Braskem Ll318 Lldpe Linear Low Density Extrusion Polyethylene

Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene

    • Product Name: Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 789339
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Melt Flow Ratio I21 I2 30
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 800%
    Flexural Modulus 240 MPa
    Vicat Softening Point 94°C
    Melting Point 123°C
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Haze 14%
    Gloss 45 50%
    Hardness Shore D 50

    As an accredited Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg polyethylene-lined bags, stacked on pallets, or 1,000 kg octabins for safe industrial transport and storage.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of Braskem LL318 LLDPE linear low density extrusion polyethylene, shrink-wrapped and secured.
    Shipping Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene ships as non-hazardous resin pellets, typically in 25 kg bags on pallets or in bulk bags. Transport in clean, dry trucks or containers at ambient conditions. Protect from moisture, sunlight, and excessive heat. Not regulated for transport.
    Storage Store Braskem LL318 LLDPE in a cool, dry, well-ventilated, indoor warehouse. Keep original packaging closed and palletized. Protect from direct sunlight, heat, moisture, and ignition sources. Avoid dust generation and static buildup. Segregate from strong oxidizers and incompatible materials. Maintain clean, dry floors; stack securely to prevent collapse. Follow first-in-first-out and consult the SDS for specific requirements. Do not expose to flames.
    Shelf Life Shelf life is typically 12 months when stored unopened in a dry, ventilated area, away from direct sunlight and heat.
    Application of Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene

    During single-screw blown-film conversion of Braskem LL318 on an 80 mm grooved-feed barrier-screw extruder with a 30:1 L/D and a 250 mm spiral mandrel die, the resin is processed in the melt-temperature band of 193–215°C, with die pressure typically remaining below 33.0 MPa when the die gap is held at 1.6 mm and the blow-up ratio is kept between 2.2:1 and 2.4:1. The grade has a nominal density of 0.918 g/cm³ per ASTM D792 and a melt index of 1.0 g/10 min per ISO 1133-1:2022. This operational window is selected for the production of 150–200 µm monolayer industrial waste containment liners used as daily landfill cell cover and as temporary lay-down barriers for contaminated soil stockpiles. The formulation is built on 100 phr of Braskem LL318, into which 2.5–3.5 wt% of a 40% carbon black masterbatch in an LLDPE carrier is added to achieve a dispersed carbon black content above 2.0% for ultraviolet stabilization during outdoor storage. A fluoropolymer-based polymer processing aid masterbatch is introduced at 0.5–0.8 wt% when spontaneous surface roughness on the outer bubble face indicates the onset of melt fracture. The blown film is quenched with an external air ring followed by an internal bubble stabilizer; the frost line is maintained at 7–9 die diameters to preserve dart impact resistance measured in accordance with ASTM D1709 method A. Industry compliance for such liners is anchored to ASTM D4635-16 for general-use polyethylene film, and tensile properties are verified by ASTM D882 at a crosshead speed of 500 mm/min. Terminal product types include landfill daily cover panels, oversize waste shrouds, and temporary containment sheets for demolition debris. Operational boundaries include the need to raise melt temperature to at least 210°C when external ambient temperature falls below 10°C; otherwise, gauge variation around the bubble circumference increases above ±8%. Recycled post-industrial regrind may be incorporated up to 15 wt%, provided the carbon black masterbatch dosage is recalculated based on total melt-phase carbon black concentration.

    Greenhouse film longevity under ISO 4892-2 weathering cycles with HALS packages

    Braskem LL318 is delivered to the mixing hopper as the primary polyolefin carrier in 180 µm triple-layer agricultural films, where the outer layers are formulated at 100 phr LL318 and the core layer consists of post-industrial recycled LLDPE at up to 30 wt%. For films intended for multi-season greenhouse and silage cover service, the stabilization package comprises 3.0–5.0 wt% of a 10% active hindered-amine light stabilizer masterbatch, corresponding to 3000–5000 ppm active HALS in the finished film, and 1.0–2.0 wt% of a 10% active benzophenone UV absorber masterbatch. This addition is specified against a target criterion of at least 50% retention of elongation at break after 3000 h of artificial weathering under ISO 4892-2 cycle 1, though published data for this specific LL318 configuration is limited and batch-specific validation on the actual extruder is required. Conversion is performed on a three-layer blown-film line with a 350 mm die and internal bubble cooling, at a die gap of 1.8 mm and a blow-up ratio of 2.5:1 to 2.8:1; melt temperatures are kept between 210°C and 230°C to disperse the stabilizer masterbatch without decomposing the benzophenone component. The frost line height is held at 8–10 die diameters. Industry compliance is specified under EN 13206:2017 for thermoplastic films used in agriculture and horticulture, with tensile and tear characterization per ISO 527-3 and ISO 6383-2. Terminal product types include multi-season greenhouse covers, silage pile covers, low tunnel films, and temporary fumigation tarpaulins. An operational boundary is documented: HALS loadings above 0.6 wt% active on a 75 mm barrier-screw extruder have been observed to elevate screw torque variability by more than 7% if the masterbatch is not pre-pelletized with a melt-index-matched carrier resin.

