Braskem Ll 218 Lldpe Cast Film Extrusion Polyethylene

Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene

    • Product Name: Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 141929
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.918 g/cm³ (typical)
    Melt Flow Rate 190 C 2 16 Kg 2.0 g/10 min (typical)
    Melt Flow Ratio I21 I2 30 (typical)
    Melting Temperature 122 °C (typical)
    Vicat Softening Temperature 96 °C (typical)
    Tensile Strength At Yield 10 MPa (typical)
    Tensile Strength At Break 25 MPa (typical)
    Elongation At Break 700% (typical)
    Flexural Modulus 240 MPa (typical)
    Dart Drop Impact 90 g (typical)
    Elmendorf Tear Strength Md 200 g (typical)
    Elmendorf Tear Strength Td 400 g (typical)
    Haze 6% (typical)
    Gloss 45 80 (typical)
    Coefficient Of Friction 0.2 (typical)
    Heat Seal Initiation Temperature 105 °C (typical)

    As an accredited Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene bags, 1,375 kg stretch-wrapped pallets, for Braskem LL 218 LLDPE cast film extrusion.
    Container Loading (20′ FCL) 20′ FCL Container Loading: Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene, 25 kg bags, palletized, approximately 18–20 metric tons.
    Shipping Braskem LL 218 LLDPE is shipped as non-hazardous polyethylene resin in 25 kg polyethylene bags or bulk sacks, palletized and stretch-wrapped. Transport in clean, dry containers or covered trucks at ambient temperature. Keep away from moisture, direct sunlight, and ignition sources. Handle with standard industrial hygiene; no special ventilation required.
    Storage Store Braskem LL 218 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizing agents. Keep original bags or containers closed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid excessive stacking and follow first-in, first-out stock rotation. Maintain normal warehouse temperatures and handle with clean equipment.
    Shelf Life Shelf life: 12 months when stored in original, unopened packaging, in a dry, cool, ventilated area away from direct sunlight.
    Application of Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene

    What governs cling-force decay in 12 μm LL218 pre-stretch machine film at -10°C?

    Braskem LL218 enters cast film extrusion with a nominal melt flow rate of 2.0 g/10 min. The test condition is 190°C/2.16 kg per ISO 1133-1:2022. The nominal density is 0.918 g/cm³ per ISO 1183-1. In three-layer machine stretch film, LL218 is placed in the core at 55–70 wt%. A metallocene-catalysed LLDPE with a melt index of 1.0–2.5 g/10 min is used in the skin layers at 20–35 wt%. The cling layer receives 0.6–1.5 wt% polyisobutylene tackifier. Erucamide slip is controlled at 500–1,200 ppm in the non-cling layer. Synthetic silica antiblock is maintained at 1,000–3,000 ppm. The target haze is below 4.0% per ASTM D1003. The cast line is configured with a 65/90/65 mm extruder group. Barrier screws have L/D 30:1. The flat die width is 2,200 mm. The lip gap is 0.5–0.8 mm. The air gap is 15–25 cm. The polished chill roll is held at 20±2°C. Melt temperature at the die entry is kept at 245±5°C. Die entry pressure is typically 150–250 bar. Line speed is set between 350 m/min and 550 m/min. Draw resonance is avoided by maintaining web tension below 8 N/mm. Cling force is measured on ASTM D5458. The target range is 4–6 N at release. At -10°C, cling force decays because polyisobutylene diffusion to the surface is temperature-dependent. The rate of surface renewal after stretching falls below consumption rate on high-speed wrapping lines. Cold crystallisation of the LLDPE amorphous fraction reduces molecular mobility. Film stored at 0°C for 48 h may show cling values below 2 N. This causes tail unwind defects. To compensate, lines raise PIB concentration to 1.8 wt%. This creates haze above 5.0% and blocking force beyond 15 N/cm². The processing window is narrow. Moisture content in the hopper must be below 0.02%. Physical targets for the 12 µm film include tensile strength above 35 MPa in the machine direction. Ultimate elongation should exceed 500% under ASTM D882 at 23°C/50% RH. Elmendorf tear in the transverse direction is typically 3–6 N under ASTM D1922. Published data for this exact grade at 12 µm is limited. Site-specific temperatures and additive packages shift tear by up to 30%.

