Braskem Ll 218 21 Lldpe Blown Film Extrusion Polyethylene

Braskem LL 218/21 LLDPE Blown Film Extrusion Polyethylene

    • Product Name: Braskem LL 218/21 LLDPE Blown Film Extrusion Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 676269
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer 1-Butene
    Density 0.918 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 2.1 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield 9 MPa
    Tensile Strength At Break 24 MPa
    Elongation At Break 800%
    Flexural Modulus 200 MPa
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Dart Drop Impact 100 g
    Haze 10%
    Gloss 45 70%
    Coefficient Of Friction 0.2

    As an accredited Braskem LL 218/21 LLDPE Blown Film Extrusion Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LL 218/21 LLDPE for blown film extrusion is packaged in 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped.
    Container Loading (20′ FCL) Braskem LL 218/21 LLDPE blown film polyethylene resin loaded in a 20-foot FCL container, palletized bags, evenly distributed and secured.
    Shipping Braskem LL 218/21 LLDPE is shipped as non-hazardous polyethylene resin pellets, typically in 25 kg moisture-resistant bags or bulk bags, palletized and stretch-wrapped. Transport in clean, dry vehicles away from heat, direct sunlight, moisture, and strong odors. Store under cool, dry conditions; handle pallets carefully to prevent bag damage.
    Storage Store Braskem LL 218/21 LLDPE in original, unopened bags or containers in a cool, dry, well-ventilated indoor area. Keep away from direct sunlight, heat, flames, and strong oxidizing agents. Prevent moisture, dust, and contamination. Stack pallets securely to avoid package damage. Protect packages from punctures and tearing. Maintain good housekeeping and follow the manufacturer’s SDS for safe handling and storage.
    Shelf Life Shelf life is typically 12 months from production when stored in original unopened packaging, dry, away from heat and direct sunlight.
    Application of Braskem LL 218/21 LLDPE Blown Film Extrusion Polyethylene

    Dart Impact at Subzero Temperatures Governs Silage Cover Formulations

    On agricultural film towers producing silage clamp covers and greenhouse side curtains, Braskem LL 218/21 is run as the main structural resin because its 0.918 g/cm³ density and 2.1 g/10 min melt flow rate, measured under ISO 1133-1:2022 at 190°C/2.16 kg, permit lower extrusion head pressure than fractional-MI LDPE while retaining tear propagation resistance in thin cover films. The standard formulation for a 150 µm white/black silage cover consists of 88–92 wt% LL 218/21 plus 8–12 wt% of a UV stabilizer masterbatch carrying hindered amine light stabilizers and benzophenone-type absorbers; carbon black is introduced at 3–5 wt% only in the black inner layer to block photosynthetically active radiation. Compliance is assessed under EN 13206 for agricultural covering films, with tensile properties measured according to ISO 527-3 and dart impact according to ASTM D1709 Method A; typical end-use specifications require a minimum dart drop of 400 g at -20°C for 150 µm film, though published data for this specific grade in low-temperature silage covers is limited. Processing uses a 75 mm single-screw extruder with 30:1 L/D and a barrier screw, die gap set to 1.8–2.4 mm, blow-up ratio 2.2:1–2.8:1, melt temperature 190–210°C, and frost line height between 600 mm and 800 mm below the die. The terminal product range includes silage clamp covers, greenhouse side rolls, and agricultural fumigation tarpaulins. Production-scale failures observed on such lines include bubble pinholes when frost line height is kept too low and centerfold blocking when frost line height is raised above 800 mm; bubble cooling air velocity must therefore be adjusted to hold the frost line stable without inducing oscillation or diameter variation.

    Can a 2.1-g/10-min LLDPE Maintain Seal Integrity at -25°C?

