Braskem Ml3600s Rotational Molding Linear Low Density Polyethylene

Braskem ML3600S Rotational Molding Linear Low Density Polyethylene

    • Product Name: Braskem ML3600S Rotational Molding Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 842508
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Application Rotational Molding
    Density 0.936 g/cm³
    Meltflowrate 190c 2 16kg 3.5 g/10 min
    Meltingpoint 124 °C
    Vicatsofteningpoint 108 °C
    Flexuralmodulus 550 MPa
    Tensilestrengthatyield 15 MPa
    Tensilestrengthatbreak 20 MPa
    Elongationatbreak 800%
    Environmentalstresscrackresistance >1000 h
    Hardnessshored 55
    Uvstabilization Yes
    Color Natural

    As an accredited Braskem ML3600S Rotational Molding Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem ML3600S Rotational Molding LLDPE is supplied in 25 kg polyethylene-lined bags, palletized at 1,000 kg.
    Container Loading (20′ FCL) 20′ FCL typically loads about 25 metric tons of Braskem ML3600S LLDPE pellets in 25 kg bags, palletized and secured.
    Shipping Braskem ML3600S is a non-hazardous linear low density polyethylene in pellet form. Supplied in 25 kg bags or 1000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry trucks or containers, protected from moisture, heat, and UV. No special shipping requirements; standard freight classification applies.
    Storage Store Braskem ML3600S in a cool, dry, well-ventilated warehouse at ambient temperature, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers sealed, clean, and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Follow manufacturer’s SDS and local regulations, using first-in, first-out stock rotation.
    Shelf Life 24 months from production date when stored in original packaging in a cool, dry, well-ventilated area, away from direct sunlight.
    Application of Braskem ML3600S Rotational Molding Linear Low Density Polyethylene

    Braskem ML3600S is a high-flow linear low-density polyethylene powder grade specified for rotational molding of hollow components with wall thicknesses from 3 mm to 25 mm and part masses above 5 kg. Typical specification sheet values include a density of 0.936 g/cm³ under ASTM D1505-18 and a melt flow rate of 5.5 g/10 min under ASTM D1238 at 190°C/2.16 kg. The grade is supplied as pellet or 35-mesh powder; if pellet is received, ambient-temperature pulverization to a nominal 500 µm maximum particle size is required before dry blending. Dry blending is performed in a high-intensity paddle or ribbon blender at 23–27°C and 40–60% RH. Powder exposed to RH greater than 60% should be pre-dried at 80°C for 2 h to reduce moisture below 0.05 wt% before charging. The following application scenarios represent verified downstream markets for this grade, each with distinct compliance, formulation, processing, and terminal product constraints.

    Compliance checklist by downstream application
    ApplicationStandard / directiveTest methodRequired property or limit
    Potable water storageFDA 21 CFR 177.1520(c) 2.1; NSF/ANSI 61; EU 10/2011overall migration via simulant A and B; extraction cell type A10 mg/dm² overall migration limit; organoleptic pass
    Agricultural chemical tanksEPA 40 CFR 264.175; ASTM D1998-15; UN Model Regulations 1H1hydrostatic pressure test; ESCR ASTM D1693no leakage at 1.5× design pressure; ESCR >200 h
    Industrial bulk containersISO 12048; EU Directive 94/62/ECstatic compression; cyclic stack loadstack deformation limit set by user facility
    Marine flotation33 CFR 183.114; ASTM D2565UV weathering; pressure decay2,000 h xenon arc no surface cracking; leak tight at 0.10–0.15 bar
    Buried wastewater tanksEN 12566-1:2016; IAPMO/ANSI Z1001soil deflection; ESCR ASTM D1693minimum ESCR 500 h; no cracking after embankment load
    Recreational watercraftEU 2013/53/EUimpact and buoyancy; weathering ASTM D2565hull integrity under small craft load cases

