| HS Code | 572164 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.918 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 2.1 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 95 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 22 MPa |
| Elongation At Break | 800% |
| Dart Drop Impact | 110 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 7% |
| Gloss 45 | 80% |
| Coefficient Of Friction | 0.20 |
| Additive Package | Slip and antiblock |
| Form | Pellets |
As an accredited Braskem LL218/21 Cast Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem LL218/21 is supplied in 25 kg polyethylene bags, 40 bags per pallet, totaling 1,000 kg per pallet. |
| Container Loading (20′ FCL) | 20′ FCL loaded with Braskem LL218/21 LLDPE cast film extrusion resin in 25 kg bags, palletized and shrink-wrapped for transport. |
| Shipping | Braskem LL218/21 Cast Film Extrusion Linear Low Density Polyethylene is a non-hazardous, non-regulated solid resin. Ship in sealed 25 kg bags or octabins, keeping packages dry, clean, and protected from heat, moisture, and sunlight. Transport in covered, ventilated vehicles; store in cool, dry conditions. |
| Storage | Store Braskem LL218/21 in original, sealed packaging in a cool, dry, well-ventilated area. Keep away from direct sunlight, heat, flames, and strong oxidizing agents. Protect from moisture, dust, and contamination. Maintain ambient temperatures and avoid excessive stacking or prolonged UV exposure. Use first-in, first-out inventory practices. Ensure containers are clearly labeled and closed when not in use. |
| Shelf Life | Typically 12 months when stored unopened in a cool, dry, well-ventilated area, away from direct sunlight, heat, and moisture. |
The conversion of Braskem LL218/21 into cast hand stretch wrap is centred on a 3-layer coextrusion line equipped with a 2,500 mm die width, 0.6–0.8 mm adjustable lip gap, and a polished primary chill roll maintained at 18–24°C. Melt temperature at the feedblock is held at 240–260°C. The lower limit reduces oxidative degradation during prolonged runs and the upper limit improves gauge uniformity at line speeds above 450 m/min. Edge trim generated at 5–8% of web width is reintroduced at 10–20 wt%. Recycled content above 25 wt% produces gel particles larger than 200 µm that are visible on laser inspection and that accumulate on the die lip after 48–72 hours of continuous production.
The nominal density of this cast-film grade is generally reported between 0.917 g/cm³ and 0.920 g/cm³ under ASTM D792. Melt-flow rate measured to ISO 1133-1:2022 at 190°C/2.16 kg is commonly in the range 1.8–2.2 g/10 min. The exact certificate value should be verified for each lot before process parameters are locked. The cling force of a 23 µm cast stretch film is adjusted with a polyisobutene masterbatch at 1–3 wt% and measured by ASTM D5458; the accepted peel cling range on a standard steel panel is 1.5–3.0 N/25 mm for machine-wrap and hand-wrap grades. Erucamide slip is dosed separately at 300–800 ppm to modify the coefficient of friction measured by ASTM D1894, but a coefficient below 0.15 increases roll telescoping during transit.
Pre-stretch at 200–250% on powered hand dispensers requires the film to retain a machine-direction elongation at break above 400% when tested by ASTM D882. Dart impact of a 20 µm film measured by ISO 7765-1 method A typically exceeds 100 g, but the value falls rapidly when chill-roll temperature is raised above 30°C or when die-lip deposit roughness exceeds 0.5 µm. Gauges below 10 µm approach the melt-fracture boundary; the die temperature is increased by 5–8°C or the lip gap is narrowed to 0.5 mm to stabilize the web. Narrow gaps raise backpressure and require backwash screen monitoring at 72-hour intervals. Chill-roll condensation below 10°C creates transverse optical bands, so the water circuit is kept at or above the plant dew point rather than cooled to the lowest permitted temperature.
When LL218/21 is converted into a 20–35 µm mono-layer film for overwrapped leafy produce or baked goods, the completed film formulation must satisfy FDA 21 CFR 177.1520(c)3.1a and EU 10/2011 as amended. Overall migration is determined under EN 1186-1:2002 using 95% ethanol and isooctane simulants; the limit is 10 mg/dm². Base resin compliance is not sufficient because slip and antiblock masterbatches must also carry food-contact approvals and must be listed in the declaration of compliance.
