Braskem Ll5801n Lldpe Blown Film Extrusion Polyethylene Copolymer

Braskem LL5801N LLDPE Blown Film Extrusion Polyethylene Copolymer

    • Product Name: Braskem LL5801N LLDPE Blown Film Extrusion Polyethylene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 714839
    Grade LL5801N
    Polymer Type Linear Low Density Polyethylene (LLDPE) Copolymer
    Comonomer Butene-1
    Application Blown Film Extrusion
    Form Pellets
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Tensile Strength At Yield Md 10 MPa
    Tensile Strength At Yield Td 10 MPa
    Tensile Strength At Break Md 30 MPa
    Tensile Strength At Break Td 26 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Dart Drop Impact 300 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Haze 12%
    Gloss 45 60
    Melting Point 122°C
    Vicat Softening Point 100°C

    As an accredited Braskem LL5801N LLDPE Blown Film Extrusion Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LL5801N LLDPE blown-film copolymer: packaged in 25 kg polyethylene bags, palletized, with optional 1000 kg bulk bags.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Braskem LL5801N LLDPE blown film extrusion polyethylene copolymer in 25 kg bags, palletized, shrink-wrapped, and secured.
    Shipping Braskem LL5801N LLDPE copolymer ships as non-hazardous, free-flowing pellets in 25 kg PE bags or 500–1000 kg bulk bags, palletized and stretch-wrapped. Transport in clean, dry trucks, railcars, or containers. Store cool, dry, away from direct sunlight, moisture, and ignition sources. No special hazard class required.
    Storage Store Braskem LL5801N LLDPE copolymer resin in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep bags sealed to prevent moisture, dust, and contamination. Use clean pallets, stack securely, avoid excessive loads, and follow FIFO rotation and manufacturer SDS/local regulations. Do not store near strong oxidizers or incompatible chemicals. Protect from physical damage and moisture.
    Shelf Life Recommended shelf life is 24 months when stored in original packaging, dry, protected from direct sunlight and temperatures below 50°C.
    Application of Braskem LL5801N LLDPE Blown Film Extrusion Polyethylene Copolymer

    In blown film lines converting Braskem LL5801N LLDPE blown film extrusion polyethylene copolymer for direct-contact frozen food packaging, the 0.918 g/cm³ density and 1.0 g/10 min melt flow rate position the butene copolymer in a processing corridor that balances bubble stability against low-temperature dart impact retention. The applicable food-contact compliance framework is FDA 21 CFR 177.1520(c) for olefin polymers, EU Regulation 10/2011 with an overall migration limit of 10 mg/dm² under the intended frozen storage condition, and GB 4806.7-2023 for China-bound converted film. Formulation addition ratios on monolayer lines typically run 70–85 wt% LL5801N, 15–25 wt% LDPE with a melt index below 2.0 g/10 min for bubble stability, and 2–5 wt% of a silica/erucamide masterbatch for coefficient of friction and antiblock control. The downstream conversion process on a 45–75 mm single-screw extruder with 24:1–30:1 L/D and barrier screw is executed at melt temperatures of 190–215 °C, a die gap of 1.8–2.2 mm, a blow-up ratio between 2.2:1 and 2.8:1, and a frost line height of 5–7 die diameters; internal bubble cooling at 15–22 °C is used to maintain gauge band below ±5% at film thickness of 30–60 µm. Erucamide migration causes die lip build-up after 8–12 h of continuous running, requiring periodic wiping and establishing the upper limit of additive masterbatch loading. Terminal finished product types include IQF vegetable bags, seafood pouches, frozen meat overwrap, and ice cream chub films.

    JurisdictionReference standardTest method / conditionRequirement
    United StatesFDA 21 CFR 177.1520(c)Specifications in 21 CFR 177.1520(c)Olefin polymer permitted for direct food contact under specified conditions of use
    European UnionEU Regulation 10/2011 Annex IEN 1186-1 migration testingOverall migration limit 10 mg/dm² or 60 mg/kg
    ChinaGB 4806.7-2023GB 31604.1 and GB 31604.8Overall migration limit 10 mg/dm²

    Low-temperature abuse of IQF bags occurs at -25 °C to -40 °C, where the butene short-chain branching of LL5801N retains Elmendorf tear strength measured by ASTM D1922 and dart impact by ASTM D1709; however, at thickness below 25 µm, bubble stability on standard air-ring equipment becomes the controlling variable rather than polymer toughness. The monolayer structure is limited to non-sharp product fill weights below 2.5 kg; above this fill weight a coextruded structure with an HDPE inner layer is introduced to resist puncture from frozen vegetables and seafood. Corona treatment is held at 38–42 dyn/cm for subsequent flexographic or rotogravure printing, and the treated surface is consumed within 48 h to avoid dyne decay in high-humidity cold storage transfer areas.