    Representative QC matrix for LL218 machine stretch cast film
    AttributeTest methodControl windowFrequency
    DensityISO 1183-10.916–0.920 g/cm³24 h
    Melt flow rateISO 1133-1:20221.8–2.2 g/10 minper shift
    HazeASTM D1003≤4.0%per roll
    Elmendorf tear TDASTM D19223–6 Nper roll
    Cling forceASTM D54584–6 Nper roll

    Control windows represent line-specific QC settings, not grade specifications.

    Dry-food pouch sealant webs based on LL218 are converted at 20–30 µm. They serve as cast lamination layers under printed PET or BOPP facestock. PIB tackifier is omitted. Residual cling would interfere with horizontal form-fill-seal transport. The formulation uses 85–100 wt% LL218 and 0–15 wt% fractional-melt LDPE for neck-in control. Slip and antiblock are added at 400–800 ppm erucamide and 1,000–2,500 ppm synthetic silica. The cast line operates with a 1,800 mm die. The lip gap is 0.6 mm. The air gap is 12–18 cm. The chill roll is held at 18±2°C. Melt temperature is 240–250°C. Line speed is limited to 150–250 m/min. Excessive speed increases web flutter and reduces chill roll contact. Seal initiation occurs at 105–115°C. Hot-tack strength above 1.0 N/25 mm is observed from 110°C to 140°C under ASTM F1921. The terminal pouch is used for granular dry foods, frozen foods and dry beverage sachets. Food-contact compliance follows 21 CFR 177.1520(c). Overall migration is assessed under EU 10/2011 with fatty food simulant D2 in laminates. Conversion trials show that increasing LL218 above 90 wt% without LDPE raises neck-in to 15% of die width. The resulting edge bead is removed as trim. Elevated trim losses reduce yield by 2–4%. At 20 µm, the film should show kinetic coefficient of friction below 0.35 against stainless steel under ASTM D1894. Haze is controlled below 6.0% for reverse-printed structures where the sealant web is visible.

    Hygiene Backsheet Lamination and Chill Roll Dew Point Control

    LL218 is extruded as an 18–25 µm cast web for hygiene backsheet lamination. The web is adhesive-laminated to spunbond polypropylene nonwoven. The laminate is used as the outer cover of infant diapers and adult incontinence pads. LL218 is selected for tear propagation resistance and low gel count. The cast line uses a 2,000 mm die. Lip gap is 0.5 mm. The air gap is 10–15 cm. Chill roll temperature is 16±1°C. The process becomes sensitive when plant dew point exceeds 18°C. Condensation on the polished roll causes microvoid defects. Surface tension becomes inconsistent. A dew point alarm at 15°C is required. Surface tension is measured at 38–42 mN/m per ASTM D2578 before lamination. If surface tension falls below 36 mN/m, hot-melt adhesion fails. LL218 is blended with 10–20 wt% metallocene LLDPE. This raises dart impact above 200 g on ASTM D1709, method A. The exact drop depends on layer construction. The film is not a barrier. Water vapour transmission rate for 20 µm monolithic PE is generally above 15 g/m² day under 38°C/90% RH on ASTM E96/E96M. The limitation is addressed by adding a breathable or filled microporous layer in the final hygiene article. The terminal backsheet must pass peel adhesion of 1.5–3.0 N/25 mm between cast film and nonwoven at 300 mm/min per ASTM D903. Film elongation at break above 600% is needed for festoon accumulators. Published data for this exact grade in hygiene lamination is limited. Converters qualify their own tie-layer blends and lamination adhesives.