Erucamide slip above 600 ppm creates visible bloom that reduces heat-seal strength and may produce roll blocking. The coefficient of friction measured by ASTM D1894 is generally specified between 0.15 and 0.30. Impulse sealing at 130–150°C and 0.3 MPa dwell must produce a seal force of at least 4 N/15 mm when tested to ASTM F88; values below this level lead to produce bag leakage at distributor level.
Surface protection films for stainless steel, anodized aluminium profiles, and furniture-grade MDF are produced from LL218/21 at 25–45 µm thickness. The web is corona-treated inline to 38–42 mN/m measured by ASTM D2578. Treatment above 50 mN/m creates low-molecular-weight oxidation products that reduce anchorage of water-based acrylic coatings; peel adhesion on stainless steel measured by ASTM D3330 may fall below 2 N/25 mm after 7 days at 40°C. Migratory additives such as erucamide are excluded above 200 ppm because warehouse aging accelerates bloom into the adhesive layer.
The cast line is run at 230–245°C and 150–250 m/min to limit gel formation. Trim recycling above 15 wt% increases die-lip deposits; the die is cleaned every 7–10 days when producing clear protection film. Machine-direction elongation at break is specified above 500% under ASTM D882 to permit removal at 180° without tearing. For electronic component protection, surface resistivity is controlled below 1012 Ω/sq by IEC 61340-5-1. Amine-based antistatic additives are incompatible with long-term clarity and should be replaced with non-amine esters when the film is stored in closed containers above 35°C.
Extrusion lamination onto 12–18 g/m² spunbond nonwoven is a cast-process variant in which Braskem LL218/21 forms the impermeable layer in diaper backsheets and sanitary pads. Die melt temperature is set at 290–315°C. Fibre penetration fails below 280°C, and thermal degradation with visible smoke begins above 330°C. At a coat weight of 23 g/m², the calculated polymer thickness is approximately 25 µm using a density of 0.918 g/cm³.
Online optical inspection rejects defects larger than 50 µm; the accepted pinhole count is 1/m² maximum because the backsheet must withstand a water penetration test at 50 mbar for 2 min. Skin-contact compliance is assessed under REACH 1907/2006 and, where specified, STANDARD 100 by OEKO-TEX class I. The film is also edge-trimmed at 6–10% and the trim can be reused in the core layer only; reuse in the skin layer above 10 wt% increases gel-related pinholes.
Stretch hood structures use LL218/21 in the core of a 3-layer to 5-layer coextruded film with total thickness 80–150 µm. The core layer is 40–60% of the total structure. The skins are generally a metallocene-catalyzed C6-LLDPE. Machine-direction tear strength measured by ASTM D1922 is maintained above 20 N/mm in the finished film. Cold-storage pallets at -20°C require a dart drop impact of at least 2.5 J at 100 µm when tested by ISO 7765-1 method A.
Heavy-gauge cast extrusion is heat-transfer limited. Line speed is held at 80–150 m/min, and the primary chill-roll wrap angle is set between 240° and 300° to reduce curl. Wrap angles below 180° produce asymmetric surface cooling and web curl that cannot be corrected at winder tension below 120 N/m. Printed films are treated to 36–40 mN/m; overloaded treatment above 44 mN/m increases the seal initiation temperature by 5–8°C, which narrows the sealing window when hoods are welded at 140–160°C. Published comparative data for LL218/21 in this specific coextruded structure is limited; the acceptance ranges above are industrial process targets and should be confirmed against the supplier lot certificate.
When LL218/21 is modified for agricultural silage bale wrap, the converter compounds carbon black at 3–5 wt% and a hindered amine light stabilizer at 2,000–4,000 ppm. The film is produced at 25–40 µm thickness. Accelerated weathering to ISO 4892-2 cycle 1 for 1,000 hours must retain at least 50% of the initial tensile elongation measured by ASTM D882. Black pigmentation increases chill-roll release temperature by 2–4°C because of higher radiant absorption; line speed is reduced by 5–10% or the water circuit temperature is lowered to maintain gauge stability. Silage acids and ammonia in storage require the exclusion of amine-based antistatic additives because those compounds accelerate yellowing and reduce UV stabilizer efficiency.
