| HS Code | 121054 |
| Density | 0.924 g/cm³ |
| Melt Index 190 C 2 16 Kg | 20 g/10 min |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 12.4 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 241 MPa |
| Vicat Softening Point | 90 °C |
| Melting Point | 120 °C |
| Hardness Shore D | 50 |
| Mold Shrinkage | 1.5-2.0% |
| Brittleness Temperature | < -70 °C |
As an accredited Braskem ML2400N LLDPE Injection Molding Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem ML2400N LLDPE Injection Molding Polyethylene is supplied in 25 kg polyethylene bags, palletized, stretch-wrapped, and labeled for shipment. |
| Container Loading (20′ FCL) | Braskem ML2400N LLDPE Injection Molding Polyethylene: 25 kg bags on pallets in a 20′ FCL, approximately 16.5 MT net. |
| Shipping | Braskem ML2400N LLDPE ships as non-hazardous polyethylene resin pellets in moisture-barrier 25 kg bags, stretch-wrapped pallets, or bulk trucks/railcars. Store in cool, dry, ventilated areas away from sunlight, heat, moisture, and contaminants. Handle with clean equipment; no special DOT shipping labels required. Protect packaging from punctures and weather during transport. |
| Storage | Store Braskem ML2400N LLDPE in a cool, dry, well-ventilated area, preferably in original sealed bags or containers. Protect from direct sunlight, moisture, heat, and ignition sources. Keep away from strong oxidizers and contaminants. Avoid excessive stacking and follow first-in, first-out stock rotation. Maintain clean handling to prevent dust and pellet loss. |
| Shelf Life | Braskem ML2400N LLDPE has indefinite shelf life when stored cool, dry, sealed, away from sunlight, moisture, and UV exposure. |
Braskem ML2400N, a linear low-density polyethylene with nominal melt flow rate 24 g/10 min at 190°C/2.16 kg per ASTM D1238 or ISO 1133-1:2022 and nominal density 0.924 g/cm³ per ASTM D792, is processed on thin-wall injection molding lines for dairy tubs and snap-on lids where flow length-to-wall thickness ratios exceed 180:1. The low melt viscosity in the shear-rate regime above 1,000 s⁻¹ permits filling of wall sections from 0.6 mm to 0.9 mm without exceeding injection pressure limits on hydraulic machines rated at 1,800 kN to 3,500 kN. A general-purpose polyolefin screw with 20:1 to 24:1 L/D ratio and compression ratio of 2.5:1 to 3.0:1 is used; back pressure is limited to 4 MPa to 8 MPa to avoid excessive shear heating, and decompression after plastication is set at 3 mm to 5 mm to prevent drool from valve-gated hot runners. Barrel zones are set from 180°C at the feed throat to 230°C at the nozzle, while mold coolant maintained at 12°C to 25°C controls post-mold warpage in oval and rectangular tubs. Injection velocity is set between 90 mm/s and 140 mm/s, with a short-shot-to-flash processing window requiring hold pressure between 40 MPa and 65 MPa and hold time not exceeding 1.2 s in hot-runner valve-gated tools. For food-contact formulations, the neat resin is dry-blended with a polyolefin-based color masterbatch and, where automated de-nesting requires surface slip, 800 ppm to 1,200 ppm erucamide slip and 1,500 ppm to 2,500 ppm synthetic silica antiblock are added through carrier-compatible masterbatches. Although neat LLDPE does not require predrying, hopper drying at 60°C to 80°C for 2 h is recommended when storage relative humidity exceeds 60% to prevent splay from surface moisture. When lot-to-lot melt flow variation of ±1 g/10 min is observed, hold pressure is trimmed within ±5 MPa to retain short-shot-to-flash balance. Compliance with FDA 21 CFR 177.1520 and EU 10/2011 requires total migration below 10 mg/dm² in food simulants; published data for the exact masterbatch combination on this specific grade is limited, so lot-specific migration testing is required before qualifying a colored dairy lid. The terminal articles are 500 mL to 1,000 mL dairy tubs and flexible snap-on lids produced at cycle times of 6 s to 9 s in multi-cavity tools; typical reject modes include gate blush, flow hesitation at the attached-lid hinge, and warp from unbalanced cooling in stack molds.