    Heavy-Duty Sack Films Select LL5801N in HDPE-Rich Blends for Stiffness-Drop Balance

    The use of 55–70 wt% LL5801N in heavy-duty sack structures is governed by drop-test requirements under ASTM D5276 and dart impact measurement under ASTM D1709, while tear resistance is evaluated in both machine and transverse directions by ASTM D1922. Formulation addition ratios in three-layer coextrusions combine 55–70 wt% LL5801N with 25–35 wt% high-density polyethylene grade having a density of 0.949–0.956 g/cm³, 5–10 wt% LDPE for melt extension, and 5–10 wt% CaCO₃ masterbatch for stiffness and cost structure; the LL5801N fraction contributes dart impact and seal initiation while the HDPE fraction controls creep and modulus. Processing on a 60–80 mm extruder with 30:1 L/D and grooved feed section operates at 190–215 °C melt temperature, die gap 2.0–2.5 mm, blow-up ratio 3.0:1–4.0:1, and a high-stalk bubble geometry of 8–10 die diameters; the bubble is stabilized by a lower collapsing-frame angle and nip roll pressure not exceeding 0.25 MPa. On production-scale lines, BUR values above 4.0:1 produce bubble flutter unless the frost line is raised 10–15% and the outer air ring lip is opened; batch-to-batch HDPE molecular weight distribution shift alters gauge band by ±3% and requires corresponding screw speed adjustment. Terminal finished product types include fertilizer sacks, polymer pellet sacks, chemical powder sacks, and construction aggregate bags.

    What Constrains Machine-Direction Tear and Stretch Hood Retention on High-Stalk Lines?

    On high-stalk blown film lines producing stretch hood structures, LL5801N is typically limited to the core or non-tackified layer at 70–80 wt% because the butene branching distribution delivers lower elastic recovery than hexene-copolymer or metallocene alternatives at pre-stretch ratios above 120%. The relevant mechanical evaluation uses ASTM D5459 for machine-direction elastic recovery and ASTM D5748 for puncture resistance; downstream load stability acceptance is typically tied to pallet stability protocols rather than a single film property. Formulation addition ratios for a three-layer structure place LL5801N at 70–80 wt% in the core, 10–20 wt% mLLDPE in the skin for seal and elastic recovery, 5–10 wt% LDPE for bubble stability, and 0.02–0.1 wt% polymer processing aid to suppress melt fracture at high output. The conversion process is run on a 65–90 mm extruder with 30:1 L/D, die diameter 300–500 mm, die gap 2.2–2.8 mm, blow-up ratio 3.5:1–4.5:1, and frost line height at 8–12 die diameters to orient molecular chains in the machine direction; dual-lip air ring and internal bubble cooling at 12–18 °C maintain gauge variation within ±2.2%. A known processing failure occurs when frost line height falls below 6 die diameters, producing anisotropic MD tear and reducing stretch hood retention on sharp-edged pallets. Terminal finished product types include pallet hoods for appliances, beverage shrink-hood replacement, and building-material unitization.

    Because silage cover film requires repeated puncture resistance after UV weathering, converters use LL5801N as the major component in monolayer or three-layer agricultural films intended for low-tunnel and clamp silage covers. The applicable standard is EN 13206 for thermoplastic covering films used in agriculture and horticulture, with supplementary UV stability evaluation by ISO 4892-2 xenon-arc weathering; films used in contact with silage leachate are specified to avoid undesirable substance transfer under REACH (EC) No 1907/2006. Formulation addition ratios in monolayer silage covers run 75–85 wt% LL5801N, 10–15 wt% LDPE, and 3–5 wt% UV masterbatch containing hindered amine light stabilizer compounds; in greenhouse covers the LL5801N fraction falls to 50–70 wt%, with 5–15 wt% EVA for heat retention and flexibility at low temperature. The downstream blown film process uses a 50–70 mm extruder with 24:1–30:1 L/D, die gap 1.8–2.5 mm, blow-up ratio 2.0:1–3.0:1, and frost line height adjusted between 4–8 die diameters depending on gauge; the film is edge-trimmed and wound on surface center-wind stations to avoid pressure-induced blocking after UV masterbatch migration. Field experience indicates that sulfur-containing agrochemical residues accelerate oxidative degradation unless the HALS package is tested by ISO 4892-2 for cumulative UV dose; equipment operators also monitor film tension at the collapsing frame to avoid wrinkles that become tear initiation points. Terminal finished product types include silage sheet and clamp covers, bale wrap, low-tunnel covers, and greenhouse side sheets.

