    Specifications
    HS Code 292663
    Comonomer Butene-1
    Density 0.918 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 1.0 g/10 min
    Melting Point 123 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 800 %
    Dart Drop Impact 110 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 450 g
    Haze 12 %
    Gloss 50 %
    Coefficient Of Friction 0.2

    As an accredited Braskem LL 118 LLDPE Blown Film Extrusion Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Braskem LL 118 LLDPE Blown Film Extrusion Polyethylene is supplied in 25 kg polyethylene-lined bags, palletized, stretch-wrapped, and labeled.
    Container Loading (20′ FCL) 20′ FCL loaded with Braskem LL 118 LLDPE Blown Film Extrusion Polyethylene in 25 kg bags, palletized and securely wrapped.
    Shipping Braskem LL 118 LLDPE is a non-hazardous polyethylene resin, shipped as pellets in 25 kg bags, octabins, or bulk trucks/railcars. Store in a cool, dry, ventilated area away from heat, sunlight, and moisture. Not regulated for DOT, IMDG, or IATA transport. Handle with standard industrial hygiene.
    Storage Store Braskem LL 118 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and strong oxidizers. Keep original bags or containers closed and palletized to prevent moisture, dust, and contamination. Maintain ambient temperatures, avoid prolonged UV exposure, and follow first-in, first-out stock rotation. Handle cleanly; no smoking or open flames. Store separately from incompatible materials.
    Shelf Life Typically 24 months when stored in original unopened packaging, cool, dry, away from sunlight, heat, moisture, and contaminants.
    Application of Braskem LL 118 LLDPE Blown Film Extrusion Polyethylene

    On high-output monolayer blown film lines, the 0.918 g/cm³ density and 1.0 g/10 min melt flow rate of LL118 are selected for webs converting into pillow pouches, side-gusseted bags, and wicketed bread bags. In a 100% LL118 formulation, a slip/antiblock masterbatch based on erucamide (500–1,500 ppm active) and synthetic silica (1,000–3,000 ppm active) is added at 2–4 wt%; converters running high-speed vertical form-fill-seal equipment monitor film-to-film coefficient of friction to remain between 0.10 and 0.30 per ASTM D1894. The extrusion process uses a die gap of 1.8–2.4 mm, a blow-up ratio of 2.2:1–2.8:1, and a melt temperature window of 193–210 °C; chilled air at 8–12 °C and a frost line height of 4–7 die diameters produce gauge profiles within ±5% on 80–120 µm webs. End-seal strength on vertical form-fill-seal machines is verified by ASTM F88/F88M-21; seal initiation is observed at 85–95 °C, and jaw dwell times below 0.3 s increase the risk of channel leakers, particularly in side-gusseted structures. Terminal films are converted into bread bags, frozen fruit pouches, tissue overwrap, and lightweight produce bags. Lot-to-lot variance in the low-comonomer section of the LL118 reactor product can shift the seal initiation plateau by ±2 °C; converters should request incoming-lot certification per ASTM D1238 and density per ASTM D1505 and set the sealing jaw temperature to compensate. Film haze after conversion is measured by ASTM D1003 and should remain below 15% for clear produce bags; additive loadings above 1,500 ppm erucamide can raise haze and reduce heat-seal strength after slip bloom develops at 23 °C for 48 h. Compliance for direct food contact relies on the following:

    Regulatory frameworkStandard or clauseMeasured parameter
    U.S. FDAFDA 21 CFR 177.1520(c) 3.1a/3.2aOlefin polymer identity and extractives limits
    European UnionEU Regulation 10/2011Overall migration limit ≤ 10 mg/dm²
    European Union GMPEU Regulation 2023/2006Food contact material manufacturing practice
    ChinaGB 4806.7-2016Plastic food contact materials

    What Oxygen Ingress and HALS Loading Boundaries Govern White/Black Silage Film on Multi-Layer Blown Film Lines?

