Braskem Lq 0518 21 Af Lldpe Blown Film Extrusion Polyethylene

Braskem LQ 0518/21 AF LLDPE Blown Film Extrusion Polyethylene

    • Product Name: Braskem LQ 0518/21 AF LLDPE Blown Film Extrusion Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 212243
    Product Name Braskem LQ 0518/21 AF LLDPE Blown Film Extrusion Polyethylene
    Manufacturer Braskem
    Grade LQ 0518/21 AF
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 0.5 g/10 min
    Melt Flow Rate 190 C 2 16 Kg 0.5 g/10 min
    Processing Method Blown Film Extrusion
    Additive Anti-fog
    Melting Point 121 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield Md 10 MPa
    Tensile Strength At Yield Td 10 MPa
    Tensile Strength At Break Md 30 MPa
    Tensile Strength At Break Td 25 MPa
    Elongation At Break Md 600 %
    Elongation At Break Td 700 %
    Dart Drop Impact 100 g
    Elmendorf Tear Md 200 g
    Elmendorf Tear Td 300 g
    Haze 12 %
    Gloss 60 70
    Film Thickness Range 25-100 µm
    Form Pellets
    Color Natural
    Packaging 25 kg bags
    Storage Conditions Dry, away from direct sunlight

    As an accredited Braskem LQ 0518/21 AF LLDPE Blown Film Extrusion Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LQ 0518/21 AF LLDPE is packaged in 25 kg polyethylene bags, palletized and stretch-wrapped for blown film extrusion.
    Container Loading (20′ FCL) 20′ FCL loaded with Braskem LQ 0518/21 AF LLDPE blown film extrusion polyethylene, palletized 25 kg bags, dry container, secured for ocean transport.
    Shipping Non-hazardous LLDPE resin pellets, Braskem LQ 0518/21 AF, for blown film extrusion. Packaged in 25 kg PE bags, palletized and stretch-wrapped, or bulk containers. Ship by truck/rail/container in dry, clean, ambient conditions, avoiding moisture, direct sunlight, and excessive heat. No special dangerous goods classification.
    Storage Store Braskem LQ 0518/21 AF LLDPE in a cool, dry, ventilated area away from sunlight, heat, ignition, and oxidizers. Keep original containers closed, clean, dry, labeled, on pallets. Avoid moisture, contamination, excessive stacking, and outdoor exposure. Do not expose to direct UV or temperatures that may soften or degrade resin. Use FIFO rotation; follow manufacturer SDS and local rules.
    Shelf Life 12 months from production date when stored in original, unopened packaging under dry, cool, ventilated conditions away from direct sunlight.
    Application of Braskem LQ 0518/21 AF LLDPE Blown Film Extrusion Polyethylene

    Heavy-Gauge Industrial Liner Film Is Run Without Post-Consumer Recyclate Dilution

    In monolayer blown film lines producing heavy-duty industrial liners, LQ 0518/21 AF is processed with a nominal melt flow rate of 2.1 g/10 min under ASTM D1238-20 at 190 °C/2.16 kg and a density of 0.918 g/cm³ under ASTM D792-20. The resin is run on grooved-feed extruders with screw diameters of 45 mm to 65 mm and 30:1 L/D ratios. Barrel temperature profiles are held from 180 °C to 205 °C, while the die head is maintained at 210 °C to 220 °C. Die gaps between 1.6 mm and 2.0 mm are selected for melt distribution at output rates up to 140 kg/h on a 150 mm annular die. The blow-up ratio is set at 2.2:1 to 2.6:1, and the frost line is controlled at 500 mm to 700 mm above the die face. Internal bubble cooling with chilled air at 12 °C to 16 °C is used to prevent draw resonance at gauge below 50 µm. The resulting liner film at 80 µm to 150 µm is fabricated into sacks for mineral fillers, regrind collection bags, and heavy-gauge waste liners. Dart impact resistance is evaluated under ASTM D1709-16a Method A; industrial liner procurement specifications often set a minimum of 300 g at 100 µm, but published data for this exact grade under the end-use formulation should be generated on the target line. Elmendorf tear propagation is measured with ISO 6383-2:1983; MD/TD tear imbalance is adjusted by raising or lowering the frost line within the specified band. Food contact inner liners are only accepted when the total migration into simulant does not exceed 10 mg/dm² under EU Regulation (EC) No 10/2011 and when the resin is covered as an olefin polymer under FDA 21 CFR 177.1520(c). Operational boundaries include die lip build-up from low-molecular-weight species when line speeds exceed 12 m/min for more than 8 h; purging at the die lip is required at the shift interval. Combinations with antibiotic or antistatic masterbatches exceeding 0.5 wt% are not recommended without first verifying organoleptic neutrality for liner contact with packaged industrial powders.

