Braskem Ll318 Lldpe Cast Film Extrusion Polyethylene Copolymer

Braskem LL318 LLDPE Cast Film Extrusion Polyethylene Copolymer

    • Product Name: Braskem LL318 LLDPE Cast Film Extrusion Polyethylene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 746262
    Polymer Type Linear Low Density Polyethylene Copolymer
    Comonomer Butene-1
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 3.2 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 94 °C
    Tensile Strength At Yield Md 10 MPa
    Tensile Strength At Break Md 28 MPa
    Tensile Strength At Break Td 24 MPa
    Elongation At Break Md 600 %
    Elongation At Break Td 700 %
    Dart Impact Strength 120 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 450 g
    1 Secant Modulus Md 190 MPa
    1 Secant Modulus Td 200 MPa
    Haze 4 %
    Gloss 45 75
    Coefficient Of Friction 0.2

    As an accredited Braskem LL318 LLDPE Cast Film Extrusion Polyethylene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped, protecting Braskem LL318 LLDPE cast film extrusion copolymer.
    Container Loading (20′ FCL) 20′ FCL loaded with Braskem LL318 LLDPE cast film extrusion polyethylene copolymer in 25 kg bags, palletized, stretch-wrapped, and secured.
    Shipping Braskem LL318 LLDPE Cast Film Extrusion Polyethylene Copolymer is shipped as non-hazardous solid polyethylene pellets in moisture-barrier bags, octabins, or bulk trucks. Keep dry, cool, and away from direct sunlight, heat, and ignition sources. Use standard industrial handling; no special DOT hazard classification is required.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers closed, labeled, and palletized to prevent moisture, contamination, and dust. Protect from UV exposure and physical damage. Avoid strong oxidizing agents. Do not store near food, drink, or animal feed. Follow the manufacturer’s SDS and local regulations. Use appropriate PPE when handling.
    Shelf Life Typically two years when stored unopened in original packaging under cool, dry, ventilated conditions, away from heat and direct sunlight.
    Application of Braskem LL318 LLDPE Cast Film Extrusion Polyethylene Copolymer

    In high-output pallet-unitization converting, Braskem LL318 is fed as the core backing resin in monolayer and A/B/C coextruded machine stretch film. The formulation window in cast-film lines typically loads LL318 at 68–82 wt% in the core layer, with a metallocene-catalyzed LLDPE skin-layer plastomer at 10–20 wt%, a glycerol-mono-oleate or polyisobutylene cling agent masterbatch at 2–5 wt%, and a fluoropolymer processing aid at 0.5–1.5 wt% to suppress melt fracture at high line speeds. Compliance verification on the converted film follows ASTM D882 for machine-direction and transverse-direction tensile properties, ASTM D5458 for cling force between film layers, ASTM D5748 for protrusion puncture resistance, and ASTM D1894 for machine-side coefficient of friction. Downstream processing runs on cast-film lines with single-screw extruders at L/D 30:1, a coat-hanger flat die with 0.6 mm die gap, air gap in the 8–12 mm band, a polished chill roll held at 18–22 °C, electrostatic edge pinning, and line speeds from 450 m/min to 650 m/min; edge trim is reintroduced through a repropelletizing loop as a dry, contaminant-limited regrind stream. Terminal products are machine-grade pallet wrap rolls commonly at 500 mm web width, 20–25 µm thickness, and 1,500–2,400 m roll lengths, specified for A-type pre-stretch carriages and high-throughput logistics wrapping of glass containers, building materials, and corrugated unit loads.

    Which Coextruded Sealant Web Formats Remain Within EU 10/2011 Migration Limits?

    For direct-contact cast sealant webs used in fresh produce, bakery, and frozen food overwrap, LL318 is evaluated under FDA 21 CFR 177.1520 olefin polymer conditions of use B through D and under Regulation (EU) No 10/2011, with compliance verified by EN 1186-1 total migration and EN 13130-1 specific migration protocols. The resin is most often specified in the sealant skin layer at 72–85 wt%, combined with a low-vicat LDPE at 5–10 wt% to widen the hot-tack sealing window, a synthetic silica/amide slip-antiblock masterbatch at 2–4 wt%, and a polyolefin plastomer at 5–12 wt% for puncture resistance in tray overwrap. Coextrusion is performed with a three-layer feedblock and a 0.8 mm die gap, a chill roll set at 22–26 °C, and corona treatment at 38–42 mN/m for subsequent flexographic printing or adhesive lamination. Operational boundaries apply above 85 °C seal-bar temperatures; converter qualification does not extend to retort sterilization, hot-fill above 80 °C, or fatty-food simulant D2 contact without layer-specific migration testing. Terminal product types include vented berry clamshell overwrap, frozen vegetable polybag, barrier lamination sealant web, and bakery tray film.