    Agricultural silage bags and bale wrap produced with LL118 in the sealing or core layer demand separate additive loading by layer. A three-layer coextrusion structure with a white outer layer and a black inner layer is built as follows: outer layer 20–25 wt% white masterbatch containing 60 wt% TiO₂ in LDPE and active hindered amine light stabiliser at 0.5–1.0 wt%; core 60–70 wt% LL118; inner black layer 20–25 wt% carbon black masterbatch at 40 wt% carbon black in LDPE. At total film thickness of 150–250 µm, oxygen permeability measured by ASTM D3985 at 23 °C, 0% RH is generally within 1,800–2,500 cm³/m²·day·atm for LLDPE-rich webs, which is acceptable only when the film is sealed within 24 h of bale wrapping; beyond that period oxygen ingress accelerates aerobic deterioration at the bale face. The extrusion process on a 55 mm grooved-feed blown film line with an L/D ratio of 30:1 uses a die gap of 2.0–2.6 mm, a blow-up ratio of 2.0:1–2.4:1, and melt temperatures of 200–215 °C. Processing difficulties appear above 1.0 wt% active HALS because plate-out on chilled air ring surfaces increases differential cooling and creates gauge bands; the corrective action is to clean the air ring lip and reduce active HALS to 0.7 wt% before restart. Separate addition of UV stabiliser to the core is not required when both skins contain HALS, but if LL118 is used in a black layer without white coextrusion, 2.5–3.5 wt% carbon black masterbatch is required to reduce photodegradation of the polyolefin matrix. Compliance includes EN 13206:2017 for thermoplastic covering films used in agriculture and horticulture; the polyolefin base resin is within the scope of EU Regulation 10/2011, but the finished additive package must be assessed separately. Terminal products include round bale silage wrap, silage clamp cover sheets, and silage tubes. Published data for LL118-specific tropical UV weathering is limited; xenon-arc testing per ISO 4892-2 should be performed before service life beyond 12 months is claimed.

    For heavy-duty industrial liners and sack film, the control of melt fracture onset at high output rates determines whether LL118 can be run at 100% or requires blending. On a 65 mm single-screw blown film line with a barrier screw and an L/D ratio of 25:1, melt temperatures are held at 205–220 °C, die gap is widened to 2.0–2.7 mm, and blow-up ratio is reduced to 1.8:1–2.2:1; these settings suppress sharkskin because LLDPE relaxes extensional stress more effectively in a wider die gap. A typical drum liner formulation is 85 wt% LL118 with 15 wt% high-pressure LDPE having a melt flow rate of 0.3–0.5 g/10 min; film thickness is 80–150 µm. Where converters downgauge to 70 µm, the addition of 10–20 wt% metallocene LLDPE raises dart impact but increases extruder head pressure by 8–12%. Melt pressure before the screen changer is typically 240–280 bar, with a screen pack of 20/40/60 mesh. Sharkskin elimination can also be assisted by 0.5–1.0 wt% polymer processing aid, but processing aid is not automatically acceptable in food-contact or transparent structures and must be evaluated against the end-use compliance framework. Compliance is benchmarked against ASTM D4976-12a for polyethylene plastics film and, for non-hazardous transport liners, tensile and dart impact are verified by ASTM D882 and ASTM D1709. Terminal products include heavy-duty industrial liners, construction films, furniture wrap, and FIBC inner liners. Chemical resistance must be confirmed by immersion testing per ISO 175 because LL118 alone is not resistant to strongly oxidising acids or aromatic solvents.

    When Stretch Hood Downgauging Falls Below 80 µm, Which Puncture and Recovery Thresholds Control the Structure?

    Stretch hood films deployed on automatic pallet-hooding machines use LL118 in the core to balance elastic recovery and puncture propagation resistance. In a three-layer structure, the core layer is 60–75 wt% LL118, the outer skins each contribute 10–20 wt% high-pressure LDPE or metallocene LLDPE, and a tackifier masterbatch may occupy 0–3 wt%; total film thickness is commonly 80–120 µm, although 65 µm is attempted for low-weight pallets. At 65 µm, puncture resistance measured by ASTM D5748 should not fall below 12 J, and dart impact per ASTM D1709 should remain above 600 g at 66 cm drop height; otherwise corner tears occur during multi-drop transit. The extrusion line uses a 70 mm barrier-screw extruder, die gap 1.8–2.4 mm, blow-up ratio 2.5:1–3.0:1, and melt temperature 190–205 °C. High BUR is required because the blown bubble is collapsed through a high-speed nip at up to 80 m/min; gauge variation must remain within ±4% or hooding machines with pre-stretch ratios above 1.1:1 tear at the pallet corners. Process conflict arises above 3.0:1 BUR because bubble instability increases at high nip speeds; a compromise BUR of 2.7:1 is commonly selected for pallet hood lines. Compliance for non-food pallet hood film is based on ISO 527-3 tensile properties, ISO 6383-2 tear resistance, and ASTM D5748 puncture propagation. Terminal products include pallet hoods for bagged cement, bottled water, home appliances, and wrapped furniture. Published data for LL118-specific recovery after sustained load at 40 °C is limited; warehouse creep testing under EN ISO 899-1 should set the maximum stacked pallet service time.