    Greenhouse tunnel and low-tunnel cover film service depends on the anti-fog (AF) additive package to shift surface condensate from discrete droplets to a continuous water layer. The film is commonly built as a three-layer coextrusion with the inner anti-fog skin containing LQ 0518/21 AF at 60–70 wt%, an ethylene-vinyl acetate copolymer at 20–30 wt%, and a UV stabiliser masterbatch at 4–8 wt% depending on the regional UV index. The anti-fog layer is usually 20–25% of total thickness and is positioned on the interior side of the tunnel. Total film thickness for multi-season covers is set from 150 µm to 200 µm. Blow-up ratio is maintained at 2.0:1 to 2.5:1, and the die gap is reduced to 1.4 mm to 1.8 mm to raise transverse orientation and reduce haze. Contact-angle performance is assessed after 1,000 h of accelerated weathering under ISO 4892-2:2013 cycle A; a sessile water contact angle below 40° is accepted for anti-fog operation in condensation-prone climates. Haze and light transmission are measured under ASTM D1003-13; transmission of photosynthetically active radiation must remain above 85% for tomato and lettuce forcing, but published data for this specific multi-layer construction must be confirmed on the production line because additive migration kinetics in polyethylene matrices change with layer thickness and core composition. The tensile properties of the aged film are evaluated under ISO 527-3:2018; a retained MD elongation above 300% after 5,000 h of xenon arc exposure is a recognised durability threshold, though site-specific testing is required. The terminal articles are greenhouse tunnel covers, shade-adjacent side curtains, and low-tunnel cloches for vegetable nurseries. Compliance with REACH and the absence of intentionally added per- and polyfluoroalkyl substances must be documented by the converter. The processing boundary is defined by the thermal sensitivity of the EVA blend component; barrel temperatures above 215 °C cause acetic acid evolution and bubble instability on long runs. Gravimetric feeding of the UV masterbatch is preferred to volumetric screw feeding to keep lot-to-lot variation of the HALS package below ±0.15 wt%.

    How Does Blown Film Orientation Affect Puncture Propagation in Frozen Vegetable Packaging?

    For freezer packaging, this C4-LLDPE resin is selected because the 0.918 g/cm³ density class and narrow crystalline melting range reduce stiffness build-up at deep-freeze conditions. Film converted at 50 µm to 75 µm is run at a blow-up ratio of 2.8:1 to 3.2:1 and a frost line height of 600 mm to 800 mm to shift orientation toward the transverse direction and compensate for the low MD tear resistance typical of linear polyethylenes. The die gap is increased to 2.0 mm to 2.4 mm on 70 mm extruders with 28:1 L/D screws to lower melt shear heating. The terminal packs are pillow pouches for frozen peas, diced carrots and IQF fruits. Puncture propagation is measured with ASTM D2582-16; frozen vegetable filling trials often require a puncture energy above 2.5 J/mm, though company-specific thresholds differ. Low-temperature dart impact is measured under ISO 7765-1:2004 at -20 °C after conditioning for 24 h; a minimum of 180 g at 50 µm is common for monolayer structures. When the packaging system requires seal-through-condensation performance, the film is coextruded with a metallocene-catalysed C6-LLDPE or polyolefin plastomer sealant layer at 10–20 wt% of total thickness. Heat-seal initiation temperature is evaluated on a laboratory film sealing machine with 0.5 s dwell, 0.28 MPa jaw pressure and 25 mm wide heated jaws; the seal strength is tested under ASTM F88/F88M-21. Hot-tack force is measured under ASTM F1921-18; values above 2 N/25 mm at 115 °C are targeted for vertical form-fill-seal filling of frozen vegetables. The operational limit is the low hot-tack plateau of conventional C4-LLDPE sealing layers; below 110 °C seal initiation, the drop-door burst failure rate rises on VFFS machines running above 80 cycles/min. Moisture vapour transmission is estimated by ASTM F1249-20 at 38 °C and 90% RH; for monolayer 50 µm film, published data for the specific grade is limited, and the converter must perform WVTR validation because barrier performance is governed by crystal thickness distribution. Compliance for freezer packaging follows FDA 21 CFR 177.1520 and EU Regulation (EC) No 10/2011 with an overall migration limit of 10 mg/dm² for the finished article. Blending with high-density polyethylene fractions above 20 wt% is not recommended because excessive lamellae thickness increases low-temperature seal pop and reduces puncture energy at freeze temperatures.

