| HS Code | 102155 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.918 g/cm3 |
| Melt Flow Rate 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 122°C |
| Vicat Softening Temperature | 100°C |
| Tensile Strength At Yield Md | 11 MPa |
| Tensile Strength At Yield Td | 10 MPa |
| Tensile Strength At Break Md | 38 MPa |
| Tensile Strength At Break Td | 32 MPa |
| Elongation At Break Md | 600% |
| Elongation At Break Td | 700% |
| 1 Secant Modulus Md | 190 MPa |
| 1 Secant Modulus Td | 220 MPa |
| Dart Impact Strength | 120 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 350 g |
| Haze | 12% |
| Gloss 45 | 60 |
| Coefficient Of Friction | 0.2 |
| Blocking | 60 g |
As an accredited Braskem Pluris 6301 Blown Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem Pluris 6301 LLDPE is supplied in 25 kg polyethylene-lined bags, palletized and stretch-wrapped for secure transport. |
| Container Loading (20′ FCL) | 20′ FCL of Braskem Pluris 6301 linear low density polyethylene for blown film extrusion, palletized bags, securely stowed for shipment. |
| Shipping | Braskem Pluris 6301 Blown Film Extrusion LLDPE is shipped as non-hazardous solid pellets, typically in 25 kg moisture-barrier bags on stretch-wrapped pallets or in bulk sacks/railcars. Transport in clean, dry trucks, railcars, or containers; protect from moisture, heat, sunlight, and contamination. Store cool and dry. Not regulated for transport. |
| Storage | Store Braskem Pluris 6301 Blown Film Extrusion LLDPE resin indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, and ignition sources. Keep original packaging closed to prevent moisture, dust, and contamination. Palletize properly, avoid excessive stacking, and protect from prolonged UV exposure. Maintain ambient conditions and segregate from strong oxidizers. Follow local regulations and manufacturer guidelines. |
| Shelf Life | Shelf life is typically 12 months when stored unopened in a cool, dry, ventilated area away from sunlight and moisture. |
On three-layer blown-film lines equipped with 70–90 mm extruders having 24:1 to 30:1 L/D ratios, Braskem Pluris 6301 is fed as the structural layer in heavy-duty industrial liner and shipping sack constructions to provide dart impact resistance and machine-direction tear propagation control at folded side gussets, with failure energy compared under ASTM D1709 and tear force under ASTM D1922. In a 100–150 µm finished liner, the manufacturing formulation uses 85–100 wt% Pluris 6301 in the core and outer layers; up to 15 wt% LDPE may be introduced to widen bubble stability on die diameters above 1,800 mm, while slip and antiblock concentrates are metered at 0.5–1.5 wt% and fluoroelastomer processing-aid masterbatch is added at 0.03–0.10 wt% when high-throughput extrusion above 2.4 kg/h/mm of die circumference produces sharkskin on the die lip. The processing envelope on this equipment is defined by a die gap of 1.5–2.2 mm, a blow-up ratio of 2.0–3.0:1, a melt temperature of 190–230 °C, and a frost-line height between 6 and 10 die diameters; exceeding 230 °C shifts the bubble into downward oscillation on tall-stalk configurations, while dropping below 2.0:1 blow-up ratio raises transverse-direction tear anisotropy and destabilizes the gusset fold. Mechanical compliance is assessed using ISO 527-3 tensile strip testing on machine and transverse directions, impact-failure energy is quantified with ASTM D1709 Method A, Elmendorf tear is measured under ASTM D1922, and seal strength after bag conversion is verified with ASTM F88/F88M. REACH Regulation (EC) No 1907/2006 Article 33 and packaging-waste Directive 94/62/EC apply to material placed on the European market. Terminal products produced from this configuration include heavy-duty shipping sacks, drum and box liners, construction rubble bags, and dunnage air retention liners.
