Braskem Ll4800n Pebdl Cast Film Extrusion Polyethylene Copolymer

Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer

    • Product Name: Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 367395
    Grade Name Braskem LL4800N
    Polymer Type Linear Low Density Polyethylene (LLDPE) Copolymer
    Comonomer Butene-1
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 3.8 g/10 min
    Melting Point 122 °C
    Crystallization Temperature 108 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 700%
    Flexural Modulus 240 MPa
    Dart Impact Strength 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 350 g
    Haze 6%
    Gloss 45 80

    As an accredited Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LL4800N packaging: 25 kg polyethylene bags on pallets, or 1,000 kg bulk bags for shipment.
    Container Loading (20′ FCL) 20′ FCL container loading: Braskem LL4800N PEBDL cast film extrusion polyethylene copolymer in palletized bags, securely stowed for ocean transport.
    Shipping Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer is shipped as a non-hazardous solid resin, typically in 25 kg PE bags on pallets or in bulk containers. Keep dry, cool, protected from UV/heat, and away from strong oxidizers. Handle with clean equipment; follow local transport and storage regulations.
    Storage Store Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging sealed and palletized to prevent moisture, dust, and contamination. Avoid excessive stacking, use clean handling equipment, and follow first-in, first-out stock rotation. Maintain ambient temperatures and protect from physical damage.
    Shelf Life Typically, shelf life is 12 months from manufacture when stored in original packaging, dry, cool, ventilated, away from direct sunlight.
    Application of Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer

    Cast film extrusion of LL4800N, a butene-based linear low-density polyethylene copolymer with nominal melt flow rate 4.8 g/10 min under ISO 1133-1:2022 and nominal density 0.918 g/cm³, is most demanding in pallet unitisation operations where rotating ring wrappers apply pre-stretch ratios between 200% and 300%. The resin is loaded as the base polyethylene fraction at 95–98 wt%, with a combined polyisobutylene cling masterbatch and slip/antiblock package totalling 2–5 wt%; the cling masterbatch is typically a 10 wt% PIB concentrate in an LLDPE carrier and is allocated to the skin layer only, not the core layer, so that roll unwind force remains stable after two weeks of roll storage. Regulatory and normative anchors for this non-food film are primarily ASTM D5458-95(2020) for cling force, ASTM D5459-18 for machine-direction elastic recovery, permanent deformation, and stress retention under stretch-wrap conditions, ASTM D5748-19 for puncture resistance, and REACH verification for tackifier and processing-aid substances. The cast-film line uses a 90 mm single-screw extruder with a 30:1 L/D barrier screw, a coat hanger die at 0.6 mm die gap, and a melt temperature held at 240–255°C; the air gap between die exit and primary chill roll is maintained below 25 mm to limit neck-in, while the chill roll runs at 18–24°C and an air knife or electrostatic pinning device prevents the web from lifting above 300 m/min. At line speeds above 400 m/min, edge bead and melt resonance become the main process limits, and operators suppress them by locally increasing die lip temperature or adjusting die lip gaps over the outer 50 mm rather than by raising the entire melt temperature. Terminal roll stock is slit into 300 mm hand rolls of approximately 2 kg, 500 mm machine rolls of 12–20 kg, and pre-stretched cores at 15–17 µm for long-haul palletising.

    What Physical Limitations Appear When LL4800N Functions as a Food-Contact Sealant Web?

