| HS Code | 665886 |
| Product Name | Braskem LL118 |
| Polymer Type | Linear Low Density Polyethylene |
| Comonomer | Butene-1 |
| Density | 0.918 g/cm³ |
| Melt Index | 1.0 g/10 min |
| Melt Flow Rate | 1.0 g/10 min |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 700% |
| Dart Impact Strength | 120 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 350 g |
| Haze | 12% |
| Gloss | 60% |
| Vicat Softening Point | 95 °C |
| Melting Point | 122 °C |
| Processing Method | Blown Film Extrusion |
As an accredited Braskem LL118 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Braskem LL118 Linear Low Density Polyethylene is packaged in 25 kg polyethylene bags, palletized and stretch-wrapped for shipment. |
| Container Loading (20′ FCL) | 20′ FCL: Braskem LL118 Linear Low Density Polyethylene in 25 kg bags, palletized, shrink-wrapped, braced, and loaded for ocean transport. |
| Shipping | Braskem LL118 Linear Low Density Polyethylene is shipped as solid pellets in 25 kg bags, octabins, or bulk trucks/railcars. Keep containers closed, dry, and away from direct sunlight, heat, and ignition sources. Store in a cool, ventilated area. It is not classified as dangerous goods; follow normal industrial hygiene practices. |
| Storage | Store Braskem LL118 Linear Low Density Polyethylene in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep in original, tightly closed containers or bags to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and stacking that may deform packaging. Maintain good housekeeping; keep away from incompatible chemicals. Follow local regulations and manufacturer recommendations. |
| Shelf Life | Recommended shelf life is 24 months when stored in original packaging, in a cool, dry, well-ventilated area, away from direct sunlight. |
On pallet-unitization cast stretch film lines, Braskem LL118 enters the extruder as a butene-copolymer linear low-density polyethylene with a nominal density of 0.918 g/cm³ tested per ASTM D1505 and a melt flow rate of 1.0 g/10 min at 190 °C under 2.16 kg load per ASTM D1238 or ISO 1133-1:2022. Industrial non-food pallet wrap is governed primarily by mechanical performance standards rather than food-contact regulation; converter specifications commonly reference ASTM D5748 for protrusion puncture resistance of stretch wrap film, ASTM D882 for tensile properties of thin plastic sheeting, ISO 527-3 for film tensile behavior, and ASTM D1894 for coefficient of friction. In a monolayer machine stretch formulation, the addition ratio typically falls between 98.0 wt% and 99.5 wt% LL118 with 0.5 wt% to 2.0 wt% tackifier and anti-block masterbatch; hand wrap grades may operate at 1.5 wt% to 3.0 wt% additive loading to raise cling force without destabilizing edge trim. The downstream process is cast film extrusion: a barrier screw with L/D of 30:1 feeds a flat die with lip gap 0.5–0.9 mm, melt temperature is controlled between 240 °C and 260 °C, and the melt is pinned to a chill roll held at 18–24 °C by an air knife and vacuum box. Machine-direction orientation is produced by pre-stretch ratios of 200–300%; at line speeds beyond 450 m/min, edge neck-in and draw resonance become more sensitive to die lip adjustment and the presence of regrind. Terminal products include machine-applied pallet wrap at 12–35 µm, hand-applied stretch wrap at 20–30 µm, and pre-stretched films at 6–10 µm. The operating boundary is explicit: blends containing more than 20 wt% metallocene LLDPE can alter extensional viscosity enough to require rebalancing of air-knife pressure and vacuum-box suction to maintain edge stability.