    Sealant Web Extrusion at 380–420 mm Die Circumference for Laminated Pouch Converting

    Process trials on a 65 mm single-screw extruder with 30:1 L/D and 380–420 mm die circumference demonstrate that LL5801N can be run as a sealant web at gauge 25–60 µm when the formulation is biased toward low coefficient of friction and stable heat seal initiation. Food-contact compliance for the sealant layer references FDA 21 CFR 177.1520(c) and EU Regulation 10/2011, with migration testing according to EN 1186-1 and overall migration below 10 mg/dm². Formulation addition ratios are 80–90 wt% LL5801N, 5–10 wt% LDPE with a density above 0.922 g/cm³ for heat seal hot-tack, 2–5 wt% slip/antiblock masterbatch, and 0.02–0.1 wt% fluoropolymer processing aid to eliminate sharkskin at high shear. The conversion process runs at 185–210 °C melt temperature with a die gap of 1.6–2.0 mm and blow-up ratio of 2.0:1–2.6:1; the film is corona treated in-line to 40–44 dyn/cm, and tension at the secondary nip is tapered from 120 N to 80 N across the roll diameter to prevent blocking. Seal strength is measured per ASTM F88; a failure mode observed on converting lines is delamination within 24 h of corona treatment when dyne level decays below 38 dyn/cm, particularly in high-humidity lamination rooms. Terminal finished product types include liquid detergent refill pouches, dried soup sachets, snack laminate back-seal webs, and frozen food laminated pouches.

    When converter line speed exceeds 150 m/min on a 65 mm grooved-feed extruder, LL5801N is selected for high-speed refuse sack and can liner structures where dart impact, gauge uniformity, and melt strength control film breaks. The applicable product standard is EN 13592 for plastic sacks for household waste collection, with mechanical evaluation by ASTM D1709 dart impact and ASTM D1922 tear resistance; formulations destined for landfill or incineration are checked against REACH (EC) No 1907/2006 for SVHC content. Formulation addition ratios vary with recycled content but commonly use 50–70 wt% LL5801N, 20–40 wt% reclaimed LLDPE/LDPE, 5–15 wt% CaCO₃ masterbatch, and 1–3 wt% slip masterbatch; the upper reclaimed fraction is limited by gauge variation and gel formation. The process operates at 180–210 °C melt temperature, die gap 1.0–1.5 mm, blow-up ratio 3.0:1–5.0:1, and high-stalk bubble with internal bubble cooling at 10–16 °C; in-line gusseting and perforation are placed after the collapsing frame to maintain tension control. A field-observed failure is feed throat bridging when reclaimed pellets have bulk density below 0.52 g/cm³, requiring feed screw cooling adjustments. Terminal finished product types include drawstring kitchen bags, janitorial liners, contractor refuse sacks, and clinical waste can liners.

    Free Quote

    Competitive Braskem LL5801N LLDPE Blown Film Extrusion Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LL5801N is a linear low-density polyethylene copolymer supplied for blown film extrusion. The resin is produced by catalytic low-pressure polymerisation with an α-olefin comonomer and is stabilised with an antioxidant package. The public datasheet reports a nominal density of 0.918 g/cm³ measured according to ASTM D1505 and a melt mass-flow rate of 1.0 g/10 min at 190 °C/2.16 kg according to ASTM D1238 or ISO 1133-1:2022. These values place the grade in the conventional linear-low-density range used for industrial liners, heavy-duty sacks, and lamination films. The base formulation does not contain slip or antiblock additives; masterbatch addition is required when specific surface-friction or blocking-resistance targets are set.

    At a film gauge of 25 µm, film mechanical properties are influenced more by die gap, blow-up ratio, frost line height, and melt-temperature profile than by resin specification alone. The following table lists representative converter-reported values obtained on air-cooled monolayer blown-film lines with a 1.8 mm die gap and a blow-up ratio near 2.5:1. The entries are not specification limits and should be used for process-development comparison only.