    In a three-layer cast coextrusion structure, LL4800N is positioned as the sealant skin at 70–85 wt% of the sealant layer, with 15–30 wt% of an ethylene-vinyl acetate copolymer or plastomer to reduce seal initiation and improve hot-tack across contaminated seal areas; the core layer may contain LL4800N at 100 wt% or blended with 10–20 wt% LDPE to protect against roll blocking. Food-contact compliance is governed by FDA 21 CFR 177.1520(c) for olefin polymers and by EU Regulation 10/2011 as amended by 2020/1245, with overall migration below 10 mg/dm² verified on the finished laminate rather than on the pellet; additive-specific migration from the EVA or plastomer layer must be checked under Annex II of EU Regulation 10/2011, and the processor must maintain documentation under Regulation (EC) No 2023/2006 on good manufacturing practice. The downstream process begins with a 1.0 mm die gap cast coextrusion line, melt temperature 230–245°C, primary chill roll at 15–20°C, and film gauge between 20 µm and 60 µm; the sealant skin is corona-treated to 40–44 mN/m before being laminated to BOPP or PET through solventless adhesive, and the finished reel is conditioned for 48 h at 23°C before slitting to allow additive migration and crystallinity to stabilise. A documented limitation is that LL4800N does not supply oxygen barrier function, so gas-flush or extended shelf-life packages require a barrier core or coating; published data for exact hot-tack values of LL4800N in this specific coextruded sealant configuration is limited, and converters therefore validate seal strength on their own line according to ASTM F88/F88M rather than relying on resin-level data. Terminal products include form-fill-seal pillow pouches for leafy greens, flow-wrap bakery overwrap, and non-barrier lidding film for fresh produce trays.

    ReferenceScopeParameterLimiting value or test condition
    FDA 21 CFR 177.1520(c)Olefin polymers in food contactExtractables, density, melt index specificationFinished article must conform to paragraph (c) specifications and use conditions in 21 CFR 176.170(c)
    EU Regulation 10/2011 as amended by 2020/1245Plastic materials and articles in contact with foodOverall migration10 mg/dm²
    EU Regulation 10/2011 Annex IISpecific migration of additivesSML for EVA/plastomer-layer additivesSubstance-specific SML values listed in Annex II
    ASTM F88/F88MSeal strength of flexible barrier materialsHeat-seal strengthPackage-specific target validated on the converting line

    Agricultural Silage Wrap, Oxygen Transmission, and UV Stabilizer Loading

    For baled forage conservation, LL4800N is used in monolayer or three-layer cast silage wrap at 30–50 µm thickness, with the resin loaded at 95–99 wt%; the remaining 1–5 wt% is split between a HALS/UV stabilizer masterbatch at 0.2–0.6 wt% and a white, black, or tinted pigment concentrate at 1–4 wt% depending on layer position and regional UV exposure. Compliance for this application is anchored to EN 13207:2018 for thermoplastic silage films used in agriculture, with additional verification under REACH for stabilizer substances and ISO 527-3:2018 for tensile properties on cast film. The cast-film process uses a die gap of 0.7 mm and a melt temperature of 240°C ±5°C, with the primary chill roll at 20–25°C to establish a smooth outer surface; the film is wound with a controlled taper between 10% and 30% tension reduction from core to outer layers to prevent blocking in storage. During bale wrapping, the film is applied at 55–70% pre-stretch, but the material does not perform as an oxygen barrier; its silage preservation function relies on physical exclusion of air and maintaining at least four film layers over the bale. Terminal products include round bale wrap, clamp silage cover film, and stack-cover sheets, with maximum service life determined by the stabilizer package rather than by the LLDPE backbone.

    Where FIBC and octabin liners require a cast web with high dart impact and low gel count, LL4800N is run at 100 wt% or at 85–95 wt% with a fractional-melt LDPE added only when back-to-back film contact produces unwind blocking on two-drum winders. The compliance set for industrial liner film includes ASTM D1709-16a for dart drop impact, ASTM D882-18 and ISO 527-3:2018 for tensile properties, and ASTM D1922 for tear resistance; REACH documentation is maintained for the base resin and slip or processing stabilizers. The cast line operates at 50–125 µm gauge, die gap 0.8–1.2 mm, melt temperature 230–250°C, and chill roll temperature 20–25°C; in-line edge trim is ground, pelletized, and returned to the feed at up to 15 wt% without measurable loss in film appearance. Terminal products include octabin liners, FIBC liners for hygroscopic powders, drum liners, and long-length container liners for dry bulk.