Silage film produced by blown extrusion on three-layer agricultural lines uses Braskem Pluris 6301 as the load-bearing external layer, with a cling-layer formulation coextruded on the inner face to deliver adhesion to the bale wrap without excessive unwind force. The outer and central layers contain 60–85 wt% Pluris 6301, 5–15 wt% metallocene LLDPE for dart impact, 3–6 wt% carbon black masterbatch with a hindered amine light stabilizer content adjusted to 0.3–1.0 wt% active HALS in the final film. The cling layer is fed separately and typically constitutes 10–20% of total film thickness; it contains 20–40 wt% of a polyisobutylene or very-low-density ethylene copolymer cling concentrate, with the balance Braskem Pluris 6301, but published data for this specific configuration is limited and converter trials are required because cling force varies nonlinearly with film temperature below 10 °C. The production process uses a die gap of 1.2–1.8 mm, a blow-up ratio of 2.5–3.5:1, and a melt temperature held at 195–220 °C; a dual-lip air ring with internal bubble cooling is specified on dies above 2,000 mm to maintain frost-line stability at output rates of 2.0–2.6 kg/h/mm. Oxygen transmission is measured under ISO 15105-2 to document the actual gas transmission rate of the film, perforation toughness and tear retention after UV aging are evaluated under EN 13206 classification for agricultural covering films, tensile properties are tested with ISO 527-3, and weathering resistance is assessed by exposure in accordance with ISO 4892-2; the carbon black masterbatch must meet dispersion requirements below a 0.02% gel count threshold to prevent pinholes. Uncoated polyethylene is not an oxygen barrier, so the final film must not be specified as a barrier layer unless laminated to an EVOH or metallized substrate. Terminal product types include silage bale wrap, silage clamp side-sheet film, and underlay agricultural film where oxygen exclusion preserves fermentation.
Thin-gauge stretch hood films coextruded on three-layer blown-film towers incorporating Braskem Pluris 6301 in the middle and exterior layers are formulated to balance elastic recovery and puncture resistance during pallet containment. The film formulation uses 70–100 wt% Braskem Pluris 6301 in the two skin layers and up to 30 wt% high-toughness metallocene LLDPE in the core to raise machine-direction elongation at break; the inside layer receives 0.5–3.0 wt% of a polyisobutylene-based cling masterbatch, while no slip or antiblock is added because coefficient-of-friction reduction degrades pallet lock. Processing on 55–80 mm extruders with 24:1 to 30:1 L/D barrier screws requires a high-stalk bubble geometry, with a die gap of 1.2–1.8 mm, blow-up ratio of 2.8–4.0:1, and melt temperature controlled at 185–210 °C; a stable high-stalk frost line is necessary because low-stalk operation converts the stress-strain curve into a stiff, brittle envelope with reduced stretch-hood recovery after pallet settling. Cling force is graded with ASTM D5458, puncture resistance with ASTM D5748, and tensile energy to break with ASTM D882; elastic recovery after elongation is tracked using a 100% elongation hold test as a production-line release criterion, not as a substitute for ASTM D5459. Regulatory compliance for industrial packaging does not invoke food-contact clearance; REACH Article 33 applies to additives and packaging-waste Directive 94/62/EC applies to end-of-life placement. Terminal products include pallet hood films, transport wraps for bagged resin, and heavy pallet containment stretch films used as replacements for shrink ovens.