    Vertical form-fill-seal lamination films are converted when a reverse-printed substrate requires an internal heat-seal layer with low temperature initiation and adequate coefficient of friction control. In this configuration, LQ 0518/21 AF is used at 40–50 wt% in the middle layer of a five-layer blown film, while the sealant layer contains 20–30 wt% metallocene LLDPE and 10–15 wt% polyolefin plastomer. The outer skin is formulated with an antiblock masterbatch at 1.5–2.5 wt% and a slip masterbatch at 0.5–1.0 wt%, both based on the same carrier resin to minimise interfacial defects. The die gap is set at 1.8 mm and the blow-up ratio is fixed at 2.5:1 on a 180 mm five-layer die. Seal initiation occurs below 110 °C when the plastomer content in the sealant layer reaches 15 wt%, as measured by ASTM F88/F88M-21 with a 0.5 s dwell and 0.28 MPa pressure. Hot-tack strength above 3 N/25 mm at 120 °C under ASTM F1921-18 is required for lamination webs running on vertical form-fill-seal machines above 100 cycles/min. The terminal articles include stand-up pouches for dry bakery mixes, frozen seafood pouches, and secondary packaging overwrap. Interlayer adhesion is checked with ASTM F904-16; a minimum lamination bond of 3 N/15 mm is specified after 24 h of curing. The anti-fog package in LQ 0518/21 AF may not be suitable for high-clarity display films because surface migration of the anti-fog additive raises haze; for such applications a non-AF blown film grade should be selected unless the end customer accepts haze measured under ASTM D1003-13 above 8%. Food contact compliance is evaluated under EU Regulation (EC) No 10/2011 and FDA 21 CFR 177.1520; migration testing must include the printing ink and lamination adhesive because residual solvents can interact with the polyolefin sealant. The processing boundary for this use is the occurrence of die-lip deposits from the anti-fog additive when output exceeds 160 kg/h on a 180 mm die; periodic lip purge every 6 h is required on such lines. Use of polypropylene-based sealing layers in the same die block is not recommended because thermal degradation of polyethylene may occur at the 230 °C processing temperature needed for polypropylene.

    When Thin-Gauge Vapour Retarders Must Meet ASTM E96 After Site Handling

    When construction vapour retarders must survive installation over gravel or concrete, the film is produced at 75 µm to 150 µm thickness. LQ 0518/21 AF is run on large bubble lines with die diameters from 250 mm to 350 mm, die gaps of 2.0 mm to 2.4 mm, and blow-up ratios of 2.0:1 to 2.3:1. A black masterbatch based on carbon black is added at 4–6 wt% for UV shielding when the membrane remains exposed for more than 7 days; the carbon black dispersion is assessed by ISO 18553:2002 to ensure particle agglomerates do not exceed 20 µm. Water vapour permeance under ASTM E96/E96M-22 Method B is controlled by thickness and resin density; for a 100 µm black film, specifiers commonly accept a permeance below 0.5 US perm, though published data for this specific grade in a black masterbatch-containing formulation should be generated on the converter’s line. Tensile properties after site installation are tested under ASTM D882-18; MD and TD tensile strength values above 18 MPa and elongation above 400% at 23 °C are used for procurement specifications. Elmendorf tear resistance under ASTM D1922-15 must remain above 200 g in the TD to prevent puncture growth from sharp aggregate edges. The film is also evaluated for low-temperature flexibility by ASTM D1790-14; installation below -5 °C is not recommended because handling-induced cracks may form at fold lines. The terminal articles are crawl-space vapour barriers, under-slab membranes, and temporary weather protection sheeting. The processing boundary is set by the carbon black masterbatch increment: addition above 6 wt% increases melt pressure at the die above 380 bar and narrows the bubble stability window on 30:1 L/D extruders. Combinations with calcium carbonate filler above 5 wt% are not recommended because the film may fail the elongation benchmark after folding and creasing. Compliance is limited to non-food construction applications, and REACH documentation must list the carbon black and any process lubricant used by the converter.