Competitive Braskem LL218/21 Cast Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem LL218/21 is a cast film extrusion linear low density polyethylene based on an ethylene-butene copolymer. The grade carries nominal density and melt flow rate values of 0.918 g/cm³ and 2.1 g/10 min under ASTM D1505 / ISO 1183-1:2019 and ASTM D1238 / ISO 1133-1:2022, respectively. The material is supplied in pellet form with antioxidant stabilization and is intended for cast film lines producing industrial packaging, lamination webs, overwrap, and thin-gauge flexible structures. It is not a blown film grade; the melt index and elongational viscosity are tuned for chill roll solidification rather than bubble stabilization. The butene comonomer differentiates the grade from hexene- or octene-copolymer linear low density polyethylene products by altering short-chain branching distribution, which influences tear resistance, hot-tack behavior, and heat seal initiation in downstream conversion. Exact additive package and lot-specific values should be confirmed against the current Braskem technical datasheet.
Processing divergence arises primarily from the 2.1 g/10 min melt flow rate and the associated molecular weight distribution. Blown film linear low density polyethylene grades intended for stable bubble formation often carry melt flow rates below 1.0 g/10 min to increase melt strength and extensional viscosity. LL218/21 trades that bubble stability for higher throughput, lower extruder motor load, and reduced die swell on cast film equipment. In a cast line, the melt curtain is unsupported between the die exit and the chill roll, so drawdown, neck-in control, and rapid quenching are more critical than bubble ductility. The lower elongational viscosity permits thin gauge reduction, but it also reduces the maximum usable air gap before edge neck-in becomes process-limiting. Published data for this specific configuration is limited; converters typically compensate by adjusting die gap, air knife position, and vacuum edge pinning. Compared with metallocene-catalyzed cast film linear low density polyethylene, the butene-copolymer polydispersity in LL218/21 generally provides a broader single-screw processing window but may reduce dart impact and balanced tear properties in the finished web. Selection therefore depends on whether the end-use requires maximum optics, maximum puncture resistance, or lower extrusion head pressure at a given output rate.
With a melt temperature at the die exit maintained between 240 °C and 260 °C, the grade can be processed on single-screw extruders with 30:1 to 33:1 L/D barrier screws and screen packs of 80–120 mesh to remove incidental contamination. The die gap is commonly set at 0.5–0.8 mm, with a die-to-chill-roll air gap of 20–40 mm for thin webs; the exact air gap influences haze, gloss, and edge neck-in. The chill roll is typically maintained between 18 °C and 35 °C, depending on roll diameter, line speed, and film thickness. Backpressure and melt temperature should be monitored because excessive screw speeds at low barrel settings can generate shear heating above 260 °C and initiate localized oxidative degradation. Pre-drying is not normally required at ambient relative humidity below 60%. If pellet condensation occurs after cold storage or prolonged exposure to humid air in open silos, a hopper dryer at 60–70 °C for 2–4 h may reduce surface defects, but the drying temperature should not exceed 70 °C to prevent pellet softening and feed throat bridging.
Cast film produced from LL218/21 on a polished chill roll can achieve a low-haze surface when melt temperature, air gap, and roll temperature are coordinated. Optical haze is evaluated according to ASTM D1003; gloss is measured under ASTM D2457; coefficient of friction is tested under ISO 8295 or ASTM D1894. The product may be supplied with slip and antiblock additives that migrate to the film surface over hours to days after extrusion. Because migration kinetics are temperature-dependent, coefficient of friction values measured immediately after winding will not represent final performance after storage at 23 °C. Erucamide and similar slip agents migrate more slowly at lower storage temperatures, while antiblock loadings affect optical clarity and reel hardness. Users should condition films at 23 ± 2 °C and 50 ± 5% relative humidity for a minimum of 24 h before reporting coefficient of friction values; published data for this specific configuration is limited. Final values depend on film thickness, slip additive concentration, chill roll surface roughness, and downstream corona treatment dosage.
Because LL218/21 is a butene-copolymer cast film grade, its heat seal initiation temperature is generally lower than high-density polyethylene and slightly higher than some plastomer or metallocene grades at comparable density. The actual heat seal window must be verified on the converter’s sealing equipment using a step-seal temperature ladder; published datasheet values may not capture the influence of film orientation, chill roll cooling rate, and surface treatment. In lamination applications, adhesion to substrates can be affected by low molecular weight oxidized species that bloom to the surface after corona treatment. Corona dosage is often set between 38 mN/m and 42 mN/m for consistent wetting, but over-treatment can cause surface crosslinking and reduce seal strength. The grade is not recommended for high-temperature retort processes above 121 °C unless the packaging structure includes a heat-resistant substrate, because the film may shrink or distort under autoclaving conditions. Users requiring retortable structures should select polypropylene-based cast film grades or high-density polyethylene with higher crystalline melting points.