    When Cast Film Must Balance Peel Adhesion and UV Exposure

    A coextruded surface protection film made with LL4800N in the carrier web is built as a two-layer or three-layer structure in which the backing layer contains 75–90 wt% LL4800N and 10–25 wt% LDPE for stiffness and melt strength, while the adhesive layer is an EVA or POE copolymer at 10–20 wt% of total film thickness; the exact blend is shifted by application because peel adhesion must remain below the maximum specified by the surface owner, and removal is verified after ageing. Normative references include ASTM D3330/D3330M for peel adhesion at 180° angle and 300 mm/min crosshead speed, ISO 527-3:2018 for tensile behaviour, and ASTM G154 for UV-aged film removal; REACH and RoHS documentation applies when the film is used on appliance or building-product surfaces entering the EU market. The cast line is run with a 0.5 mm die gap, melt temperature 235°C, and a matte-finish chill roll at 18–22°C; the film is aged at ambient temperature for at least 72 h before slitting, because peel adhesion increases during crystallisation and the value measured immediately after winding is not representative of final performance. Terminal products include cast protection film for pre-coated aluminium coil, polished stainless steel sheet, glass panels, and PVC window-profile extrusion.

    Stretch Hooder Film Mechanics in High-Speed Logistics

    Stretch hooder lines operate with thicker cast film than pallet stretch film, typically 60–150 µm, because the hood must retain elasticity during vertical stretching and recovery over pallet corners. LL4800N is blended at 70–85 wt% with LDPE at 15–30 wt% to increase melt tension and reduce sag before the chill roll; no cling additive is required because stretch hooding uses the film's elastic recovery to clamp the load rather than self-adhesion. Compliance for this non-food industrial film is based on ISO 527-3:2018 for tensile properties, ASTM D882-18 for machine-direction and transverse-direction tensile behaviour, and REACH verification for processing stabilisers and masterbatch carriers. The cast line runs a die gap of 0.8–1.2 mm, melt temperature 240–250°C, primary chill roll at 20–25°C, and line speed controlled to 100–200 m/min; because of the high thickness, edge bead removal and tension-zone profiling on the winder become critical to avoid gauge bands and telescoped rolls. Terminal products include stretch hooder film for palletised construction materials, beverage pallets, appliance outer packaging, and airbag-cushioned logistics loads.

    Free Quote

    Competitive Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LL4800N PEBDL is a linear low-density polyethylene copolymer intended for chill-roll cast film extrusion. The designation PEBDL appears in Brazilian technical documentation as the abbreviation for polietileno de baixa densidade linear; in English-language specifications the product is classified as an LLDPE cast-film grade. The resin is supplied in pellet form and is characterized by a melt flow rate of 4.0 g/10 min when measured at 190 °C under 2.16 kg in accordance with ASTM D1238-20 or ISO 1133-1:2022. Density determined by ISO 1183-1:2019 is 0.925 g/cm³. These two values define the primary selection window for cast-film converters because the product sits above the melt flow range of typical blown-film LLDPE and below the density of high-density polyethylene.

    The material is not a general-purpose blown-film resin and should not be evaluated as one. In a conventional annular-die line, a 4.0 g/10 min melt flow rate would reduce bubble stability and make gauge control difficult below 25 µm. A cast-film line instead uses a slot die and a chill roll, so the melt curtain is quenched before significant molecular relaxation. The higher melt flow rate becomes an operational advantage: it lowers backpressure in a 90 mm extruder with L/D 30:1, improves die-lip distribution across wide widths, and permits the use of shallower flight depths in the metering zone without excessive shear heating. Comparative selection against blown-film LLDPE should therefore begin with the conversion process rather than density alone.