    Potable Water Contact: Migration Limits and Resin Selection

    For polyethylene intended for potable water contact, the governing compliance framework in North America is FDA 21 CFR 177.1520(c) 2.1 for olefin polymers and NSF/ANSI 61 for finished tanks and liners; in the European Union, Commission Regulation (EU) No 10/2011 Annex I sets an overall migration limit of 10 mg/dm² using food simulants A, 10% ethanol, and B, 3% acetic acid, under time-temperature conditions representative of long-term ambient water storage. The base resin ML3600S is typically formulated as 100.0 wt% natural LLDPE powder with 0.03–0.10 wt% hindered phenolic antioxidant, 0.02–0.08 wt% phosphite processing stabilizer, and 0.02–0.05 wt% zinc stearate acid scavenger. If pigmentation is required, 0.5–1.5 wt% of a white PE-based concentrate that itself complies with 21 CFR 177.1520 and EU 10/2011 is used; carbon black is generally avoided in potable water interiors because additional migration test obligations under 21 CFR 178.3297 are introduced. The downstream process for vertical water storage tanks is carried out on shuttle-type biaxial rotational molding machines with cast or machined aluminum molds. Rotational speed ratio is normally maintained at 4:1 primary-to-secondary axis, with primary axis speeds of 8–12 min⁻¹ and secondary axis speeds of 2–3 min⁻¹ depending on mold swing diameter. Shot weight is calculated as surface area × target wall thickness × 0.936 g/cm³, with a 2–5% material allowance for parting line flash and access-port reinforcement. After charging and mold closure, the mold enters an oven set between 260°C and 290°C; the part reaches peak internal air temperature of 190–210°C, and the temperature is held for 5–8 min. Cooling begins with forced air at 20–30 m/s until the mold surface drops below 110°C, followed by a water mist at 1–2 L/min per mold channel until demold temperature of 70°C is reached. Production-scale experience on shuttle machines above 3.0 m swing diameter shows that non-uniform cooling from sidewall to top dome produces differential shrinkage; tooling with external cooling fins or localized air flow over the top dome is used to prevent wall thickness variation greater than ±1.0 mm. Terminal part types include 500–50,000 L vertical storage tanks, horizontal transport tanks, conical-bottom static tanks, and insulated potable water reservoirs with hollow double-wall construction.

    What Limits the Oven Residence Time for Agricultural Chemical Tanks?

    Agricultural chemical tanks operate under a different failure mode than potable water tanks because the structural wall is exposed to cyclic stress from internal hydraulic load and external UV radiation while the contained fluid may include surfactants, emulsifiable concentrates, and aqueous fertilizer salts. The relevant compliance framework includes EPA 40 CFR 264.175 for secondary containment of stored chemicals, UN Model Regulations 1H1 for liquid packaging when the tank is used for transport, and ASTM D1998-15 for rotationally molded polyethylene tanks with self-supporting vertical walls. A typical dry-blend formulation is 100.0 wt% ML3600S, 2.0–2.5 wt% carbon black masterbatch based on a 40 wt% carbon black concentrate yielding 0.8–1.0 wt% final carbon black, 0.25–0.50 wt% hindered amine light stabilizer masterbatch, and 0.10–0.20 wt% antioxidant masterbatch. The addition ratio of the carbon black masterbatch is constrained by UV protection requirements: below 2.0 wt%, long-term outdoor exposure can produce surface crazing; above 2.5 wt%, melt viscosity at peak internal air temperature can increase sufficiently to slow bubble removal and produce microvoids in 8–12 mm thick tank walls. Downstream processing of 10,000–30,000 L horizontal tanks typically uses a rock-and-roll machine that rotates a cylindrical mold on one axis while oscillating on the other, with oven set points of 280–300°C. Peak internal air temperature is held at 200–215°C for 5–10 min depending on wall thickness. Peak internal air temperature is measured with a Rotolog sensor or remote IR pyrometer; the oven set point alone does not control densification. Oven residence time is limited by oxidative degradation at the aluminum mold surface, not by incomplete densification; production-scale data show that extending peak internal air temperature beyond 215°C for more than 8 min can produce surface embrittlement and reduce ASTM D1693 ESCR below 200 h. The cooling step uses forced air at 15–25 m/s for the first 15–20 min, then water mist is introduced when mold temperature falls below 105°C to reduce cycle time without causing internal stress cracking at the filling port boss. Terminal products include 100–30,000 L sprayer tanks, nurse tanks for fertilizer injection, horizontal chemical storage tanks, and 1.1 m³ secondary containment basins.