Injection-molded child-resistant dispensing closures molded from ML2400N rely on controlled post-mold crystallization to preserve dimensional tolerances in the ratchet and spring elements. The resin’s nominal density of 0.924 g/cm³ produces a semi-crystalline matrix with a broad melting peak; when the tool is run at 18°C to 28°C, cooling rates in wall sections from 1.2 mm to 2.0 mm create a crystallinity gradient that affects both hoop stiffness and environmental stress crack resistance. For closures requiring repeated engagement and disengagement, formulation adjustment commonly includes 300 ppm to 600 ppm of a high-molecular-weight silicone processing aid to reduce gate blush and improve fill in the interrupted thread sections without reducing coefficient of friction sufficiently to allow back-off under vibration. Erucamide content is kept at or below 500 ppm to limit excessive slip on the tamper-evident band; if static charge accumulation occurs during automated assembly, 0.5 wt% to 1.5 wt% of an antistatic masterbatch based on glycerol monostearate is added. Process conditions on a 1,200 kN toggle-clamp injection machine with a 16-cavity cold-runner mold typically use barrel temperatures from 190°C to 220°C, injection velocity 60 mm/s to 100 mm/s, and hold pressure 35 MPa to 50 MPa; clamp force per cavity is maintained at 75 kN to 100 kN to avoid flash. Excessive hold pressure above 55 MPa increases molded-in stress in the ratchet root, producing stress whitening and loss of engagement force after fewer than 50 cycles. Compliance for closures used in pharmaceutical and personal-care packaging requires FDA 21 CFR 177.1520, EU 10/2011, and USP <661.1> plastic packaging suitability; when the closure is paired with a PET or PP bottle, torque retention is evaluated under ISTA 6-style package testing rather than by a single ASTM method. Published data for this specific unfilled ML2400N configuration in child-resistant geometries is limited, but the relevant mechanical aging failure modes are dominated by environmental stress cracking rather than simple creep.
Block-style toy components injection-molded from ML2400N are typically produced in multi-cavity cold-runner tools where the part mass is below 15 g and wall stock ranges from 1.5 mm to 4.0 mm. The grade’s narrow molecular weight distribution supports fast crystallization and short cooling times, but also raises the risk of sink marks over thick bosses used for interlocking studs; tooling therefore specifies a minimum radius of 0.5 mm at the boss base and uses conformal cooling channels where the part exceeds 3.0 mm. Formulations for toy applications include a heavy-metal-free organic or inorganic color concentrate at 1 wt% to 4 wt%; for soft-touch overmolded parts, a styrenic block copolymer TPE is used in a two-shot process, but ML2400N remains the rigid substrate. Melt temperature is held between 190°C and 215°C to avoid thermal degradation that can produce odor and extractable low-molecular-weight species; injection speed is reduced in thick transitions to prevent jetting, with a velocity profile starting at 40 mm/s and ramping to 80 mm/s. Compliance is governed by ASTM F963, EN 71-3:2019+A1:2021, and REACH Annex XVII; the low-density LLDPE matrix does not require plasticizers, and migration of the restricted elements under EN 71-3 remains below the specified limits when tested on a representative toy component. Dimensional stability is measured in accordance with ASTM D790 flexural modulus and ASTM D256 notched Izod impact; typical LLDPE of 0.924 g/cm³ density exhibits no-break Izod behavior at 23°C, while notched impact remains above 300 J/m at -20°C. Production-scale observations indicate that color masterbatch loading above 5 wt% can reduce melt-flow consistency and produce flow lines around the interlocking studs on an 8-cavity family mold. The terminal articles are construction blocks, toy food items, and nesting play sets, where ESCR against saliva, soap, and detergent contact is maintained because the grade’s comonomer distribution provides tie-molecule density. Published data for the exact ML2400N masterbatch blend in toy geometries is limited.
