Braskem Ll118 21 Blown Film Extrusion Linear Low Density Polyethylene

Braskem LL118/21 Blown Film Extrusion Linear Low Density Polyethylene

    • Product Name: Braskem LL118/21 Blown Film Extrusion Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 949007
    Productname Braskem LL118/21
    Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene
    Application Blown Film Extrusion
    Meltflowrate 190c 2 16kg 1.0 g/10 min
    Density 0.918 g/cm³
    Meltingpoint 120 °C
    Vicatsofteningpoint 94 °C
    Tensilestrengthatyield Md 10 MPa
    Tensilestrengthatbreak Md 30 MPa
    Tensilestrengthatbreak Td 25 MPa
    Elongationatbreak Md 600%
    Elongationatbreak Td 700%
    Dartdropimpact 120 g
    Elmendorftear Md 200 g
    Elmendorftear Td 350 g
    Haze 12%
    Gloss 45deg 60

    As an accredited Braskem LL118/21 Blown Film Extrusion Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LL118/21 typically supplied in 25 kg polyethylene bags, 40 bags per pallet, totaling 1,000 kg net.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Braskem LL118/21 blown film LLDPE resin in bags, palletized, shrink-wrapped, and secured for ocean transport.
    Shipping Braskem LL118/21 Blown Film Extrusion Linear Low Density Polyethylene is a non-hazardous, non-regulated LLDPE resin. It ships as pellets in 25 kg bags or 1000 kg bulk bags, palletized and stretch-wrapped, in clean, dry trucks or containers at ambient temperature, protected from moisture, heat, sunlight, and contamination.
    Storage Store in a cool, dry, well-ventilated warehouse. Keep original containers sealed, labeled, and off the floor. Protect from direct sunlight, heat, ignition sources, moisture, dust, and strong oxidizers. Avoid excessive stacking, physical damage, and static buildup. Maintain good housekeeping and first-in, first-out stock rotation. Follow local regulations and the manufacturer’s safety data sheet recommendations. Do not store near food, feed, or drinking water.
    Shelf Life Shelf life: typically 12 months when stored unopened in a cool, dry, ventilated area away from direct sunlight and heat.
    Application of Braskem LL118/21 Blown Film Extrusion Linear Low Density Polyethylene

    On a 65 mm grooved-feed blown film line with a 30:1 L/D screw, a 250 mm die, and a dual-lip air ring, Braskem LL118/21 — specified at nominal density 0.918 g/cm³ and melt flow rate 1.0 g/10 min under ISO 1133-1:2022 — is processed as the primary load-bearing layer in heavy-duty industrial sacks. The converter-level formulation places Braskem LL118/21 at 80–85 wt%, LDPE at 15–20 wt%, and an antiblock masterbatch at 0.5–1.0 wt%; this ratio maintains dart impact under ASTM D1709-16ae1 while preventing blocking at film thicknesses of 200–250 µm. The production process is monolayer blown film extrusion with a die gap of 2.0 mm, a blow-up ratio of 2.0:1, a melt temperature between 200°C and 210°C, and internal bubble cooling engaged above 180 kg/h output. Compliance for export lot release is anchored to ISO 8367-2:1993 for thermoplastic sack dimensions, ASTM D4976-20 for the material designation, and EU 94/62/EC for heavy metals; direct food contact is not implied unless the converter separately validates the finished article under 21 CFR 177.1520(c). Terminal finished product types include 25 kg polymer granule sacks, mineral powder sacks, animal feed sacks, and insert liners for FIBC constructions rated at 500–1000 kg. At thickness above 250 µm, collapsing frame surface temperatures must be maintained below 35°C to avoid blocking bridges; on similar high-output lines, exceeding 220 kg/h without internal bubble cooling is known to increase film thickness variation to more than ±8%.

    When Does Low-Temperature Seal Strength Override Film Yield in Frozen Food Packaging?