    Where frozen-food packaging requires a 60–80 µm sealant web with hot-tack strength sufficient to hold a nitrogen-flushed vertical form-fill-seal seal during product drop, Braskem LL318 is incorporated at 70–80 wt% in the heat-seal layer of a five-layer coextruded blown film, with the remaining 20–30 wt% comprising a high-pressure LDPE with a melt index of 2.0 g/10 min to lower the seal initiation temperature and increase bubble stability. The sealant layer is formulated on a 100 phr basis: 70–80 phr LL318, 20–30 phr LDPE, and 0.5–1.0 phr of a combined slip/antiblock masterbatch with active erucamide content of 2000–4000 ppm and active silica content of 5000–8000 ppm. Downstream conversion occurs on a five-layer coextrusion blown-film line with a 400 mm die, internal bubble cooling, and a die gap of 1.6 mm; the melt temperature in the sealant layer is held at 195–215°C, the blow-up ratio is limited to 2.0:1–2.3:1, and the frost line is placed at 4–6 die diameters to suppress orientation-driven curl after lamination. The resulting film is used as the inner sealant layer in polyester/PE and oriented polyamide/PE laminations for frozen vegetable, seafood, and prepared meal pouches. Compliance is established under FDA 21 CFR 177.1520(c) 3.1a for olefin polymers and EU Regulation (EU) No 10/2011, with overall migration testing conducted in food simulants A, B, and D2 as applicable. For fatty-food contact under EU 10/2011, specific migration of erucamide must be validated against the applicable SML; published data for this specific LL318 blend is limited, and the converter is required to test the exact laminated structure. An operational incompatibility is noted: amine-based photogravure lamination inks that are not fully cured can react with erucamide in the sealant layer, causing peel-strength loss at the lamination interface.

    What governs dart impact retention when FFS lines convert high-bulk-density fertilizers?

    On automated form-fill-seal packaging lines operating at 20–30 bags/min with a vertical fill head, the film converted from Braskem LL318 must balance dart impact resistance after creasing against the low coefficient of friction required for film transport over forming collars. Braskem LL318 is extruded into 120–180 µm monolayer FFS sack film on a 70 mm single-screw blown-film line with a 300 mm die, at a melt temperature of 200–220°C, a die gap of 2.0 mm, and a blow-up ratio of 2.0:1–2.5:1. The formulation uses 100 phr of LL318, 1.0–1.5 wt% of a 10% active erucamide slip masterbatch to achieve a kinetic coefficient of friction below 0.25 per ASTM D1894, and 0.8–1.2 wt% of a 20% active silica antiblock masterbatch to prevent blocking on the roll after heavy-gauge winding. Industry compliance for the finished sacks is anchored to ISO 21898 for drop resistance of filled sacks, while film tensile properties are measured per ISO 527-3 and impact resistance per ASTM D1709 method A. Terminal product types include fertilizer sacks, polymer resin bags, salt and mineral bags, and petrochemical packaging. The process window is narrow: increasing the slip masterbatch above 1.5 wt% to reduce the coefficient of friction below 0.20 typically forces a revalidation of dart impact resistance per ASTM D1709 method A because excess erucamide migrates to the film surface and creates stress discontinuities. Conversely, reducing the antiblock masterbatch below 0.8 wt% on a paper-interleaved roll can lead to blocking at storage temperatures above 30°C. The film is converted on FFS lines with a forming shoulder angle of 45°; the film’s machine-direction tear must exceed 4.0 N/mm according to ISO 6383-2 to avoid splitting during the fill-cycle shock.

