Braskem Ml3601u Lldpe Rotomolding Polyethylene

Braskem ML3601U LLDPE Rotomolding Polyethylene

    • Product Name: Braskem ML3601U LLDPE Rotomolding Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 626728
    Product Name Braskem ML3601U LLDPE Rotomolding Polyethylene
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Density 0.936 g/cm³
    Melt Flow Rate 3.6 g/10 min
    Melting Point 124 °C
    Vicat Softening Point 116 °C
    Tensile Strength At Yield 17 MPa
    Tensile Strength At Break 27 MPa
    Elongation At Break >800%
    Flexural Modulus 700 MPa
    Environmental Stress Crack Resistance >1000 h
    Low Temperature Impact Strength 60 ft-lb
    Hardness Shore D 55
    Uv Stabilization Yes

    As an accredited Braskem ML3601U LLDPE Rotomolding Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem ML3601U LLDPE rotomolding polyethylene comes in 25 kg moisture-resistant bags, 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) Braskem ML3601U LLDPE rotomolding polyethylene, 20′ FCL loading: 25 kg bags, palletized, approximately 25 MT net per container.
    Shipping Braskem ML3601U LLDPE rotomolding polyethylene is typically shipped as solid pellets in 25 kg polyethylene bags on pallets, stretch-wrapped, or in bulk trucks/containers. It is non-hazardous under normal transport conditions. Keep dry, cool, ventilated, and away from direct sunlight, heat, moisture, and contamination. Follow SDS and local regulations.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers tightly closed and protect from moisture, dust, and contamination. Avoid contact with strong oxidizing agents. Do not exceed recommended stacking heights. Use first-in, first-out stock rotation. Maintain normal ambient temperatures; avoid prolonged UV exposure to prevent material degradation. Store separately from incompatible substances.
    Shelf Life Shelf life: 24 months from production date when stored sealed in a cool, dry, ventilated area, away from direct sunlight.
    Application of Braskem ML3601U LLDPE Rotomolding Polyethylene

    In vented, double-walled containment basins with 10–15 mm nominal wall thickness, Braskem ML3601U is processed as a 35-mesh rotomoulding powder after cryogenic pulverization on a 45 kW disk mill. The grade’s 0.935 g/cm³ density (ASTM D1505) and melt flow rate of 3.5 g/10 min at 190 °C/2.16 kg (ASTM D1238) establish a processing window in which internal air temperature reaches 280–300 °C while the mold surface is held at 220–230 °C for 18–22 min during the curing plateau. Compliance for upright storage tanks is assessed under ASTM D1998-21, while secondary containment structures are designed under EPA 40 CFR 264.175. Food-contact uses fall under FDA 21 CFR 177.1520. Formulation addition ratios for this scene are 100 parts by weight ML3601U, 2.5 parts of a 2% carbon black/UV HALS masterbatch, 0.15 parts hindered phenolic antioxidant, and 0.10 parts phosphite co-stabilizer. Downstream, the powder is loaded into a multi-axis shuttle machine with a 2.6 m swing arm, heated under forced air at 290 °C for 18 min, then cooled with 5–7 °C/min forced air and water mist only below 90 °C surface temperature to minimize warpage. Terminal products include vertical storage tanks, secondary containment basins, dosing cabinets, and double-walled sump liners.

    Specification or test methodCondition or parameterApplication boundary
    ASTM D1998-21Upright storage tank specificationChemical storage vertical tanks
    ASTM D1693-15bCondition B, 100% Igepal CO-630, F50ESCR screening; 1,000 h is typical release threshold
    ASTM D638-22Type IV dogbone, 50 mm/minTensile yield and break
    ASTM D1238190 °C / 2.16 kgMelt flow rate 3.5 g/10 min
    FDA 21 CFR 177.1520Olefin polymersFood-contact surfaces
    EPA 40 CFR 264.175Secondary containmentChemical containment basins

    What Changes When Diesel Immersion Replaces Aqueous Alkali Exposure?

    Diesel immersion shifts design emphasis from environmental stress cracking in alkaline media to dimensional stability under ASTM D543-21 exposure, with the rotomoulded wall measured after 70 h at 50 °C in IRM 903 oil. The ML3601U formulation for fuel-adjacent tanks uses 100 parts by weight ML3601U, 2.0 parts of carbon black masterbatch with 1 µm average agglomerate size, 0.15 parts zinc stearate as internal mold release, and 0.10 parts phosphite co-stabilizer. No post-mould flame treatment is applied because oxidation reduces weld-line elongation at the parting line. Compliance is evaluated under EN 13341:2005 + A1:2011 for static thermoplastic tanks for heating oil, with additional permeability testing referenced to SAE J1737 for diesel permeation. On a double-shuttle machine with rotating arm speed 4.2 rpm, a two-piece steel mold is used; the oven setpoint of 285 °C is maintained until internal air temperature reaches 265–275 °C, after which cooling is quenched at 6 °C/min until 120 °C, then slowed to 2 °C/min to avoid stress cracking at boss inserts. Terminal products include generator fuel day tanks, agricultural auxiliary diesel tanks, marine fuel saddles, and hydraulic reservoir covers.