    Film structures intended for frozen vegetable, seafood, and ice cream packs are run at 30–80 µm, where the low-temperature ductility of Braskem LL118/21 becomes the controlling property rather than tensile yield. In this segment, the polymer fraction is blended at 85–90 wt% Braskem LL118/21, 10–15 wt% LDPE, 0.5–1.0 wt% antiblock masterbatch, and 0.08–0.12 wt% erucamide slip; slip loading above 0.15 wt% is avoided because migration to the sealant surface narrows the hot-tack window on high-speed vertical form-fill-seal equipment and can transfer to filling jaws. The compliance matrix for this segment includes 21 CFR 177.1520(c) for US food contact, EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm², and GB 4806.7-2016 for China-bound packs; water vapor transmission rate is measured under ASTM F1249-20 at 38°C and 90% RH, while tear propagation is recorded under ASTM D1922-15. Processing is performed on a 50 mm grooved-feed single-screw extruder with a 200 mm die, a die gap of 1.8 mm, a blow-up ratio of 2.5:1, and a melt temperature of 190–200°C; secondary air cooling at 5–10°C reduces blocking during roll formation. Terminal finished products include pre-formed frozen vegetable pouches, individually quick-frozen seafood bags, ice cream bags, and frozen bakery overwrap. A known processing boundary is bubble chatter when the frost line is held below 300 mm, which produces gauge bands that fail downstream leak and seal integrity tests.

    Stretch Hood Pallet Wrap Puncture Propagation and High-Stalk Bubble Stability

    Palletizing lines for bagged cement, construction blocks, and ceramic products impose puncture and tear loads that cannot be satisfied by monolayer LDPE alone; Braskem LL118/21 is therefore blended at 60–70 wt% with C6-LLDPE at 20–30 wt% and LDPE at 10–15 wt%. A fluoropolymer processing aid is added at 0.02–0.05 wt% on lines equipped with a 350 mm die, a die gap of 1.8 mm, a blow-up ratio of 3.0:1, and a high-stalk bubble configuration; the stalk length is held at 700–900 mm with internal bubble cooling to stabilize the bubble against ambient air turbulence. Puncture resistance is recorded under ASTM D5748-19, tensile under ASTM D882-18, and propagation tear under ASTM D1922-15. Export consignments to the EU require heavy metals assessment under EU 94/62/EC, with combined lead, cadmium, mercury, and hexavalent chromium below 100 mg/kg in packaging. Terminal finished product types are stretch hoods of 60–100 µm for pallet loads of cement bags, brick stacks, appliance cartons, and chemical drums. Exceeding 35 wt% C6-LLDPE creates measurable melt-pressure oscillation and raises dart drop absolute variation above 15%; this configuration is not recommended where pallet loads present sharp steel-edge or strapping contact.

    On three-layer coextrusion lines running black silage cover film at outputs above 180 kg/h, Braskem LL118/21 is used in the core and inner layers at 85–90 wt% of the total polymer fraction, with LDPE at 10–15 wt% and a carbon black masterbatch at 2–4 wt%. The carbon black loading is not cosmetic; it provides weather resistance for silage covers that must remain intact over 12–24 months of outdoor exposure. A hindered amine light stabilizer is added at 0.3–0.6 wt%, and a fluoropolymer process aid at 0.03 wt% controls melt fracture without altering surface tension to levels that compromise winding. The relevant agricultural film standard is EN 13206:2017; when exported to EU member states, the final article must also demonstrate compliance with REACH Regulation (EC) No 1907/2006, Annex XVII restrictions for polycyclic aromatic hydrocarbons, and the packaging waste directive EU 94/62/EC. Extrusion is performed with a layer distribution of approximately 30/40/30, a die gap of 2.2 mm, a blow-up ratio of 2.0:1, and a melt temperature of 200–215°C. The film is wound at 150–200 µm, and thickness tolerance is held at ±5% because variation above this range produces localized thinning under bale wrap edge pressure. Terminal finished products include bale wrap, bunker silage covers, and tube-stored silage bags used in dairy and biogas operations. When carbon black masterbatch exceeds 4 wt%, screen pack pressure rises above acceptable thresholds on 80 mm extruders, and tear propagation resistance under ASTM D1922-15 declines; this is the primary formulation ceiling for this application segment.

    If Adhesive Lamination Converters Run Thin Sealant Webs Above 300 m/min, Corona Retention Becomes the Controlling Variable

    Adhesive lamination converters processing sealant webs for stand-up pouches and stick packs use Braskem LL118/21 as a 20–40 µm blown film layer in duplex or triplex laminates. The polymer fraction in this segment is 92–95 wt% Braskem LL118/21, 5–8 wt% LDPE, and 0.5–1.0 wt% antiblock masterbatch; slip additive is kept at 0.1–0.2 wt% because higher slip levels can reduce the initial peel strength of solventless polyurethane adhesive bonds to PET and BOPP. US food contact status is assessed under 21 CFR 177.1520(c), and EU status under EU Regulation (EU) No 10/2011 with overall migration below 10 mg/dm²; converters must validate migration under the food simulant and time-temperature conditions assigned in Annex III of the regulation for the specific food category. Processing conditions for the blown sealant web are a die gap of 1.2–1.5 mm, a blow-up ratio of 2.5:1, a melt temperature of 195–210°C, and corona treatment to 38–42 mN/m. Lamination is then performed at line speeds above 300 m/min; at these speeds the interval between corona discharge and adhesive application is the main variable controlling bond durability. Terminal finished product types include stand-up pouches, stick packs, sachets, and lidding film. Surface energy below 36 mN/m after 30 days of roll storage is a common failure boundary; converters storing film rolls beyond this interval in RH > 60% conditions should re-check dyne level or apply atmospheric plasma retreatment before lamination.