    PropertyTest MethodRepresentative Value or RangeFilm / Specimen Condition
    Melt mass-flow rateASTM D1238 / ISO 1133-1:20221.0 g/10 min190 °C, 2.16 kg
    DensityASTM D1505 / ISO 1183-1:20190.918 g/cm³23 °C, compression-moulded plaque
    Tensile strength at break, MD/TDASTM D88238–45 MPa / 30–36 MPa25 µm blown film
    Elongation at break, MD/TDASTM D882700–850% / 850–1000%25 µm blown film
    Secant modulus, 1%, MD/TDASTM D882180–220 MPa / 190–230 MPa25 µm blown film
    Elmendorf tear, MD/TDASTM D1922100–160 gf / 320–430 gf25 µm blown film
    Dart drop impact, F50ASTM D1709100–140 gMethod A, 25 µm
    HazeASTM D10038–14%25 µm
    Gloss, 45°ASTM D245755–70 GU25 µm
    Vicat softening temperatureASTM D152597–103 °CLoading 10 N, 50 °C/h
    Melting peak temperatureASTM D3418121–124 °CSecond heating, 10 °C/min

    Batch-to-batch control at the converting site typically checks melt mass-flow rate, density, and dart drop impact on a 25 µm test film. A decrease in Elmendorf tear at constant density can indicate overheating in the extruder or excessive regrind loading. Gel counts are monitored optically at 45° incident light, because gel specks are more readily visible under low-angle illumination than under normal transmission.

    On production-scale monolayer blown-film lines equipped with 65 mm grooved-feed extruders having L/D 30:1 barrier screws and 80 mm spiral-mandrel dies, process observations indicate stable operation at melt temperatures between 190 °C and 225 °C, with barrel temperatures set from 170 °C to 210 °C. Throughput on these lines is typically held between 0.8 kg/h per mm and 1.2 kg/h per mm of die circumference. At die-lip shear rates above approximately 150 s⁻¹, surface melt fracture can appear; the onset can be shifted upward by opening the die gap to 2.0–2.5 mm or reducing die temperature. Prolonged operation with melt temperature above 235 °C and residence time exceeding 5 min increases oxidative gel formation. If the line is stopped with LL5801N in the barrel, purging with low-melt-flow LDPE reduces restart gel specks.

    Capillary rheometry of LL5801N at 190 °C shows shear-thinning behaviour; apparent viscosity is of the order of 1.8–2.4 kPa·s at 10 s⁻¹ and 350–450 Pa·s at 100 s⁻¹. The power-law index over the 50–500 s⁻¹ interval is approximately 0.55–0.65. These values support grooved-feed extruder operation with moderate compression ratios, but capillary data should be re-measured on the production lot because additive package and pellet geometry can shift the pressure-flow curve. Published data for this specific configuration is limited, particularly for melt-temperature effects on extensional viscosity and bubble strain hardening.

    Extrusion backpressure on the 65 mm line described above is typically between 25 MPa and 35 MPa at 120 kg/h output with a 1.8 mm die gap. If backpressure falls below 20 MPa at constant screw speed, pellet feed slip or screw wear is more probable than resin viscosity drift. If backpressure rises above 40 MPa, the die gap or screen pack should be checked before assigning the change to the resin lot. These observations are field-derived and should be verified against the actual screw design and heater control.

    LL5801N is processed across a film gauge range from 20 µm to 200 µm in monolayer and coextruded constructions. Below 20 µm, dart impact and Elmendorf tear become more sensitive to die-gap uniformity and melt-temperature ripple, while above 150 µm the limiting factor is typically heat removal rather than resin flow. For thick liners, the die gap is often opened to 2.5 mm and the cooling air temperature is reduced to maintain bubble diameter.

    The film property values are sensitive to frost line height. A frost line height below 4 die diameters typically raises transverse-direction elongation but reduces bubble stability; a frost line above 8 die diameters can reduce dart drop impact because the polymer chains have a longer melt-state orientation history before solidification. On air-cooled lines, the frost line is therefore maintained between 4 and 8 die diameters unless specific optical targets require a shorter or longer stalk.

    How Does LL5801N Compare with High-Pressure LDPE and mLLDPE?

    Relative to high-pressure LDPE, LL5801N has a linear molecular architecture with short-chain branching rather than long-chain branching. The practical consequence is that at equal film thickness, LL5801N can provide higher tensile strength at break and higher dart drop impact, but lower melt strength and less bubble stability in high-stalk lines. High-pressure LDPE remains more stable at blow-up ratios above 3.0:1, whereas LL5801N is typically run at blow-up ratios between 2.0:1 and 3.0:1. In side-by-side testing, LL5801N films also show higher elongation at break and higher puncture resistance than a 0.918 g/cm³ high-pressure LDPE when measured by ASTM D1709, but the exact margin depends on gauge and frost-line management.