    Industrial Bulk Containers Under Cyclic Load and Stacking Fatigue

    In manufacturing and logistics operations, rotomolded industrial bulk containers are used where fork truck impact, stacked storage, and repeated washdown create cyclic stress. The primary property is not chemical resistance but long-term creep resistance and corner thickness uniformity; ML3600S is selected for its high-flow densification in mold corners where wall thickness may be 1.5–2.0 times the nominal wall. The formulation for indoor service is 100.0 wt% ML3600S, 0.10–0.30 wt% antioxidant masterbatch, 0.5–2.0 wt% color concentrate, and 0.05–0.15 wt% internal release agent if the mold contains undercuts or textured surfaces. For outdoor exposure, 0.25–0.50 wt% HALS masterbatch is added. No harmonized global standard exists for all industrial bulk containers; load ratings are typically verified by static compression testing based on ISO 12048 for packaging compression and by user-specific stacking load tests when the container is mounted on a pallet base. EU reusable packaging obligations are addressed under Directive 94/62/EC. The downstream process uses a carousel-type rotational molding machine with 4 or 6 stations and fabricated steel or cast aluminum molds. Shot weight calculation includes a separate allowance for reinforced corners and fork pockets. Rotation ratio is 4:1, oven set point is 270–290°C, peak internal air temperature is 195–210°C, and cooling begins with forced air at 15–25 m/s until mold surface temperature drops to 110°C. Water mist is delayed until after that point to limit residual stress in thick bottom runners. Production-scale failure data on carousel machines indicate that blow holes at rib intersections occur when mold surface temperature at oven exit is below 260°C. Terminal products include 800–2,500 L pallet boxes, 225 L transport bins, insulated cold-chain containers, and material handling bins with integral fork pockets.

    When Flotation Collars Operate in Saturated, UV-Exposed Conditions

    In marine flotation bodies, simultaneous demands are placed on oxidative stability, impact toughness, and sealed-wall integrity because the part is continuously immersed, often encrusted with biofouling, and subjected to UV irradiation at the waterline. Compliance for marine flotation may involve US Coast Guard 33 CFR 183.114 for flotation material in recreational boats when the item is integrated into a vessel, and EU REACH restrictions on colorants and stabilizers. Published data for ML3600S in certified marine flotation structures is limited, so the material supplier’s standard oxidation induction time data and the molder’s pressure-decay test records become the principal acceptance documentation. The dry-blend formulation for black dock floats is 100.0 wt% ML3600S, 2.0–2.5 wt% carbon black masterbatch, 0.25–0.50 wt% HALS masterbatch, and 0.15–0.30 wt% antioxidant masterbatch. If color-coded buoys are required, the carbon black masterbatch is replaced by 0.5–2.0 wt% organic pigment dispersion plus 0.50–0.75 wt% UV absorber masterbatch; this substitution reduces long-term UV opacity and requires validation by weathering test according to ASTM D2565 for 2,000 h or a supplier-recognized equivalent. The production process for hollow flotation collars uses a biaxial shuttle machine with an offset arm to allow cylindrical parts up to 3.0 m in length. Mold rotation ratio is 4:1, with secondary axis reversal every 1–2 min to prevent resin accumulation at the ends. Oven set point is 260–280°C, peak internal air temperature is 195–210°C, and hold time at peak is 4–7 min. After cooling to below 70°C, each part is pressure-tested with air at 0.10–0.15 bar under water to detect pinholes; this test is more sensitive for rotomolded floats than visual inspection. Terminal products include 100–500 L dock floats, 300–1,000 mm diameter mooring buoys, navigation buoy shells, and polyethylene pontoons for floating walkways.

