Braskem Pluris 4303 Blown Film Extrusion Linear Low Density Polyethylene

Braskem Pluris 4303 Blown Film Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem Pluris 4303 Blown Film Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 141182
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Melt Index 190 C 2 16 Kg 0.8 g/10 min
    Density 0.924 g/cm³
    Melting Point 124 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 750%
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 400 g
    Haze 12%
    Gloss 45 55
    Coefficient Of Friction 0.2
    Blocking 20 g

    As an accredited Braskem Pluris 4303 Blown Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically supplied in 25 kg polyethylene bags, palletized at 55 bags per pallet (1,375 kg total).
    Container Loading (20′ FCL) 20′ FCL container loading of Braskem Pluris 4303 Blown Film Extrusion LLDPE: palletized 25 kg bags, approx. 18–20 MT net.
    Shipping Braskem Pluris 4303 is shipped as non-hazardous LLDPE resin pellets in 25 kg polyethylene bags, stacked on pallets and stretch-wrapped. Transport in clean, dry trucks or containers, away from heat, moisture, and direct sunlight. Follow local regulations; no special hazard classification required. Ensure packages remain sealed and protected from contamination.
    Storage Store Braskem Pluris 4303 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original packaging sealed to prevent moisture and contamination. Avoid prolonged UV exposure. Stack pallets securely and follow first-in, first-out rotation. Maintain clean handling areas; no smoking. Use suitable PPE when handling. Ensure containers are closed when not in use.
    Shelf Life When stored properly in original packaging, dry, away from sunlight at moderate temperatures, shelf life is typically 24 months.
    Application of Braskem Pluris 4303 Blown Film Extrusion Linear Low Density Polyethylene

    In the vertical form-fill-seal (VFFS) packaging of dry granular foods and frozen vegetables, Pluris 4303 is converted into monolayer blown film with the base resin fraction maintained between 95 wt% and 98 wt%, the remaining fraction split among high-melt-strength LDPE, antiblock, slip, and processing aid masterbatches. The grade is a butene-based linear low density polyethylene with nominal density 0.918 g/cm³ and melt flow index 1.0 g/10 min at 190°C/2.16 kg per ISO 1133-1:2022. The formulation addition ratio comprises 2.0 wt% to 4.0 wt% LDPE for bubble stability, 0.10 wt% to 0.30 wt% silica antiblock, 0.05 wt% to 0.12 wt% erucamide slip, and optional fluoropolymer processing aid at 0.10 wt% to 0.30 wt% when melt fracture appears on narrow die gaps. Industry compliance for the final film is evaluated under FDA 21 CFR 177.1520(c) olefin polymer provisions, Commission Regulation (EU) No 10/2011 with overall migration below 10 mg/dm², and Good Manufacturing Practice Regulation (EC) No 2023/2006. Downstream processing uses air-cooled blown film lines with die diameters of 250 mm to 400 mm, die gap 1.8 mm to 2.4 mm, blow-up ratio 2.5:1 to 3.0:1, melt temperature 195°C to 215°C, and frost line height 6 to 8 die diameters. On a 300 mm die at 120 kg/h output, bubble flutter is observed when the LDPE fraction drops below 2.0 wt%, while exceeding 4.0 wt% LDPE reduces dart impact at 60 µm below 90 g per ASTM D1709-16a Method A. The terminal product set includes pillow pouches, gusseted bags, and stand-up pouch inner liners for cereals, frozen peas, and pre-portioned rice, with seal initiation between 95°C and 105°C and hot tack force above 1.8 N/25 mm at 110°C per ASTM F1921-12.

    What Limits Drawdown on High-Versatility Liquid Packaging Lines Using Butene-LLDPE Sealant Webs?