When Braskem Pluris 6301 is used as a blown-film sealant web for extrusion lamination or as a direct food-contact pouch layer, the polyethylene must comply with both U.S. and European migration frameworks. Under 21 CFR 177.1520(c), the olefin polymer is permitted for food contact provided the density and extractable fraction meet the specifications of the regulation; European food contact clearances are managed under Regulation (EU) No 10/2011, with migration of additives verified using food simulants and permitted substances listed in Annex I and Annex II, and good manufacturing practice under Regulation (EC) No 2023/2006. Formulation for a 35–70 µm food pouch web uses 70–100 wt% Braskem Pluris 6301 in the sealant layer, 0–20 wt% LDPE in the exterior skin for heat-seal strength, and 0.10–0.50 wt% of slip/antiblock masterbatch to achieve a coefficient of friction low enough for vertical form-fill-seal jaw conveyance. Antioxidant loading is selected to provide thermal stabilization during extrusion but is not adjusted upward without reviewing migration limits under EU 10/2011; primary antioxidants based on hindered phenolic chemistry are therefore maintained at the minimum effective concentration. The production process uses a die gap of 1.2–1.8 mm, a blow-up ratio of 2.0–2.8:1, and melt temperatures of 185–215 °C to limit off-flavor precursors; bubble cooling air is filtered to 25 µm to reduce particulate contamination, and corona treatment above 40 mN/m is applied only to the lamination side to avoid seal-strength decay. Heat-seal initiation and hot-tack performance are measured under ASTM F1921, seal strength under ASTM F88/F88M, and oxygen transmission is specified only after lamination to a barrier substrate because uncoated LLDPE film exhibits negligible oxygen barrier and must not be specified as a barrier layer. Terminal products include frozen food pouches, bakery overwrap, cereal liner films, and heat-sealable lidding web for laminated tray packaging.
| Scenario | Regulatory reference | Performance standard | Control metric |
|---|---|---|---|
| Heavy-duty liners | REACH (EC) No 1907/2006, 94/62/EC | ISO 527-3, ASTM D1709, ASTM D1922, ASTM F88/F88M | Dart impact failure energy, tear ratio, seal strength |
| Silage film | REACH, EN 13206 classification | ISO 527-3, ISO 4892-2, ISO 15105-2 | UV retention, gel dispersion, oxygen transmission rate |
| Stretch hood | REACH Article 33, 94/62/EC | ASTM D5458, ASTM D5459, ASTM D5748, ASTM D882 | Cling force, elastic recovery, puncture resistance |
| Food-contact pouch | 21 CFR 177.1520(c), EU 10/2011, EC 2023/2006 | ASTM F1921, ASTM F88/F88M | Migration limits, seal initiation, hot-tack strength |
| Refuse sacks | REACH, 94/62/EC, EN 13592 | ISO 527-3, ASTM D1709 | Dimensional stability, dart impact retention with PCR |
| Bag-in-box liners | 21 CFR 177.1520, EU 10/2011 | ASTM F392, ASTM F88/F88M | Flex-crack pinholes, seal integrity under pressure |
Refuse sacks and bin liners manufactured from Braskem Pluris 6301 and post-consumer recycled polyethylene are run on high-speed single and three-layer blown-film lines where gel count, melt-pressure variation, and dart impact retention determine the permissible recycled-content ceiling. The formulation uses 50–85 wt% Braskem Pluris 6301 as the skin and core dilution resin, with 15–50 wt% washed post-consumer LLDPE/LDPE recyclate added through a side feeder; a calcium-carbonate anti-slip or antiblock concentrate is dosed at 0–5 wt% only when sacks are specified for outdoor collection bins and require reduced surface blocking. Higher recycled fractions above 30 wt% require a screen pack of 80–120 mesh in addition to the primary 40–60 mesh screen to prevent die-lip buildup from non-melting contaminants; melt-pressure variation at the screen changer should not exceed ±8% of baseline pressure or bubble instability increases at the frost line. Processing parameters use a die gap of 1.2–2.0 mm, blow-up ratio 2.0–3.0:1, melt temperature 180–210 °C, and backpressure limits governed by the extruder’s maximum melt pressure rating. Compliance for refuse sacks includes dimensional and mechanical requirements under EN 13592, tensile evaluation under ISO 527-3, dart impact under ASTM D1709 Method A, and EU packaging waste Directive 94/62/EC, while REACH Article 33 applies to recycled input streams. Terminal products include star-sealed refuse sacks, drawstring bin liners, and kerbside collection bags with printed collection calendars on the outer surface.