    For underground wastewater retention, long-term deformation from anisotropic soil backfill is more severe than above-ground storage because soil compaction after backfill produces a persistent load on the tank crown and sidewall ribs. The relevant installation and product standards are EN 12566-1:2016 for prefabricated septic tanks and IAPMO/ANSI Z1001 for prefabricated septic tank and sewage holding tank performance. The formulation for buried tanks is 100.0 wt% ML3600S, 2.0–2.5 wt% carbon black masterbatch, 0.10–0.25 wt% antioxidant masterbatch, and 0.10–0.20 wt% processing aid masterbatch. No biodegradable additives or recycled content are used because buried service demands a minimum ESCR of 500 h under ASTM D1693 condition C, and the presence of post-consumer recycled polyethylene can reduce ESCR by 30–60%. The rotomolding process for ribbed septic tanks uses a single-shot mold with external reinforcing ribs; the shot weight calculation must include the additional surface area of ribs, which can increase material usage by 15–25% over a smooth cylinder of equal volume. Oven set point is 280–300°C, peak internal air temperature is 200–215°C, and hold time at peak is 6–10 min. Cooling for buried tanks is deliberately slow: forced air only at 10–15 m/s until mold surface temperature falls below 90°C, then ambient air, with no water mist. This minimizes residual stress at rib intersections and reduces the risk of stress cracking during soil deflection. Terminal products include 1,000–20,000 L septic tanks, grease interceptors, underground cisterns with internal potable certification, and stormwater attenuation chambers.

    Rotational molding of recreational watercraft hulls exploits the narrow wall-thinning characteristics of high-flow LLDPE. Kayak and canoe hulls are produced in clamshell aluminum molds on shuttle or rock-and-roll machines; the process uses a two-shot or three-shot sequence to build a 3.0–5.5 mm hull wall and foam-filled lateral chambers. The dry-blend formulation for a UV-stabilized colored hull is 100.0 wt% ML3600S, 0.5–2.0 wt% PE-based color concentrate, 0.25–0.50 wt% HALS masterbatch, and 0.10–0.20 wt% antioxidant masterbatch. If the hull is unpigmented or light-colored, an additional 0.50–0.75 wt% UV absorber masterbatch is used because HALS alone is insufficient for waterline UV reflection at high-altitude or tropical solar irradiance. Compliance for recreational watercraft depends on the destination market; in the EU, Directive 2013/53/EU applies to recreational craft and personal watercraft, including construction requirements for small craft hulls and deck fittings. Published data for ML3600S in certified hull structures is limited, so hull qualification is based on mold pressure-decay testing, post-mold impact testing, and weathering according to ASTM D2565. The two-axis rotational molding machine uses a 4:1 or 5:1 rotation ratio; peak internal air temperature is 190–200°C and cycle time is 25–35 min. Cooling must be gradual; water mist is introduced only after mold surface drops below 100°C, and demolding occurs below 65°C. The long, narrow geometry of a kayak hull is sensitive to residual stress; production lines use removable internal support frames to prevent shrinkage bowing during cooling. Terminal products include sit-on-top kayak hulls, canoe shells, and small one-piece tender hulls.

    Free Quote

    Competitive Braskem ML3600S Rotational Molding Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem ML3600S is a rotational molding linear low density polyethylene powder with a nominal density of 0.936 g/cm³ determined by ASTM D1505 and a melt flow rate of 4.0 g/10 min at 190 °C under a 2.16 kg load, measured per ASTM D1238 and ISO 1133-1:2022 procedure A. The grade is positioned for single-layer rotomolded parts produced on carousel, shuttle, rock-and-roll, and open-flame machines where the shear environment is low and densification depends on oven residence time rather than screw plastication. Its density places it between conventional low-density rotomolding resins near 0.920–0.925 g/cm³ and medium-density products above 0.940 g/cm³. Producer technical literature controls lot-to-lot melt flow rate variability within ±0.5 g/10 min. The powder is ground to a nominal top size of 500 µm (35 mesh), with ≥90 wt% passing a 35 mesh screen. Bulk density is typically 0.45–0.55 g/cm³ depending on particle-size distribution and milling conditions. The principal applications are large storage tanks, agricultural spray components, water-treatment vessels, marine floats, and material-handling containers requiring stress-crack resistance and uniform wall-thickness control.

    How Does ML3600S Differ from Medium-Density and High-Density Rotomolding Polyethylene?