    Pallet-Hood Film Melt Strength and Outdoor UV Stabilization in Logistics Films

    Stretch hood and logistics wrap films rely on the melt strength of the blown film bubble to produce a thin but extensible medium that survives pallet-load stabilisation. LQ 0518/21 AF may be layered as the core of a three-layer stretch hood film at 50–70 wt% of total thickness, with outer skins made from metallocene C6-LLDPE or C8-LLDPE for puncture and cling performance. The die gap is set to 1.6 mm to 2.0 mm, and the blow-up ratio is increased to 3.0:1 to 3.5:1 to obtain balanced tensile characteristics. Frost line height is maintained at 700 mm to 900 mm on 200 mm dies to stabilise bubble movement at haul-off speeds above 35 m/min. The terminal articles are pallet hoods for brick, tile, beverage and panelised construction material loads. Dart impact resistance of the finished hood is measured under ASTM D1709-16a; values above 350 g at 80 µm are targeted for sharp-edged loads. Elmendorf tear under ASTM D1922-15 is specified with TD values above 250 g because vertical tear propagation is the main failure mode when pallet wrap contacts nail heads or banding clips. UV-stabilised hoods for outdoor yard storage incorporate a HALS/UV absorber masterbatch at 3–5 wt%; after 1,000 h of ISO 4892-2:2013 cycle A exposure, retained tensile elongation must exceed 300% according to ISO 527-3:2018. The melt strength required for the bubble is quantified indirectly through the maximum take-up speed before bubble instability; under the stated conditions, the stability limit is reached at approximately 42 m/min, but published data for this exact grade and coextrusion structure is limited. The anti-fog package may migrate to the surface and alter cling force when the grade is used in an outer cling skin; therefore, LQ 0518/21 AF is positioned in the core or the inner non-cling skin rather than the outer surface of two-sided cling films. Processing compatibility with tackifier-laden skins is limited; combinations with polyisobutylene-based cling masterbatches above 2 wt% in the same layer are not recommended because they can reduce additive migration and create surface streaks. Compliance for industrial packaging falls under general REACH obligations, and no food contact claim is made for pallet hoods unless migration testing of the finished plastic article under EU Regulation (EC) No 10/2011 is completed.

    Free Quote

    Competitive Braskem LQ 0518/21 AF LLDPE Blown Film Extrusion Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LQ 0518/21 AF is a linear low-density polyethylene resin formulated specifically for blown film extrusion. The model designation identifies the product class and its nominal melt-state and solid-state flow profile: the base resin carries a nominal density of 0.918 g/cm³ when determined according to ASTM D1505, and a melt mass-flow rate of 2.1 g/10 min when measured under ASTM D1238 at 190 °C with a 2.16 kg load. The polymer is a Ziegler-Natta-catalyzed ethylene-butene copolymer; the AF suffix denotes a formulated anti-fog additive package rather than a change in polymer backbone architecture. Converters use the grade in single-layer and coextruded structures where condensed water on the film surface must be converted from discrete droplets into a continuous transparent water film. The resin is therefore encountered in agricultural low-tunnel and greenhouse cover film, silage and bale wrap, frozen food packaging, fresh produce packaging, and carrier film structures. On single-screw blown film lines equipped with barrier-type screws having length-to-diameter ratios from 24:1 to 30:1, melt temperatures are typically held between 180 °C and 210 °C. Die gaps from 1.5 mm to 2.0 mm and blow-up ratios from 2.0:1 to 2.5:1 are commonly used to balance bubble stability and gauge uniformity. High-pressure LDPE is not required for bubble stability, although converter-specific blends with LDPE may be used to modify melt strength or optical properties.