    Bag-in-Box Liner Film Is Extruded at 40–70 µm With Flex-Crack Cycle Requirements

    Bag-in-box filling lines for 3 L, 5 L, and 10 L liquid packaging require a monolayer blown film tube that survives repeated flexing during transport and spout insertion. In this application Braskem LL118/21 is blended at 85–90 wt% with metallocene LLDPE at 10–15 wt% and LDPE at 5–10 wt%; this ratio improves flex-crack resistance while retaining bubble stability on a 55 mm grooved-feed extruder. Food contact compliance for wine, dairy, and liquid food service is evaluated under 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011, with overall migration not exceeding 10 mg/dm²; flex durability is measured under ASTM F392-93 using the A or B test mode selected by the converter and accepted by the brand owner. The tube is extruded at 40–70 µm through a 1.5 mm die gap with a blow-up ratio of 2.5:1 and a melt temperature of 190–205°C. After collapsing, the tube is perforated for spout insertion, heat-sealed at the top and bottom, and leak-tested by air inflation prior to loading into corrugated cases. Terminal finished product types include bag-in-box liners for wine, dairy concentrates, post-mix syrup, and non-hazardous liquid chemicals in 3 L to 20 L formats. At film thickness below 40 µm, pinhole counts in flex-crack testing increase sharply; for wine bag-in-box liners a minimum of 50 µm is common because oxidative ingress through pinholes compromises shelf life.

    Household refuse sack production is the most cost-sensitive segment in this group; formulations are adjusted continuously against post-consumer recycled LDPE availability. Braskem LL118/21 is added at 70–80 wt% of the virgin polymer fraction, with LDPE at 20–30 wt%, colored masterbatch at 1–2 wt%, and calcium carbonate masterbatch at 5–10 wt% only when downgauging below 40 µm is not part of the product specification. The applicable standard is EN 13592:2017 for household refuse sacks, with dart impact under ASTM D1709-16ae1; EU packaging waste compliance is demonstrated under EU 94/62/EC with combined heavy metals below 100 mg/kg. Processing on a monolayer line with an 80 mm grooved-feed extruder, a 400 mm die, a blow-up ratio of 3.0:1, and melt temperature 190–205°C yields 20–60 µm film at high output. Terminal finished product types include drawstring refuse sacks, bin liners, and heavy-duty trash bags for municipal collection. Calcium carbonate loadings above 10 wt% reduce dart drop and increase melt pressure; screen packs are set at 60/80/100 mesh to remove agglomerates that would otherwise generate pinholes at the collapsing frame.

    Free Quote

    Competitive Braskem LL118/21 Blown Film Extrusion Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LL118/21 is a linear low-density polyethylene resin formulated for air-cooled tubular blown film extrusion. The nominal density is 0.918 g/cm³ when tested under ASTM D792-20 or ISO 1183-1:2019, and the nominal melt flow rate is 1.0 g/10 min at 190°C/2.16 kg under ASTM D1238-20 or ISO 1133-1:2022. The polymer is a butene comonomer linear low-density polyethylene; the ethyl short-chain branches introduced by butene reduce crystallinity relative to high-density polyethylene. The grade suffix /21 identifies a proprietary additive package that includes a processing stabilizer, acid neutralizer, slip amide, and inorganic antiblock. Exact additive concentrations are not disclosed in the standard technical bulletin. The resin is intended for monolayer and coextruded blown film structures used in industrial liners, agricultural films, and overwrap. It is not formulated for injection molding, cast film, or blow molding.

    Film processors evaluating this grade should distinguish between nominal resin properties and fabricated film properties. The latter are a function of die gap, blow-up ratio, frost line height, gauge control, and cooling air temperature. Published data for this specific configuration is limited; comparative film data should be generated on a defined production line rather than inferred from resin density or melt flow rate alone. A typical evaluation conversion for a 25 µm film uses a single-screw extruder of 60 mm diameter and 24:1 L/D, a 250 mm die, a 1.5 mm die gap, a 2.5:1 blow-up ratio, and a frost line height of 8 to 10 die diameters. All film measurements should be performed after conditioning for 40 h at 23°C ± 2°C and 50% ± 5% RH under ASTM D618-21.