    Predominantly in frozen vegetable and fruit packaging, blown film converters specify LL118 at 30–60 µm gauge for low-temperature seal initiation and hot-tack strength on high-speed vertical and horizontal form-fill-seal machines. The formulation is 90–100 wt% LL118 with 0–10 wt% high-pressure LDPE; an antiblock masterbatch is added at 1–3 wt% to maintain film-to-film coefficient of friction below 0.25 per ASTM D1894, and slip additive is limited to 500–1,000 ppm active erucamide to avoid depressing seal initiation. On a 50 mm barrier-screw extruder, the die gap is 1.5–2.2 mm, blow-up ratio 2.3:1–3.0:1, and melt temperature 190–210 °C; frost line height is set at 5–8 die diameters to raise crystallinity before nip collapse and reduce blocking in freezer storage. Seal initiation on jaw-type sealers is expected at 85–95 °C, with hot tack force above 2.0 N/25 mm measured by ASTM F1921; this is critical because frozen product load is applied immediately after sealing. Compliance for direct food contact follows FDA 21 CFR 177.1520(c) 3.2a, EU Regulation 10/2011, and migration testing per EN 1186. Terminal products include frozen vegetable bags, fruit pouches, ice cream bags, and frozen meat overwrap. Total erucamide should not exceed 1,500 ppm because bloom-induced haze after freezer cycling creates optical defects; haze above 15% on 50 µm film measured by ASTM D1003 is generally rejected for printed frozen food bags.

    Corona-Treated Sealant Webs in BOPET/PE and BOPP/PE Laminations

    For laminations using 12–18 µm BOPET or 20–30 µm BOPP as the outer web, monolayer LL118 blown film serves as the heat-seal layer at 25–50 µm thickness. The sealant formulation is 95–100 wt% LL118 with 0–5 wt% LDPE, plus 0.5–1.5 wt% processing-aid masterbatch on 45 mm smooth-bore extruders prone to melt fracture above 150 kg/h output. A die gap of 1.8–2.4 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 195–215 °C are used; inline corona treatment raises surface energy to 38–44 dyn/cm per ASTM D2578 before winding so that solvent-free polyurethane adhesives achieve destructive tear bonds. Rewind tension should not exceed 10 N/cm of web width at 30 µm thickness to avoid blocking of the treated surface after 72 h at 25 °C. Surface treatment decay after 72 h requires re-treatment before lamination; otherwise adhesive failure in BOPET/PE laminates appears as tunneling after pouch filling. Compliance for the sealant layer in food laminations includes FDA 21 CFR 177.1520(c) 3.1a/3.2a and EU Regulation 10/2011; for retortable structures, heat-seal strength after retorting at 121 °C for 30 min is verified by ASTM F88/F88M-21. Terminal products include stand-up pouches, coffee bags, sauce pouches, and vacuum packaging for processed meat. Residual slip additive bloom can reduce lamination bond strength; published data for LL118 in high-speed adhesive lamination is limited, so line trials with the selected polyurethane adhesive are required before commercial release.

    Free Quote

    Competitive Braskem LL 118 LLDPE Blown Film Extrusion Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Braskem LL 118 is a butene-comonomer linear low density polyethylene resin engineered for tubular blown film extrusion. The pelletized grade is characterized by a nominal melt flow rate of 1.0 g/10 min determined at 190 °C and 2.16 kg in accordance with ISO 1133-1:2022 or ASTM D1238-20, and a nominal solid-state density of 0.918 g/cm³ determined under ISO 1183-1:2019 or ASTM D792-20. These values position LL 118 in the medium-molecular-weight, low-density segment used for unfilled film packaging. Typical converting lines convert the resin into tubular films from 15 µm to 200 µm for general-purpose liners, carrier bags, garment bags, agricultural mulch, frozen food overwrap, and protective packaging. The butene short-chain branch architecture is less effective at generating tie-chain populations than hexene or octene comonomer distributions at similar density, and this controls the film’s dart impact, tear, puncture, and haze response after orientation.