    Surface protection webs constructed from LL218 are converted at 40–60 µm. They protect anodised aluminium, polycarbonate and PMMA sheets during transport and fabrication. The film is cast in a two-layer structure. The backing layer contains 90–100 wt% LL218. The adhesive layer is a coextruded ethylene-vinyl acetate or polyolefin elastomer blend. It contains 0.15–0.30 wt% hindered amine light stabiliser and 0.05–0.10 wt% phenolic antioxidant. Melt temperature is 235–250°C. The chill roll is a 1,200 mm polished roll at 22±2°C. Line speed is 100–180 m/min. Adhesion to stainless steel is 0.4–1.0 N/25 mm under ASTM D3330. Elongation at break exceeds 500% under ASTM D882. Gel count is limited to 5 gels/m² above 200 µm. Slip additives are held below 600 ppm to avoid transfer to the protected surface. The film is stripped after routing or bending operations.

    When LL218 is diluted with 8–15% LDPE for high-slip bundling film

    Bundling film for PET bottles, beverage cans and cartons is cast at 25–35 µm. The film uses a dilute blend of LL218 and LDPE. LDPE is added at 8–15 wt%. It increases shear thinning in the die. It reduces neck-in during high-speed draw. The blend is processed on a 90 mm single-screw extruder. The screw has L/D 33:1. The screen pack is 60/80/100 mesh. The die is 2,000 mm wide. Lip gap is 0.6 mm. Melt temperature is 245±5°C. Chill roll temperature is 20±2°C. Line speed is 200–350 m/min. Erucamide slip is added at 1,000–1,500 ppm. The target kinetic coefficient of friction is below 0.20 under ASTM D1894. Diatomaceous earth antiblock is added at 2,000–3,500 ppm. The terminal film must dart drop exceed 200 g under ASTM D1709, method A. The process becomes unstable if LDPE content exceeds 15 wt%. Excessive LDPE lowers the cloud point of the melt. It promotes draw resonance above 300 m/min. Edge neck-in is controlled below 10% of die width. The air gap is adjusted to 15–20 cm. If erucamide exceeds 1,500 ppm, static coefficient falls below 0.15. Finished rolls telescope during transport. If antiblock exceeds 3,500 ppm, haze rises above 8.0%. The bundle film loses clarity needed for barcode scanning. Moisture content is held below 0.02%. The bundling film is not food-contact by design. The same LLDPE regulatory status supports incidental contact under 21 CFR 177.1520 if required.

    Frozen seafood and vegetable packaging lines convert LL218 into 50–75 µm cast direct wrap or bag-in-box liner. The line uses a 1,800 mm die, 0.7 mm lip gap, 15–20 cm air gap, and 18±2°C chill roll. Melt temperature is 240–250°C. Output is 80–150 m/min. LL218 is melt-compounded with 0.05–0.10 wt% phenolic antioxidant and 0.10–0.15 wt% secondary phosphite. The film must remain ductile at -25°C. Target brittle temperature is below -70°C under ASTM D746. Minimum puncture force is 15 N for 60 µm film using a 50 mm probe at 300 mm/min. Dart impact under ASTM D1709, method A, is generally above 300 g for 60 µm specimens. For direct food contact, the film is qualified under 21 CFR 177.1520. Edge trim reuse above 20 wt% may reduce dart impact by 25% through gel clusters. The cast web is corona-treated to 38–42 mN/m per ASTM D2578 if printing is required.

    Free Quote

    Competitive Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LL 218 is a linear low-density polyethylene resin formulated for cast film extrusion. The grade is supplied as pelletized LLDPE produced with a short-chain branching distribution sufficient to achieve a nominal density of 0.918 g/cm³ under ASTM D1505-18 and a nominal melt flow rate of 2.0 g/10 min under ASTM D1238-20 at 190°C and 2.16 kg. In industrial practice, LL 218 is specified for monolayer and coextruded cast film where chill-roll quenching, low gel content, and controlled neck-in are more important than blown-film bubble stability. Typical end uses include cast stretch film, industrial overwrap, lamination film, and general packaging webs. The material is not optimized for high-throughput blown film; on blown film lines, bubble stability and machine-direction tear performance may be lower than those of blown-film-specific LLDPE grades.