    Seal failure in frozen food webs at -25°C is caused less by the base polyethylene than by slip-agent migration and inadequate hot tack during vertical form-fill-seal jaw closure. A representative formulation for a 40–60 µm frozen vegetable or seafood film uses 70–85 wt% LL 218/21, 15–30 wt% of an autoclave LDPE with melt index 0.3–0.5 g/10 min, and 1.0–2.5 wt% of a slip/antiblock masterbatch. Compliance for direct food contact is referenced under 21 CFR 177.1520 and EU Regulation No 10/2011 Annex I, with overall migration testing under OM2 or OM3 conditions depending on storage duration and temperature profile. The film is produced on a blown line with die gap 0.8–1.2 mm, blow-up ratio 2.0:1–2.4:1, reverse barrel temperature profile 175–195°C, die temperature 195–210°C, and a low frost line at 4–6 die diameters to improve gauge uniformity. Terminal products include frozen vegetable bags, ice cream pouches, and frozen fish laminates. Operational boundaries are explicit: if slip agent concentration exceeds 2.5 wt%, the film’s kinetic coefficient of friction may fall below 0.15, producing web tracking faults and jaw sticking on vertical form-fill-seal machines; if the slip masterbatch is not pre-dried at 60–70°C for 2–4 h when ambient relative humidity exceeds 60%, moisture-induced melt pressure fluctuations appear as transverse gauge bands.

    Industrial Liner Puncture Resistance and Oxidation Induction Time in Heavy-Gauge Extrusion

    Heavy-gauge liners for FIBCs, e-commerce mailer stacks, and shipping sacks place a different demand on bubble cooling than thin food films because film thickness of 125–200 µm raises residence time and increases oxidative gel risk if melt temperature exceeds 220°C. The formulation for a 175 µm heavy-duty liner is 60–75 wt% LL 218/21, 20–35 wt% of an HDPE with density 0.945–0.957 g/cm³ and melt index 0.2–0.5 g/10 min, and 2–3 wt% of a fluoroelastomer processing aid when gauge exceeds 150 µm to reduce die-lip buildup. Compliance is verified through ASTM D882 for tensile yield and elongation at break, ASTM D1709 Method B for dart impact, and ASTM D1922 for Elmendorf tear; where liners are used inside UN-certified FIBCs, the outer FIBC is qualified under UN Recommendations on the Transport of Dangerous Goods, Chapter 6.1, while the liner itself is tested for puncture resistance. On a mono-layer blown film line, die gap is set at 2.2–2.6 mm, blow-up ratio is kept low at 1.8:1–2.2:1 to reduce film width variation and edge curl, melt temperature is 200–220°C, and haul-off speed is reduced to maintain target gauge. Terminal products include FIBC inner liners, heavy-duty shipping sacks, and flat-bottom mailers. A documented processing boundary is that bubble cooling air flow must be lowered when frost line oscillation becomes visible; conversely, raising the frost line above 8 die diameters at 180 µm has produced inside-surface blocking on the bubble collapse frame and blocking on downstream gusset boards.

    When Blown Sealant Films Are Coextruded with Barrier Webs

    Corona-treated sealant webs for dry-mix pouches and lidding films are produced on three-layer coextrusion towers where LL 218/21 forms the innermost sealing layer. A typical lamination web uses 85–100 wt% LL 218/21 and 0–15 wt% metallocene LLDPE to reduce seal initiation temperature and improve low-temperature seal strength. Compliance is anchored to 21 CFR 177.1520 and EU Regulation No 10/2011 for direct food contact, while seal strength and hot tack are evaluated under ASTM F88/F88M and ASTM F2029, respectively. Processing uses a coextrusion die gap of 1.2–1.8 mm, blow-up ratio 2.0:1–2.4:1, melt temperature 185–205°C, and corona treatment to 38–42 dyn/cm; the sealant layer thickness is 20–50 µm within a 60–120 µm total laminate structure. Terminal products include stand-up pouches, lidding films, and pre-made side-gusset bags. The operational limit is that corona treatment above 44 dyn/cm can degrade heat seal strength through excessive surface oxidation, and inline priming must be fully dried before winding to prevent blocking in rewind rolls.

    Pallet load containment films for stretch hood machines demand a balance between machine-direction elongation, elastic recovery, and puncture resistance at corner stress points. On extrusion lines fitted with internal bubble cooling and a high-stalk bubble configuration, LL 218/21 is formulated at 70–85 wt% with 15–30 wt% VLDPE or metallocene LLDPE having density 0.900–0.912 g/cm³; slip masterbatch is kept at 1.0–2.0 wt%. Compliance is measured with ASTM D5458 for cling and ASTM D5459 for machine-direction elastic recovery and permanent set, while tensile is checked by ISO 527-3. Processing uses die gap 1.8–2.2 mm, blow-up ratio 2.5:1–3.0:1, melt temperature 190–210°C, and film gauge 50–80 µm. Terminal products include stretch hood films, pallet top sheeting, and irregular-load containment wrap. Published data for this specific grade in high-recovery stretch hood structures is limited; permanent set at 100% extension must be characterized on the target line before qualification, and blends containing more than 30 wt% VLDPE can produce bubble instability at BUR above 3.0:1.