Monolayer agricultural greenhouse covers impose simultaneous demands: high dart impact at low ambient temperature, stable light transmission, and resistance to UV-induced chain scission across service intervals of 24–36 months in Mediterranean or desert climates. The applicable compliance benchmark is EN 13206:2017 for thermoplastic covering films used in agriculture and horticulture; converters additionally verify film tensile properties by ISO 527-3 and tear resistance by ASTM D1922. In a typical monolayer greenhouse formulation, Braskem LL118 is used at 89–93 wt%, LDPE at 5–8 wt% for bubble stability, a hindered amine light stabilizer masterbatch at 0.5–1.5 wt%, and a processing aid and antioxidant package at 0.2–0.6 wt%; the exact addition ratio depends on target film thickness and local UV dose. The downstream production process is blown film extrusion through a grooved-feed extruder with die diameter 100–250 mm, die gap 0.8–1.4 mm, blow-up ratio 2.0–3.0, and frost-line height maintained between 500 mm and 900 mm by external air-ring cooling. For butene LLDPE at these gauge levels, bubble instability is more pronounced when the stalk is raised above 900 mm with a die gap under 0.9 mm; operators compensate by increasing internal bubble air pressure and reducing haul-off speed rather than raising melt temperature above 220 °C, because excessive temperature accelerates additive degradation. Terminal products include greenhouse covers, low tunnel covers, and temporary horticultural cladding in widths 4–12 m and thicknesses 80–180 µm. A limitation is that neat LL118 has no inherent UV protection; any formulation missing the HALS masterbatch below 0.5 wt% will show rapid embrittlement under full-sun exposure.
Due to its high dart-impact strength and seal-initiation temperature in the range of 100–115 °C commonly reported for butene LLDPE films, Braskem LL118 is blended into coextruded frozen-food webs as a sealant layer resin. Food-contact compliance is not a property of the resin alone; it requires finished film testing under EU Regulation 10/2011, including overall migration limits of 10 mg/dm² and specific migration limits for each intentional additive, as well as FDA 21 CFR 177.1520 for olefin polymers and REACH 1907/2006 for substance registration. In a three-layer frozen-food film, the sealant layer commonly uses 70–85 wt% LL118, 10–20 wt% LDPE or metallocene LLDPE for seal strength, and 2–5 wt% slip and antiblock masterbatch; the core layer may contain HDPE or LLDPE at 50–70 wt% of total structure. Downstream production is typically a three-layer coextrusion blown film line with die diameter 200–400 mm, die gap 1.0–1.6 mm, high-stalk configuration at 8–10D stalk height, and melt temperature in the sealant layer held at 190–220 °C to avoid gel formation. At high stalk heights, butene LLDPE occasionally displays bubble instability if the frost line fluctuates by more than 10% of total stalk height; this is corrected by reducing extrusion output rather than increasing melt temperature. Terminal products include pillow pouches for frozen vegetables, resealable freezer bags, and side-weld bags for iced confectionery at thicknesses from 25 µm to 80 µm. The explicit limitation is that cook-in or retort applications are outside the operating envelope, and any amine-containing antistatic masterbatch must be pre-approved for EU 10/2011 specific migration before use.
| Standard / clause | Constraint for LL118 frozen-food sealant use |
|---|---|
| EU 10/2011, Annex I | Overall migration limit 10 mg/dm²; specific migration of additives per Annex II |
| FDA 21 CFR 177.1520 | Permitted olefin polymer status subject to extractables and end-use temperature conditions |
| REACH 1907/2006 | Substance registration and SVHC screening for imported compound |
| ISO 1133-1:2022 | Verifies melt flow rate of incoming LL118 at 190 °C / 2.16 kg |
Industrial liners for intermediate bulk containers, construction debris containment, and box liners require puncture and tear values that exceed general packaging film. There is no single ISO standard governing all industrial liner configurations; converter specifications typically invoke ASTM D1709 for dart drop, ASTM D1922 for Elmendorf tear, ISO 527-3 for tensile behavior, and ISO 7765-1 for impact resistance by the free-falling dart method, while finished packages may follow ISO 21898:2022 when used as FIBC inner liners. In a monolayer heavy-duty liner, Braskem LL118 is formulated at 70–90 wt%, post-industrial recycled LLDPE at 10–30 wt% if required by cost and sustainability specifications, carbon black masterbatch at 2–4 wt% for opacity and UV resistance, and process aid at 0.5–1.0 wt% to suppress melt fracture. The downstream process is blown film extrusion with a grooved-feed extruder, screen changer fitted with 100/60/100 mesh screens, die diameter 150–350 mm, die gap 1.0–1.8 mm, blow-up ratio 1.8–2.5, and melt temperature 200–230 °C. In production-scale trials, the most frequent instability occurs when the die gap is reduced below 1.2 mm while recycled content exceeds 20 wt%; bubble edges oscillate and dart impact deteriorates because melt memory and contamination from regrind create local draw points. Maintaining a melt pressure differential across the screen pack of 20–30 bar and scheduling screen changes before reaching 35 bar are operational practices that reduce this variability. Terminal products include FIBC liners at 100–250 µm, construction debris chute liners at 150–300 µm, and industrial box liners at 80–150 µm. The boundary condition is clear: this film is not designed for direct food contact unless a separate food-grade layer is added, and post-industrial regrind must be pre-dried at 70 °C for 2 h if exposed to relative humidity above 60% to avoid surface moisture defects.
