Not DOT/IMDG/IATA regulated. Transport by truck, rail, or sea. Ensure bags remain sealed and pallets are secured.
    Storage Store indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep original packaging sealed, palletized, and off the floor to prevent moisture and contamination. Avoid contact with strong oxidizers. Maintain ambient temperatures and follow the manufacturer’s SDS and local regulations. Handle with clean equipment; protect from physical damage.
    Shelf Life Typically two years from production date when stored in original, unopened packaging, dry, ventilated, below 50°C, and away from sunlight.
    Application of Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer

    In monolayer heavy-duty sack and liner production, Braskem Pluris 9300 LLDPE blown film extrusion polyethylene quatropolymer is introduced either as the sole resin at 100 wt% or as a toughness modifier in LDPE-rich blends at 20–40 wt%, depending on the required balance between dart impact, melt strength, and bubble stability. For non-food industrial liners, the applicable chemical-control framework is REACH Regulation (EC) No 1907/2006; when the same structure is intended for indirect food contact, the film must additionally satisfy FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011 with overall migration below 10 mg/dm². The downstream conversion line for this application is typically a blown film extruder with a grooved feed section and L/D 30:1, a barrier screw, a screen changer fitted with 120/160 mesh breaker plates, and a spiral mandrel die with die gap 1.8–2.4 mm. Melt temperature is controlled between 195 °C and 225 °C, blow-up ratio is set at 2.0:1–2.6:1, and the frost-line height is maintained at 6–10 die diameters to limit film blocking without producing excessive transverse direction shrinkage. The web is gusseted, surface-treated, and converted on bottom-seal or side-weld bag machines into industrial liners, refuse sacks, FIBC liners, and construction sheeting. The principal production-scale failure mode occurs at the die lip: combinations of melt temperature above 230 °C, die gap below 1.5 mm, and high screw speed can produce die-lip buildup that transfers to the bubble as die lines, while insufficient back pressure can destabilize the melt film and create gauge bands. The control response is to adjust die gap and screw speed together, keeping melt pressure stable within ±15 bar of the line’s steady-state value and observing bubble diameter stability for at least 30 min after any change. Batch-to-batch variance in quatropolymer comonomer distribution can appear as scatter in dart impact and tear values; the relevant laboratory methods are ISO 527-3:2018 for tensile properties, ASTM D1922-15 for Elmendorf tear, ASTM D1709-16a for dart impact, and ISO 1183-1:2019 for film density. Published data for this specific grade configuration remains limited, so lot-specific certificates of analysis should be used to establish the actual property balance before running at full line speed.

    Control points for monolayer heavy-duty sack film based on Braskem Pluris 9300
    Control pointEquipment or test standardTypical setpoint or range
    Melt temperatureInfrared melt probe195–225 °C
    Die gapSpiral mandrel die1.8–2.4 mm
    Blow-up ratioAir ring/bubble cage2.0:1–2.6:1
    Dart impactASTM D1709-16a≥ 350 g at 100 µm
    Elmendorf tearASTM D1922-15MD/TD balance within ±15%
    Film densityISO 1183-1:2019report against supplier certificate

    What Governs Low-Temperature Seal Integrity in Coextruded Frozen Food Webs?

    Three-layer coextruded frozen food packaging assigns Braskem Pluris 9300 to the sealant layer, where the film must maintain seal integrity after repeated flexing at temperatures below -18 °C and resist puncture from frozen vegetables or seafood edges. The sealant layer formulation commonly contains 60–80 wt% Braskem Pluris 9300, 10–25 wt% LDPE, and 10–20 wt% polyolefin plastomer, with the plastomer content adjusted to shift seal initiation below 95 °C while preserving hot-tack strength. The food-contact compliance pathway for such a structure is FDA 21 CFR 177.1520(c) for the polyolefin sealant layer and Regulation (EU) No 10/2011 for the European Union, with overall migration below 10 mg/dm²; the layer is also subject to extractables control under FDA 21 CFR 177.1520(c) hexane extraction at 66 °C for 2 h. The production line is a three-layer blown film coextruder with die gap 1.2–1.8 mm, blow-up ratio 2.0:1–2.8:1, and melt temperature from 190 °C to 230 °C, followed by in-line corona treatment to 42–46 mN/m for printing or lamination adhesion. End products include frozen vegetable pouches, ice cream overwrap, seafood film, and formed lidding. The main process conflict in this application is the trade-off between low seal initiation and hexane extractables: very low seal initiation is usually achieved by reducing peak crystalline order, but the same molecular features can increase extractables and require tighter supplier control over comonomer distribution. Operational boundaries include limiting corona power density so that surface energy does not exceed 50 mN/m, because excessive surface oxidation can reduce seal strength and increase coefficient of friction during downstream packaging. Published data for this specific grade configuration is limited; seal-strength and hot-tack curves should therefore be generated on the actual coextrusion line because lab-scale cast films do not reproduce the same quench rate and layer distribution.