    Because refuse sack converting includes perforation and drawstring insertion, gauge uniformity at 18–45 µm controls downstream tear propagation more than melt flow alone. In household and institutional can liner production, LL 218/21 is formulated at 75–85 wt% with 10–20 wt% recycled post-industrial LDPE and 3–5 wt% carbon black or color masterbatch. Compliance is specified under EN 13592 for household waste sacks, with tensile and tear measured by ISO 527-3 and ISO 6383-2. Processing uses a monolayer bubble line with die gap 0.8–1.4 mm, blow-up ratio 2.0:1–2.5:1, melt temperature 180–205°C, and frost line height 4–7 die diameters. Terminal products include drawstring bin liners, institutional can liners, and leaf collection sacks. Below 18 µm, perforation lines for drawstring insertion create tear propagation; film gauge is typically raised to 20–25 µm when recycled content exceeds 20 wt%, and drum cooling before gusseting is required to prevent blocking.

    Free Quote

    Competitive Braskem LL 218/21 LLDPE Blown Film Extrusion Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LL 218/21 is a butene-comonomer linear low-density polyethylene intended for blown film extrusion. The grade designation is associated with a nominal density of 0.918 g/cm³ when measured according to ASTM D792-20 and a nominal melt mass-flow rate of 2.1 g/10 min when measured at 190°C with a 2.16 kg weight according to ISO 1133-1:2022. The resin is supplied as pelletized material with a producer-stated additive package that may include processing stabilizers, slip agents, and antiblock agents. Lot-specific additive composition and loading should be confirmed from the Braskem product datasheet or certificate of analysis before film surface properties are fixed.

    The product code identifies the density class and flow grade. The 218 segment positions the resin in the nominal 0.918 g/cm³ density range, while the /21 suffix corresponds to the nominal 2.1 g/10 min melt flow rate. This distinction is relevant when comparing LL 218/21 with LL 118/21, a lower-melt-flow butene LLDPE in the same density family, or with hexene- and octene-based linear low-density polyethylene grades that modify short-chain branching architecture and impact-tear balance.

    What Distinguishes Butene-Comonomer LLDPE from Higher-Alpha-Olefin Resins in Blown Film?

    Butene-based LLDPE contains shorter side-chain branches than hexene- or octene-based copolymers. At equivalent nominal density of 0.918 g/cm³ and melt flow rate of 2.1 g/10 min, a butene copolymer typically produces lower dart drop impact and lower Elmendorf tear than a hexene or octene copolymer. The property differences are evaluated using ASTM D1709-16a for dart impact and ASTM D1922-15 for Elmendorf tear; however, published data for this specific configuration is limited, and absolute film values must be established by converter trials on the actual blown film line.

    The shorter branch length also affects melt-state extensional behavior. The bubble on an air-cooled blown film line may be less stable during high-stalk processing than a higher-alpha-olefin grade because the entangled network is disrupted more readily at blow-up ratios above 3.0:1. The resulting processing window favors low-stalk, moderate-blow-up operation rather than high-stalk tubular film production. This does not preclude film production at higher blow-up ratios, but bubble stability must be managed through air ring selection, die gap, and frost line height.

    On a production-scale monolayer line using a 65 mm single-screw extruder with a 30:1 L/D barrier screw and a 250 mm spiral mandrel die having a 2.0 mm die gap, LL 218/21 is processed at melt temperatures between 190°C and 220°C. Prolonged exposure above 230°C may produce oxidized gel defects depending on stabilizer consumption and residence time. The die lip shear stress should be kept below the melt fracture threshold; increasing the die gap from 1.8 mm to 2.5 mm or raising melt temperature reduces surface roughness when sharkskin appears. These settings are equipment-dependent and require adjustment for die diameter, air ring type, and output rate.