    On high-speed three-layer cast stretch-film lines with 900 mm slot dies and three-roll cooling stacks, Braskem LL318 is metered into the core layer at 25–35 wt% of the total film mass, while the remaining 65–75 wt% is a metallocene LLDPE with a melt index of 4.0 g/10 min selected to reduce neck-in and maintain drawability at 500–700 m/min. The formulation is prepared as a gravimetric blend: 100 phr total polyolefin comprising 25–35 phr LL318 and 65–75 phr metallocene LLDPE; cling layers are separately dosed with 2–4 wt% of polyisobutylene-based cling masterbatch, and the outer slip layer receives 1.0–1.5 wt% of an erucamide/silica masterbatch. Conversion is performed at melt temperatures of 230–245°C, with the die gap set at 0.5 mm and the air gap adjusted to 120–150 mm before the primary chill roll maintained at 18–22°C. The film is drawn to 18–25 µm final thickness. Industry compliance for stretch film selection and testing is specified under ASTM D4649 and cling adhesion is measured per ASTM D5458. Terminal product types include industrial pallet unitisation film, high-containment stretch hoods, and manual hand-wrap rolls. The technical boundary is defined by the low melt index of 1.0 g/10 min for LL318: at line speeds above 700 m/min, melt pressure at the die entry can exceed the extruder manufacturer’s continuous-pressure limit on a 120 mm extruder, producing visible chevron melt fracture in the core layer unless the fluoropolymer processing aid dosage is increased to 0.8 wt%.

    When inline corona treatment reaches 44 mN/m for pressure-sensitive adhesive coating

    When inline corona treatment reaches 44 mN/m for pressure-sensitive adhesive coating, the cast film produced from Braskem LL318 is directed into a solventless adhesive coating station without an intermediate primer, provided the film is cooled to below 25°C before winding. This scenario is used for 30–60 µm mono- or three-layer surface-protection films for architectural polycarbonate panels and painted metal coil during transport and installation. The formulation is built on 100 phr of LL318, with 1.0–2.0 wt% of a 10% active erucamide slip masterbatch and 0.5–1.0 wt% of a 20% active silica antiblock masterbatch; a thinner skin layer is coextruded with 15–20 wt% of an ethylene-vinyl acetate copolymer containing 9–18 wt% vinyl acetate to improve anchorage of the pressure-sensitive adhesive. Downstream production is conducted on a 120 mm single-screw cast-film line with a 1,200 mm slot die and polished chrome chill roll; melt temperature is controlled at 215–230°C, die gap at 0.6 mm, and air gap at 90–120 mm. The chilled web is corona treated in-line to 42–46 mN/m wetting tension measured per ASTM D2578, then coated with a solventless acrylic pressure-sensitive adhesive at 5–10 g/m² dry coat weight. Industry compliance for peel adhesion is verified under ASTM D3330/D3330M, and film tensile properties are tested per ASTM D882. Terminal product types include temporary protective films for polycarbonate sheets, pre-painted aluminium coil, and glass edge guards. An operational boundary exists: erucamide loadings above 1.5 wt% can cause time-dependent adhesion decline on polycarbonate because surface migration changes the adhesive anchoring interface; quantitative adhesion-aging values must be established on the actual substrate.

    Free Quote

    Competitive Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LL318 is a linear low density polyethylene extrusion resin supplied in pellet form for blown film and related extrusion processes. It is classified by the manufacturer as an ethylene-alpha-olefin copolymer with a linear backbone and short-chain branching; this structure gives lower melt strength than high-pressure LDPE but higher melt extensibility and better downgauging potential. Under ASTM D1505 density-gradient testing, the typical density is 0.918 g/cm³. Under ASTM D1238 at 190°C and 2.16 kg, the typical melt flow rate is 1.0 g/10 min. The corresponding ISO 1133-1:2022 method uses the same nominal temperature and load, although interlaboratory bias between ASTM and ISO capillary dies can produce small differences. Density and melt flow rate are not sufficient to predict film performance; molecular weight distribution, short-chain branching distribution, and additive composition are lot-specific variables that must be confirmed from the certificate of analysis. Published data for the exact additive package of LL318 are limited; therefore, slip and antiblock levels should be obtained from Braskem technical documentation before line trials.