    Sealant webs laminated to BOPP or PET in solventless flexible packaging are produced from Pluris 4303 as a monolayer blown film at 20 µm to 35 µm. The process operates with a die gap above 2.0 mm, blow-up ratio 2.0:1 to 2.5:1, melt temperature 190°C to 205°C, and frost line height 5 to 7 die diameters to preserve low haze. Draw resonance and pinhole formation initiate above 80 m/min unless a high-melt-strength LDPE fraction of 3.0 wt% to 5.0 wt% is added. The additive package comprises 0.15 wt% to 0.25 wt% natural silica antiblock and 0.08 wt% to 0.12 wt% erucamide. Slip loadings above 0.15 wt% generate laminate bond decay below 2.0 N/15 mm after 72 h cure per ASTM F904-16, because slip migration blocks secondary urethane crosslinking in solventless adhesives. In-line corona discharge treatment to 42 dyn/cm to 46 dyn/cm is applied immediately before rewinding; surface energy decays by 6 to 10 dyn/cm within 30 days under 23°C/50% RH storage. Regulatory compliance requires EU Regulation (EU) No 10/2011 Annex III migration screening, FDA 21 CFR 177.1520(c), (EC) No 2023/2006, and REACH SVHC verification under Regulation (EC) No 1907/2006. Terminal webs are used as the inner sealant layer in pouches for liquid detergent sachets, oil sachets, and coffee bricks. For aggressive surfactant packaging, environmental stress crack resistance screening under ASTM D1693-15 Method B is recommended; published data for this specific configuration is limited, and converters should qualify each final laminate under the target filling head temperature and product chemistry.

    Heavy-Duty Sack Extrusion and Creep Resistance Under Stacked Storage

    Industrial sacks for resin pellets, fertilizers, and building additives are extruded from Pluris 4303 at basis weights of 100 µm to 180 µm on blown film dies of 350 mm to 500 mm. The compound is blended with 2.0 wt% to 3.0 wt% carbon black-loaded LLDPE masterbatch for UV stabilization in outdoor storage, and 0.5 wt% to 1.0 wt% fluoropolymer processing aid to reduce melt fracture when die gap is narrowed to 1.8 mm. Process settings include die gap 1.8 mm to 2.4 mm, blow-up ratio 2.0:1 to 2.5:1, melt temperature 200°C to 225°C, and gusseted layflat widths of 400 mm to 600 mm. On production lines crossing 60 m/min, bubble wandering increases thickness variation beyond ±8% and decreases drop impact by 15% to 20%. Mechanical acceptance for non-hazardous bulk goods uses tensile properties per ISO 527-3:2018, dart impact per ASTM D1709-16a, and Elmendorf tear per ASTM D1922-15. When the sack is intended for dangerous goods, UN Model Regulations Chapter 6.5 drop testing at 1.2 m and stacking at 3 m require closure integrity and tear propagation verification; published data for this exact formulation under UN certification is limited. Terminal product types include pinch bottom valve sacks, form-fill-seal pouches on tubular lines, and liner bags for flexible intermediate bulk containers.

    In silage bale wrap production, Pluris 4303 serves as the base polyolefin at 88 wt% to 94 wt%, combined with 0.5 wt% to 1.2 wt% hindered amine light stabilizer masterbatch, 0.2 wt% to 0.5 wt% phenolic/phosphite antioxidant, and 0.5 wt% to 1.5 wt% titanium dioxide or 2.0 wt% to 3.0 wt% carbon black masterbatch depending on UV protection and aesthetic requirements. Cling is developed via 1.0 wt% to 3.0 wt% polyisobutylene masterbatch applied to one surface through an extrusion or surface application step. The blown film line runs a die gap of 1.8 mm to 2.2 mm, blow-up ratio 2.7:1 to 3.2:1, melt temperature 190°C to 210°C, and layflat width 500 mm to 750 mm on towers with frost line height 8 to 12 die diameters. At high blow-up ratio conditions, bubble instability can elevate thickness variation to ±10%, requiring internal bubble cooling set between 10°C and 18°C. For silage bale wrap, EN 14932:2018 specifies tensile elongation at break above 300% in machine direction and above 350% in transverse direction, tear resistance, and UV durability after 12 months outdoor exposure. REACH Annex XVII and Regulation (EC) No 1907/2006 apply to EU market access; the final film is not considered food contact. Terminal product is a 25 µm to 40 µm pre-stretched or conventional silage bale wrap supplied in rolls of 1000 m to 1500 m.