High-speed cast film lines operating above 350 m/min introduce an air boundary layer that follows the chill roll surface and can become trapped between the melt curtain and the roll. This entrainment produces gauge bands, haze streaks, and localized slip variation. An air knife or vacuum box is typically required at these speeds to remove entrained air and pin the melt curtain to the chill roll. The die-to-roll air gap must be reduced to the minimum that avoids freeze-off or roll wrap defects; on some lines, an air gap below 15 mm yields improved optical quality but increases the risk of melt curtain oscillation. Tension control at the winding and secondary nip must be set to prevent machine-direction elongation. Because LL218/21 has lower melt strength than blown film grades, uncontrolled draw resonance can produce periodic thickness oscillation that is difficult to detect on a fast-moving web. Published data for this specific configuration is limited; line audits are required to establish the draw ratio, edge pinning settings, and chill roll speed that maintain a stable melt curtain.
Mechanical property declarations for cast film are typically obtained on 25 µm or 50 µm samples conditioned at 23 ± 2 °C and 50 ± 5% relative humidity. Tensile properties are determined under ASTM D882 or ISO 527-3; tear resistance under ASTM D1922; dart drop impact under ASTM D1709. Because cast film orientation is unbalanced, machine-direction and transverse-direction property differences are inherent. LL218/21 may show lower transverse-direction tear strength than blown film grades of equivalent thickness due to the absence of biaxial bubble orientation. Converters must not use a single tensile value as a specification for food packaging or heavy-duty sack applications; the appropriate test should be selected according to the failure mode observed on the packaging line. Compared to a hexene-copolymer cast film linear low density polyethylene of similar density, a butene-copolymer grade such as LL218/21 generally presents a less refined short-chain branching distribution, which can translate into lower puncture resistance and hot-tack strength but also lower resin cost and lower extrusion pressure. The difference is not always detectable in monolayer film at thick gauges; however, in multilayer stretch film formulations, the selection of skin and core resins modifies clarity, cling, and roll memory. Multilayer formulations should be developed with laboratory cast film trials rather than relying solely on individual resin datasheets.
The standard stabilization package is designed for cast film extrusion temperatures up to 260 °C and typical warehouse storage in unopened original packaging. The grade is not a universal material; prolonged exposure to temperatures above 280 °C or repeated extrusion cycles can consume the phenolic and phosphite antioxidants, increasing the carbonyl index and yellowness over time. Users should not blend the product with high levels of recycled polyethylene that may contain residual acids, metals, or polar contaminants without first evaluating melt filtration and stabilizer consumption. Avoid blending with hydrolyzable polymers such as ethylene-vinyl acetate copolymers that can release acetic acid at cast film temperatures, causing corrosion and film defects. The grade should also be kept away from direct contact with copper-based alloys in hot processing equipment because copper ions can accelerate oxidative degradation under certain conditions.
Food-contact compliance for the grade must be verified against the converter’s final article, because the polymer resin alone does not determine the regulatory status of a finished multilayer packaging structure. The following references are commonly evaluated for such cast film applications.
| Regulatory reference | Scope |
|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers for food contact, subject to end-use conditions and any applicable limitations of the subparagraph. |
| EU Regulation (EU) No 10/2011 | Overall migration and specific migration limits for plastic materials and articles intended to come into contact with food. |
| REACH Regulation (EC) No 1907/2006 | Substances of very high concern screening according to manufacturer declaration and current chemical inventory. |
| RoHS Directive 2011/65/EU | Lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls, and polybrominated diphenyl ether screening. |
The nominal physical property profile of Braskem LL218/21 is summarized for specification screening. These values are typical, not specification limits, and must be verified against the certificate of analysis for each production lot.
| Property | Test method | Nominal value |
|---|---|---|
| Nominal density at 23 °C | ASTM D1505 / ISO 1183-1:2019 | 0.918 g/cm³ |
| Nominal melt flow rate at 190 °C / 2.16 kg | ASTM D1238 / ISO 1133-1:2022 | 2.1 g/10 min |
| Comonomer type | Internal FTIR / ¹³C NMR | Butene |
| Supplied form | Manufacturer specification | Pellets with antioxidant stabilization |