    Because the melt flow rate is 2.1 g/10 min, head pressure and motor load are lower than for a 1.0 g/10 min grade of the same density. Higher screw speeds may be possible on the same extruder at equivalent motor amperage, but published data for this specific conversion line is limited. Bubble stability becomes the limiting constraint rather than extruder pressure, especially when air ring velocity is high or when the frost line is positioned more than 3.0 die diameters above the die. Edge guide tracking fluctuations can also disturb the bubble when melt strength is low.

    Film gauge capability is governed by die gap, blow-up ratio, and draw-down ratio. With a die gap of 1.8 mm to 2.5 mm and a blow-up ratio between 2.5:1 and 3.5:1, LL 218/21 can be drawn into films from approximately 20 µm to 120 µm on conventional air-ring equipment. Below 20 µm, the probability of bubble breathing and gauge bands increases unless a dual-lip air ring, internal bubble cooling, or a higher-viscosity blend partner is used. Above 120 µm, cooling rate and blocking at the nip become limiting, and the film may require additional slip or antiblock as determined by coefficient of friction testing under ASTM D1894-14.

    If Coextrusion or Heavy-Duty Film Requires Higher Puncture Resistance

    In multilayer film structures, LL 218/21 may be assigned to a core layer or an internal skin where its flow behavior can improve gauge uniformity. If the film must resist high dart impact or aggressive loading, a hexene or octene LLDPE, or a bimodal medium-density polyethylene, may be required. Comparative evaluations are conducted under ASTM D1709-16a for dart impact and ASTM D1922-15 for Elmendorf tear; at equivalent 50 µm thickness, butene LLDPE typically falls below higher-alpha-olefin copolymers. The difference is not an artifact of nominal density but arises from short-chain branch length, tie-molecule concentration, and molecular weight distribution.

    A converter considering replacement of LL 118/21 with LL 218/21 should expect lower extruder pressure, lower melt viscosity, and potentially higher throughput, but also a reduction in dart impact and tear if film gauge remains unchanged. The substitution may be acceptable for general-purpose liners and lightweight films but is not recommended for heavy-duty sacks, frozen food packaging with high impact requirements, or agricultural films exposed to repeated wind load. The final decision should be based on film property data generated under the intended blow-up ratio and film thickness rather than resin data alone.

    Comparative test methods for blown film grade differentiation
    Standard method Property Relevance to LL 218/21 blown film conversion Typical trend versus 1.0 g/10 min butene LLDPE
    ISO 1133-1:2022 Melt mass-flow rate at 190°C/2.16 kg Indicates extruder backpressure, motor load, and die lip flow Higher for LL 218/21; lower apparent viscosity at typical die lip shear rates
    ASTM D792-20 Density Correlates with film stiffness and moisture vapor transmission resistance Comparable nominal density; lower modulus than HDPE film grades
    ASTM D1709-16a Dart drop impact Measures film puncture resistance under impact; sensitive to molecular weight and comonomer type Often lower than a 1.0 g/10 min butene grade and lower than hexene/octene copolymers at equivalent density
    ASTM D1922-15 Elmendorf tear Assesses tear propagation resistance in machine and transverse directions Often lower than lower-melt-flow or higher-alpha-olefin copolymers
    ASTM D882-18 Tensile properties Controls load retention, elongation at break, and film handling May show lower strain at break due to lower molecular weight

    Melt rheology data for butene LLDPE with a melt flow rate of 2.1 g/10 min show shear-thinning behavior in the extrusion shear-rate range. At 200°C, the apparent viscosity at a wall shear rate of 100 s⁻¹ is lower than that of a 1.0 g/10 min butene grade, which reduces die pressure but also lowers bubble tension. The viscosity curve is typically measured by capillary rheometry using ISO 11443 or parallel-plate oscillatory rheometry using ISO 6721-10. The crossover of elastic modulus and viscous modulus, often used to indicate molecular weight distribution, is not a substitute for full film testing.

    At low shear rates associated with bubble stretching, extensional viscosity becomes limiting. Butene copolymer with a 2.1 g/10 min melt flow rate may not strain-harden sufficiently at high strain rates, and the melt may rupture rather than stabilize under excessive draw. This is why blow-up ratios above 3.5:1 are not recommended without a melt-strength-enhancing blend partner or internal bubble-cooling system. The precise limitation depends on die gap, melt temperature, and air ring configuration.