    Agricultural Water Troughs and the UV Stabilizer Loading Window

    Rotational molds for livestock water troughs are charged with a dry blend of 100 parts by weight ML3601U, 0.25 parts hindered amine light stabilizer, 0.15 parts phenolic antioxidant, and 2.0 parts carbon black masterbatch. The 2.2 wt% total pigment/stabilizer fraction is maintained below 3.0 wt% because higher loadings reduce ESCR F50 values by more than 30% in ASTM D1693-15b condition B testing. NSF/ANSI 61 applies for potable water contact, ISO 17885-1:2018 governs dimensional tolerances and quality requirements for rotomoulded parts, and EU Regulation (EU) No 10/2011 applies where the trough is used for animal drinking water in export jurisdictions. Downstream, the powder is processed on a four-arm independent carousel with a swing radius of 2.8 m; peak internal air temperature is 255–265 °C, mold surface temperature is 210–220 °C, and the cooling cycle uses forced air to 95 °C followed by 15 °C water mist at 10 L/min to maintain flatness across a 1.8 m trough length. Terminal products include dairy calf waterers, sheep troughs, cistern liners, and irrigation header tanks.

    Because material-handling bins are demolded at wall thicknesses between 6 mm and 9 mm and then subjected to forklift tine impact at −20 °C, the ML3601U formulation is adjusted to 100 parts by weight resin, 1.8 parts carbon black masterbatch, 0.20 parts antioxidant, and 5–15 parts of internally generated post-industrial regrind from spur trimmings, provided the regrind particle distribution is controlled through a 40-mesh screen after disk mill pulverization. Regrind above 15 parts creates internal voiding near rib intersections when melt flow index shifts upward more than 0.5 g/10 min. This scenario is evaluated under ISO 8611-1:2021 for flat pallet test methods and ISO 8611-2:2021 for performance requirements in pallet handling, while food-contact tubs fall under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011. During production, a rock-and-roll machine with 45° tilt angle and 4:1 rotation ratio is used to distribute melt into cavity ribs; internal air temperature reaches 275–285 °C, and cooling is staged from 5 °C/min in air to 90 °C, followed by pressurized air at 0.4 MPa through internal cores to set rib deflection below 2 mm/m. Terminal products include insulated fish tubs, nestable bulk bins, pallet boxes, and ribbed container bases.

    If Marine Buoyancy Modules Require Foam-Core Back-Filling and Low-Temperature Impact

    Marine buoyancy modules with 8–12 mm skin thickness are rotationally moulded from a formulation of 100 parts by weight ML3601U, 2.5 parts UV-HALS masterbatch, 0.15 parts antioxidant, and 0.10 parts processing aid. After demoulding, closed-cell polyurethane foam of 60 kg/m³ nominal core density is injected through a 50 mm vent hole, and the foaming pressure is limited to 0.15 MPa to prevent skin delamination at the weld line. Compliance for recreational craft components is referenced to the applicable conformity procedures of Directive 2013/53/EU, and buoyancy retention is verified by a 28-day water absorption test under ISO 2896:2001, with volume change limited to 5%. In process terms, the mould is filled on a shuttle machine with a 3.0 m swing arm and heated to an internal air temperature of 260–270 °C for 20–24 min; the cooling cycle uses 5 °C/min forced air until 80 °C, then the part is removed from the mold and post-cured for 24 h at 40 °C before foam injection. Terminal products include mooring buoys, boat fenders, aquaculture cage floats, and pontoon float shells.

    Playground Enclosures Are Governed by EN 71-3 Migration Limits, Not Only by Wall Thickness

    When rotomoulded panels are intended for children’s play equipment, the formulation uses 100 parts by weight ML3601U, 2.0 parts heavy-metal-free pigment masterbatch, 0.20 parts antioxidant, and 0.10 parts zinc stearate. Migration-limit compliance is tested under EN 71-3:2019 + A1:2021 for specific elements, ASTM F963-23 for heavy-element solubility and mechanical hazards, REACH EC 1907/2006 Annex XVII for restricted substances, and EU 2009/48/EC for toy safety. Heavy-metal-free organic pigments can shift the processing window by ±5 °C depending on particle size and IR absorption behavior; certain organic reds extend cycle time because they absorb less oven radiation than carbon black. Production uses double-walled two-piece steel molds on a shuttle machine with internal air temperature at 260–270 °C and mold surface temperature at 210–220 °C. Cooling proceeds at 5 °C/min to 85 °C, and no external mold release is applied to avoid surface migration that would compromise EN 71-3 extraction results. Terminal products include slides, climbing structure panels, tunnel roofs, and ride-on shell panels.