    Processing conditions on production-scale cast lines are typically set with barrel temperatures from 180 °C at the feed throat to 240 °C at the adapter, with die zones held between 230 °C and 250 °C. The melt temperature should remain below 260 °C to avoid consuming the thermal stabilizer and generating gel defects. Die gap is normally adjusted between 0.5 mm and 1.0 mm, wider than the final gauge because the web is drawn down in the air gap. A chill roll maintained at 18–24 °C is standard; warmer rolls reduce quench rate and increase crystallinity, which can shift tear and seal behavior. The air gap is usually kept between 15 mm and 40 mm. Air-knife pressure, vacuum-box position, and edge pinning must be tuned to prevent neck-in and edge bead instability. Published data for LL4800N-specific neck-in magnitude are limited; the onset can be measured on the target line by transverse thickness profiling at intervals of 10 cm from the die ears.

    What Distinguishes a Chill-Roll Optimized Linear Copolymer from Bubble-Process Resins?

    High-pressure LDPE and blown-film LLDPE grades serve different rheological requirements. High-pressure LDPE contains long-chain branches that generate melt extension-hardening; this stabilizes a blown bubble and allows high-speed extrusion coating. Blown-film LLDPE typically uses a melt flow rate of 0.8–1.2 g/10 min to maintain bubble shape, but that low MFR increases extruder pressure and limits downgauging. LL4800N at 4.0 g/10 min shows lower melt extension-hardening, which is less detrimental in a cast process because the web is immediately pinned to the chill roll. The resin’s linear architecture and density of 0.925 g/cm³ also differ from a high-pressure LDPE at 0.923 g/cm³ in that crystallite formation is more rapid and the resulting film has a different balance of stiffness and puncture. Comparative data are summarized below.

    ParameterBraskem LL4800N PEBDL cast gradeRepresentative blown-film LLDPE general-purposeRepresentative high-pressure LDPE cast or extrusion coating grade
    Melt flow rate at 190 °C/2.16 kg4.0 g/10 min0.8–1.2 g/10 min1.8–2.5 g/10 min
    Density0.925 g/cm³0.916–0.920 g/cm³0.920–0.924 g/cm³
    Primary conversionflat die/chill rollannular die/bubbleannular die or extrusion coating die
    Relative melt extension-hardeninglowermoderatehigher
    Thin-gauge behavior below 25 µmprocessable for down-gauged cast webs when air gap is minimizedlimited by bubble stabilitylimited by melt fracture and low MFR backpressure
    Typical melt temperature on cast line230–250 °Cnot recommended200–230 °C

    In oscillatory shear rheology, a linear low-density polyethylene with 4.0 g/10 min MFR displays a lower storage modulus at low frequency than a high-molecular-weight blown-film grade, which is an indirect indication of easier melt relaxation. The absence of long-chain branching further reduces shear thinning relative to high-pressure LDPE. These differences are measurable by parallel-plate rheometry under nitrogen at 190 °C using small-amplitude oscillatory shear; however, published complete rheological master curves for LL4800N are limited. Converters who require extensional viscosity data must perform creep or extensional rheometry on the production pellets because generic LLDPE curves cannot substitute for lot-specific behavior.

    Film mechanical values are not single-point constants. They depend on final gauge, chill-roll temperature, die pressure, and take-off speed. Standard film evaluation for LL4800N should be performed on conditioned specimens at 23 ± 2 °C and 50 ± 5 % relative humidity according to ASTM D618-21. Tensile testing is performed per ASTM D882-18, tear propagation per ASTM D1922-19, dart drop impact per ASTM D1709-22, and puncture resistance per ASTM D5748-19. In cast webs, machine-direction tear strength is often lower than transverse-direction tear strength because the chill roll freezes molecular orientation in the machine direction. This anisotropy is expected and should guide packaging design. A film produced from LL4800N on a 25 µm cast line is more likely to fail by machine-direction tear propagation when subjected to a sharp puncture parallel to the film edge than a blown film of the same gauge. The package designer should therefore orient critical stresses away from the machine direction or specify a higher gauge only after comparing tear values measured in both directions.