    Silage Bale Wrap: Oxygen Ingress, UV Quenching, and Cling Decay

    Baled silage wrap made with LL318 carries the primary function of maintaining anaerobic fermentation through high pre-stretch cling and puncture survival. The application-specific compliance benchmark is EN 14932, with tensile properties measured by ISO 527-3, tear propagation by ISO 6383-1, and UV weathering by EN 13206 covering-film protocols where regional specifications require separate UV-stability documentation. Formulation typically places LL318 at 60–70 wt% in the outer and core layers, an octene-based metallocene LLDPE at 18–25 wt% for dart impact retention, a hindered-amine light stabilizer and carbon-black or titanium dioxide masterbatch at 3–5 wt%, and a cling agent masterbatch at 0.5–1.5 wt%. Production uses a 1.0 mm die gap with a matte-finished chill roll at 20–25 °C, line speed limited to 300–400 m/min to retain film flatness, and an in-line pre-stretch unit that simulates baler application at 55–70% elongation before winding into 25–35 µm, 750 mm wide rolls. LL318 is not an oxygen-barrier polymer; oxygen transmission through a 25 µm film is governed by ASTM D3985, but no barrier claim is made and the film is positioned strictly as a cling and mechanical protective layer. Terminal product types are round bale wrap for grass silage, haylage, maize silage, and bale stack covers in seasonal forage storage.

    When Pre-Stretch Activation Approaches Yield Across 300% Draw Ratios

    High-yield pre-stretch machine films represent the most technically demanding cast-film application for LL318. The converter operates two counter-rotating rollers that impose a draw ratio of 200–300% before the film contacts the pallet load; this places the film beyond the yield point but below the machine-direction break point. LL318 is formulated in the core at 65–80 wt%, with a metallocene-catalyzed LLDPE skin-layer resin at 12–20 wt%, a polyisobutylene cling masterbatch at 2–4 wt%, and a processing aid at 0.3–0.8 wt%. Elastic recovery and retained load-holding capacity are characterized by ASTM D5459 for machine-direction stretch cling film, ASTM D882 for tensile hysteresis, ASTM D5748 for puncture resistance after pre-stretch, and ASTM D5458 for cling. The critical processing conflict is neck-in after die exit; with LL318-rich formulations, a 0.6–0.8 mm die gap and an 8–12 mm air gap produce neck-in of 8–12% on the chill roll, which if not compensated by edge-trim and die-deckle tuning causes edge bead and uneven stretch activation. Melt-curtain instability appears at line speeds above 550 m/min when the process temperature at the die exit drops below 225 °C; the converter must therefore run flat temperature profiles of 220–245 °C across zones and limit chill roll water temperature drift to ±1.5 °C to avoid thermal striations. Published data for this specific configuration is limited, so the following table represents a conservative converter specification window rather than universal values.

    ParameterTest Method200% Pre-Stretch250% Pre-Stretch300% Pre-Stretch
    Retained MD elongation at breakASTM D882≥350%≥280%≥220%
    Protrusion puncture resistance retentionASTM D5748≥85%≥75%≥65%
    Cling force, hand-roller methodASTM D545850–90 g45–80 g40–70 g

    Terminal products are pre-stretched machine film rolls for high-speed pallet wrappers certified for 300% pre-stretch carriages; any lot failing the retained puncture floor is diverted to lower-draw manual applications.

    After a corona-treated low-slip skin layer is added to a cast coextrusion, LL318-based films are used as temporary surface-protection masking on flat metal, rigid polymer sheet, and pre-painted coil. The product is specified not by food-contact legislation but by ASTM D3330 for peel adhesion to stainless steel, ASTM D882 for tensile elongation, ASTM D2578 for wetting tension after corona treatment, and ISO 527-3 for film tensile properties. Typical converter formulation loads LL318 at 65–75 wt% in the bulk layer, low-density polyethylene at 10–20 wt% to adjust the peel plateau, an ethylene-vinyl acetate copolymer at 5–10 wt% for conformability, and an antistatic/anti-UV masterbatch at 1–3 wt% where masking periods exceed 30 days outdoors. Production is run on a cast line with a 0.8 mm die gap, a matte chill roll to prevent blocking, skip-plasma treatment on one face only, and slitting to custom widths between 50 mm and 1,500 mm. The most common failure is peel escalation after heat aging; converters therefore validate peel retention at 60 °C for 72 h and reject lots if stainless-steel peel exceeds 2.0 N/25 mm after aging, as measured by ASTM D3330. Terminal product formats include laser-protective masking for stainless steel architectural sheet, temporary film for PVC window profiles, and polycarbonate glazing protection during fabrication.