    Free Quote

    Competitive Braskem ML3601U LLDPE Rotomolding Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem ML3601U LLDPE Rotomolding Polyethylene is a linear low-density polyethylene powder grade developed for single-layer rotational molding of large hollow parts such as agricultural sprayer tanks, water storage vessels, playground enclosures, and recreational hulls. The grade is supplied as a ground powder with a controlled particle-size distribution to maintain consistent dry-flow and uniform pickup on the internal mold surface. It is not a cross-linkable polyethylene and does not require a post-mold curing step. Because rotomolding powders are exposed to elevated temperatures for relatively long cycles, the base stabilization package is designed to address the specific oxidation conditions of air-filled ovens rather than injection-molding melt residence.

    Typical values from manufacturer-published product data are provided below for comparison with other Braskem rotomolding grades. They are not lot-release specifications. Fabricators should verify the certificate of analysis for the specific lot because lot-to-lot variance in melt flow rate and density can influence oven dwell time and part weight.

    PropertyTest methodTypical value
    Melt flow rate (190 °C, 2.16 kg)ASTM D1238-23 / ISO 1133-1:20226.0 g/10 min
    DensityASTM D1505 / ISO 1183-10.936 g/cm³
    Tensile yield strengthASTM D638-14 / ISO 527-218 MPa
    Elongation at breakASTM D638-14 / ISO 527-2>800%
    Flexural modulus (1% secant)ASTM D790-17 / ISO 178600 MPa
    Vicat softening temperatureASTM D1525-17 / ISO 306122 °C
    Environmental stress crack resistance (100% Igepal CO-630)ASTM D1693-21 / ISO 22088-3>1000 h
    Brittleness temperatureASTM D746-20<-75 °C

    The density of 0.936 g/cm³ and melt flow rate of 6.0 g/10 min position this grade at the upper flow end of the rotomolding LLDPE range. In addition to the ASTM D1238-23 value, the melting behavior should be evaluated by differential scanning calorimetry or by observing the powder sintering plateau during mold trials. The high ASTM D1693-21 ESCR value of >1000 h indicates resistance to slow crack growth in the presence of nonionic wetting agents, but it is not a direct measure of chemical compatibility with concentrated fertilizers or hydrocarbon cleaning fluids.

    Thermal and Rheological Baseline Under ASTM and ISO Conditions

    The ISO 1133-1:2022 melt flow rate is a single-point capillary index, not a complete viscosity curve. In rotomolding, densification and bubble removal are controlled by low-shear particle coalescence, so a resin with an MFR of 6.0 g/10 min may not process exactly like another grade with the same MFR if its molecular weight distribution or comonomer length differs. The reported tensile properties are obtained from compression-molded plaques per ASTM D638-14 or ISO 527-2. Rotomolded walls typically cool more slowly than compression-molded plates; this slower cooling can reduce yield strength and flexural modulus below the datasheet values while increasing impact toughness. The flexural modulus of 600 MPa is a 1% secant value and should not be treated as a design modulus for long-term creep. For continuous load, creep modulus and allowable strain must be derived from ISO 899-1 or equivalent.

    The Vicat softening temperature of 122 °C is not a maximum continuous-use temperature. It is a short-term softening point measured under controlled load. Rotomolded tanks exposed to hot water above 60–80 °C require additional thermal-stabilizer evaluation because antioxidant depletion accelerates with temperature. The brittle temperature of <-75 °C provides a low-temperature ductility index, but impact performance of a finished part also depends on cooling-rate-induced crystallinity and weld-line stress.

    In practice, the powder should be conditioned to the molding hall temperature before charging. When sacked or gaylorded material is moved from an unheated warehouse into a warm molding shop during winter, condensation on the powder surface can occur at relative humidity above 60%. This moisture does not require extended drying in the manner of hygroscopic polyamides, but a heated air or desiccant storage cabinet is used in high-humidity plants to keep the powder surface dry. Moisture-related defects typically appear as small voids or rough inner surfaces because steam expansion during heating disrupts the coalescence of the powder bed.

    What Limits Peak Internal Air Temperature During Rotational Molding?

    On a multi-arm carousel machine with a 3.0 m swing and a 4:1 major-to-minor rotation ratio, the oven set point is often maintained between 260 °C and 320 °C. The oven air temperature is not the limiting process variable; the internal air temperature inside the mold is the practical indicator of heat delivery. For ML3601U, peak internal air temperature is usually targeted at 190–210 °C for wall thicknesses of 6–10 mm. If the peak internal air temperature remains below 180 °C, pinholing and incomplete densification can persist at inside corners and vent locations. If it exceeds 230 °C, the internal surface may yellow and the ASTM D1693-21 ESCR can decline because the antioxidant package is consumed by prolonged exposure to hot air.