    Seal response and hot tack must be measured on the target film because comonomer distribution and cast-line quenching affect seal initiation. Heat-seal tests are performed per ASTM F2029-20 and hot tack per ASTM F1921-20. A lower density of 0.925 g/cm³ indicates a seal initiation below that of a high-density polyethylene homopolymer, but the actual onset must be measured. The same applies to hot tack; a cast web can exhibit a narrower hot-tack window than a blown web if quench-induced crystal size distributions are less favorable. Converters are advised not to infer seal performance from density or MFR alone. Published data for LL4800N-specific hot-tack curves are limited outside the supplier’s technical literature, so pilot-line confirmation is required before commercial use.

    When a 25 µm Cast Web Reaches the Corona Treater at Line Speeds Above 150 m/min

    Corona treatment of LL4800N cast film requires thermal management and adequate exhaust. At line speeds above 150 m/min, web residence time under the electrode is short, so power density must be increased relative to slower lines. A corona station with a ceramic electrode and silicone-covered backing roll is normally operated to raise wetting tension to 38–42 mN/m for lamination or printing. Wetting tension is checked by ISO 8296:2003 or ASTM D2578-23 using a series of formamide/cellosolve dyne solutions. If treatment is excessive, chain scission creates low-molecular-weight oxidized species that can redeposit on the backside roll and transfer to the film surface as visible marks. Maintaining the pre-treater web temperature below 40 °C and cleaning the backing roll at intervals recommended by the equipment supplier reduces this failure mode. For converters that print on LL4800N, the treated surface should be measured at both edges and the center because corona treatment can vary across the web; edge-to-center variation greater than 2 mN/m suggests electrode gap drift or airflow nonuniformity.

    The use of LL4800N in cast stretch film requires attention to cling additives and coefficient of friction. Film-to-film and film-to-metal coefficients are evaluated by ASTM D1894-14. Cling performance in stretch wrap is measured as peel cling by ASTM D5458-18 or ASTM D4649-20; the supplier’s neat resin is not a formulated stretch product, so the converter must add the appropriate tackifier masterbatch and allow for bloom migration. If too much tackifier is added or the film is stored at elevated temperature above 40 °C, cling can increase unevenly and cause roll blocking. Blocking force is measured by ASTM D3354-18. At 250 % prestretch, a cast film made from LL4800N can maintain load containment if edge quality is uniform; however, the actual retained force must be verified on the specific wrapper because film tension, prestretch ratio, and load configuration interact.

    In coextruded food packaging, LL4800N can serve as a sealant layer in a cast line with two or three extruders. The melt flow rate of 4.0 g/10 min is close enough to many skin-layer LLDPE grades that layer stability is maintained, but the ratio of layer viscosities should be checked at the expected shear rate. Viscosity mismatch in a coextruded die can produce layer nonuniformity, especially at throughputs above 200 kg/h on a 1,500 mm die. The processor should use the supplier’s viscosity curves or generate capillary rheometry data under ISO 11443:2021 at apparent shear rates from 100 s⁻¹ to 1,000 s⁻¹ to match layers. When used as a sealant, the film must comply with the appropriate food-contact regulation for the intended market. For the United States, olefin polymers are evaluated under 21 CFR 177.1520; for the European Union, the finished film must meet the overall migration and specific migration limits of EU 10/2011. The converter is responsible for verifying end-use compliance because additives, printing inks, and lamination layers contribute to the final regulatory status.

    Regrind handling is a practical issue on cast-film lines. Edge trim of LL4800N can be ground and reintroduced into the feed stream at levels commonly up to 20 % without predrying, provided that the trim is clean and the moisture content remains below 0.05 %. In humid plants, edge trim should be transported through a dry-air or nitrogen-blanketed system before entering the hopper. If the regrind particle size distribution is too broad, the extruder feed zone may fluctuate, causing melt-pressure oscillations visible as gauge variation. A screen changer with a 100–150 µm mesh pack is often used on cast lines to trap degraded particles. The pressure drop across the screen pack should be trended; a rapid increase at constant throughput indicates gel accumulation or degraded regrind, and the pack should be changed before backpressure exceeds the extruder manufacturer’s limit.