    Wide-Die Stretch Hood Converting Constrains Melt Curtain Stability and Transverse Draw

    Stretch hood converters use LL318 in the outer layers of coextruded cast film because the resin’s low gel count and draw-down stability reduce the incidence of melt-curtain sag on wide dies. The governing performance standards for the finished hood are ASTM D882 for tensile properties, ASTM D5748 for puncture resistance, ASTM D5458 for cling behavior, and EN 14932 where pallet hoods are compared with bale-wrap stretch films; warehouse logistics buyers additionally audit ASTM D5414 for load-containment film behavior under vibratory motion. Standard formulations allocate 55–65 wt% LL318, 15–25 wt% very-low-density polyethylene or plastomer for low-temperature impact strength, 5–12 wt% metallocene LLDPE for tear resistance, 2–4 wt% slip/antiblock masterbatch, and 0.5–1.0 wt% processing aid. The cast line is configured with a 1.2 mm die gap, a 1,200–1,800 mm die width, air gap below 10 mm, a 30–35 °C textured chill roll for matte outer surfaces, and downstream gusseting that forms 50–120 µm hoods. Neck-in on wide dies is managed by die-deckle adjustments and edge trim at 3–6% of web width; if the melt curtain enters the chill roll with variable velocity across the web, the resulting transverse thickness variation creates weak points during pallet hood application. Terminal products are stretch hoods for palletised building materials, chemical drums, bagged cement, and appliance loads, where the film is applied by stretch hood machines at 80–120% stretching in both machine and transverse directions.

    Free Quote

    Competitive Braskem LL318 LLDPE Cast Film Extrusion Polyethylene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LL318 is a linear low-density polyethylene copolymer supplied as a cast-film extrusion grade. The nominal density is 0.918 g/cm³ when tested to ASTM D1505, and the nominal melt flow rate is 2.7 g/10 min at 190 °C/2.16 kg when tested to ASTM D1238. Producer technical literature identifies the product as a hexene-comonomer LLDPE for high-drawdown cast film; however, the specific molecular weight distribution and comonomer placement are not fully disclosed in public datasheets. The base resin is thermally stabilised, and surface functionality such as slip or antiblock is typically added by masterbatch dosing at the extruder hopper. The balance of density and melt flow places LL318 in the thin-gauge cast film segment, where melt strength is intentionally lower than blown-film grades to allow rapid quench and gauge reduction below 25 µm.

    In direct comparison with Braskem LL218, which is specified at 2.0 g/10 min for blown-film bubble stability, LL318 runs with lower head pressure and permits higher screw speed on a given single-screw line. The trade-off is that LL318 has lower melt tension and is not recommended for tubular film processes requiring self-supporting bubble geometry. Compared with metallocene-catalyzed LLDPE grades used in high-clarity cast film, LL318 is generally described in producer literature as a conventional Ziegler-Natta grade: broader molecular weight distribution supplies shear thinning and drawdown robustness, while optical haze remains higher than a metallocene grade of equivalent density. Published data for the exact molecular weight distribution of LL318 is limited.

    Table 1 summarises the typical physical property profile from producer technical literature. The values are not lot-release specifications; they depend on film thickness, chill roll temperature, line speed, and additive loading. Machine-direction and transverse-direction values are measured on 25 µm cast film unless otherwise noted.

    Typical property profile of Braskem LL318 cast film
    PropertyTest methodTypical value
    DensityASTM D15050.918 g/cm³
    Melt flow rateASTM D12382.7 g/10 min
    Tensile strength at break, MDASTM D88235–41 MPa
    Tensile strength at break, TDASTM D88228–34 MPa
    Elongation at break, MDASTM D882600–700%
    Elongation at break, TDASTM D882700–820%
    Elmendorf tear, MDASTM D192280–110 gf
    Elmendorf tear, TDASTM D1922300–400 gf
    Dart drop impact, F50ASTM D1709A70–85 g
    HazeASTM D10032.5–4.5%
    Gloss at 60°ASTM D245780–90

    What Limits the Use of LL318 in Tubular Film Processes?