    Why Does Butene Branching Dictate the Balance Between Seal Initiation Temperature and Film Toughness?

    The ethyl short-chain branches introduced by butene reduce crystallinity and lamellar thickness. Under ASTM D3418-15, the crystalline melting peak for this density class generally lies between 119°C and 124°C. The reduction in melting point lowers heat seal initiation temperature relative to autoclave low-density polyethylene by approximately 5°C to 15°C, although end-use seal strength and hot-tack must be measured under ASTM F88/F88M-21 and ASTM F1921-18. The lower density also increases the concentration of tie molecules that bridge adjacent lamellae, which improves puncture and dart impact but reduces modulus and load-bearing capacity. At 25 µm, published industrial data for butene LLDPE in this density and melt flow rate class typically show tear propagation resistance under ASTM D1922-15 that is anisotropic, with transverse-direction tear often exceeding machine-direction tear by a factor of 2 to 4. Dart impact under ASTM D1709-15a usually falls between 60 g and 120 g for such film, but the exact value depends on frost line height, die gap, and additive package. Haze measured under ASTM D1003-13 for antiblock-containing butene LLDPE film generally lies between 6% and 15%. These ranges are class-typical data and are not specification limits.

    PropertyNominal ValueTest Method
    Density0.918 g/cm³ASTM D792-20, ISO 1183-1:2019
    Melt flow rate, 190°C/2.16 kg1.0 g/10 minASTM D1238-20, ISO 1133-1:2022
    Comonomerbutenenot a standardised test value
    Additive packageantioxidant, neutralizer, slip amide, inorganic antiblockproprietary

    The rheological signature differs from low-density polyethylene of equal melt index. The absence of long-chain branching reduces melt tension and extensional strain-hardening; shear viscosity at typical die shear rates is higher, increasing extruder head pressure and screw torque. On a 24:1 L/D single-screw extruder fitted with a barrier screw and Maddock mixer, barrel temperatures should be profiled from 160°C at the feed throat to 220°C at the die, with melt temperature measured at the adapter maintained between 190°C and 230°C. Lower melt temperature reduces oxidation and odor but raises melt viscosity and die pressure; higher melt temperature reduces haze but can degrade slip amide and cause plate-out on the air ring. The die gap should be set between 1.0 mm and 2.5 mm. A narrower gap improves orientation balance but increases shear stress and melt fracture risk; a wider gap reduces die pressure and improves tear but lowers gauge uniformity. The blow-up ratio is typically maintained between 2.0:1 and 2.8:1 to balance machine-direction and transverse-direction tensile properties. Frost line height is normally 6 to 10 die diameters. A frost line below 20 cm from the die face produces insufficient lateral expansion and high blocking; a frost line above 40 cm destabilises the bubble and increases gauge variation.

    Processing Conditions That Prevent Melt Fracture and Reduce Gel Formation in LL118/21

    Melt fracture in butene LLDPE film extrusion typically appears as sharkskin or orange peel on the film surface when the shear stress at the die land exceeds the critical stress of the resin. The condition is more pronounced at narrow die gaps and high output rates. A fluoropolymer processing aid masterbatch at 200 ppm to 500 ppm is often used to lower die pressure and suppress sharkskin; the exact addition level should be adjusted so that die pressure stabilizes within 15 min of masterbatch addition. Gels are not a specified property of LL118/21, but they can be generated by contamination with polyamide, polyethylene terephthalate, or crosslinked material from previous runs. Before processing LL118/21, the line should be purged with a lower-viscosity polyolefin and the screen pack should be checked for degraded polymer. A screen pack of 40/60/80 mesh is common for blown film extrusion. LL118/21 does not require pre-drying under normal storage conditions because polyolefins are not hygroscopic. However, when sacks are stored at relative humidity above 60%, surface condensation can introduce moisture into the hopper; pre-drying at 70°C to 80°C for 2 h to 4 h removes surface moisture and reduces bubble instability caused by steam bubbles.

    The /21 additive package affects downstream performance. Slip amide migrates to the film surface over time; kinetic film-to-film coefficient of friction measured under ASTM D1894-14 reaches a stable value only after 24 h to 72 h at 23°C ± 2°C. Immediately after extrusion, film may exhibit blocking; full slip development is required before high-speed converting. Antiblock reduces blocking in wound rolls but creates surface micro-roughness, increasing haze. The trade-off is nonlinear: increasing antiblock loading from 0 ppm to 1000 ppm can reduce blocking force by more than 50%, but may raise haze by 2 to 3 percentage points. The exact additive concentrations in LL118/21 are proprietary and are not controlled by resin density or melt flow rate.