Houseware storage bins with integrally molded living hinges and latching tabs made from ML2400N are evaluated for impact after conditioning at -20°C for 24 h and for environmental stress cracking after exposure to common household cleaners. The resin’s low-temperature toughness arises from the linear low-density chain architecture; notched Izod impact per ASTM D256 typically remains above 300 J/m at -20°C, while ESCR per ASTM D1693 Condition B (10% Igepal CO-630, 50°C) generally exceeds 500 h at F50 failure for molded samples in this density range. Processing conditions for a 2,000 kN hydraulic machine running a 2-cavity stack mold with a 2.5 mm nominal wall require barrel temperatures from 170°C to 210°C, a mold temperature of 15°C to 30°C, and an injection velocity profile that starts at 100 mm/s through the hinge region and tapers to 50 mm/s before switch-over at 95% fill. Because the integral hinge is flexed during demolding, mold-open sequencing and ejector stroke are set to avoid over-bending beyond 90 degrees; production failures at the hinge typically appear as stress whitening after fewer than 1,000 flex cycles when the melt temperature is below 180°C and the polymer is not fully relaxed. Formulation includes 0.5 wt% to 1.0 wt% of a nucleating masterbatch based on a polyolefin carrier with a sorbitol-free nucleator to refine spherulite size in the thick latch area; antistatic additive at 1.0 wt% to 2.0 wt% prevents dust accumulation on transparent smoked-tint bins. Compliance for direct food storage applications requires FDA 21 CFR 177.1520 olefin polymer clearance and, for products sold into the EU, EU 10/2011 overall migration testing in 3% acetic acid, 10% ethanol, and olive oil simulants. The terminal articles are stackable storage containers with external latch hinges and modular drawer units; the main limitation is not tensile strength but long-term ESCR in the presence of glycol ether cleaners, and published data for this exact molded-bin configuration is limited.
Non-sterile medical waste containment components such as rigid sharps containers and secondary packaging for diagnostics are injection-molded from ML2400N where puncture resistance, chemical compatibility, and low-temperature ductility are required. The neat resin is processed in a 1,200 kN to 2,500 kN injection molding machine with a heated nozzle bushing and a 2-cavity or 4-cavity mold; barrel temperatures are set between 185°C and 220°C, and the tool is cooled to 15°C to 25°C. For sharps containers, the critical wall section is the base and lid locking rim where thickness exceeds 3.0 mm; pack-and-hold pressure of 50 MPa to 70 MPa for 6 s to 12 s is used to prevent sink and internal voids that would compromise puncture resistance. Formulation modifications consist of a color concentrate at 1 wt% to 2 wt% and, where required by transportation regulations, a UV stabilizer masterbatch at 0.5 wt% to 1.0 wt% using a hindered amine light stabilizer; the polyethylene matrix does not require plasticizer, and extractable leachables are minimized by avoiding slip additives in the base formulation. Compliance is evaluated under ISO 23907-1:2019 for sharps injury protection, with puncture resistance in the base and side walls tested after conditioning at 23°C; no universal ASTM standard is imposed for non-patient-contact plastic waste containers, but FDA 21 CFR 177.1520 may be invoked if the container is used to package regulated medical devices. Dimensional stability is tested via ASTM D648 heat deflection temperature under 0.45 MPa load; the LLDPE grade has a relatively low HDT compared to polypropylene, so maximum service temperature in stacked storage is limited to 50°C unless additional annealing is performed. Production-scale handling has shown that excessive barrel residence time above 5 min at 220°C causes yellowing and generation of peroxide species that can create an odor nonconformity in closed-container packaging. The terminal articles are puncture-resistant sharps containers, clinic waste bins, and non-sterile device secondary packaging; published data for the specific ML2400N formulation in ISO 23907-1 puncture configurations is limited and must be established by lot release testing.