    For screw selection, a barrier screw with a Maddock shear mixer is preferred to homogenize melt temperature and reduce gels. A compression ratio of 2.8:1 to 3.5:1 and a length/diameter ratio of 24:1 to 30:1 are common for LLDPE blown film. When using a smooth-bore extruder, output stability depends on feed-particle conveying; a grooved-feed throat can increase throughput but also raises melt temperature. LL 218/21 can be processed on both smooth-bore and grooved-feed extruders, but the latter may require a lower barrel profile to avoid exceeding 230°C.

    Processing Faults Related to Melt Fracture and Air Ring Imbalance

    Melt fracture in LL 218/21 appears as regular surface roughness, most often sharkskin on the film surface. It occurs when the shear stress at the die land exceeds a resin-specific critical stress. The risk increases at low melt temperatures, narrow die gaps, and high screw speeds. Operators can suppress sharkskin by raising the melt temperature to 220°C, increasing the die gap from 1.8 mm to 2.5 mm, or reducing screw speed to lower die pressure. Air ring imbalance creates a different defect: periodic gauge bands or rhythmic bubble oscillation. A capacitance thickness scanner can separate gauge variation from surface roughness; if roughness remains at constant thickness, melt fracture is likely.

    Bubble instability in low-stalk operation is often misdiagnosed as insufficient melt strength. In many cases the cause is excessive air ring velocity or a frost line position that is too low, which cools the film surface before the inner layer has oriented. For a melt flow rate of 2.1 g/10 min, the frost line should be raised or the cooling airflow reduced to maintain bubble symmetry before introducing a higher-viscosity blend partner. Changes to air ring flow should be made in increments and confirmed by thickness profile measurement.

    Regrind can be incorporated into LL 218/21 film production, but the stabilizer package is not unlimited. Repeated heat history from high-temperature extrusion can consume antioxidants and raise the gel count. A lot-to-lot gel count under ISO 18553 or equivalent optical defect methods should be monitored when regrind content exceeds 20 wt%; above this level, film appearance may degrade depending on the previous film’s additive load and contamination level. Edge trim and start-up scrap should be reground only if free of foreign polymer fractions that reduce compatibility.

    Verify Food-Contact and Regulatory Compliance Before Converting

    The olefin polymer base of LL 218/21 is expected to meet FDA 21 CFR 177.1520 for olefin polymers when used under conditions of intended food-contact use. The resin is supplied within Braskem’s global regulatory systems, including REACH registration for European Economic Area supply. However, the converter is responsible for final food-contact status because masterbatch, slip/antiblock concentrates, printing inks, and lamination adhesives can introduce non-compliant substances. Final migration testing should follow Commission Regulation (EU) No 10/2011 or relevant national methods for the finished film.

    LL 218/21 is not intended for medical devices, pharmaceutical packaging, or applications involving high-temperature sterilization unless specific converter validation confirms extractables, hemolysis, cytotoxicity, and other healthcare requirements. This limitation is due to the standard stabilizer and lubricant package rather than the polyethylene backbone itself. The producer datasheet should be consulted before any regulated end use, and the converter must maintain documentation of additive compliance.

    Polyethylene does not require drying under normal storage. If pellets are exposed to high humidity or condensation, surface moisture can enter the feed throat and create steam-induced film defects. A short desiccant-air drying step at 70°C for 2 h to 3 h can remove surface moisture, but the producer datasheet may not require routine drying. Avoid overheating pellets above 80°C during drying to prevent pellet agglomeration and additive depletion.

    In industrial liner production at film thicknesses of 30 µm to 80 µm, LL 218/21 can provide acceptable toughness and modulus when the converter maintains a consistent frost line and blow-up ratio. The film’s machine-direction tear and transverse-direction tear are influenced by orientation; increasing blow-up ratio from 2.5:1 to 3.5:1 shifts molecular orientation and changes tear balance as measured by ASTM D1922-15. Converters must measure both machine-direction and transverse-direction properties because film performance is anisotropic. Applications requiring isotropic tear or high puncture resistance should be evaluated against alternative resins rather than inferred from nominal flow or density data.