    Because cast film processing imposes different melt elasticity requirements than blown film, the molecular weight distribution of LL 218 is balanced for stable flow through a flat-die lip. The density of 0.918 g/cm³ reflects a moderate level of short-chain branching, which suppresses crystallinity relative to high-density polyethylene and yields a lower melting point and reduced stiffness. The 2.0 g/10 min melt flow rate indicates a medium-flow resin: at typical cast film melt temperatures of 240°C to 280°C, the resin possesses sufficient flow to support high drawdown, while retaining adequate melt strength to limit draw resonance. Published rate-dependent viscosity data for LL 218 is limited; processors should establish shear viscosity curves by capillary rheometry according to ISO 11443:2021 or ASTM D3835-16 before specifying screw speed and die pressure limits.

    Does the Molecular Weight Distribution of LL 218 Produce Shear Thinning Characteristics Relevant to Flat-Die Operation?

    The melt flow rate of 2.0 g/10 min places LL 218 in a viscosity band that can be processed on single-screw extruders with L/D ratios from 24:1 to 33:1 without excessive motor load. In LLDPE resins of this class, increasing apparent shear rate from 100 s⁻¹ to 1000 s⁻¹ is generally accompanied by a viscosity reduction of 0.5 to 0.8 decade, depending on molecular weight distribution and temperature; this shear thinning reduces pressure drop across the die and improves melt homogeneity. The degree of die-lip buildup is governed less by shear viscosity than by low-molecular-weight components, antioxidant bloom, and polymer gel content. On cast film lines, the primary resin-dependent processing threats are neck-in, draw resonance, and die-lip deposit formation. LL 218, by virtue of its medium flow and short-chain branching, is normally processed with a lower melt temperature than a high-viscosity blown-film grade; this lowers the oxidative degradation rate and reduces gel formation during extended runs.

    When the melt film exits the die, the balance between shear thinning and extensional viscosity determines the maximum draw ratio before edge weave or draw resonance occurs. A narrow molecular weight distribution can reduce neck-in but may also produce sharper shear viscosity transitions that complicate feedblock control. The broader distribution typical of LL 218 supports stable layer formation in coextruded structures, although the specific distribution must be confirmed from the batch certificate rather than inferred from melt flow rate alone.

    Cast Film Extrusion Parameters for LL 218 on High-Output Lines

    Representative processing conditions are equipment-dependent and are not specification limits. A smooth-bore extruder with a barrier screw and 30:1 L/D is typically started with a feed zone at 180°C, a compression zone from 200°C to 230°C, a metering zone from 240°C to 260°C, and an adapter/die at 260°C to 280°C. The melt temperature measured at the die exit is normally maintained between 240°C and 280°C. The chill roll is operated between 20°C and 40°C; lower temperatures increase optical haze by rapidly freezing the web before sufficient relaxation, while higher temperatures can promote blocking and reduce line speed. The air gap between the die lip and chill roll is typically 5 cm to 15 cm. A shorter air gap reduces neck-in but may create melt wave instability; a longer air gap improves edge stability at the expense of higher neck-in and reduced melt strength.

    Processors running LL 218 on coextruded lines should monitor layer thickness uniformity. Interfacial flow instabilities in cast film can occur when the viscosity ratio between adjacent layers exceeds approximately 1:3 at the shear rates in the feedblock. Because LL 218 has a medium melt flow, it is commonly paired with LDPE or mLLDPE of matched viscosity; the use of high-viscosity HDPE skins may require separate extrusion temperature management. Feedblock temperature additions of 5°C to 10°C above the melt temperature are sometimes used to reduce interfacial instability, but excessive feedblock temperatures can degrade heat-sensitive outer layers.

    The following table provides representative film properties for LL 218 measured on 25 µm cast film produced under laboratory chill-roll conditions. These ranges are drawn from typical LLDPE cast film grade data and may differ from the current certificate of analysis; they are not specification limits.