    For a 0.918 g/cm³ linear low density polyethylene, differential scanning calorimetry under ISO 11357-3 typically records a broad melting endotherm in the 120–124°C range. The broader composition distribution of a conventional Ziegler-Natta butene-based LLDPE typically produces a polydispersity index of 3–5, compared with 2–3 for many metallocene-catalysed grades. These class-level values are not a substitute for lot-specific analytical data for LL318. The resin should be stored indoors and allowed to reach ambient temperature before opening packaging at high humidity; condensation on cold pellets can introduce feed-throat moisture.

    What separates butene-based LL318 from LDPE and metallocene grades on blown film equipment?

    LDPE carries long-chain branching and a broad molecular weight distribution, which produces strain hardening and high melt strength. This allows large blow-up ratios and stable bubbles with die gaps up to 2.5 mm. Butene-based LL318 lacks long-chain branching and consists of a linear backbone with heterogeneous short-chain branching from a conventional Ziegler-Natta catalyst. Its extensional viscosity is lower at high Hencky strain rates, so a monolayer bubble can sag or flutter if the die gap is too wide or the frost line is too high. Typical die gaps for LL318 are 1.5–2.0 mm, and blow-up ratios of 2.0:1–3.0:1 are used on standard air-ring lines. Compared with metallocene-catalysed LLDPE, LL318 generally has broader composition distribution, lower extrusion pressure at the same melt flow rate, higher tolerance for LDPE/LLDPE recycle blends, and lower clarity. Its dart impact and tear balance may also differ at the same gauge because the broader short-chain branching distribution broadens the distribution of tie molecules. Shear rheology by ASTM D3835 or dynamic oscillatory rheology by ISO 6721-10 should be used for die design, because single-point melt flow rate at 1.0 g/10 min does not describe the low-shear structure that governs bubble stability. No universal blend ratio with recycled material can be fixed without melt filtration, gel-count measurement, and bubble-stability trials on the production die.

    Relative to high-density polyethylene extrusion grades, LL318 has a density near 0.918 g/cm³ and therefore produces softer, tougher films with lower tensile modulus. HDPE film grades with densities above 0.941 g/cm³ show higher stiffness but lower dart impact at equivalent gauge. Relative to high-pressure LDPE film grades, LL318 provides higher tensile strength and dart impact at equivalent gauge, but the low-melt-strength rheology narrows the bubble stability window and may require a lower die gap.

    On production-scale blown film lines, LL318 is typically processed on grooved-feed single-screw extruders with screw diameters of 45–75 mm and L/D ratios of 24:1–30:1. Die exit melt temperature is normally maintained between 180°C and 230°C. The upper limit is set by thermal degradation and odour generation; the lower limit is set by melt pressure and unmelted polymer. For a monolayer die with a diameter of 200 mm, frost line height is commonly set at 3–5 die diameters to balance machine-direction and transverse-direction orientation. Dual-lip air rings and internal bubble cooling, where fitted, increase output stability and reduce blocking. In cast film operations, LL318 can be run at melt temperatures of 230–260°C, but the lower melt strength relative to LDPE requires a shorter air gap and careful draw-ratio control to prevent edge weave and thickness variation. Output stability is also sensitive to pellet moisture; at relative humidity above 60%, condensation on cold pellets can introduce water into the feed throat, causing melt pressure oscillation and reduced throughput. Screen-pack selection is normally 20/40/100 mesh in monolayer film lines, but the finest mesh should be removed if melt temperature approaches 240°C to avoid excessive pressure drop.

    When a line is retrofitted with internal bubble cooling, output of butene-based LLDPE can increase by 20–40% on a 200 mm die, provided the air ring and die geometry are matched to the resin. The benefit is not intrinsic to LL318 alone but arises from the higher draw rates achievable with lower melt temperature and reduced heat-loss limitation.

    The decision between blown film and cast film is governed by the end-use property requirements. Blown film made from LL318 develops a higher degree of molecular orientation and folding symmetry, which favours balanced tear and dart impact in heavy-gauge liners. Cast film made from the same resin provides better clarity and thickness uniformity, but it has lower machine-direction toughness per unit gauge because of the low orientation and rapid quenching. Both processes require separate verification because the same pellet melt flow rate does not produce the same film properties under ASTM D882 and ASTM D1922.