    Melt tension and elongational viscosity are the limiting variables. In a blown-film line, the bubble is supported by internal air pressure; a polymer with 2.7 g/10 min melt flow and low melt strength tends to exhibit bubble instability, draw resonance at lower blow-up ratios, and poor gauge uniformity. Production-scale evaluation on a 90 mm 30:1 L/D blown-film extruder would require a melt temperature below 200 °C to preserve bubble stability, which then reduces output and increases extruder torque. The operational window becomes too narrow for economical processing. Cast film lines avoid this limitation by quenching the melt curtain on a chill roll within 10–25 mm of the die exit.

    In cast film, the critical process variables include die gap, air gap, chill roll temperature, and vacuum box pressure. A typical high-speed line configuration for 20 µm LL318 film uses a coat-hanger die with a die gap of 0.6 mm, an air gap of 12 mm, and a chill roll surface temperature between 15 °C and 25 °C. The melt temperature at the die is commonly maintained between 240 °C and 260 °C. Below 230 °C, melt fracture may appear as transverse surface roughness; above 280 °C, oxidative gel particles become more frequent after prolonged residence time. The resin is not hygroscopic and does not require pre-drying under normal handling; moisture issues in cast film are generally attributable to reclaimed trim or hygroscopic masterbatch.

    Capillary rheometry data for LL318 are not provided in public datasheets; however, with a melt flow rate of 2.7 g/10 min, the resin's low-shear viscosity at 190 °C is lower than extrusion grades specified at 1.0 g/10 min. In a single-screw extruder, this reduces specific energy input but also reduces viscous heating. Processors sometimes compensate by running higher barrel temperature set points or by selecting a screw with more aggressive solids conveying. Published shear-viscosity data for this specific configuration is limited.

    Air-Gap Quenching and Mechanical Anisotropy in Cast Film

    Short air gaps and low chill roll temperatures increase quench rate, reduce spherulite size, and improve optical haze. At the same time, rapid quenching of an already drawn melt curtain freezes in molecular orientation. As a result, Elmendorf tear values in the machine direction are typically lower than in the transverse direction. The property profile in Table 1 gives an MD tear of 80–110 gf and a TD tear of 300–400 gf, a ratio that can approach 4:1. This anisotropy is not specific to LL318 alone; it is characteristic of cast-film LLDPE and becomes more pronounced at line speeds above 300 m/min. When transverse-direction tear resistance is the critical end-use requirement, the air gap should be kept at the lower end of the recommended range, but at the cost of increased edge neck-in. This trade-off is a central process conflict in high-speed cast film production.

    Dart drop impact follows a thickness-sensitive response. At 25 µm, the typical value is in the range of 70–85 g; at 12 µm, published data for this specific configuration is limited, but the practical rule is that dart impact does not scale linearly with thickness. Converters targeting high puncture resistance in thin stretch film often blend LL318 with a metallocene LLDPE at addition levels between 10 wt% and 30 wt% to recover toughness without sacrificing drawdown. The blend is prepared by pellet mixing at the hopper; a single-screw extruder with a Maddock mixing section is usually sufficient for homogeneity.

    When Edge Neck-In and Draw Resonance Dictate Line Settings

    The melt curtain exiting a cast die is subjected to uniaxial extension in the air gap. Edge neck-in reduces final web width and creates thickened edges that must be trimmed. With LL318, neck-in increases when air gap is lengthened, melt temperature is raised, or die lip opening is narrowed. On a 1,500 mm die running 20 µm film, the internal deckle is normally set 5–8% wider than the target trimmed width. Edge trim may be reclaimed by an in-line grinder and fed back to the extruder at levels up to 10 wt% without significant loss of optical quality, provided the trim is clean and adequately ground.

    Draw resonance appears as alternating thick and thin bands in the machine direction, visible as gauge variation on the winder. It is sensitive to the extension rate and the melt curtain's resistance to strain hardening. LL318, like many linear polyethylenes, lacks strong extensional strain hardening, so the stable processing window closes at high draw ratios. The typical correction sequence is to reduce line speed, reduce air gap, increase die gap, or lower melt temperature. In some lines, a vacuum box or electrostatic pinning system stabilises the curtain and permits higher line speed; vacuum box pressure is usually regulated between 5 mbar and 20 mbar relative to ambient. Published data for the precise onset of draw resonance in industrial LL318 processing is limited because line geometry and film thickness introduce strong interactions.