Distribution lids for plastic pails and drums are injection-molded from ML2400N when the end-use duty includes stacked warehouse storage at variable temperatures and occasional contact with mineral oil, diesel fuel, or dilute detergent. The grade’s ESCR resistance under ASTM D1693 Condition A (100% Igepal CO-630, 50°C) typically exceeds 1,000 h for molded plaques of 2 mm thickness, but the actual molded lid stress state depends on the gate design and the orientation of the gasket groove. A 2-cavity or 4-cavity tool with a diaphragm gate in the lid center is preferred over edge gating to produce radial flow that minimizes weld lines at the gasket retention bead. Melt temperatures are run at 200°C to 230°C, with mold temperature held at 15°C to 25°C; injection velocity is set at 120 mm/s to 160 mm/s, and the pack-and-hold phase uses 45 MPa to 60 MPa for 5 s to 10 s to densify the gasket groove. Formulation for industrial lids often includes 2 wt% to 4 wt% of a high-density polyethylene or polypropylene carrier-based color masterbatch and 0.2 wt% to 0.5 wt% of an external lubricant such as calcium stearate to aid part ejection from a textured tool surface; no slip additive is used in the food-grade version to preserve gasket adhesion. Uncontrolled peroxide masterbatch addition must be avoided in this application because polyethylene can crosslink or generate gel specks during melt processing; any flow modification should be performed only in a controlled compounding step with off-line testing. Compliance is governed by FDA 21 CFR 177.1520 for food-grade pail lids and by REACH and RoHS for industrial packaging; when the lid is used for UN-rated hazmat packaging, closure performance is evaluated under 49 CFR 178.606 stacking load and leakproofness after drop. The operational boundary is a maximum continuous service temperature of 50°C; at 70°C stacking load above 80 kg can cause creep-induced dishing and loss of gasket compression. Published data for the specific ML2400N grade in molded lid geometries under stack load is limited, but the failure mode is well characterized as slow crack growth across the gasket groove weld line.
Competitive Braskem ML2400N LLDPE Injection Molding Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem ML2400N is an injection-molding grade of linear low-density polyethylene supplied as pelletized feedstock for thermoplastic conversion. The material is specified by a nominal melt flow rate of 24 g/10 min measured under ISO 1133-1:2022 at 190°C/2.16 kg and a nominal density of 0.924 g/cm³ measured under ISO 1183-1:2019. These values define the primary processing and stiffness envelope: the high melt flow rate supports thin-wall filling and reduced injection pressures, while the density below 0.930 g/cm³ places the grade in the low-to-intermediate crystallinity region of polyethylene. Tensile yield strength, elongation at break, flexural modulus, and notched Izod impact are typically determined according to ISO 527-2, ISO 178, and ISO 180/A; current batch-specific acceptance limits should be retrieved from the supplier’s technical datasheet because final values vary with additive package and conversion conditions.
The linear polyethylene backbone with short-chain branching gives a shear-thinning rheology that is useful in multi-cavity injection tools. At injection shear rates, the viscosity decreases with increasing shear rate, reducing viscous heating in hot runners and permitting lower melt temperatures than higher-viscosity linear resins of lower melt flow rate. Because linear low-density polyethylene is not hygroscopic, pre-drying is not routinely required; however, surface condensation on cold pellets transferred into a warm production hall can introduce splay or surface defects. Incoming inspection should therefore verify melt flow rate, density, and visual pellet condition against the supplier’s certificate of analysis.
Low-density polyethylene injection grades produced by high-pressure free-radical polymerization commonly have densities in the range of 0.918–0.922 g/cm³ and contain long-chain branching that reduces crystallinity, flexural modulus, and tensile strength. High-density polyethylene injection grades with densities of 0.950–0.960 g/cm³ provide higher rigidity, top-load strength, and heat resistance, but often require elevated melt temperatures and can show lower environmental stress crack resistance at equivalent melt flow. ML2400N at 0.924 g/cm³ occupies an intermediate position. The linear low-density structure offers a combination of ductility, low-temperature impact resistance, and processability that is difficult to obtain with either LDPE or HDPE in thin-wall, high-cavitation tools.
| Parameter | ML2400N typical target | LDPE injection family | HDPE injection family | Test method |
|---|---|---|---|---|
| Density | 0.924 g/cm³ | 0.918–0.922 g/cm³ | 0.950–0.960 g/cm³ | ISO 1183-1 |
| Melt flow rate | 24 g/10 min | 20–30 g/10 min | 10–40 g/10 min | ISO 1133-1 |
| Tensile yield strength | 10–12 MPa | 8–10 MPa | 20–30 MPa | ISO 527-2 |
| Flexural modulus | 250–300 MPa | 150–250 MPa | 900–1,300 MPa | ISO 178 |
| Low-temperature notched Izod | ductile; datasheet-dependent | ductile | partially ductile to brittle | ISO 180/A |
The values in the table are screening comparisons for commercial injection-molding polyethylene families. ML2400N batch-specific values must be verified against the current Braskem technical datasheet. Compared with LDPE injection grades of similar melt flow, ML2400N generally exhibits higher tensile yield and flexural modulus because the linear backbone permits tighter chain packing and higher crystallinity. Compared with HDPE injection grades, the lower density reduces rigidity and heat resistance but improves ductility and can lower internal stress in shallow parts. The high melt flow rate can reduce injection pressure and clamp tonnage in multi-cavity tools, but it may also increase the tendency to flash at worn parting lines or in tools with inadequate clamping force.