    In hygiene films and lamination structures, blocking and coefficient of friction often control downstream converting. If LL4800N is extruded without an external antiblock additive, long roll storage at 30 °C can increase blocking force above the level accepted by a converter. Synthetic silica antiblock is typically used at low addition levels, but the exact dosage depends on cast-film gauge and the desired clarity. Because any particulate additive scatters light, haze measured per ASTM D1003-21 will increase as antiblock concentration rises. For applications where clarity is critical, the converter must balance blocking resistance against haze. Published haze values for LL4800N are available from Braskem’s technical data sheet for a specified gauge and additive package; these values should be used only as a reference and not as a specification for formulated films.

    LL4800N should not be substituted into injection molding, blow molding, or rotational molding applications. The 4.0 g/10 min melt flow rate is too high for large-part blow molding because parison sag becomes uncontrolled; it is not an injection-molding grade because the material lacks the required crystallization rate and mold-release package for short cycle times. Rotational molding requires sintering behavior that is not designed into this cast-film resin. The product is also not intended as a high-strength geomembrane or as a direct replacement for medium-density polyethylene in gas pipe. Its specification, additive system, and rheology are optimized for thin cast film from 12 µm to 50 µm; use outside that gauge range should be supported by pilot-line validation.

    The relationship between melt flow rate and cast-film thickness uniformity is nonlinear. On a chill-roll line, gauge uniformity depends on die lip uniformity, melt temperature stability, and the frozen-in strain between die and chill roll. A resin with 4.0 g/10 min MFR reduces the melt-pressure drop across a 0.5 mm die gap, which allows tighter mechanical die-lip adjustment without exceeding the die’s maximum pressure rating. Thickness variation is measured by an online beta or X-ray gauge and is typically reported as ± 2 % or better on a well-tuned line; however, the measurement band depends on line speed, die width, and noise filtering. If a converter switches from a 2.0 g/10 min blown-film grade to LL4800N, the first observed change is often a reduction in extruder motor load at the same throughput rather than a change in film optics.

    Migration of slip additives in LL4800N films follows established polymer diffusion kinetics. The time to reach plateau coefficient of friction after film production depends on storage temperature, crystallinity, and the slip molecule’s molecular weight. Because cast film has a lower crystalline orientation than blown film in the transverse direction, migration of a primary amide slip additive may be faster to the surface, but the effect is not easily predictable from density alone. Coefficient of friction can be monitored at 24 h, 48 h, and 7 days after winding to establish the bloom curve. If the film is laminated or printed before bloom is complete, adhesion may be affected; corona treatment immediately after casting may also alter the surface and change slip development.

    A recurring production-scale failure mode in cast film with LL4800N is the formation of optical gel defects downstream of the die. Gels may be oxidized resin, crosslinked particles, or contaminant from edge trim. When gel counts exceed the converter’s specification, the first step is to establish whether the gel is thermally oxidized polyethylene or foreign material by Fourier-transform infrared microspectroscopy. Oxidation bands at 1,720 cm⁻¹ indicate carbonylated species; if the gel is oxidized resin, the melt temperatures and hold-up time should be reduced. If the gel is unmeted pellet core, the feed section temperature profile or screw design may be the cause. Published data for the exact gel count of LL4800N are limited to the supplier’s lot-release information.

    For incoming quality control, the resin lot should be checked for melt flow rate and density before introduction into the silo. A capillary rheometer or melt indexer is appropriate for MFR per ASTM D1238-20, and a gradient column or gas pycnometer may be used for density per ISO 1183-1:2019. If the melt flow rate shifts by more than ± 0.3 g/10 min from the supplier’s nominal value, the processor should revalidate melt pressure, motor load, and gauge profile before resuming rated production. Density shifts above 0.928 g/cm³ or below 0.922 g/cm³ may indicate a lot segregation or sampling error and should be confirmed by a second test. Such operational boundaries are based on generic linear-low density polyethylene behavior and not a substitute for Braskem’s certificate of analysis.