    Gel count measurements on cast film are typically performed using a laser gel counter or camera system. For LL318 in 25 µm film, acceptable gel counts are usually defined by end-use specifications rather than by a universal standard. Oxidative gels originating from stagnant melt regions can be reduced by streamlined die design and by avoiding barrel temperature setpoints above 260 °C in the rear zones. A screw with a barrier profile and low-shear mixing elements reduces local viscous heating; this becomes relevant when the extruder is run near maximum speed.

    In multilayer cast film, LL318 is frequently assigned to a core layer for drawdown and economics. If the adjacent skin layer is a high-viscosity LDPE or high-melt-strength material, the viscosity ratio should be kept below 2:1 at the processing shear rate to avoid interfacial instability. Layer instability may appear as wavy interfaces or surface mottling before it is detected by ordinary thickness gauges. The melt distribution is controlled by a feedblock, and the use of melt pumps on each extruder improves layer uniformity to within ±0.5 µm on a 20 µm three-layer structure.

    Cast stretch films require controlled surface friction to unwind without blocking. The base LL318 without slip additive may exhibit blocking at high roll hardness. Erucamide or oleamide slip concentrates are added at 0.1–0.3 wt% active slip, but the slip migration to the surface occurs over hours to days. Immediately after winding, the coefficient of friction is higher; after 24–48 h, it stabilises to a range of 0.20–0.30 when measured to ASTM D1894. Excess slip above 0.5 wt% can cause plate-out on the chill roll and surface haze. The specific slip package must be selected against the desired unwinding equipment and post-processing steps such as printing or lamination.

    Corona Treatment and Surface Decay in Cast Stretch Films

    For printing, metallisation, or lamination, LL318-based cast film is subjected to corona discharge treatment. The surface tension is typically raised from an untreated level of 30–32 mN/m to 40–46 mN/m, measured with ASTM D2578 test fluids. Treatment decay occurs over time, especially in the presence of migrating slip additives or high storage temperature. For a 20 µm cast film stored at 35 °C, rechecking surface energy before lamination is necessary after 30 days; otherwise wetting failures can occur. In-line corona treatment at the cast line immediately before the winder is preferred to off-line treatment because the fresh surface has fewer oxidised species at the point of treatment.

    Heat sealability of unblended LL318 is limited by its melting point and density. In lamination and overwrap structures, sealing is achieved by blending with a lower melting plastomer or by coextruding a sealing skin. The seal initiation temperature of unblended LL318 is above 105 °C; a useful seal plateau for medium-duty packaging is typically reached at 120–140 °C with 0.5–1.0 s dwell and 2–4 bar jaw pressure. Published data for this specific configuration is limited.

    In turret-style cast stretch lines operating at 600 m/min, the pre-stretch ratio for LL318-based film is commonly set between 200% and 250%. The limiting factor is not the film's machine-direction elongation but the propagation of transverse tears at the film edge. Edge quality before pre-stretch becomes critical, because a small nick in the trimmed edge can propagate under high tension and cause web breaks. Some converters therefore use in-line edge slitting with razor blades positioned within 5 mm of the pinned film edge to maintain a clean cut.

    Regulatory compliance for LL318 depends on the additive package and final film construction. For U.S. food-contact applications, the resin is evaluated against 21 CFR 177.1520(c) 3.2a; the converter must verify that the finished article meets the intended use conditions and migration limits. For EU applications, Regulation (EU) 10/2011 applies to plastic food-contact materials, including overall migration testing under food simulants. Other frameworks encountered in supply-chain documentation include REACH Regulation (EC) 1907/2006 and the RoHS Directive 2011/65/EU. Braskem product stewardship documentation should be consulted for lot-specific regulatory statements; no independent certification is implied by property data.

    Regulatory reference points commonly requested for cast-film LLDPE packaging
    FrameworkReferenceScope
    US food contact21 CFR 177.1520(c) 3.2aOlefin polymers for food packaging subject to FDA conditions
    EU food contactRegulation (EU) 10/2011Plastic materials and articles intended for food contact
    REACHRegulation (EC) 1907/2006Substance registration and SVHC screening
    RoHSDirective 2011/65/EURestriction of hazardous substances in electrical/electronic equipment

    Operational boundaries for LL318 include a maximum continuous melt temperature of 280 °C; excursions above 290 °C increase the risk of oxidative gel formation, especially in dead spots in the die and feedblock. The resin should not be stored in direct sunlight or at temperatures above 50 °C for extended periods because oxidation and additive migration may occur. It is not suitable for continuous service above 80 °C or for hot-fill containers requiring low creep. The polymer is olefinic and can swell in aromatic solvents, chlorinated hydrocarbons, and certain mineral oils; such contact should be avoided unless validated for the specific service condition.