    In agricultural silage and greenhouse film lines, Braskem Pluris 9300 operates under a different regulatory loading than food-contact packaging; the applicable product norm is EN 13206:2017, with REACH Regulation (EC) No 1907/2006 covering chemical registration and restriction obligations. The formulated film typically contains 80–90 wt% Braskem Pluris 9300, 6–12 wt% UV-stabilizer masterbatch, and 1–3 wt% antiblock/processing-aid masterbatch, with phosphite-based process stabilizers preferred over amine-based packages to avoid UV stabilizer antagonism. The process is a three-layer blown film coextrusion with die gap 1.8–2.2 mm, blow-up ratio 2.2:1–2.8:1, and melt temperatures from 190 °C to 220 °C, with the recycled core layer limited to 30 wt% when optical transmission is critical. End products include silage stretch film, greenhouse cover film, and low-tunnel film, with thickness selected between 60 µm and 180 µm according to expected UV dose and installation period; published data for this specific grade configuration is limited, so outdoor weathering trials are required before commercial quotation.

    When LLDPE Quatropolymer Replaces Conventional C4-LLDPE in Stretch Hood Applications, How Does the Force Plateau Shift?

    Replacement of conventional C4-LLDPE with Braskem Pluris 9300 in pallet stretch hoods shifts the load-elongation plateau and requires the film to sustain radial elongation of 40–70% during hood application, retain load-bearing tension on the pallet, and resist corner puncture during transport. In this application, Braskem Pluris 9300 is typically formulated at 70–85 wt% with 15–30 wt% polyolefin plastomer, and optionally 0.5–2.0 wt% of a cling-enhancing concentrate, with the exact ratio set by the stiffness-elongation balance required for the stretch hood machine. The relevant test methods are ASTM D5458-95 for peel cling, ISO 527-3:2018 for tensile properties, and ASTM D1894-14 for coefficient of friction; for food-contact pallet hoods used in direct contact with primary packages, FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011 may also apply. The downstream process is a high-stalk blown film line with die gap 1.8–2.5 mm, blow-up ratio 2.5:1–3.5:1, and melt temperatures from 190 °C to 220 °C, with in-line slitting to the hood width and optional antistatic treatment. End products include pallet hoods for beverage, appliance, and chemical bag pallets. The process conflict on production-scale equipment is that the transition from conventional C4-LLDPE to a quatropolymer can shift the force plateau at 50% elongation; if the plateau is too low, the hood may not maintain tension, while a high plateau can overload the stretch hood machine and produce corner thinning. Cling performance is also sensitive to surface oxidation: corona treatment beyond 38 mN/m can reduce cling by increasing surface polarity, so only the outside surface is treated when antistatic printability is required. Published data for this specific grade configuration is limited; plant trials should measure force-elongation curves under ISO 527-3:2018 on the actual high-stalk bubble line because tubular orientation history determines the load-elongation hysteresis.

    For lamination-grade sealant webs, Braskem Pluris 9300 is produced for adhesive lamination to oriented polyester, biaxially oriented polyamide, or aluminium foil in stand-up pouches, gusseted liquid liners, and condiment sachets. The polyolefin sealant layer follows FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, with overall migration below 10 mg/dm²; the film is run at 100 wt% Braskem Pluris 9300 or at 80–90 wt% with a minor polyolefin plastomer to reduce seal initiation. During lamination, the sealant web is produced on a blown film line with die gap 1.5–2.0 mm, blow-up ratio 1.8:1–2.4:1, and melt temperatures from 190 °C to 220 °C, then corona-treated in line to 42–48 mN/m and adhesive-laminated using solventless or solvent-based adhesives at 1.5–2.5 g/m² dry coat weight. End products include stand-up pouches, gusseted liquid liners, and sachets; published data for this specific grade configuration is limited, so seal-strength and interlayer adhesion trials should be performed after corona treatment because surface polarity decays with storage time and can raise the failure risk at the adhesive-polyolefin interface.

    Free Quote

    Competitive Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The Braskem Pluris 9300 resin is supplied as a linear low-density polyethylene quatropolymer for blown film extrusion on single-screw and high-output grooved-feed film lines. The grade designation is consistent with a nominal density of 0.930 g/cm³ as determined by ASTM D792-20 or ISO 1183-1:2019. The term quatropolymer indicates an ethylene interpolymer containing more than two comonomer species, which produces a mixed short-chain branch-length distribution not typically available in conventional butene-only LLDPE grades. The supplier may adjust comonomer ratios, slip agents, and antiblock packages across regional production sites, so the controlling specification must be the current Braskem technical datasheet and certificate of analysis for the specific lot. Melt flow rate is evaluated at 190 °C under a 2.16 kg load according to ASTM D1238-23 or ISO 1133-1:2022.