    Because the comonomer is butene, the short-chain branch distribution differs from that of hexene- or octene-based LLDPE. At equal density and melt index, a butene copolymer typically exhibits lower dart impact resistance and lower Elmendorf tear propagation than a hexene or octene copolymer. Film property comparisons are valid only when specimen thickness, blow-up ratio, frost-line height, haul-off speed, and laboratory conditioning are controlled to the same values. Published data for this specific configuration is limited; the current manufacturer certificate of analysis should be consulted for specification limits and lot-specific values.

    What Limits Anti-Fog Performance in Ethylene-Butene Film Structures?

    Anti-fog performance is governed by the migration of nonionic surfactant additives from the bulk polymer to the film surface. In LLDPE, additive migration is slower than in high-pressure LDPE because of higher crystallinity and lower free volume at comparable density. The residence time before satisfactory anti-fog action develops therefore depends on storage temperature, film thickness, and the specific additive loading. Condensation cabinets used for process control typically impose a temperature differential of 20 °C to 60 °C while the film is inclined at 30°; anti-fog failure is recorded when visible droplet coverage exceeds the agreed area fraction. Because no universally binding ASTM method exists for anti-fog activity, converters often specify internal condensation-chamber criteria and correlate those results with field exposure on agricultural tunnels. On production-scale blown film lines, premature additive bloom can appear as a greasy deposit on the collapsing frame, nip rolls, or treatment electrodes. This deposit reduces surface energy and can create backside film fouling. Field observations with similar formulations indicate that the condition is controlled by limiting melt temperature to 210 °C, reducing extruder speed during short stops, and using chrome-plated die lips. The additive package may also lower the coefficient of friction; corona treatment levels should therefore be verified after storage, and surface wetting tension should be measured according to ASTM D2578 before lamination or printing.

    Although polyethylene is non-hygroscopic, pellet surface moisture from condensation at relative humidity above 60 % can introduce feed-throat slip and bubble defects in thin film. Dry-air purge or hopper heating is recommended when bulk storage conditions exceed this threshold. The base resin is not inherently UV-stable; if used outdoors without a suitable UV stabilizer package, tensile retention under ASTM G154 or ISO 4892-3 cycles will decline rapidly. Additive interactions between the anti-fog system and UV stabilizers should be evaluated on the target film line because historical data from other AF formulations may not transfer directly to this grade.

    Nominal Property Framework and Film Test Methodology

    The following test framework is used by incoming-quality laboratories and film converters to characterize the grade. Values listed as nominal in the manufacturer technical datasheet should be confirmed against the lot certificate.

    Property Test method Test condition or reported unit
    Density ASTM D1505 23 °C; g/cm³
    Melt mass-flow rate ASTM D1238 190 °C / 2.16 kg; g/10 min
    Tensile strength at break ASTM D882 500 mm/min crosshead speed; MPa
    Elmendorf tear strength ASTM D1922 0.025 mm specimen; gf
    Dart drop impact ASTM D1709 Method A 25 µm film; g
    Haze ASTM D1003 %
    Gloss ASTM D2457 45°; GU

    In agricultural low-tunnel film, the anti-fog additive must function under nocturnal temperature inversion and high relative humidity. Film thickness is typically 25 µm to 50 µm, and the film is exposed to UV radiation, pesticide contact, and mechanical stress from frame fastening. The butene LLDPE base provides puncture resistance measured by ASTM D5748 that is higher than high-pressure LDPE at equal thickness, permitting limited downgauging. However, butene LLDPE has lower long-term UV stability than a specifically formulated greenhouse grade; anti-UV additives are not implied by the AF designation. Converters adding UV stabilizer must verify interaction with the migratory anti-fog package and confirm film tensile retention after accelerated weathering according to ASTM G154 or ISO 4892-3. In frozen food packaging, interior fog reduction is critical when packages transfer from freezer to ambient retail display. The migratory additive lowers the contact angle of condensed water on the film surface, but time to achieve visible anti-fog action after film production can range from several hours to several days at ambient storage. Packagers should condition reels for 24 h to 48 h at 20 °C to 25 °C before forming and filling.