    When Coextruded with EVA and mLLDPE for Frozen Food Surface Gloss

    Three-layer coextruded films for frozen meat, seafood, and ice cream packaging use Pluris 4303 in the core layer at 55 wt% to 65 wt%, while the sealant layer contains 70 wt% to 80 wt% mLLDPE and 20 wt% to 30 wt% EVA, and the outer skin contains 60 wt% to 70 wt% Pluris 4303 with high-clarity mLLDPE. Antiblock addition is 0.10 wt% to 0.20 wt% in the skin only, slip addition 0.05 wt% to 0.10 wt% in the skin only, and process aid 0.10 wt% to 0.20 wt% in the core to manage shear heating. The production line uses a 5-layer die, die gap 1.8 mm, blow-up ratio 2.2:1 to 2.8:1, melt temperature 200°C to 220°C, and a dual-lip air ring with internal bubble cooling set at 8°C to 12°C to stabilize the bubble and raise cooling capacity. For frozen food contact, the finished film must meet FDA 21 CFR 177.1520(c), EU Regulation (EU) No 10/2011 overall migration below 10 mg/dm², and (EC) No 2023/2006. Terminal films of 40 µm to 80 µm are converted into vacuum pouches, tubular ice cream bags, and lidding film with seal initiation 90°C to 100°C. Monolayer Pluris 4303 film has insufficient gloss for high-gloss frozen food displays; the coextruded skin is required because butene-LLDPE gloss at 60° typically falls to 45% to 55%. Published data for this exact coextruded configuration under low-temperature puncture testing ASTM D3763-18 is limited.

    In stretch hood film for pallet unitization, Pluris 4303 is compounded at 80 wt% to 90 wt% with 10 wt% to 20 wt% mLLDPE or high-melt-strength LDPE to raise melt elasticity and with 0.2 wt% to 0.5 wt% UV stabilizer masterbatch for outdoor warehouse exposure. The formulation is processed on large blown film dies of 300 mm to 500 mm, die gap 2.0 mm to 2.5 mm, blow-up ratio 2.2:1 to 2.8:1, melt temperature 200°C to 215°C, and internal bubble cooling set at 12°C to 20°C to stabilize the bubble below the frost line. The process bottleneck is melt pressure buildup at outputs above 200 kg/h, where fluoropolymer processing aid at 0.10 wt% to 0.20 wt% is added to reduce screw amperage and eliminate sharkskin. Mechanical property acceptance follows ISO 527-3:2018 for tensile properties, ASTM D882-18 for secant modulus, and puncture resistance via ASTM D5748-19; load stability for European transport is assessed under EUMOS 40509:2020. Terminal product types are stretch hood films of 60 µm to 100 µm and layflat widths 1.2 m to 2.0 m, used on automatic stretch hood machines to secure pallets of beverages, building materials, and bagged chemicals. Published data for Pluris 4303 under EUMOS 40509:2020 is limited, and converter qualification should include full pallet stability testing under the target wrapping machine.

    Free Quote

    Competitive Braskem Pluris 4303 Blown Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem Pluris 4303 is a blown film extrusion linear low density polyethylene (LLDPE) manufactured with a butene comonomer. The resin is supplied in pellet form for monolayer and coextruded film structures. Nominal melt index is 2.0 g/10 min when determined at 190 °C with 2.16 kg load according to ASTM D1238 or ISO 1133-1:2022. Nominal density is 0.918 g/cm³ when tested under ASTM D1505 or ISO 1183-1:2019. These values position the product in the general-purpose blown film LLDPE category used for heavy-duty sacks, industrial liners, and secondary packaging films. The grade is not marketed for cast film, extrusion coating, or injection molding. Compared with high-pressure LDPE, the higher elongation at break and higher tensile strength at break of LLDPE at similar density are the principal performance advantages; the lower melt strength and higher shear viscosity are the principal processing differences. Published lot-specific datasheets from Braskem remain the controlling source for product specifications.

    What distinguishes butene LLDPE architecture from hexene-copolymer and single-site grades?