Liquid bag-in-box liner films coextruded with Braskem Pluris 6301 as the liquid-contact layer are specified for flex-crack resistance and seal integrity under repeated pressure cycling, not for oxygen barrier performance. The film formulation uses 85–100 wt% Braskem Pluris 6301 in the inner liquid-contact layer, 0–15 wt% high-toughness metallocene LLDPE in the core for pinhole resistance, and 0.2–0.8 wt% of a slip-free clarification or stabilization masterbatch selected so that additive migration does not exceed food-contact limits. The production process operates with a die gap of 1.2–1.8 mm, blow-up ratio 2.0–2.5:1, melt temperature 180–200 °C, and internal bubble cooling to stabilize caliper below ±5% variation; after winding, the film is adhesive-laminated to a metallized polyester or aluminum-foil barrier layer, with the polyethylene side serving as the heat-seal surface. Flex durability is evaluated under ASTM F392/F392M by subjecting the film to repeated flex cycles and measuring pinhole formation after specified conditioning, while seal integrity is tested under ASTM F88/F88M before and after pressure cycling; regulatory clearance for food and liquid contact is reviewed under 21 CFR 177.1520 and Regulation (EU) No 10/2011. The operational boundary of uncoated polyethylene must be recognized: without lamination to a barrier film, the structure does not prevent oxygen ingress and is unsuitable for oxygen-sensitive liquid filling unless nitrogen flushing or external overpacking is specified. Terminal products include bag-in-box liners for non-oxygen-sensitive liquid foods, water-based industrial fluids, and chemical buffer solutions where flex-crack pinhole resistance is the primary failure criterion.
Competitive Braskem Pluris 6301 Blown Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem Pluris 6301 is a pelletized linear low density polyethylene designated for blown film extrusion. The grade is produced with a butene comonomer and carries a manufacturer-published nominal density of 0.926 g/cm³ when tested under ASTM D1505 and a melt mass-flow rate of 1.0 g/10 min under ASTM D1238, condition 190 °C/2.16 kg. The base stabilization package is intended for standard extrusion heat history; the resin is supplied without intentionally added slip or antiblock additives. Film coefficient of friction, blocking behaviour, and surface morphology are therefore governed by converter-selected additive masterbatches rather than by a fixed resin-bound additive formulation.
Blown film processors use the grade in monolayer and coextruded structures in which downgauging from high-pressure LDPE is a specified objective. The butene comonomer introduces short-chain branches that reduce crystallinity relative to HDPE and yield a different balance among secant modulus, tear, and dart impact than high-pressure LDPE. Density and flow-rate position the material for industrial liners, heavy-duty sacks, agricultural film, and lamination substrates. In three-layer coextrusion, the resin may act as a toughness core layer or as a sealant layer when the package seal requirements remain within C4-LLDPE limits. The processing window is narrower in melt tension than high-pressure LDPE, and die-gap choice is more critical for melt-fracture control. Pre-drying is not normally required when storage is below 60% relative humidity; if condensation is present, drying at 70 °C for 2 h in a desiccant dryer reduces pinhole formation and surface defects. Sustained melt temperatures above 230 °C can increase gel formation, and regrind content above 30% by weight tends to narrow the bubble-stability window and reduce dart impact.
The resin’s melting behaviour is consistent with the density class. Differential scanning calorimetry under ASTM D3418 shows a peak melting temperature in the range of 122 °C to 126 °C for C4-LLDPE near 0.926 g/cm³. The melt-flow ratio of high-load melt index to standard melt index is typically between 25 and 27, which reflects a moderately broad molecular weight distribution and contributes to shear thinning that is more pronounced than in high-pressure LDPE but less controlled than in single-site metallocene grades.
Coextruded structures containing polyamide or EVOH barrier layers require tie-layer optimization because the nonpolar surface of LLDPE limits adhesion to polar barrier materials. Maleic anhydride grafted tie resins are specified, with typical tie-layer thickness between 3 µm and 5 µm, to prevent delamination under flex-crack conditions. The final film performance is therefore a system property rather than a resin-only specification.