    PropertyTest methodRepresentative value
    Melt flow rate, 190 °C/2.16 kgISO 1133-1:2022 / ASTM D1238-201.0 g/10 min
    Density, 23 °CISO 1183-1:2019 / ASTM D792-200.918 g/cm³
    Tensile strength at break, MD/TDISO 527-3:2018 / ASTM D882-1838 MPa / 28 MPa
    Elongation at break, MD/TDISO 527-3:2018 / ASTM D882-18650% / 750%
    Secant modulus, MD/TD, 1% strainISO 527-3:2018 / ASTM D882-18220 MPa / 240 MPa
    Dart impact, F50ISO 7765-1:1988 / ASTM D1709-16a110 g
    Elmendorf tear, MD/TDISO 6383-2:1983 / ASTM D1922-15300 g / 450 g
    Haze, 25 µm filmISO 14782:1999 / ASTM D1003-1312%

    The values in Table 1 are representative film properties obtained at 25 µm gauge and 2.5:1 blow-up ratio. They are not lot-specific limits; lot release data on the certificate of analysis should be used for process capability studies and incoming resin acceptance.

    What Distinguishes LL 118 from LDPE Homopolymer and Higher-Alpha-Olefin LLDPE Grades?

    Braskem LL 118 differs from high-pressure LDPE homopolymer of comparable density and melt flow rate in molecular architecture and shear rheology. The long-chain branching present in high-pressure LDPE provides high melt tension and pronounced shear thinning at die-lip shear rates. LL 118 is a linear polymer with short butene branches and lower melt tension, but the linear backbone increases strain hardening in the solid state and improves puncture resistance after crystallization. In monolayer liner applications, this permits gauge reduction from 60 µm LDPE to 45 µm LL 118 while maintaining dart impact above 90 g on equipment with wide die gaps. The trade-off appears in bubble stability: the lower melt tension of LL 118 makes the bubble more sensitive to ambient air currents, die-face turbulence, and collapse-frame misalignment. Converters operating older lines frequently widen the die gap from 1.0 mm to 1.8–2.2 mm to reduce die-lip shear stress and maintain a stable frost line.

    Against a hexene-comonomer LLDPE of similar 1.0 g/10 min melt flow rate and 0.918 g/cm³ density, LL 118 typically exhibits lower dart impact, lower puncture resistance, and higher haze because butene branches are shorter and generate fewer effective tie chains between crystal lamellae. At 25 µm, published data for hexene-based film grades often report dart impact in the 140–180 g range, while LL 118 falls between 100 g and 120 g under equivalent processing. The processing advantage of LL 118 is a broader melt fracture window on conventional grooved-feed blown film lines and lower melt pressure at equivalent output. Compared with metallocene-catalyzed LLDPE of the same density and melt index, LL 118 has a broader molecular weight distribution and therefore better bubble stability on older lines, but lower tensile balance and lower clarity. The selection of LL 118 over a higher-alpha-olefin grade is therefore a trade between film toughness and extrudability on existing equipment.

    On a 65 mm single-screw extruder with 25:1 L/D, grooved feed section, barrier screw, and 80 mm annular die with 2.0 mm die gap, LL 118 at 150 kg/h typically develops a melt temperature of 205 °C to 220 °C and a die-head pressure of 300 bar to 380 bar. If the die gap is reduced to 1.0 mm, shear stress at the die lip can exceed the critical level for sharkskin melt fracture in butene LLDPE. Surface roughness appears as transverse ridges and is not corrected by raising melt temperature alone. Stable operation requires die-face temperature uniformity within ±2 °C across the circumference; deviations beyond this produce gauge bands in the slit film. Blow-up ratio is normally held between 2.0:1 and 3.0:1. Below 2.0:1, transverse orientation decreases; above 3.0:1, bubble breathing and instability increase, especially in films thinner than 25 µm. Frost line height is set between 250 mm and 400 mm for gauge ranges from 25 µm to 50 µm. A frost line above 500 mm produces low web tension and increases the risk of wrinkling in collapsed film. Melt temperatures below 185 °C can carry unmelted resin into the bubble, producing gel-like defects; melt temperatures above 230 °C accelerate thermo-oxidative degradation, visible as yellowing, gel formation, and loss of elongation at break.

    LL 118 is not hygroscopic under normal shielded storage, but at relative humidity above 60% surface moisture on pellets can enter the extruder with the feed stream and create microbubbles in the film. Pre-drying at 60 °C for 4 h may be applied when moisture-induced bubble instability appears. The resin is stabilized with a primary/secondary antioxidant package sufficient for storage and normal film extrusion below 230 °C, but not for sustained hot-fill or long-term ultraviolet exposure without additional additive masterbatch. Batch-to-batch melt flow rate variation is controlled within the producer’s normal specification window, but film converters running close to the melt fracture threshold should verify incoming lot melt flow rate and pellet surface lubricant levels before startup.