    When LQ 0518/21 AF Replaces High-Pressure LDPE on Blown Film Lines

    Replacing high-pressure LDPE with this LLDPE grade changes bubble stability, drawdown, and film stiffness. The linear architecture has lower extensional viscosity than long-chain-branched LDPE, so the bubble is more susceptible to instability at high blow-up ratios and the die pressure may be higher at equal output. The recommended die gap of 1.5 mm to 2.0 mm is wider than that used for high-pressure LDPE; this adjustment reduces melt fracture and allows the film to be drawn without excessive orientation. Frost-line height is typically maintained at 2 to 4 die diameters to control bubble chill and gauge bands. On lines without internal bubble cooling, maximum achievable output may be limited by bubble flutter rather than by screw capacity. If the grade is dry-blended with 10 % to 20 % LDPE by gravimetric feeder, bubble stability increases and dart impact may shift toward the LDPE value; the anti-fog additive level is correspondingly diluted, so field anti-fog performance must be rechecked.

    Die-lip deposit rates may increase when melt temperature exceeds 220 °C and residence time is prolonged. The condition appears as greasy streaks at the die exit and can transfer to the film surface in the form of faint oily bands. Production-scale corrective actions include reducing barrel zone setpoints, increasing extruder throughput to shorten residence time, and cleaning the die lip with a non-abrasive polymer purge before restart. If the deposit persists, the additive package should be reviewed with the resin supplier because the anti-fog component may be migrating too early under the line conditions.

    Comparative Difference Against Unmodified Butene LLDPE and High-Pressure LDPE

    Table 2 summarizes the directional property differences that a converter can expect when comparing LQ 0518/21 AF with an unmodified butene LLDPE and with high-pressure LDPE. The comparisons are based on standard film test methods and typical commercial behavior, not on a single universal specification.

    Characteristic Braskem LQ 0518/21 AF Unmodified butene LLDPE High-pressure LDPE
    Polymer architecture Ziegler-Natta ethylene-butene Ziegler-Natta ethylene-butene Autoclave or tubular LDPE
    Anti-fog additive Present Absent Absent
    Density by ASTM D1505 0.918 g/cm³ Comparable 0.920–0.925 g/cm³
    Melt mass-flow rate by ASTM D1238 2.1 g/10 min Comparable 1.8–2.2 g/10 min
    Dart impact at 25 µm by ASTM D1709 Higher than LDPE; lower than hexene LLDPE Similar to LQ base Lower
    Elmendorf tear by ASTM D1922 TD higher than MD; lower than hexene LLDPE Similar to LQ base MD lower, TD higher
    Haze by ASTM D1003 May increase slightly during additive bloom; stabilizes after conditioning Low Higher at equal film thickness
    Surface wetting tension Altered by additive bloom; verify per ASTM D2578 Stable after corona Stable after corona

    The difference between this AF grade and an unmodified butene LLDPE is primarily surface chemistry, not melt rheology. The base resin density and melt mass-flow rate are unchanged, so screw and die settings can remain substantially the same when switching grades on a production line. However, the anti-fog additive bloom modifies film surface energy, coefficient of friction, and corona retention, and these changes require converter adjustment of treated-film storage time and printing press parameters. Against a hexene or octene LLDPE of equal density, the butene grade has lower dart impact and tear propagation values, which may require an increase in film thickness in demanding agricultural or heavy-duty packaging applications. Against high-pressure LDPE, the grade provides higher puncture resistance and secant modulus, but lower melt strength and a narrower processing window for bubble stability. Additive interactions with slip and antiblock packages should be characterized on the same blown film line because historical dry-blend data from other AF formulations may not transfer directly to this formulation.

    Top