    Dwell time alone is not a reliable transfer parameter. A 6 mm nominal wall may require 18–26 min of oven residence on a given clamshell machine, but this range shifts with mold gauge, oven air velocity, shot weight, and ambient plant conditions. The preferred control method is to log peak internal air temperature with a through-the-wall thermocouple or a noncontact infrared sensor and adjust dwell time to hold the target plateau. Cooling is equally important. Forced-air cooling from peak internal air temperature to below 100 °C should precede any water mist; demolding is normally performed below 65 °C for dimensionally stable flat panels. Rapid quenching from high temperature freezes the outer skin while the core remains molten, producing internal stresses that can reduce low-temperature impact and increase warpage.

    Internal air pressure can be used on sealed molds to improve replication of recessed texture, but pressure should remain below 10 kPa because excessive pressurization can force melt into vents or create blowholes. Regrind of rotomolded parts into subsequent layers can shift melt flow and particle size if ground too coarse; maximum regrind addition should be validated by differential scanning calorimetry and particle-size analysis. Avoid adding unknown regrind containing polypropylene or cross-linkable polyethylene because melt-phase incompatibility can produce visible splay and weld-line weakness.

    For agricultural sprayer tanks and chemical storage vessels, ML3601U is specified when resistance to slow crack growth in wetting-agent environments and low-temperature ductility are primary requirements. The grade is not recommended for continuous immersion in aromatic hydrocarbon solvents, strong oxidizing acids, or highly permeating ketone streams. Chemical compatibility should be tested on rotomolded plaques under ASTM D543-21 or ISO 175:2010 using the actual concentration and service temperature, because compression-molded data do not account for wall-thickness effects or internal sinter defects.

    Compared with an HDPE rotomolding grade in the 0.945–0.950 g/cm³ density range, ML3601U typically shows lower flexural modulus and yield strength but higher low-temperature impact and longer ESCR under wetting-agent exposure. The lower stiffness means large flat panels may require additional ribs or a thicker nominal wall to satisfy the same deflection limit under ISO 178 three-point bending. Compared with a lower-density LLDPE rotomolding grade in the 0.925–0.930 g/cm³ range, ML3601U shifts the balance toward higher stiffness and heat resistance while retaining adequate impact.

    Kayak hulls, ice fishing shelters, and playground components are molded from this grade where shell impact resistance and surface replication are important. In deep-draw or narrow-channel molds, the secondary-axis rotation speed may need reduction to prevent resin pooling and to maintain uniform wall thickness. Machining rotomolded polyethylene creates stress concentrations; holes should be placed away from knit lines and corners. Drilling with sharp high-speed steel at low rotational speed reduces melt-dragged burrs and localized heat-affected zones.

    When Potable-Water Certification Is Required for Rotomolded Tanks

    A resin-level food-contact statement under FDA 21 CFR 177.1520 can be requested for ML3601U when the final article meets the conditions of use and all colorants, processing aids, and regrind are cleared. This statement does not certify the finished tank. Potable-water approvals such as NSF/ANSI/CAN 61, BS 6920, or AS/NZS 4020 are article-level certifications that require testing on the actual roto-molded part with the final formulation. Fabricators must also control concentration of retained release agents, mold cleaning residues, and regrind fraction because these can affect extraction test results. Under European REACH and RoHS frameworks, the base polymer is generally regarded as compliant as an article component, but importers should obtain the lot-specific regulatory declaration and safety data sheet because polymerization catalyst residues or additive-candidate substances can vary by supply chain.

    When the end-use involves repeated hot-water cleaning or steam sanitation above 80 °C, the stabilization package should be reviewed. Long-term exposure to hot water can extract antioxidant constituents, leading to oxidative embrittlement despite the room-temperature datasheet values. The fabricator should specify a heat-aging test such as ISO 4577 or a multi-temperature oxidative induction time analysis to confirm that the selected stabilization package matches the cleaning protocol.

    In ultraviolet-exposed outdoor service, the base rotomolding powder may require additional light stabilizers. Carbon black masterbatch at 2–3 wt% is commonly used for agricultural tanks, but black surfaces can reach temperatures above 60 °C in direct sun, which accelerates antioxidant depletion. Weatherability tests should be carried out using ASTM G154-23 or ISO 4892-2:2013 on rotomolded plaques containing the final pigment and additive package. Incoming powder lots should be checked for MFR and density shifts before scheduling a production run, because deviations in these base properties can alter peak internal air temperature response, wall thickness distribution, and demolding stability.

    Top