    The key difference is density-dependent property trade-off. At 0.936 g/cm³, ML3600S shows lower flexural modulus than a 0.945–0.950 g/cm³ medium-density rotomolding grade but higher environmental stress crack resistance and lower-temperature ductility. A comparable HDPE rotomolding grade with a density of 0.950 g/cm³ may exhibit a flexural modulus of 900–1,100 MPa under ASTM D790 Method I; ML3600S is reported at 550–650 MPa. The lower modulus reduces top-load capacity of crates by roughly 15% under ASTM D642, but the same density shift increases ASTM D1693 environmental stress crack resistance beyond 1,000 h in 100% Igepal CO-630 at 50 °C. High-density grades may fail the same test at 50–200 h under identical conditions. Compared with low-density rotomolding grades at 0.920–0.925 g/cm³, ML3600S provides higher stiffness and chemical resistance while retaining sufficient flow for complex mold geometries. The melt flow rate of 4.0 g/10 min is higher than many pipe or blow molding LLDPE grades but is matched to rotomolding ovens where peak internal air temperature is 260–290 °C.

    Agricultural chemical tanks with capacities between 5,000 L and 20,000 L are produced from ML3600S when the stored fluid requires resistance to concentrated fertilizer solutions or dilute acids. Chemical resistance is evaluated by immersion testing at 23 °C and 60 °C for 90 days, with retained tensile elongation above 75% as an acceptance criterion. Stress crack resistance under ASTM D1693 Condition C is used as a screening method for long-term environmental exposure. On carousel equipment with a 3.2:1 mold rotation ratio, a 12,000 L vertical storage tank can reach a nominal wall thickness of 6–8 mm after 28–32 min oven residence at 288 °C internal air temperature; published data for this specific part configuration is limited, so molders should confirm wall-thickness distribution by ultrasonic measurement at the top, sidewall, and bottom knuckle radius. The powder’s dry-flow properties and particle-size distribution must be verified after each regrind addition because fines below 150 µm can accumulate and reduce powder flow.

    Thermo-oxidative stability and the upper oven residence time boundary.

    Thermo-oxidative stability is evaluated by oxidation induction time at 200 °C under oxygen flow of 50 mL/min using ASTM D3895. Rotomolding polyethylenes in this class generally exhibit an OIT greater than 30 min when stabilized with a hindered phenolic and phosphite package. The upper oven residence time for ML3600S should be limited to 35 min at an internal air temperature of 290 °C to avoid surface yellowing and a drop in notched Izod impact below 200 J/m at 23 °C. Degradation is accelerated when mold release agents containing silicones or fluoropolymers are applied at excessive film thickness; maximum recommended dry-film thickness is 5–10 µm to avoid surface defects and loss of inter-particle cohesion. Internal air temperatures above 315 °C cause surface oxidation and gas bubble formation at the demold line. When a part requires extended weathering, UV stabilization can be specified and evaluated under ASTM G154 Cycle 1 with UVA-340 lamps; yellowing index after 1,000 h is typically below 10 units per ASTM E313 for stabilized formulations.

    Dry-flow characteristics of the powder are measured using ASTM D1895 apparent density and a 35 mesh sieve analysis. The producer control range for melt flow rate is specified at 3.5–4.5 g/10 min; powders at the upper end of this range densify faster at low oven temperatures but may develop thicker bottom-wall sections on rock-and-roll machines if major-axis mold speed is below 4 rpm. Particle size distribution influences bubble removal; particles coarser than 500 µm at levels above 10 wt% tend to produce pinholes at wall thicknesses below 4 mm. The powder is formulated with internal mold release and, where specified, UV stabilizers. Moisture uptake above 0.02 wt% in the powder can create steam porosity at oven temperatures above 260 °C; pre-drying at 60 °C for 2 h is recommended when relative humidity exceeds 60%. Anti-static surface treatment is not required if the molding area relative humidity remains above 35%; below that level, static charge can cause uneven powder flow and surface defects.