During blown film conversion of refuse sacks containing post-industrial recycled LLDPE, the prime resin contribution is used to preserve tensile strength and dart impact after the recycled component has been introduced. The applicable regulatory framework includes EN 13592:2017 for plastics sacks for household waste collection, EU Directive 94/62/EC for packaging and packaging waste, and ISO 14021:2016 for self-declared environmental claims; no food-contact approval is required unless the finished sack is sold for food-waste collection with direct food contact. In a recycled-content refuse sack formulation, Braskem LL118 is added at 40–70 wt%, post-industrial recycled LLDPE at 20–50 wt%, black masterbatch at 2–5 wt%, and processing aid at 0.5–1.0 wt%; post-consumer recyclate above 30 wt% typically requires an additional melt filtration step to prevent gel-related film punctures. The production process is mono-layer or two-layer blown film extrusion through a die diameter of 100–250 mm, die gap 0.8–1.4 mm, blow-up ratio 2.0–3.0, screen pack of 120/80/120 mesh, and melt temperature not exceeding 230 °C; a melt pump after the screen changer is standard on high-output lines to stabilize die pressure. The key production bottleneck is not bubble cooling but screen pack blinding: contaminated recycled flakes can increase pressure differential rapidly, causing low melt pressure and visible shark-skin on the film surface. Operators observe that batches with recycled content above 50 wt% require more frequent screen changes and tighter melt temperature control to avoid odor generation above 220 °C. Terminal products include municipal refuse sacks at 20–80 µm, heavy-duty waste bags at 80–120 µm, and tear-resistant garden waste sacks. The limitation is that mechanical properties at 20 µm can drop below EN threshold values if the recycled fraction exceeds 50 wt% and the prime LL118 content falls below 40 wt%; published data for this exact LL118 grade in post-consumer streams is limited, so line trials remain mandatory.
Competitive Braskem LL118 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Braskem LL118 is a linear low density polyethylene resin intended for blown and cast film extrusion. The grade is a butene-1 copolymer with a nominal density of 0.918 g/cm³ at 23 °C and a melt flow rate of 1.0 g/10 min at 190 °C/2.16 kg when tested according to ASTM D1238 and ISO 1133-1:2022. The resin is supplied as pellets and is used in general-purpose film structures where a balance of puncture resistance, tear propagation resistance, and drawability is required. Unlike high-pressure low density polyethylene produced in autoclave or tubular reactors, LL118 contains no long-chain branching; its short-chain branches derived from butene-1 control crystallinity and solid-state mechanical properties. The nominal values in the table below are lot-independent indicators, and the certificate of analysis for the supplied lot takes precedence over any printed property tables when setting extrusion or release specifications.