    Melt fracture, die-lip buildup, and screw geometry boundaries

    Sharkskin melt fracture in LL318 is a die-lip instability that becomes visible when the wall shear stress at the die lip exceeds a critical value. On production dies, the onset can occur at die-lip shear rates near 1000 s⁻¹, but the exact threshold depends on die gap, melt temperature, polymer lot, and the presence of processing aids. Reducing die-lip shear by increasing die gap above 2.0 mm is not always an acceptable remedy because the melt strength of LL318 may then permit bubble sag. A more effective correction is to raise the die exit temperature toward 210–220°C or to use a polymer processing aid to lower wall slip resistance. Die-lip buildup is controlled by limiting die exit temperature to 230°C or below and by maintaining clean air surfaces. On a 45 mm grooved-feed extruder with a 30:1 L/D barrier screw, screw speeds above approximately 120 min⁻¹ can cause viscous heating that raises melt temperature beyond the set-point, increasing gel count and reducing bubble stability. For shutdown and purging, a low-melt-index LDPE purge is used to displace stagnant melt from spiral mandrel gaps and die lips. When die gap is increased from 1.5 mm to 2.0 mm, die-lip shear rate at constant output decreases by approximately 25%, but the resulting thicker melt web may increase orientation in the transverse direction and alter tear balance.

    When film thickness falls below 25 µm, dart impact and tear anisotropy dominate

    For monolayer film below 25 µm, machine-direction tear resistance is often lower than transverse-direction tear because rapid quenching and high draw orient the polymer chains in the machine direction. Converters should evaluate tear by ASTM D1922 Elmendorf and ISO 6383-2, tensile properties by ASTM D882 or ISO 527-3, and dart impact by ASTM D1709 Method A or Method B, depending on expected impact level. A single dart impact value cannot capture tear anisotropy, and the result is sensitive to frost line height, blow-up ratio, die gap, and melt temperature. Published data for the specific LL318 configuration at all gauge points is limited; lot-specific film property data must be obtained from Braskem technical service or from pilot-line trials. Increasing blow-up ratio toward 2.5:1–3.0:1 and reducing frost line height may partially rebalance tear properties, but the effect must be verified with full-cross-direction property mapping under the same test methods. At high blow-up ratios, transverse-direction tear can improve while machine-direction tear decreases further; therefore, the optimum frost line is not fixed and must be determined according to the end-use loading direction.

    LL318 is an ethylene-alpha-olefin copolymer covered by polyolefin food-contact regulations when supported by appropriate migration testing. The base polymer is intended to be used under FDA 21 CFR 177.1520 for olefin polymers; the extractives limits are prescribed in 21 CFR 177.1520(d) and depend on food type and temperature. For European Union applications, EU Regulation 10/2011 applies to plastic materials and articles intended to come into contact with food. Overall migration testing under EN 1186-1 must not exceed 10 mg/dm² or 60 mg/kg, and specific migration limits for additives are given in EU 10/2011 Annex I. For REACH, the polymer itself is exempt from registration as a polymer under Article 2(9), but monomers and additives must be registered; article notification under REACH Article 33 applies if a substance of very high concern is present above 0.1% w/w. The resin should be stored in dry indoor conditions and allowed to reach room temperature before opening packaging at high humidity to avoid condensation on pellet surfaces. If the resin is compounded with colour masterbatch or processing aids, the final article must be retested for migration and organoleptic effects because additive interaction can shift specific migration results.

    Standard or regulationMethod or clauseBoundary relevant to LL318
    ASTM D1238Melt flow rate, 190°C / 2.16 kgTypical value 1.0 g/10 min; lot range must be confirmed
    ASTM D1505Density by gradient columnTypical value 0.918 g/cm³
    ISO 1133-1:2022Melt mass-flow rateSame nominal conditions as ASTM D1238
    FDA 21 CFR 177.1520Olefin polymers for food contactExtractives limits per 177.1520(d); fatty-food conditions require separate confirmation
    EU 10/2011Plastic food-contact articlesOverall migration 10 mg/dm² or 60 mg/kg under EN 1186-1
    REACH Article 33SVHC communicationThreshold 0.1% w/w in article

    Typical applications include general-purpose blown film, liners, carrier bags, and agricultural film. In these applications, LL318 is selected when the converter requires a balance between downgauging, tear resistance, and processability on conventional extruders. The final material choice must be validated by measuring dart impact under ASTM D1709, tear under ASTM D1922, and film tensile properties under ASTM D882 on production film, because screw geometry, die gap, air ring, and frost line height shift the property envelope more than the pellet melt flow rate alone.