    The product designation places the resin in the upper range of linear low-density polyethylene by density, which raises crystallinity and flexural modulus while potentially reducing low-speed dart impact and increasing haze if the film is quenched too rapidly. Differential scanning calorimetry according to ISO 11357-3:2018 can be used to calculate the crystalline fraction from the melting endotherm. For linear low-density polyethylene near 0.930 g/cm³ after cooling at 10 °C/min, the crystalline weight fraction commonly falls between 40% and 55%, although the exact value is cooling-rate dependent. The crystalline morphology controls the diffusion path for oxygen and water vapor; converters seeking measurable barrier performance should verify film samples using ASTM D3985-17 for oxygen transmission rate and ASTM F1249-20 for water vapor transmission rate.

    What Structural and Morphological Factors Distinguish the Quatropolymer from Standard C₄ and C₆ Linear Low-Density Grades?

    The main structural distinction is the heterogeneity of short-chain branch lengths. A butene-based LLDPE introduces ethyl branches of relatively uniform length, while a hexene-based LLDPE introduces longer butyl branches that disrupt crystallinity more effectively. A quatropolymer that incorporates olefinic comonomers of varying chain length introduces different branch populations along the same chain or across chains, which broadens the distribution of lamellar thickness and alters the tie chain concentration. The result is often a broader melting endotherm in ISO 11357-3:2018 DSC analysis, with peak melting temperatures for linear low-density resins near 0.930 g/cm³ commonly reported between 120 °C and 126 °C. The increased branching heterogeneity can raise low-speed dart impact as measured by ASTM D1709-22 and improve puncture propagation resistance as measured by ASTM D5748-19, but these effects are sensitive to frost line height, die gap, and draw direction.

    Because the molecular weight distribution of quatropolymer film grades is generally broader than that of metallocene LLDPE resins and narrower than autoclave LDPE, the shear viscosity and elongational response must be assessed differently. At blown film die shear rates from 50 s⁻¹ to 500 s⁻¹, the resin exhibits pseudoplastic flow; at lower shear in the bubble neck, extensional viscosity limits drawdown and may require a taller frost line for stable bubble geometry. The resin does not contain long-chain branching comparable to LDPE, so bubble stability at blow-up ratios above 3.0:1 is generally not equivalent to an LDPE control. The practical limitation should be established by measuring thickness variation according to ASTM D8136-17 and by recording bubble position over time on the actual die.

    On blown film lines with grooved-feed extruders of 25:1 to 30:1 L/D and barrier screws, a rising barrel temperature profile from 170 °C to 220 °C is typically applied. Die zones are held between 210 °C and 230 °C, while the actual melt temperature is measured with an immersion probe because shear heating can raise the melt by 10 °C to 20 °C above the barrel set point. The die gap is selected between 1.8 mm and 2.5 mm for conventional LLDPE; for higher-viscosity quatropolymer lots, widening the gap to 3.0 mm reduces die-lip shear and suppresses sharkskin but may increase thickness variation. The onset of sharkskin in polyethylene blown film is commonly associated with a critical die-lip shear stress from 0.14 MPa to 0.20 MPa. When the die gap is below 1.5 mm and output exceeds the critical shear stress, the film surface can show periodic ridges that are not corrected by raising melt temperature alone. A spiral mandrel die may reduce local shear rate but increases residence time and can promote gel formation in the hotter zones.

    Process variableWorking rangeFailure mode outside range
    Die gap1.8–2.5 mmSharkskin below 1.5 mm; gauge variation above 3.0 mm
    Blow-up ratio2.0:1–3.5:1Low transverse tear below 2.0:1; bubble instability above 3.5:1
    Frost line height1.5–3.0 die diametersReduced dart impact below 1.5; increased blocking above 3.0
    Melt temperature at die exit200–230 °COxidative gel formation above 240 °C; poor homogenization below 190 °C
    Regrind fraction0–20%Dart impact loss and gel formation above 20%

    When Seal Initiation Is Lowered by Branched-Comonomer Heterogeneity, Hot-Tack Windows Become the Critical Control

    The mixed branch-length distribution of the quatropolymer can reduce seal initiation temperature relative to a butene-only LLDPE at the same density, but the shift must be quantified with ASTM F2029-22 for seal strength and ASTM F1921-20 for hot tack. The converter should establish the seal initiation temperature on a flat-jaw heat sealer using 25 mm wide film specimens, controlled dwell time, and a specified jaw pressure; the target seal force is package-dependent because transport and filling loads vary. A lower crystalline melting onset as measured by ISO 11357-3:2018 indicates earlier seal initiation, but it can narrow the hot-tack plateau if the resin lacks sufficient crystallization kinetics after the seal jaws open. Hot-tack force should be measured at 0.5 s cooling time for high-speed packaging lines, and the failure mode should be recorded as film tear, interface peel, or seal-area distortion.