    When Downgauging Liner, Agricultural Mulch, and Freezer Film Requires Property Trade-offs

    LL 118 is used in refuse sacks, industrial liners, agricultural mulch, garment bags, and frozen food packaging. At 45 µm, monolayer liner film produced with 2.5:1 blow-up ratio and 2.0 mm die gap typically retains a dart impact above 95 g; at 25 µm representative values remain in the 100–120 g range under identical processing. For agricultural mulch, the resin is normally dry-blended with 3 wt% to 6 wt% carbon black masterbatch or a UV stabilizer masterbatch containing hindered amine light stabilizers and a phenolic antioxidant. The blend reduces photodegradation but may lower dart impact by 10% to 20% at equal gauge. In freezer overwrap service, film at -20 °C maintains ductile behavior, but puncture resistance is reduced relative to 23 °C. Published data for LL 118 film performance below -30 °C is limited; end-use testing under ISO 7765-2 is recommended before specifying a particular freezer structure.

    The grade is not supplied with slip and antiblock levels sufficient for very low-coefficient-of-friction packaging. Converters add synthetic silica or erucamide masterbatch at 0.5 wt% to 1.5 wt% for film separation and machinability. Erucamide addition lowers the coefficient of friction after migration but may increase haze. Migration kinetics in the polymer matrix depend on film crystallinity, orientation, and storage temperature; full surface effect is typically reached after 24 h to 72 h at 23 °C. Overaddition of slip masterbatch above the recommended dosage can produce plate-out on the collapsing frame and unwanted reduction in heat-seal strength.

    For tensile and seal performance, heat-seal initiation temperature in monolayer LL 118 film is approximately 110–120 °C on laboratory gradient sealers, but published data for the specific measurement condition is limited. The actual heat-seal window depends on film thickness, seal bar configuration, dwell time, and pressure. In side-weld carrier bag applications, the seal strength is typically controlled by fusion of the LLDPE phase and is less sensitive to contamination than LDPE-rich formulations. In refuse sacks, the combination of dart impact and Elmendorf tear provides resistance to puncture from irregular waste, but at gauge below 30 µm MD tear can become the limiting property because the machine-direction orientation generated by the bubble reduces crack-propagation resistance in that axis.

    Coextruded Structures With HDPE and LDPE Skins

    LL 118 is also used as a core layer in three-layer and five-layer blown film structures where high-density polyethylene skins provide modulus and linear low density polyethylene contributes puncture resistance. In a 50/60/50 mm three-layer blown film line producing 40 µm film with 20% HDPE in each skin and 60% LL 118 in the core, the secant modulus increases relative to 100% LL 118, but dart impact decreases nonlinearly. The reduction is larger when the HDPE skin fraction exceeds 30% of total thickness because the stiffer skins concentrate stress at the interface. Conversely, adding LL 118 as a core to LDPE skins improves dart impact and tear resistance compared with a 100% LDPE film at the same total gauge. Published data for this specific coextruded configuration is limited, and monolayer film properties cannot be used to predict coextruded film behavior without pilot-line confirmation.

    In heavy-duty sacks, LL 118 is dry-blended with HDPE to increase top-load and tear resistance. The blend morphology depends on melt temperature and screw mixing. At 210 °C melt temperature in a single-screw barrier screw with low dispersive mixing, the HDPE and LLPE phases remain largely separate; film haze increases and tear strength depends on island size. Use of a grooved feed and a Maddock mixing section improves dispersion. At HDPE addition above 20 wt%, the bubble becomes stiffer and frost line height must be reduced to avoid bubble instability. Film toughness in such blends is not a weighted average of the individual resin properties; the deviation from linearity should be confirmed for each film line.

    Regulatory compliance for LL 118 is documented under EU Regulation (EC) No 10/2011 for plastic food contact materials and under U.S. FDA 21 CFR 177.1520(c) for olefin polymers in contact with food. The resin is suitable for food contact only when the finished film meets the migration limits specified in Annex I and Annex II of the European regulation; the converter is responsible for end-use compliance. Under REACH Regulation (EC) No 1907/2006, the resin is registered for European market placement. Heavy metal content is controlled to meet the requirements of Directive 2011/65/EU as amended by (EU) 2015/863, Annex II. The pelletized resin is not classified as hazardous under the Globally Harmonized System of Classification and Labelling of Chemicals. No phthalates or bisphenol A are intentionally added. Lot-level test reports include melt flow rate, density, ash content, and selected film properties measured under ISO 527-3:2018, ISO 6383-2:1983, ISO 7765-1:1988, and ISO 14782:1999.

    Top