    When LL118/21 Replaces LDPE or Metallocene Grades in Coextruded Structures

    In a three-layer coextruded film, LL118/21 can be used in the core or outer layers to increase toughness and reduce seal initiation temperature relative to a low-density polyethylene control. Replacement of autoclave low-density polyethylene with LL118/21 at equal gauge increases dart impact and tear resistance, but also increases extruder motor load and reduces bubble stability because melt tension is lower. The die pressure increase can be 15% to 25% at the same output rate when measured at the extruder head, although the exact value depends on die gap and melt temperature. Seal initiation temperature is lower, permitting faster heat seal cycles, but the seal plateau may require verification because slip amide bloom can interfere with hot-tack. Hot-tack measured under ASTM F1921-18 should be part of conversion qualification. Compared with metallocene-catalysed LLDPE of similar density, LL118/21 has a broader molecular weight distribution and a less uniform comonomer distribution. This improves bubble stability and melt fracture resistance, but reduces puncture toughness and clarity. At 25 µm, metallocene grades can provide haze values below 5% under ASTM D1003-13, whereas antiblock-containing butene LLDPE typically provides haze of 6% to 15%. Against hexene or octene LLDPE, LL118/21 generally shows lower dart impact and Elmendorf tear resistance because ethyl branches are less effective than longer branches at producing tie molecules. Blending LL118/21 with LDPE is common; a blend ratio of 10% to 30% LDPE improves bubble stability and haze with only moderate loss of tear strength.

    LL118/21 is compatible with polyethylene-based tie resins and ethylene vinyl acetate layers in coextruded structures. It is not compatible with polar barrier polymers such as polyamide or ethylene vinyl alcohol without an appropriate tie layer. In structures containing polyamide, the interface can delaminate if corona treatment is excessive; wetting tension should be kept below 45 mN/m under ASTM D2578-23 for unwind, while downstream printing may require 38 mN/m to 42 mN/m.

    Regulatory Compliance Boundaries for Food Contact and Secondary Packaging

    Compliance claims for LL118/21 must be made against the current revision of each regulation and the specific food contact use. The resin is based on olefin polymers covered by FDA 21 CFR 177.1520; compliance for a finished article depends on conditions of use, food type, and overall and specific migration testing. Under EU Regulation (EU) No 10/2011, overall migration from the final packaging must not exceed 10 mg/dm², and the specific migration limits for additives depend on the additive package. REACH Regulation (EC) No 1907/2006 requires that substances of very high concern not be present above 0.1 wt%. RoHS Directive 2011/65/EU applies to electrical and electronic equipment packaging and restricts lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls, and polybrominated diphenyl ethers. The standard grade does not contain ultraviolet stabilizers; outdoor film requires additional UV masterbatch. It is not intended for medical or pharmaceutical applications without supplementary conformity assessment.

    Regulation or StandardCompliance Boundary
    FDA 21 CFR 177.1520Olefin polymer base; finished article subject to end-use migration testing
    EU Regulation (EU) No 10/2011Overall migration limit 10 mg/dm²; specific migration limits per Annex I
    REACH Regulation (EC) No 1907/2006No SVHC above 0.1 wt% in Candidate List
    RoHS Directive 2011/65/EUPb 0.1 wt%, Hg 0.1 wt%, Cd 0.01 wt%, Cr(VI) 0.1 wt%, PBB 0.1 wt%, PBDE 0.1 wt%

    Heavy-duty industrial liners produced from LL118/21 are typically specified at 75 µm to 125 µm gauge. The selection should be based on slow-rate penetration resistance under ASTM F1306-19 and tear propagation under ASTM D1922-15, not on tensile yield alone. Additives such as slip and antiblock reduce blocking during high-speed winding, but film-to-film friction under ASTM D1894-14 should be allowed to stabilize for 24 h after extrusion because slip amide migration is time-dependent. For agricultural film, LL118/21 does not contain a UV stabilizer; a UV stabilizer masterbatch is required for exposed applications. For high-clarity overwrap, the grade is generally unsuitable if haze below 5% under ASTM D1003-13 is specified. The resin should not be considered for applications requiring continuous service above 80°C without verifying thermal aging, because oxidative stabilization is designed for film extrusion and normal storage, not long-term thermal exposure.

    Top