| Property | Test method | Nominal value |
|---|---|---|
| Melt flow rate | ASTM D1238 / ISO 1133-1:2022 | 1.0 g/10 min at 190 °C/2.16 kg |
| Density | ASTM D1505 / ISO 1183-1 | 0.918 g/cm³ at 23 °C |
| Comonomer | — | butene-1 |
| Recommended melt temperature | — | 180–230 °C blown film; 200–250 °C cast film |
| Typical film thickness range | — | 20–200 µm |
The absence of long-chain branching in LL118 is the primary differentiator from high-pressure LDPE. In blown film, LDPE imparts bubble stability through extensional strain hardening and a broad molecular weight distribution. LL118 relies instead on a higher zero-shear viscosity at equivalent melt index and on controlled frost line cooling. The practical consequence is that a converter replacing an LDPE of 1.0 g/10 min MFR with LL118 on the same extrusion line should expect higher motor load at equivalent screw speed and may need to raise melt temperature by 10–20 °C to reduce head pressure. Relative to a metallocene-catalyzed LLDPE of identical density, LL118 typically shows a broader comonomer distribution and less pronounced dart impact enhancement; the difference is most evident in 25 µm monolayer film tested according to ASTM D1709, where metallocene grades often yield higher dart drop values at equivalent density.
Against hexene- or octene-copolymer LLDPE of the same 0.918 g/cm³ density, the butene-1 architecture of LL118 reduces the concentration of short-chain branches that are most effective at tying together crystallites during deformation. This is expressed as lower Elmendorf tear strength in 50 µm film measured under ASTM D1922 and lower slow puncture propagation resistance under ASTM D5748, although the resin can still satisfy less demanding packaging and agricultural film specifications. Relative to a high-density polyethylene with nominally identical MFR but density near 0.958 g/cm³, LL118 has lower yield strength and flexural modulus but better low-temperature dart impact and lower sealing temperature. In coextruded structures, LL118 is therefore placed in sealing layers and abuse-resistance layers rather than in the load-bearing core. The difference in modulus can be quantified with ASTM D790 or ISO 178; converters should not replace a stiff HDPE layer with LL118 without recalculating the bending stiffness of the total structure.
On single-screw blown film lines with a barrier screw and an L/D of 24:1–30:1, LL118 is processed with a flat or reverse barrel temperature profile from 160 °C at the feed throat to 200–230 °C at the die. A screen pack of 60/80/100 mesh is commonly used to trap gels and to build head pressure; a melt pump downstream reduces surging and improves gauge control. Because LL118 does not show the same extensional strain hardening as LDPE, the use of a dual-lip air ring and internal bubble cooling becomes more important at outputs above 150 kg/h on a 250 mm die. Without internal bubble cooling, the maximum stable output may be limited by bubble breathing rather than extruder capacity.
Bubble stability with LL118 is less forgiving than with high-pressure LDPE because the resin does not strain-harden significantly under extension. A stable bubble is obtained when the frost line is positioned above the point where the melt has relaxed sufficiently to resist circumferential thickness variation. Particularly on air-cooled dies with a single-lip air ring, the use of internal bubble stabilization and a double-lip air ring is recommended when running below 30 µm. The melt pressure at the die entrance for a 90 mm extruder producing 150 kg/h of 25 µm film may reach 25–35 MPa, which is higher than an equivalent LDPE due to the linear architecture.
Gauge uniformity is controlled by die gap and cooling symmetry. For 0.8 mm die gaps, the draw-down ratio at 2.5:1 blow-up ratio and 25 µm final gauge approaches 12:1, which increases orientation in the machine direction. This is advantageous for tensile strength measured under ASTM D882, but it also increases the tendency to split along the machine direction when the film is notched; Elmendorf tear data under ASTM D1922 should be evaluated on both axes before the film is specified for heavy-filled sacks. Common defects observed on production-scale blown film lines include bubble sag, frost line oscillation, and roll blocking. Bubble sag occurs when the melt temperature exceeds 230 °C or when the cooling air is insufficient; it is addressed by lowering the melt temperature, increasing the air ring output, or raising the frost line. Frost line oscillation below 5 die diameters generally indicates excessive quench or an unbalanced air ring, and it produces gauge bands that appear as hard and soft zones in the wound roll. Roll blocking at film thickness above 80 µm is controlled by reducing winding tension and by adding antiblock masterbatch to the skin layers.