On production injection molding lines, the process window is established on the actual machine and tool because published data for ML2400N-specific flow-length ratios is limited. A conventional reciprocating-screw machine with a general-purpose polyolefin screw of 20:1–24:1 L/D and a compression ratio of 2.5:1–3.5:1 is generally suitable. The melt temperature window is commonly 200–230°C; the melt stream should not be held above 250°C for extended residence times because oxidative chain scission can generate yellowing and loss of mechanical properties. Mold temperatures of 10–30°C are used for fast cycle times in thin-wall packaging and housewares, while mold temperatures of 30–50°C improve surface finish, weld-line strength, and dimensional stability in thicker technical parts.
Injection and holding pressures typically fall within 350–450 bar for thin-wall parts. For a tool with a total projected area of 600 cm², clamp-force requirement would be approximately 210–270 kN plus a safety margin; actual values must account for runner and gate projected area, cavity imbalance, and pack pressure decay. The high melt flow of ML2400N can permit shorter holding time, but packing must remain sufficient to minimize sink marks and post-mold shrinkage. Hot runner systems with valve gates are commonly used in high-cavitation lids and closures; hot runner manifold temperatures are normally maintained within the same 200–230°C range to avoid local degradation during production interruptions.
Mold shrinkage data are geometry-dependent and should be established on the production tool or by using ISO 294-3 test plaques. Generic LLDPE injection grades may exhibit linear mold shrinkage in the range of 1.5–2.5% depending on wall thickness, mold temperature, packing pressure, and flow direction. Warpage is controlled by balancing gate locations, cooling layout, and pack time rather than by melt temperature alone. Because ML2400N has a lower flexural modulus than HDPE, parts may show reduced warpage in shallow geometries but also lower top-load retention in deep, load-bearing containers.
Environmental stress crack resistance is commonly screened by ASTM D1693 using notched specimens in 10% Igepal CO-630 at 50°C. Linear low-density polyethylene grades of similar density typically show extended failure times, but ML2400N-specific values should be obtained from the supplier. The material is not intended for pressure-pipe applications, blow molding, or film extrusion, where molecular weight distribution and melt strength requirements differ from injection molding grades.
Braskem ML2400N is an olefin polymer that may be assessed for food contact under FDA 21 CFR 177.1520 and European Commission Regulation (EU) No 10/2011, subject to the specific additive package and applicable migration limits. Compliance is not self-certifying by the raw material alone; the finished article manufacturer must verify overall migration, specific migration, and organoleptic properties under migration test methods such as EN 1186-1 or ISO 1186-1. Documentation should also confirm compliance with REACH Regulation (EC) No 1907/2006, RoHS Directive 2011/65/EU for restricted heavy metals, and applicable packaging heavy-metal requirements.
| Regulation or standard | Scope | Required action |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers for food contact | Obtain grade-specific compliance letter from supplier |
| (EU) No 10/2011 | Plastic materials and articles intended for food contact | Migration testing on final article; confirm additive compliance |
| REACH | Registration, evaluation, authorization, and restriction of chemicals | Supplier confirmation of SVHC status |
| RoHS 2011/65/EU | Restricted heavy metals and brominated flame retardants | Verify lead, mercury, cadmium, hexavalent chromium, PBB, PBDE |
| CONEG model legislation | Packaging heavy-metal limits | Confirm total lead, cadmium, mercury, and chromium by summing system |
Outdoor exposure and weathering are not inherent properties of unpigmented linear low-density polyethylene. UV stabilization packages are required for exterior housewares, recreational parts, or long-term outdoor service. If the grade is used in cold-chain applications, low-temperature ductility is advantageous compared with many HDPE injection grades, but constant-load creep and top-load retention are lower. Published data for ML2400N under long-term hydrostatic or creep conditions is limited; design calculations should use creep modulus curves obtained from the supplier for the specific temperature, stress, and service environment. Typical conversion applications include thin-wall housewares, food containers, lids, caps, closures, appliance housings, and toys where high flow, short cycle time, and moderate stiffness are required.