    PropertyTest MethodRepresentative Value or Range
    Melt flow rateASTM D1238-202.0 g/10 min (190°C/2.16 kg)
    DensityASTM D1505-180.918 g/cm³
    Tensile strength at break, MDASTM D882-1830–40 MPa
    Tensile strength at break, TDASTM D882-1825–35 MPa
    Elongation at break, MDASTM D882-18400–600%
    Elongation at break, TDASTM D882-18600–800%
    Dart drop impact, F50ASTM D1709-16a70–100 g
    Elmendorf tear, MDASTM D1922-1560–120 g
    Elmendorf tear, TDASTM D1922-15300–450 g
    HazeASTM D1003-21<3.0%
    Gloss, 60°ASTM D2457-2175–90

    The tensile and tear directionality in cast film arises from machine-direction orientation during draw. The higher TD Elmendorf tear is characteristic of LLDPE cast film because machine-direction crystallization and orientation reduce MD tear resistance. When LL 218 is drawn at higher ratios or with a low chill-roll temperature, TD elongation may decrease while MD modulus increases. These shifts should be tracked by tensile testing under ASTM D882-18 and tear testing under ASTM D1922-15 during process optimization.

    When LL 218 Replaces a Butene-Comonomer Cast Film Resin in High-Clarity Film

    The substitution of LL 218 for a butene-comonomer LLDPE at equivalent density and melt flow rate typically shifts the tear and dart impact balance upward. Hexene-comonomer short-chain branching in LL 218 is associated with a more uniform distribution of tie chains in the semicrystalline network, which improves resistance to crack propagation under dangling dart impact and Elmendorf tear. Comparative film evaluations under ASTM D1709-16a and ASTM D1922-15 are used to quantify the change. This property advantage is most pronounced in TD tear; MD tear may remain lower because of orientation effects.

    The optical performance of LL 218 may be slightly different from butene LLDPE because chill-roll contact and crystallization rate are affected by comonomer length. Haze measurements under ASTM D1003-21 and gloss measurements under ASTM D2457-21 should be recorded at fixed chill-roll temperature and air gap, since changes in quench rate can alter surface roughness and internal haze. In multilayer constructions, the replacement may also require adjustment of the outer-layer slip additive loading because coefficient of friction under ASTM D1894-14 is influenced by surface crystal morphology and additive bloom rate.

    In coextruded cast film, LL 218 is used as a core or skin layer. The resin may provide a broader processing window than a metallocene LLDPE of similar density because its molecular weight distribution reduces feedblock pressure sensitivity, but it generally exhibits lower melt strength than LDPE. These differences affect layer encapsulation in feedblocks and die-lip wetting. If LL 218 is placed adjacent to mLLDPE, the interface can exhibit laminar mixing but not necessarily full melt-stream penetration; feedblock temperature is usually raised to 250–270°C to reduce viscoelastic instability. Compared with LDPE, LL 218 has superior dart drop and tear at equivalent thickness, but lower melt strength and greater neck-in; die geometry and air-gap control are therefore more critical.

    Regulatory Compliance, Storage, and Operational Boundaries

    The base olefin polymer may be covered by FDA 21 CFR 177.1520 when the conditions of use and composition are within the cited paragraph. Converters must confirm that the specific lot of LL 218 has food-contact status for the intended food type, temperature, and thickness; a grade-specific regulatory certificate from Braskem is required for food-contact applications. European converters must verify compliance with Regulation (EU) No 10/2011 as amended and Regulation (EC) No 1907/2006 (REACH); specific migration limits depend on article thickness, food simulant, and contact time.

    LL 218 does not require predrying under normal indoor storage below 60% RH. If pellets are transferred from cold storage to a humid warm production area, condensation on pellet surfaces can introduce water into the feed throat and cause surface defects; a hopper blanket or dehumidified-air sweep at 40–50°C is recommended. Processing above 300°C or prolonged hold-up time at high temperature can induce chain scission and carbonyl formation, producing visible gels and off-odour. The grade is not inherently UV-stabilized; outdoor service is outside the typical design envelope unless a converter incorporates a UV stabilizer masterbatch.

    For cast stretch film, LL 218 may be formulated with tackifier masterbatches and slip/antiblock concentrates to achieve the desired unwinding force and cling force. Cling response is formulation-dependent and is not governed by a single universal ASTM method; converters should evaluate final film performance on pilot lines using the actual chill-roll, air-gap, and draw-ratio conditions. The selection of LL 218 as a core resin therefore requires confirmation of final film properties under production-scale conditions rather than reliance solely on resin melt flow rate and density.

    Top