    The butene comonomer in Pluris 4303 produces short-chain branches that reduce density to 0.918 g/cm³ and interrupt crystallinity. The branch length and distribution create a lower tie-molecule concentration than hexene- or octene-LLDPE at equivalent density, which reduces free-falling dart impact and Elmendorf tear strength per unit thickness. Under ASTM D1922, unreinforced butene-LLDPE blown film often shows lower machine-direction tear than C6/C8-copolymer LLDPE; under ASTM D1709, dart impact for a given gauge is also lower than metallocene-catalyzed grades in the same density class. The broader molecular weight distribution of this Ziegler-Natta grade improves processability on older blown film lines by reducing screw pressure fluctuation and increasing bubble tolerance at high screw speed. Single-site metallocene LLDPE types provide better optical clarity, lower extractables, and higher hot tack, but require tighter processing control and typically cost more. Pluris 4303 is therefore selected where tensile strength, extrusion throughput, and film economics outweigh ultimate tear and optical performance. Product-specific tear and dart values should be obtained from the Braskem technical bulletin; independent published data for this exact configuration are limited.

    On conventional blown film lines, Pluris 4303 is typically processed with a die gap between 1.8 mm and 2.3 mm, a blow-up ratio of 2.0:1 to 3.0:1, and a frost-line height of 7 to 10 die diameters. These settings are not unique to the grade but reflect the low melt strength of butene LLDPE relative to LDPE. Melt temperatures measured at the adapter are generally kept between 190 °C and 220 °C for monolayer film; higher temperatures lower melt viscosity and die pressure but increase the risk of oxidative degradation. Because the linear backbone lacks long-chain branching, bubble oscillation is more sensitive to frost-line height and air-ring turbulence than with high-pressure LDPE. In production practice, bubble stability is restored by lowering frost-line height, reducing blow-up ratio, or adding internal bubble cooling rather than by raising melt temperature indefinitely.

    Melt rheology control is exercised through the melt index and density, but the high-shear viscosity of Pluris 4303 is what determines extruder pressure and screw power. On a 90 mm grooved-feed extruder with a 30:1 L/D ratio and a 250 mm spiral mandrel die, increasing output from 80 kg/h to 120 kg/h raises head pressure more steeply than for LDPE and increases melt temperature. Head pressure ceilings are typically set at 35–40 MPa according to die manufacturer limits; the melt temperature should remain below 240 °C. A reverse barrel profile with the feed zone at 200–210 °C and the metering zone at 190–200 °C is used to compensate for shear heating. High backpressure and excessive melt temperature both increase gel formation, which reduces dart impact and can generate die lip deposits.

    If Pluris 4303 displaces fractional-melt LDPE in a 25 µm industrial liner

    When a converter replaces a fractional-melt LDPE with Pluris 4303 in a 25 µm industrial liner, slow puncture and gauge reduction are driven by the higher elongation at break of LLDPE. Slow puncture propagation resistance under ASTM D5748 or ASTM D2582 may be retained at lower gauge than LDPE, but the specification must be verified lot by lot because puncture performance depends on film fabrication conditions. Machine-direction tear strength under ASTM D1922 is often lower than LDPE at the same gauge, so a tear-sensitive application may require a blend or coextruded structure. Blending with LDPE at 20–30 wt% improves bubble stability and melt strength but raises film haze and reduces dart impact at fixed thickness. Seal initiation temperature measured by ASTM F88 is generally lower for LLDPE than for LDPE, which can increase sealing line speed when jaw temperature and dwell time are held constant. The lower melt strength of Pluris 4303 means that a direct replacement without reducing frost-line height or adjusting air volume may produce visible gauge bands.

    Gauge variation sources and gel formation control on conventional blown film lines

    Gauge uniformity in butene LLDPE film depends on die land parameter, die gap uniformity, and air-ring flow symmetry. On production lines, die lip misalignment of 0.05 mm around the circumference is sufficient to generate visible thickness variation exceeding ±5 % on an otherwise stable bubble. The air ring should be centered within 1 mm of the die centerline and cleaned to prevent asymmetric cooling. Melt temperature and head pressure stability are indirect indicators of degradation; sustained adapter temperatures above 240 °C and head pressure oscillations greater than 10 % of mean may indicate degraded resin or screw wear. Purging with a fractional-melt LDPE or commercial purge compound after each campaign reduces crosslinked residue in the die lip and mandrel. The use of an automatic profile die with capacitance thickness feedback can reduce gauge variation to ±2–4 %, but the capital cost is not always justified for short-run heavy-duty sack production.