The melt exhibits lower extension-hardening behaviour than long-chain branched LDPE, so die gap, blow-up ratio, and frost-line height collectively determine whether the bubble oscillates, sags, or develops melt fracture. Extruders with length/diameter ratios of 24:1 to 30:1 and barrier screws are specified to restrict melt-temperature overshoot. Barrel profiles commonly range from 160 °C in the feed zone to 190 °C at the metering section, with adapter and die zones set between 200 °C and 220 °C. Die gaps of 1.5 mm to 2.5 mm are used because C4-LLDPE is more shear-sensitive than high-pressure LDPE; narrower gaps can induce sharkskin at output rates above approximately 0.4 kg/h per mm of die circumference.
Blow-up ratios between 2.0:1 and 3.0:1 balance transverse orientation against bubble flutter. Frost-line heights of 6 to 10 die diameters allow the crystalline network to develop before the film reaches the collapsing frame. When the frost line is lowered below 4 die diameters at elevated internal bubble temperature, gauge variation and sag are observed on monolayer lines equipped with 45 mm grooved-feed extruders and 30:1 L/D screws. Addition of 10% to 20% high-pressure LDPE raises melt tension and stabilizes the bubble, but the resulting film shifts toward LDPE-like dart impact and seal initiation. Output limits are not exclusively melt-temperature dependent; die-pressure stability often becomes the first constraint when the die gap is at the lower end of the recommended range and bubble cooling is high.
Dual-lip air rings improve gauge uniformity by reducing stagnation zones on the outside of the bubble. Internal bubble cooling can raise output by 20% to 30% over external cooling alone in films from 50 µm to 70 µm because heat removal is increased without imposing additional melt extension. High die-lip temperatures above 225 °C combined with a very low frost line can increase blocking tendency and reduce tear properties due to slower quench and larger crystallite formation. The die-lip temperature should therefore be held within the upper processing range only when needed to maintain melt-fluid clarity and die-lip wetting.
At 25 µm gauge, monolayer film produced from Pluris 6301 is evaluated under ASTM D882 for tensile properties, ASTM D1922 for Elmendorf tear, ASTM D1709 method A for dart impact, and ASTM D1003 for haze. Manufacturer technical literature should be consulted for exact specification values because film properties depend on blow-up ratio, frost-line height, die gap, and melt temperature. Published datasets for C4-LLDPE resins with density near 0.926 g/cm³ and melt flow rate near 1.0 g/10 min place machine-direction tensile strength at break in the range of 35 MPa to 45 MPa and elongation at break above 500%. Elmendorf tear in the transverse direction is typically higher than in the machine direction; transverse values above 300 gf are reported for 25 µm film. Dart impact strength is above that of high-pressure LDPE at equivalent gauge but below that of hexene and metallocene LLDPE grades.
Secant modulus at 1% strain under ASTM D882 generally falls between 180 MPa and 240 MPa in the machine direction for 25 µm film, depending on orientation and frost-line height. Puncture resistance measured under ASTM D5748 is above that of high-pressure LDPE and below that of C6 or metallocene LLDPE at parallel gauge. These relationships permit the resin to be specified in applications where moderate stiffness and improved tear relative to LDPE are required, but where maximum toughness is not the governing specification.
Optical and surface properties of the base resin are modified by antiblock, slip, and processing-aid masterbatches. Haze and gloss in C4-LLDPE films are controlled by die-gap finish, frost-line height, and additive choice. The base resin is not a high-clarity metallocene grade and should not be specified for applications requiring haze below 5% after conversion unless supported by laboratory trials. Erucamide or oleamide slip masterbatches are used at 500 ppm to 1500 ppm active amide to control static and kinetic coefficient of friction under ISO 8295. Synthetic silica antiblock is typically added at 1000 ppm to 5000 ppm; over-addition above 5000 ppm can increase haze and reduce transverse tear. Coextrusion of Pluris 6301 as a core layer permits a thin skin layer of high-clarity mLLDPE or LDPE to carry surface gloss and slip while retaining downgauged toughness in the core.