    Compared with metallocene LLDPE, LL5801N generally produces higher haze and lower gloss because of broader short-chain branching distribution and crystalline heterogeneity. Heat-seal and hot-tack initiation temperatures are higher; side-by-side seal tests may shift the seal initiation temperature upward by 5–10 °C relative to a 0.918 g/cm³ metallocene hexene LLDPE. Published data for this specific configuration is limited, so the seal-temperature difference should be verified with the intended jaw geometry, dwell time, and seal pressure. Conversely, the broader molecular weight distribution of LL5801N can reduce extrusion head pressure and improve output stability on conventional grooved-feed lines that are not designed for narrow-molecular-weight-distribution metallocene resins.

    Within the LLDPE family, comonomer type controls the short-chain branching distribution and tear performance. At equivalent density and melt flow rate, a butene-based Ziegler-Natta grade such as LL5801N generally exhibits lower Elmendorf tear strength than a hexene or octene copolymer, especially in the transverse direction, because the comonomer is less effective at connecting crystalline lamellae. LL5801N is therefore used in heavy-duty sacks and industrial liners where impact and puncture requirements are moderate, but not as the sole resin in frozen-food packaging where sub-zero puncture tests at -20 °C are specified.

    LL5801N differs from higher-density LLDPE grades such as 0.926 g/cm³ film resins in that the lower density reduces secant modulus and increases impact resistance. For applications requiring top-load or stacking strength, the 0.918 g/cm³ density may be insufficient, and a blended structure or higher-density core layer is required. The 1% secant modulus measured by ASTM D882 at 25 µm is approximately 180–220 MPa in the machine direction and 190–230 MPa in the transverse direction; this is below the 250–300 MPa range typical of 0.926 g/cm³ film grades.

    When LL5801N Is Blended with LDPE for Higher-Stalk Film Lines

    Blending with high-pressure LDPE is used to increase melt strength when a packaging line cannot maintain bubble stability with pure LLDPE. At 80:20 LLDPE:LDPE mass ratios, bubble flutter decreases without removing the tensile and impact advantages of the LLDPE component. At 70:30 mass ratios, the bubble can be run on higher-stalk configurations, but haze may increase to 15–20% and dart drop impact may fall by 15–25% compared with pure LL5801N film of the same gauge. The blend should be homogenised before entering the die because the two phases have different extensional viscosities. Inadequate mixing appears as optical chatter bands across the film width rather than as a discrete peak.

    For coextruded structures, LL5801N is often placed in the seal layer of three-layer films. In PA/tie/LL5801N structures, the sealant melt temperature is held below 225 °C to reduce oxidative gel formation and preserve hot-tack performance. Reducing the sealant die gap below 0.8 mm in a 50 µm total film can produce interfacial waviness when the neighbouring adhesive tie layer has a melt mass-flow rate below 2.0 g/10 min. That condition reflects a viscosity mismatch rather than a deficiency of the sealant resin.

    Regulatory Status Requires Converter-Specific Verification

    For food-contact applications, converter verification is required because the base-resin approval does not cover the finished package. LL5801N belongs to the olefin polymer class described in FDA 21 CFR 177.1520, but end-use extraction limits depend on film thickness, food type, temperature, and contact time. Under EU Regulation 10/2011, overall migration must be demonstrated against the intended food simulant; the general limit is 10 mg/dm² when tested according to EN 1186 conditions. The polymer itself is generally exempt from registration under REACH Article 3(5), but the converter must verify that residual monomers and additives are registered and that no substance of very high concern exceeds 0.1% w/w in the article.

    Regulatory ReferenceRelevant StatusVerification Condition / Requirement
    FDA 21 CFR 177.1520Olefin polymer; finished-article extraction limit applies21 CFR 177.1520(c) end-use testing
    EU Regulation 10/2011Plastic food-contact material; overall migration limit applies10 mg/dm² by EN 1186 in appropriate food simulant
    REACHPolymer exempt from registration; monomers and additives must be registeredArticle 3(5); SVHC content <0.1% w/w
    RoHS Directive 2011/65/EUNot generally applicable to packaging unless incorporated into EEEPb, Hg, Cr(VI), PBB, PBDE <1000 ppm; Cd <100 ppm
    ISO 1133-1:2022Melt mass-flow rate method for quality controlProcedure A, 190 °C/2.16 kg

    Storage of unopened pellet containers at relative humidity above 60% is permitted, but unprotected silo storage can introduce surface moisture that appears as micro-voids at the die lip. The resin does not require pre-drying under normal handling. Direct blending with hygroscopic polar barrier resins should be avoided unless the polar component is dried separately, because water carryover into the LLDPE layer can destabilise the bubble and increase die-lip deposit formation.

    Top