Cast film lines running LL118 benefit from a lower melt temperature and a smaller die-to-chill-roll gap than high-pressure LDPE. When a 0.5–1.0 mm slot die is used with a chill roll temperature of 15–30 °C, the resin exhibits sufficient quench rate to limit haze and reduce gloss; final optical properties should be measured under ASTM D1003 and ASTM D2457. The absence of long-chain branching increases neck-in and draw resonance relative to high-pressure LDPE unless the air gap is kept below 10 cm. For monolayer lamination film in the 30–60 µm range, LL118 is often blended with 10–20 wt% LDPE to improve tear strength and to stabilize the cast web at higher line speed. In cast stretch film applications, a hexene-copolymer LLDPE may be selected instead when higher prestretch retention and puncture resistance are required; published data for LL118 in high-prestretch configurations is limited.
When post-consumer or post-industrial LLDPE is let down into LL118 at levels above 20 wt%, the mixture should be characterized for melt flow stability, gel count, and film appearance before extrusion. A blown film line with a 75 mm grooved-feed extruder and a melt pump is preferred for such blends because the feed instability associated with pellet-size variation can be damped. If the recycled fraction contains high-pressure LDPE, the blend retains some long-chain branching and bubble stability improves, but the density and seal initiation temperature shift; densities above 0.922 g/cm³ in the final blend, measured under ASTM D1505, can increase film stiffness and reduce tear resistance.
High-antioxidant masterbatches containing phenolic or phosphite stabilizers are generally compatible with LL118. Addition above 5 wt% of a carrier resin with MFR higher than 4 g/10 min when measured under ASTM D1238 can lower melt viscosity and alter the frost line height, leading to gauge bands unless the air ring is retuned. Avoid uncontrolled addition of peroxide masterbatches used for vis-breaking or crosslinking; these additives can shift the MFR outside the 0.8–1.2 g/10 min window under ASTM D1238, which changes heat seal strength and dart impact. Any film intended for direct food contact must be evaluated against migration limits in EU Regulation (EC) No 10/2011 and FDA 21 CFR 177.1520.
The base resin is designed to meet the requirements for olefin polymers under FDA 21 CFR 177.1520 when used in accordance with the specified conditions of use. For the European Union, compliance is normally established under EU Regulation (EC) No 10/2011; migration testing is the responsibility of the converter because the final film may contain additional masterbatches or recycled content. The table below lists the normative references applicable to the base resin.
| Framework | Reference | Typical status |
|---|---|---|
| U.S. food contact | FDA 21 CFR 177.1520 | Olefin polymer compliance under specified conditions of use |
| EU food contact | EU Regulation (EC) No 10/2011 | Compliance subject to migration testing of final article |
| REACH | EC 1907/2006 | Polymer exempt from registration; monomers and imported constituents registered |
| RoHS | 2011/65/EU | No restricted substances intentionally added |
In warehouse storage, LL118 should be kept below 40 °C and protected from direct sunlight. Polyethylene is not hygroscopic, but condensation can occur when cold pellets are transferred to a humid environment; if visible surface moisture is present, a 60–70 °C desiccant drying step for 2 h is sufficient before extrusion. The resin should not be stored adjacent to strong odorants or volatile organic compounds because polyolefins can absorb and release them in film form. Agricultural silage and mulch films in the 25–150 µm range are typical applications for LL118. The resin is processed with carbon black masterbatch or white masterbatch at let-down ratios of 6–12 wt%; the final film should be tested for tensile elongation after UV exposure under ASTM G154 or ISO 4892-2. In lamination film for flexible packaging, LL118 can be used as a sealant web because its seal initiation temperature is lower than that of high-pressure LDPE of similar density. Heat seal strength is evaluated under ASTM F88; the optimal seal temperature for a given dwell time and pressure should be established on the converter’s jaw sealer before setting production specifications. For film intended to resist outdoor weathering, the final formulation must include a UV stabilizer package validated under ASTM G154 or ISO 4892-2; the natural resin alone is not suitable for long-term agricultural exposure.