    Film property evaluation for this grade should follow the same conditioning and test protocols used for LLDPE blown film. Specimens should be conditioned at 23 ± 2 °C and 50 ± 5 % relative humidity for not less than 40 h according to ASTM D618 before tensile testing. Tensile strength at break and elongation at break should be measured under ASTM D882 at a jaw separation speed of 500 mm/min for film below 1.0 mm thickness. Because film mechanical properties are thickness-dependent, tensile values for 25 µm film should not be directly compared with 100 µm film without normalization. Secant modulus at 1 % and 2 % strain may be reported for stiffness comparisons; published product-specific secant modulus values for Pluris 4303 are not consistently reported in the public literature and should be confirmed from the certificate of analysis. Elmendorf tear strength should be measured with ASTM D1922, and the results should be expressed per unit thickness if films of different gauge are compared. Dart impact should be measured under ASTM D1709, with method A or B stated because the values are not directly interchangeable.

    Seal initiation and hot tack remain thickness-dependent unless additives migrate to the surface

    Seal performance of Pluris 4303 is controlled by melting of the surface layer and is therefore heating-time dependent. Heat seal strength measured by ASTM F88 and hot tack measured by ASTM F1921 should be reported with film thickness, jaw geometry, jaw pressure, and dwell time; comparing hot tack values without these parameters is misleading. Butene LLDPE in the 0.918 g/cm³ density class generally exhibits a lower seal initiation temperature than LDPE and a broader sealing window than metallocene LLDPE of similar density, but product-specific values for Pluris 4303 should be obtained from Braskem technical documentation. Slip and antiblock additives, if present in the grade suffix, reduce coefficient of friction but can compromise seal strength and hot tack after migration to the film surface. The coefficient of friction should be tested under ASTM D1894, and haze under ASTM D1003; these optical and surface values are influenced by film thickness and additive package.

    For food-contact packaging converters relying on supplier compliance documents, Braskem Pluris 4303 must be evaluated against FDA 21 CFR 177.1520 for olefin polymers. The specific clearance depends on density and extraction limits in paragraph (c), and the end-use food type and temperature must be confirmed against the applicable conditions of use. In the European Union, plastics intended to contact food are evaluated under Regulation (EU) No 10/2011 and its amendments, with overall migration limits and specific migration limits listed in Annexes I and II. The grade may be subject to REACH Article 33 communication obligations if a substance of very high concern is present above 0.1 wt%; the supplier safety data sheet and product compliance statement are the operative documents. Packaging heavy metal restrictions under EU Directive 94/62/EC Article 11 require a combined lead, cadmium, mercury, and hexavalent chromium concentration not exceeding 100 mg/kg by weight. Compliance with RoHS Directive 2011/65/EU applies only if the film is incorporated into an electrical or electronic product, and the restricted substance limits in Annex II must then be evaluated.

    Regulatory referenceScopeControlling limit or test basis
    FDA 21 CFR 177.1520Olefin polymer food contact, United StatesDensity 0.918 g/cm³; extraction limits per paragraph (c); end-use conditions per paragraph (d)
    Regulation (EU) No 10/2011Plastics food contact, European UnionOverall migration and specific migration limits in Annexes I and II; compliance declaration required
    EU Directive 94/62/ECPackaging heavy metalsSum of Pb, Cd, Hg, Cr(VI) not exceeding 100 mg/kg under Article 11
    REACHEU chemical safetySVHC communication above 0.1 wt%; polymer monomers registered

    Pellets should be stored in a dry area at temperatures below 50 °C and protected from direct sunlight. Pre-drying is not normally required for this grade; however, if pellets are transferred from cold storage to a warm processing bay, condensation on the pellet surface should be allowed to dissipate before hopper loading to prevent feed bridging and surface defects. Fines accumulation in the hopper and central loading system should be controlled because dusting can cause feed instability in grooved-feed extruders. The resin should be re-evaluated after storage beyond the manufacturer-specified shelf life if lot certification is a requirement.