    In coextruded structures, the quatropolymer may be placed in a sealant or toughness layer, while a butene-based LLDPE serves as a lower-cost core. The distinction is not solely density; it is the breadth of the branch-length distribution that can shift the tear balance measured by ASTM D1922-15. In a symmetric three-layer blown film, placing the quatropolymer in the outer layers can raise machine-direction tear resistance while maintaining transverse-direction tear, but the effect is amplified by die rotation and film gauge uniformity. Thickness mapping should follow ASTM D8136-17 to confirm that a ±5% gauge variation is not masking the resin-specific contribution. At film gauges below 30 µm, the benefit of comonomer heterogeneity may be masked by orientation-induced anisotropy, and both machine-direction and transverse-direction tensile properties should be evaluated according to ASTM D882-18.

    Crystalline Relaxation After Extrusion Is Governed by Frost Line Height and Windup Tension

    The final solid-state properties of the quatropolymer film are not fixed at the die exit; they are strongly dependent on cooling rate and winding tension. A frost line height from 1.5 to 3.0 die diameters is generally used. Below 1.5 die diameters, the film may show lower haze as measured by ASTM D1003-21 but can lose dart impact as measured by ASTM D1709-22 because the crystalline lamellae are quenched into a less interlocked network. Above 3.0 die diameters, surface tack and blocking risk increase, especially when slip-agent migration is incomplete during the first 24 h after extrusion. Blocking force should be measured according to ASTM D3354-21 after conditioning at 23 °C and 50% relative humidity for 24 h. Winding tension should be kept below the point at which residual stress in the roll causes gauge-band self-indentation; the limit is typically established by measuring roll hardness and by inspecting the film surface after 72 h of blocked roll storage.

    Regrind-Addition Oxidative Stability Boundaries and Slip-Agent Migration Kinetics

    Processing stability is determined by the phenolic and phosphite antioxidant package rather than by the polymer backbone alone. Oxidation induction time as measured by ISO 11357-6:2018 is used to compare incoming pellets, first-generation film, and regrind streams. When the regrind fraction exceeds 20 wt%, the film can show carbonyl index increases and reduced bubble stability because oxidized oligomers lower the polymer-vapour interfacial tension. Slip-agent migration is also affected: erucamide-loaded films develop their design coefficient of friction within 24 h to 72 h at 23 °C. If the film is tested immediately after extrusion according to ASTM D1894-14, the measured kinetic coefficient of friction may be higher than the equilibrium value. The static coefficient of friction is generally higher for quatropolymer films because the surface has a broader melting endotherm and may retain heat longer during winding.

    Film propertyStandard designationSpecimen or conditioning note
    DensityASTM D792-20 / ISO 1183-1:201923 °C; method A
    Melt flow rateASTM D1238-23 / ISO 1133-1:2022190 °C; 2.16 kg
    Dart impactASTM D1709-22Method A or B; 50% failure
    Elmendorf tearASTM D1922-15MD and TD; trouser tear
    Tensile propertiesASTM D882-18 / ISO 527-1:2019500 mm/min for ASTM; 25 mm width
    Haze and transmittanceASTM D1003-2123 °C, 50% RH
    Gloss at 60°ASTM D2457-21Non-banded film surface
    Kinetic and static COFASTM D1894-14Film-to-film; 23 °C, 50% RH
    Puncture propagationASTM D5748-19Heavy-duty packaging films
    Seal strengthASTM F2029-22Flat-jaw sealer; 25 mm width
    Hot tackASTM F1921-200.5 s cooling time
    DSC thermal transitionsISO 11357-3:2018N₂ atmosphere; 10 °C/min
    Oxidation induction timeISO 11357-6:2018200 °C in O₂ atmosphere

    The product is not formulated for injection molding or blow molding. Processors should avoid contamination of the grade with polypropylene or high-density polyethylene regrind because immiscible domains in the film core reduce dart impact values measured by ASTM D1709-22 and can create visible gels at film thickness below 25 µm. When the storage environment exceeds 60% relative humidity, pre-drying at 70 °C for 2 h to 4 h is required to prevent surface moisture defects. Food-contact compliance statements must be verified for the specific regional grade because compliance with FDA 21 CFR 177.1520 and Commission Regulation EU No 10/2011 depends on additive composition and migration testing under the intended film thickness and temperature conditions.