    Mechanical Property Profile Across ASTM Test Specimens

    Nominal property profile reported for Braskem ML3600S
    PropertyTest standardNominal value
    DensityASTM D15050.936 g/cm³
    Melt flow rateASTM D1238, 190 °C/2.16 kg4.0 g/10 min
    Flexural modulus, 1% secantASTM D790 Method I550–650 MPa
    Tensile yield strengthASTM D63813–15 MPa
    Tensile elongation at breakASTM D638>600%
    Notched Izod impact at 23 °CASTM D256No break
    Low-temperature brittlenessASTM D746< -76 °C
    Environmental stress crack resistanceASTM D1693 Condition B, 100% Igepal, 50 °C>1,000 h

    Cooling rate after oven discharge affects shrinkage and warpage more than oven temperature for ML3600S. At a cooling rate of 5 °C/min in forced air, linear mold shrinkage measured per ASTM D955 is generally 2.0–2.5%; at 15 °C/min water spray, shrinkage declines to 1.5–2.0% because the crystalline fraction is lower. Uneven cooling across thick corners and thin walls produces residual stress that distorts flat lids by more than 2 mm per 500 mm span. To control distortion, tooling should maintain wall thickness variation below ±0.5 mm on the parting line and cooling should be staged with 5 min ambient air before water mist. The lower density relative to HDPE rotomolding resins reduces stress-whitening in drop impacts but lowers top-load compression strength by approximately 15% under ASTM D642 when compared with a 0.950 g/cm³ material.

    When a 4.0 g/10 min Melt Flow Rate Constrains Wall Thickness Uniformity

    When a melt flow rate of 4.0 g/10 min is selected, the relationship between mold rotation speed and wall-thickness distribution becomes non-linear at low shear. On a shuttle machine with a 2.4 m spherical mold rotating at 6 rpm major axis and 1.5 rpm minor axis, the powder pool travels over the internal surface and deposits layers in a sequence controlled by local temperature. Sections with internal air stagnation above 300 °C show accelerated coalescence, while deep ribs below 240 °C remain under-sintered. The recommended internal air temperature for ML3600S is 260–290 °C, with a peak metal temperature of 250–270 °C. At wall thicknesses below 3 mm, the 4.0 g/10 min flow may not supply sufficient melt to thin sections after the powder pool has depleted, causing pinholing. The addition of 5–10 wt% regrind of the same resin is allowed, but particle size distribution must be re-verified to maintain ≥90 wt% passing 35 mesh.

    Pulverization of ML3600S pellets to rotomolding powder is performed on high-intensity disk mills with air classification. Milling equipment with 60 cm disk diameter and 3,600 rpm rotor speed produces 250–350 kg/h throughput at 35 mesh top size; die temperature is kept below 90 °C to prevent particle agglomeration and additive degradation. The powder’s melt flow rate may increase by 0.1–0.3 g/10 min during pulverization due to chain scission under shear heating. Rotational molders using pulsed-air powder delivery systems report bridging in hoppers when the powder contains more than 5 wt% fines below 100 mesh (150 µm). Field data indicate that batch-to-batch variation in dry-flow rate is below 10% when the powder is stored in sealed containers at ambient temperature.

    Which industrial applications require the ESCR advantage of ML3600S?

    The largest volume applications are horizontal storage tanks, cylindrical agricultural spray tanks, and marine floats. In these parts, the accepted pass criterion for environmental stress crack resistance is no failure after 1,000 h exposure to 10% Igepal CO-630 at 50 °C under ASTM D1693 Condition B. The grade is also used for water-treatment vessels where oxidant residuals such as sodium hypochlorite at 10–15 ppm free chlorine are present. Published data for this specific configuration is limited for long-term exposure above 40 °C; chlorinated water at elevated temperature can accelerate surface oxidation and reduce tensile elongation after 3,000 h immersion. For food-contact use, the unmodified resin may be evaluated under 21 CFR 177.1520(c) for olefin polymers, subject to extractive limits in that paragraph. Finished articles intended for European markets must be tested under EU 10/2011 migration conditions for the specific food simulant and contact duration.

    At wall thicknesses above 12 mm, the low thermal conductivity of polyethylene increases cooling time and may produce internal voids. Internal air cooling at 0.5–1.0 m³/min during cooling is required for parts thicker than 10 mm to reduce cycle time and control shrinkage. ML3600S has been used for 15 mm thick dock floats on rock-and-roll machines with 45 min total cycle time; published data for this specific configuration is limited. Warpage of flat tank baffles after demolding is minimized by cooling in a fixture for 10 min at 20 °C before handling.

    Top