Pluris 6301 differs from hexene-based C6-LLDPE primarily in comonomer branch length. Hexene introduces longer short-chain branches that enhance tie-molecule formation and raise dart impact, tear, and puncture at equivalent density. Butene-based LLDPE is selected where conversion economics, melt-flow stability, and equipment availability are more important than maximum toughness. Compared with high-pressure LDPE, the grade exhibits higher tensile and tear performance at equal gauge but lower melt tension and reduced bubble stability in high-stalk operations. Compared with metallocene LLDPE, the grade has a broader molecular weight distribution and generally lower hot-tack strength, higher seal initiation temperature, and higher haze, while metallocene resins offer lower extractables and improved seal-through-contamination behaviour but typically require higher extrusion pressure.
Ziegler-Natta C4-LLDPE has a broader molecular weight distribution than single-site metallocene LLDPE. This lowers melt pressure and permits operation on conventional single-flight screws with lower torque demand, but the melt tension remains lower than that of high-pressure LDPE. The combination of moderate flow-rate and butene branching therefore places the grade in a processing window that is less demanding in shear than metallocene resins but more demanding in bubble control than LDPE. High-stalk extrusion with very high frost-line heights is generally less suited to this architecture than low-to-intermediate stalk geometries.
| Property | Pluris 6301 class (C4-LLDPE) | C6-LLDPE | mLLDPE | High-pressure LDPE |
|---|---|---|---|---|
| Density (g/cm³, ASTM D1505) | 0.926 | 0.918–0.925 | 0.918–0.925 | 0.920–0.930 |
| Melt flow rate (g/10 min, ASTM D1238, 190 °C/2.16 kg) | 1.0 | 0.5–1.0 | 0.5–1.5 | 0.2–2.0 |
| Dart impact at 25 µm (ASTM D1709 A, g) | 90–150 | 150–300 | 200–400 | 50–120 |
| Elmendorf tear, transverse direction (ASTM D1922, gf) | 300–550 | 500–800 | 500–800 | 100–200 |
| Tensile strength at break, machine direction (ASTM D882, MPa) | 35–45 | 35–50 | 35–50 | 20–30 |
| Haze (ASTM D1003, %) | 12–18 | 10–17 | 3–8 | 5–12 |
| Seal initiation range (ASTM F88, °C) | 100–110 | 95–105 | 90–100 | 100–115 |
Values in the table represent class-level typical ranges for blown films of comparable density and flow rate; exact product values are established by the manufacturer’s current datasheet and may vary with fabrication conditions and additive loading.
When seal initiation and hot-tack requirements govern the package, Pluris 6301 is used only after comparison with metallocene sealant grades. Under ASTM F88 and ASTM F1921, C4-LLDPE sealants typically require higher jaw temperatures to reach a given seal strength and exhibit lower hot-tack across contaminated seal surfaces than mLLDPE. Packaging lines with seal dwell times below 0.3 s or dust-prone fill areas may require a metallocene sealant or C6-LLDPE blend. Addition of high-pressure LDPE to Pluris 6301 raises seal initiation temperature and lowers hot-tack strength further, so LDPE additions for bubble stability are limited when seal performance is the governing specification.
Regulatory assessment is made on the final article, not on the pellet alone. The base olefin polymer is evaluated under FDA 21 CFR 177.1520 and EU Regulation 10/2011 for food-contact use when final film composition and migration limits meet applicable requirements. Converter obligations under REACH (EC 1907/2006) and restrictions under RoHS Directive 2011/65/EU must be confirmed for the finished film, including converter-added colorants, slip, antiblock, and processing aids. The standard stabilization package contains no intentionally added perfluoroalkyl substances, but final certification depends on all additive masterbatches introduced during conversion.
Film structures thinner than 15 µm and high-speed lines operating above 0.5 kg/h per mm of die circumference may generate conditions outside the stable window described here; published data for this specific configuration is limited, and pilot-scale evaluation is required before commercial specification.